L. Yu. Mezhevaia
Research Subjects
L. Yu. Mezhevaia has a total of 21 co-authors. Here are the top co-authors by number of shared publications:
- Vitaliy V. Sanin
JSC “Giredmet” named after N.P. Sazhin
2 shared publications Л. Ю. Межевая
АО «Гиредмет» им. Н.П. Сажина
2 shared publications- Almaz Yunirovich Nazarov
Ufa University of Science and Technology
1 shared publication - Elizaveta Sergeevna Koshel
JSC «Giredmet» n.a. N.P. Sazhin
1 shared publication - Iuliia Mikhailovna Modina
Ufa University of Science and Technology
1 shared publication K. N. Ramazanov
Ufa University of Science and Technology
1 shared publication
Latest Publications
- Open Access
- 4 October 2026
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- Vol. 32 (3) , 51-61
A combined method for producing defect-free ingots of the high-entropy alloy TiZrAlVCr and their use as cathode targets for coating deposition
This article presents the results of producing a high-entropy alloy of the Ti–Zr–Al–V–Cr system, intended for practical use as cathode targets in NNV-6.6 vacuum arc systems, using a combined method of melting and remelting. It is shown that direct remelting of the components by vacuum arc melting (VAM) in a copper mould leads to cracking of ingots due to high thermal stresses (cooling rate of 10 2 –10 3 °C/s), while switching off cooling causes copper contamination. To solve the problem, a combined method is proposed: preliminary melting of the components by VAM, followed by vacuum induction remelting (VIM) and casting into a mold. A special ceramic lining based on oxides containing up to 2 wt. % rare-earth metal oxides was used, ensuring minimal impurity contamination. The optimal crystallization parameters were selected: reduction of the cooling rate to 5–10 °C/s, use of a copper base plate for directional heat extraction and a feeder head to compensate for shrinkage effects. Scanning electron microscopy and energy-dispersive X -ray spectroscopy confirmed the chemical homogeneity of the resulting ingots (the contents of Ti, Zr, Al, V, and Cr were 16–27 at. %). The microhardness of the alloy was 768–789 HV with high reproducibility across batches. The cathode targets were successfully tested in the NNV-6.6-I1 installation: single-layer and two types of multilayer coatings were deposited on substrates made of Ti–6Al–4V titanium alloy. The developed technology ensures the production of defect-free ingots of a specified geometry (\(\emptyset \)80–85 mm, h = 45 mm), suitable for industrial use in vacuum arc deposition processes for protective coatings.- 4 October 2026
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- Vol. 32 (3) , 51-61
Open AccessA combined method for producing defect-free ingots of the high-entropy alloy TiZrAlVCr and their use as cathode targets for coating deposition
This article presents the results of producing a high-entropy alloy of the Ti–Zr–Al–V–Cr system, intended for practical use as cathode targets in NNV-6.6 vacuum arc systems, using a combined method of melting and remelting. It is shown that direct remelting of the components by vacuum arc melting (VAM) in a copper mould leads to cracking of ingots due to high thermal stresses (cooling rate of 10 2 –10 3 °C/s), while switching off cooling causes copper contamination. To solve the problem, a combined method is proposed: preliminary melting of the components by VAM, followed by vacuum induction remelting (VIM) and casting into a mold. A special ceramic lining based on oxides containing up to 2 wt. % rare-earth metal oxides was used, ensuring minimal impurity contamination. The optimal crystallization parameters were selected: reduction of the cooling rate to 5–10 °C/s, use of a copper base plate for directional heat extraction and a feeder head to compensate for shrinkage effects. Scanning electron microscopy and energy-dispersive X -ray spectroscopy confirmed the chemical homogeneity of the resulting ingots (the contents of Ti, Zr, Al, V, and Cr were 16–27 at. %). The microhardness of the alloy was 768–789 HV with high reproducibility across batches. The cathode targets were successfully tested in the NNV-6.6-I1 installation: single-layer and two types of multilayer coatings were deposited on substrates made of Ti–6Al–4V titanium alloy. The developed technology ensures the production of defect-free ingots of a specified geometry (\(\emptyset \)80–85 mm, h = 45 mm), suitable for industrial use in vacuum arc deposition processes for protective coatings. - Open Access
- 28 March 2024
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 1,p. 24-41
Structural characteristics and properties of heat-resistant nickel β-alloys produced via the centrifugal SHS-casting method
Employing centrifugal self-propagating high-temperature synthesis (SHS) metallurgy, complemented by advanced metallurgical processes such as vacuum induction melting (VIM) and vacuum arc remelting (VAR), yielded the alloy formulation denoted as base–2.5Mo–1.5Re–1.5Ta–0.2Ti. This study investigates the effects of various technological modes and additional metallurgical treatments on the alloy's impurity and non-metallic inclusion content, structural characteristics, mechanical behavior under compression, and its oxidation mechanisms and kinetics when exposed to temperatures of 1150 °C for 30 h. With increasing centrifugal acceleration, the proportion of non-metallic inclusions (number of points) drops from 5 to 1–2 points. The best combination mechanical properties, including σucs = 1640 ± 20 MPa, σys = 1518 ± 10 MPa, and residual deformation were observed in alloys processed under conditions of increased gravitational force (g = 50). Within a centrifugal force range of g = 20÷300, the composition of the synthesis products aligned with the theoretical expectations. The total content of impurities is 0.15 ± 0.02 %, with a decrease in gas impurities–oxygen and nitrogen levels reduced to 0.018 % and 0.0011 %, respectively. The structural analysis of the alloys revealed the presence of globular and streaked inclusions of a chromium-based solid solution embedded within the matrix. Inclusions with thickness of 2–8 μm are present in the intergranular space: (Cr)Ni,Mo,Co, (Cr)Mo,Re and (Cr)Re,Mo. The formation of the Ni(Al,Ti) phase at grain boundaries was identified, contributing to an enhancement in plastic resistance and overall strength of the alloy. Oxidation mechanisms varied across different processing modes, with the size of structural components significantly influencing oxidation kinetics. The weight gain observed in SHS samples was 70 ± 10 g/m2 with oxidation predominantly occurring along the NiAl interphase boundaries and penetrating into the depth of the sample. TEM facilitated the identification of phases enriched with Ti microadditions, reducing the levels of dissolved nitrogen and oxygen within the intermetallic phase to a combined weight percentage (ΣO,N) of 0.0223 wt.%.
- 28 March 2024
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 1,p. 24-41
Open AccessStructural characteristics and properties of heat-resistant nickel β-alloys produced via the centrifugal SHS-casting method
Employing centrifugal self-propagating high-temperature synthesis (SHS) metallurgy, complemented by advanced metallurgical processes such as vacuum induction melting (VIM) and vacuum arc remelting (VAR), yielded the alloy formulation denoted as base–2.5Mo–1.5Re–1.5Ta–0.2Ti. This study investigates the effects of various technological modes and additional metallurgical treatments on the alloy's impurity and non-metallic inclusion content, structural characteristics, mechanical behavior under compression, and its oxidation mechanisms and kinetics when exposed to temperatures of 1150 °C for 30 h. With increasing centrifugal acceleration, the proportion of non-metallic inclusions (number of points) drops from 5 to 1–2 points. The best combination mechanical properties, including σucs = 1640 ± 20 MPa, σys = 1518 ± 10 MPa, and residual deformation were observed in alloys processed under conditions of increased gravitational force (g = 50). Within a centrifugal force range of g = 20÷300, the composition of the synthesis products aligned with the theoretical expectations. The total content of impurities is 0.15 ± 0.02 %, with a decrease in gas impurities–oxygen and nitrogen levels reduced to 0.018 % and 0.0011 %, respectively. The structural analysis of the alloys revealed the presence of globular and streaked inclusions of a chromium-based solid solution embedded within the matrix. Inclusions with thickness of 2–8 μm are present in the intergranular space: (Cr)Ni,Mo,Co, (Cr)Mo,Re and (Cr)Re,Mo. The formation of the Ni(Al,Ti) phase at grain boundaries was identified, contributing to an enhancement in plastic resistance and overall strength of the alloy. Oxidation mechanisms varied across different processing modes, with the size of structural components significantly influencing oxidation kinetics. The weight gain observed in SHS samples was 70 ± 10 g/m2 with oxidation predominantly occurring along the NiAl interphase boundaries and penetrating into the depth of the sample. TEM facilitated the identification of phases enriched with Ti microadditions, reducing the levels of dissolved nitrogen and oxygen within the intermetallic phase to a combined weight percentage (ΣO,N) of 0.0223 wt.%.