Anas Bariquddin Amali
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Anas Bariquddin Amali has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Agus Dwi Anggono
Mechanical Engineering Department, Universitas Muhammadiyah Surakarta (UMS), Jl. Ahmad Yani No. 157 Pabelan, Kartasura, Sukoharjo 57169, Jawa Tengah, Indonesia
1 shared publication - Agus Hariyanto
Mechanical Engineering, Universitas Muhammadiyah Surakarta, Jl. Ahmad Yani, Surakarta 57162, Indonesia
1 shared publication - Dessy Ade Pratiwi
Mechanical Engineering, Universitas Muhammadiyah Surakarta, Jl. Ahmad Yani, Surakarta 57162, Indonesia
1 shared publication - Ngafwan Ngafwan
Postgraduate Mechanichal Engineering, Advanced Materials and Structure Research Group, Universitas Muhammadiyah Surakarta, Surakarta 57169, Indonesia
1 shared publication - Sekar Melaty
Mechanical Engineering, Universitas Muhammadiyah Surakarta, Jl. Ahmad Yani, Surakarta 57162, Indonesia
1 shared publication - Supriyono Supriyono
Universitas Muhammadiyah Surakarta
1 shared publication
Latest Publications
- Open Access
- 28 February 2024
- Published by MDPI AG in Engineering Proceedings
- Vol. 63 (1) , 14
Effect of Volume Fraction of Epoxy Matrix Coconut Shell Composite on Tensile and Impact Loads
This research aims to determine the effect of the volume fraction of coconut shell composite, with an epoxy matrix at 10% coconut shell water content, on the composite’s tensile strength, impact, density, and fracture results with the macrostructure. The materials used to make this composite are coconut shell particles, with a diameter of 1mm at a water content of 10%, and epoxy matrix and hardener, in a ratio of 1:1. Variations in volume fraction are 10%, 20%, 30%, 40% and 50%. The composite was manufactured using a press mold. Composite testing was in accordance with ASTM standards for tensile testing, using ASTM D 638-02 and impact testing using ASTM D 256-00. Macro photo results that determine the type of fracture that occurred were taken of the fracture resulting from tensile and impact tests. The test results showed that the highest tensile strength was at a volume fraction of 40% of 21.59 MPa, and the lowest was at 10% of 7.15 MPa. The highest impact value was shown in a composite with a volume fraction of 50% of 0.074 J/mm2, and the lowest had a volume fraction of 10% of 0.010 J/mm2. The highest density was a composite with a volume fraction of 50% of 1.067 gr/cm3, and the lowest had a volume fraction of 10% of 1.014 gr/cm3. In observing the fracture after tensile and impact testing, it can be seen that the fracture was brittle, and the direction of crack propagation is perpendicular to the direction of the tensile stress that is acting to produce a relatively flat fracture surface.
- 28 February 2024
- Published by MDPI AG in Engineering Proceedings
- Vol. 63 (1) , 14
Open AccessEffect of Volume Fraction of Epoxy Matrix Coconut Shell Composite on Tensile and Impact Loads
This research aims to determine the effect of the volume fraction of coconut shell composite, with an epoxy matrix at 10% coconut shell water content, on the composite’s tensile strength, impact, density, and fracture results with the macrostructure. The materials used to make this composite are coconut shell particles, with a diameter of 1mm at a water content of 10%, and epoxy matrix and hardener, in a ratio of 1:1. Variations in volume fraction are 10%, 20%, 30%, 40% and 50%. The composite was manufactured using a press mold. Composite testing was in accordance with ASTM standards for tensile testing, using ASTM D 638-02 and impact testing using ASTM D 256-00. Macro photo results that determine the type of fracture that occurred were taken of the fracture resulting from tensile and impact tests. The test results showed that the highest tensile strength was at a volume fraction of 40% of 21.59 MPa, and the lowest was at 10% of 7.15 MPa. The highest impact value was shown in a composite with a volume fraction of 50% of 0.074 J/mm2, and the lowest had a volume fraction of 10% of 0.010 J/mm2. The highest density was a composite with a volume fraction of 50% of 1.067 gr/cm3, and the lowest had a volume fraction of 10% of 1.014 gr/cm3. In observing the fracture after tensile and impact testing, it can be seen that the fracture was brittle, and the direction of crack propagation is perpendicular to the direction of the tensile stress that is acting to produce a relatively flat fracture surface.