BZBo Zhao

Bo Zhao

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Bo Zhao has a total of 10 co-authors. Here are the top co-authors by number of shared publications:

  • Bingqing Cao

    Key Laboratory of Special Equipment Safety and Energy-saving for State Market Regulation, China Special Equipment Inspection & Research Institute, Beijing 100029, China

    1 shared publication
  • Bingxiao Shi

    Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China

    1 shared publication
  • Dong Jin

    Key Laboratory of Special Equipment Safety and Energy-saving for State Market Regulation, China Special Equipment Inspection & Research Institute, Beijing 100029, China

    1 shared publication
  • Fan Bai

    China Special Equipment Inspection and Research Institute, Beijing 100029, China

    1 shared publication
  • Hongchang Qian

    National Materials Corrosion and Protection Data Center, Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China

    1 shared publication
  • Jianhua Yang

    China Special Equipment Inspection and Research Institute, Beijing 100029, China

    1 shared publication

Latest Publications

  • Open Access

    Study the Effect of Heat Treatment on the Corrosion Resistance of AISI 347H Stainless Steel

    by Yunyan Peng, Bo Zhao, Jianhua Yang, Fan Bai, Hongchang Qian, Bingxiao Shi, Luntao Wang

    AISI 347H stainless steel is widely used in high-temperature environments due to its excellent creep strength and oxidation resistance; however, its corrosion performance remains highly sensitive to thermal oxidation, and the effects of thermal history on its passive film stability are not yet fully understood. This study addresses this knowledge gap by systematically investigating the influence of solution treatment on the corrosion and oxidation resistance of AISI 347H stainless steel. The specimens were subjected to solution heat treatment at 1050 °C, followed by air cooling, and then evaluated through electrochemical testing, high-temperature oxidation experiments at 550 °C, and multiscale surface characterization techniques. The solution treatment refined the austenitic microstructure by dissolving coarse Nb-rich precipitates, as confirmed by SEM and EBSD, and improved passive film integrity. The stabilizing effect of Nb also played a critical role in suppressing sensitization, thereby enhancing resistance to intergranular attack. Electrochemical measurements and EIS analysis revealed a lower corrosion current density and higher charge transfer resistance in the treated samples, indicating enhanced passivation behavior. ToF-SIMS depth profiling and oxide thickness analysis confirmed a slower parabolic oxide growth rate and reduced oxidation rate constant in the solution-treated condition. At 550 °C, oxidation was suppressed by the formation of compact, Cr-rich scales with dual-distributed Nb oxides, effectively limiting diffusion pathways and stabilizing the protective layer. These findings demonstrate that solution treatment is an effective strategy to improve the long-term corrosion and oxidation performance of AISI 347H stainless steel in harsh service environments.


  • Open Access

    Study on the Effect of Polyamine Water Treatment Agent on Metal Corrosion Inhibition in Boiler Steam–Water System

    by Zhijuan Zhao, Bingqing Cao, Bo Zhao, Sheng Chen, Dong Jin

    A polyamine water treatment agent was prepared with the film-forming amine (N-oleyl-1,3-propylenediamine) and the neutralizing amine (cyclohexanamine) under optimal conditions. The copper sulfate liquid drop experiment showed that a protective film was formed by the polyamine water treatment agent on carbon steel. The analyses of the polarization curve and electrochemical impedance spectroscopy of carbon steel indicated that the polyamine water treatment agent exhibited geometric effects, which could inhibit both anode and cathode reactions of carbon steel, and the corrosion inhibition effect of the polyamine water treatment agent showed an extreme-concentration phenomenon. A metal corrosion experiment in a simulated boiler steam–water system indicated that the polyamine water treatment agent mitigated the corrosion of carbon steel at different temperatures, and the corrosion inhibition rates of the polyamine water treatment agent in liquid and gas environments at 150 °C were 53.84% and 67.43%, respectively, better than that at 350 °C. SEM-EDS characterization indicated that the formation of the corrosion product, iron oxide, on the carbon steel was reduced with the addition of the polyamine water treatment agent in the simulated boiler steam–water system.