Wenbo Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Wenbo Liu has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Aoke Jiang
School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China
1 shared publication - Boyuan Zhou
School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China
1 shared publication - Hongqun Tang
School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China
1 shared publication - Shaoxuan Wu
School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China
1 shared publication - Sheng Li
School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China
1 shared publication - Xiaoying Zhang
School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China
1 shared publication
Latest Publications
- Open Access
Pre-Deformation-Assisted Retrogression and Re-Aging Treatment for Achieving Strength–Corrosion Synergy in 2195 Al–Cu–Li Alloy: Insights into Cu Redistribution and Grain Boundary Evolution
Al–Cu–Li alloys face an intrinsic trade-off between precipitation strengthening and intergranular corrosion susceptibility. This trade-off restricts the simultaneous improvement of their strength and corrosion resistance. In this work, a pre-deformation-assisted retrogression and re-aging (RRA) strategy was developed to regulate Cu redistribution and balance the mechanical and corrosion properties of 2195 Al–Cu–Li alloy. The results show that short-time retrogression maintains effective strengthening while limiting Cu depletion near grain boundaries, thereby achieving an improved strength–corrosion balance under the investigated processing conditions. The RRA-5 min sample exhibited the optimum performance, with a yield strength of 533 MPa, ultimate tensile strength of 562.6 MPa, and polarization resistance of 19,605 Ω·cm2. Prolonged retrogression promoted Cu redistribution toward grain boundaries, potentially promoting precipitate-free zone (PFZ) evolution, electrochemical heterogeneity, and intergranular corrosion susceptibility. XPS analysis revealed that the corrosion film consisted mainly of Al oxides and hydroxides, Li- and Mg-containing compounds, and Cu-enriched species, suggesting selective dissolution and corrosion film reconstruction during exposure. The coupled Cu diffusion–grain boundary absorption model predicted the evolution tendency of PFZ widening with increasing retrogression time, which was consistent with the experimental trend. This study provides insights into the regulation of Cu redistribution through RRA processing for achieving strength–corrosion synergy in aerospace Al–Cu–Li alloys under the present processing conditions.
Open AccessPre-Deformation-Assisted Retrogression and Re-Aging Treatment for Achieving Strength–Corrosion Synergy in 2195 Al–Cu–Li Alloy: Insights into Cu Redistribution and Grain Boundary Evolution
Al–Cu–Li alloys face an intrinsic trade-off between precipitation strengthening and intergranular corrosion susceptibility. This trade-off restricts the simultaneous improvement of their strength and corrosion resistance. In this work, a pre-deformation-assisted retrogression and re-aging (RRA) strategy was developed to regulate Cu redistribution and balance the mechanical and corrosion properties of 2195 Al–Cu–Li alloy. The results show that short-time retrogression maintains effective strengthening while limiting Cu depletion near grain boundaries, thereby achieving an improved strength–corrosion balance under the investigated processing conditions. The RRA-5 min sample exhibited the optimum performance, with a yield strength of 533 MPa, ultimate tensile strength of 562.6 MPa, and polarization resistance of 19,605 Ω·cm2. Prolonged retrogression promoted Cu redistribution toward grain boundaries, potentially promoting precipitate-free zone (PFZ) evolution, electrochemical heterogeneity, and intergranular corrosion susceptibility. XPS analysis revealed that the corrosion film consisted mainly of Al oxides and hydroxides, Li- and Mg-containing compounds, and Cu-enriched species, suggesting selective dissolution and corrosion film reconstruction during exposure. The coupled Cu diffusion–grain boundary absorption model predicted the evolution tendency of PFZ widening with increasing retrogression time, which was consistent with the experimental trend. This study provides insights into the regulation of Cu redistribution through RRA processing for achieving strength–corrosion synergy in aerospace Al–Cu–Li alloys under the present processing conditions.
- Open Access
Towards Understanding Formation Mechanism of Cellular Structures in Laser Powder Bed Fused AlSi10Mg
A new approach is proposed that identifies three different zones of the Si-rich network structure (the cellular structure) in laser powder bed fused (LPBF) AlSi10Mg alloy, based on the variation in morphology, grain growth transition, and melt pool solidification conditions. The three identified zones are denoted in the present work as the liquid solidification zone (LSZ), the mushy solidification zone (MSZ), and the heat affected zone (HAZ). The LSZ is the result of liquid–solid transformation, showing small planar growth at the boundary and large cellular growth in the center, while the MSZ is related to a semisolid reaction, and the HAZ arises from a short-time aging process. The boundary between the LSZ and MSZ is identified by the change of grain growth direction and the Si-rich network advancing direction. The boundary between MSZ and HAZ is identified by the start of the breakdown of the Si-rich network. In addition, it is found that the fracture is generated in and propagates along the HAZ during tensile tests.
Open AccessTowards Understanding Formation Mechanism of Cellular Structures in Laser Powder Bed Fused AlSi10Mg
A new approach is proposed that identifies three different zones of the Si-rich network structure (the cellular structure) in laser powder bed fused (LPBF) AlSi10Mg alloy, based on the variation in morphology, grain growth transition, and melt pool solidification conditions. The three identified zones are denoted in the present work as the liquid solidification zone (LSZ), the mushy solidification zone (MSZ), and the heat affected zone (HAZ). The LSZ is the result of liquid–solid transformation, showing small planar growth at the boundary and large cellular growth in the center, while the MSZ is related to a semisolid reaction, and the HAZ arises from a short-time aging process. The boundary between the LSZ and MSZ is identified by the change of grain growth direction and the Si-rich network advancing direction. The boundary between MSZ and HAZ is identified by the start of the breakdown of the Si-rich network. In addition, it is found that the fracture is generated in and propagates along the HAZ during tensile tests.