Niklas Trogisch
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Niklas Trogisch has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
Albert Albert
BMW Group, D-80788 Munich, Germany
4 shared publicationsRüdiger-A. Eichel
Institute of Physical Chemistry, RWTH Aachen University, D-52074 Aachen, Germany
3 shared publications- Alexandra Hartig-Weiss
Chemistry, Technical University of Munich, Lichtenbergstrasse 4, Garching, Bayern, 85748, GERMANY
1 shared publication - Alin Orfanidi
BMW Group, D-80788 Munich, Germany
1 shared publication Danilo Babik
BMW Group, D-80788 Munich, Germany
1 shared publicationFengmin Du
BMW Group, D-80788 Munich, Germany
1 shared publication
Latest Publications
- 1 July 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (7) , 074501
Modelling the Chemical Degradation of PFSA Membranes in Proton Exchange Membrane Fuel Cells – Effect of Low Relative Humidity on the Degradation of the Sulfonic Acid Group
The chemical membrane degradation of automotive proton exchange membrane (PEM) fuel cells gains significant importance due to the increased stress caused by high temperature and low relative humidity (RH) operation required to reduce humidification and cooling system complexity. While several models have been introduced describing the ether cleavage and main chain unzipping mechanisms, the degradation of the sulfonic group has not been modeled yet. This is critical, because at low RH, the degradation of the sulfonic acid group, followed by the unzipping along the backbone, is expected to be the dominant chemical degradation mechanism. In this study, the acid-base equilibrium of the sulfonic acid groups was solved as a function of the membrane water content to derive the number of reactive, hydrated sulfonic acid groups and to calculate the reaction rate of the initial radical attack. The simulation was combined with a Fenton model and a coarse grain approach to derive the fluoride emission rate as a function of RH. It was found that the hydration ratio of the sulfonic acid group changes by six orders of magnitude between 25% and 95% RH, leading to an almost two orders of magnitude higher degradation rate at dry conditions.
- 1 July 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (7) , 074501
Modelling the Chemical Degradation of PFSA Membranes in Proton Exchange Membrane Fuel Cells – Effect of Low Relative Humidity on the Degradation of the Sulfonic Acid Group
The chemical membrane degradation of automotive proton exchange membrane (PEM) fuel cells gains significant importance due to the increased stress caused by high temperature and low relative humidity (RH) operation required to reduce humidification and cooling system complexity. While several models have been introduced describing the ether cleavage and main chain unzipping mechanisms, the degradation of the sulfonic group has not been modeled yet. This is critical, because at low RH, the degradation of the sulfonic acid group, followed by the unzipping along the backbone, is expected to be the dominant chemical degradation mechanism. In this study, the acid-base equilibrium of the sulfonic acid groups was solved as a function of the membrane water content to derive the number of reactive, hydrated sulfonic acid groups and to calculate the reaction rate of the initial radical attack. The simulation was combined with a Fenton model and a coarse grain approach to derive the fluoride emission rate as a function of RH. It was found that the hydration ratio of the sulfonic acid group changes by six orders of magnitude between 25% and 95% RH, leading to an almost two orders of magnitude higher degradation rate at dry conditions.
- 29 May 2025
- Published by Elsevier in Journal of Power Sources
- Vol. 649
Degradation of automotive PEM fuel cells under accelerated stress tests – The effect of high operating temperature
- 29 May 2025
- Published by Elsevier in Journal of Power Sources
- Vol. 649
Degradation of automotive PEM fuel cells under accelerated stress tests – The effect of high operating temperature
- 14 May 2025
- Published by Elsevier in Journal of Power Sources
- Vol. 647
Temporary high temperature operation of an automotive PEM fuel cell: Analysis of local degradation mechanisms
- 14 May 2025
- Published by Elsevier in Journal of Power Sources
- Vol. 647
Temporary high temperature operation of an automotive PEM fuel cell: Analysis of local degradation mechanisms
- 1 October 2024
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 171 (10) , 104506
Effect of High-Temperature Operation on Voltage Cycling Induced PEMFC Degradation: From Automotive Customer Drive Cycles to an Accelerated Stress Test
Degradation of the Pt catalyst during load cycling constitutes a major durability issue for proton exchange membrane fuel cells (PEMFCs) in automotive applications. In this study commercial 5 cm2 electrodes were exposed to 20 k voltage cycles between 0.6–0.9 VRHE at temperatures ranging from 75 to 120 °C. The electrochemical surface area (ECSA), the roughness factor (rf), and the oxygen transport resistance were investigated over the course of the test. The degradation was mainly governed by Pt agglomeration and was accelerated with increasing temperature. Interestingly, operation at high temperature (120 °C and 30% RH) caused the same ECSA loss as at standard conditions (90 °C and 90% RH), suggesting that when maintaining dry conditions high-temperature operation is not critical for the durability of the catalyst material. The experimental results were used to validate an existing 0D catalyst degradation model, which was then applied to an automotive customer drive cycle. The calculated degradation over the whole automotive lifetime (excluding startup shutdown and idle events) equals 20 k voltage cycles (0.6–0.9 V, 10 s hold time) at 90 °C and 30% RH, which provides a guideline for the assessment of the suitability of novel catalyst materials for automotive applications.
- 1 October 2024
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 171 (10) , 104506
Effect of High-Temperature Operation on Voltage Cycling Induced PEMFC Degradation: From Automotive Customer Drive Cycles to an Accelerated Stress Test
Degradation of the Pt catalyst during load cycling constitutes a major durability issue for proton exchange membrane fuel cells (PEMFCs) in automotive applications. In this study commercial 5 cm2 electrodes were exposed to 20 k voltage cycles between 0.6–0.9 VRHE at temperatures ranging from 75 to 120 °C. The electrochemical surface area (ECSA), the roughness factor (rf), and the oxygen transport resistance were investigated over the course of the test. The degradation was mainly governed by Pt agglomeration and was accelerated with increasing temperature. Interestingly, operation at high temperature (120 °C and 30% RH) caused the same ECSA loss as at standard conditions (90 °C and 90% RH), suggesting that when maintaining dry conditions high-temperature operation is not critical for the durability of the catalyst material. The experimental results were used to validate an existing 0D catalyst degradation model, which was then applied to an automotive customer drive cycle. The calculated degradation over the whole automotive lifetime (excluding startup shutdown and idle events) equals 20 k voltage cycles (0.6–0.9 V, 10 s hold time) at 90 °C and 30% RH, which provides a guideline for the assessment of the suitability of novel catalyst materials for automotive applications.
- 28 February 2024
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 171 (3) , 036506
Limitations of Liquid Electrolyte RDE Experiments for the Determination of OER Catalyst Activity: The Effect of the Catalyst Layer Thickness
Developing novel oxygen evolution reaction (OER) noble metal catalysts with a low metal packing density is key for the wider large-scale implementation of polymer electrolyte membrane water electrolysis (PEMWE). OER activities of these new catalysts are commonly measured in liquid electrolytes using half-cell configurations, such as rotating-ring-disk electrodes (RDE). Recent studies in liquid electrolyte cells showed that the accumulation of microscopic oxygen bubbles within the OER catalyst layer causes shielding of active catalyst sites. In this study, three different OER catalysts were screened for their activity at different loadings in a liquid electrolyte RDE setup. Potential sweeps using bare Ir black, a commercially available IrO2/TiO2 and a homemade Ir/ATO (antimony doped tin oxide) catalyst with different loadings were performed. It was demonstrated that the mass activity of the Ir/ATO catalyst decreases by more than 50% with a catalyst loading increase, which is attributed to the accumulation of microscopic oxygen bubbles within the catalyst layer and was correlated to the coating thickness of the catalyst layer. We suggest screening the OER catalyst activity of low packing catalyst materials in a loading analysis by testing minimum three different loadings within the kinetic Tafel slope region to avoid underestimation of the catalyst activity.
- 28 February 2024
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 171 (3) , 036506
Limitations of Liquid Electrolyte RDE Experiments for the Determination of OER Catalyst Activity: The Effect of the Catalyst Layer Thickness
Developing novel oxygen evolution reaction (OER) noble metal catalysts with a low metal packing density is key for the wider large-scale implementation of polymer electrolyte membrane water electrolysis (PEMWE). OER activities of these new catalysts are commonly measured in liquid electrolytes using half-cell configurations, such as rotating-ring-disk electrodes (RDE). Recent studies in liquid electrolyte cells showed that the accumulation of microscopic oxygen bubbles within the OER catalyst layer causes shielding of active catalyst sites. In this study, three different OER catalysts were screened for their activity at different loadings in a liquid electrolyte RDE setup. Potential sweeps using bare Ir black, a commercially available IrO2/TiO2 and a homemade Ir/ATO (antimony doped tin oxide) catalyst with different loadings were performed. It was demonstrated that the mass activity of the Ir/ATO catalyst decreases by more than 50% with a catalyst loading increase, which is attributed to the accumulation of microscopic oxygen bubbles within the catalyst layer and was correlated to the coating thickness of the catalyst layer. We suggest screening the OER catalyst activity of low packing catalyst materials in a loading analysis by testing minimum three different loadings within the kinetic Tafel slope region to avoid underestimation of the catalyst activity.