Guilleromo Godoy‐Pérez
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Guilleromo Godoy‐Pérez has a total of 37 co-authors. Here are the top co-authors by number of shared publications:
- Alvaro del Prado
Departamento de Estructura de la Materia, Física Térmica y Electrónica. Facultad de Ciencias Físicas. Universidad Complutense de Madrid
3 shared publications - Daniel Caudevilla
Universidad Complutense de Madrid, Spain,Fsica Trmica y Electrnica,Dpto. Estructura de la Matera,Madrid,Spain
3 shared publications - David Pastor
Departamento de Estructura de la Materia, Física Térmica y Electrónica, Universidad Complutense de Madrid 1 , Fac. de CC. Físicas. Plaza de las Ciencias 1, E-28040 Madrid
3 shared publications - Enrique San Andres
Departamento de Estructura de la Materia, Física Térmica y Electrónica. Facultad de Ciencias Físicas. Universidad Complutense de Madrid
3 shared publications - Eric García Hemme
Departamento de Estructura de la Materia, Física Térmica y Electrónica. Facultad de Ciencias Físicas. Universidad Complutense de Madrid
3 shared publications - Francisco Pérez-Zenteno
Departamento de Estructura de la Materia, Física Térmica y Electrónica. Facultad de Ciencias Físicas. Universidad Complutense de Madrid
3 shared publications
Latest Publications
- Open Access
- 12 August 2026
- Published by Elsevier in Materials Science in Semiconductor Processing
- Vol. 216
High-efficiency phosphorus activation in Ge0.95Sn0.05 enabled by ion implantation and flash lamp annealing with preserved alloy integrity
- 12 August 2026
- Published by Elsevier in Materials Science in Semiconductor Processing
- Vol. 216
Open AccessHigh-efficiency phosphorus activation in Ge0.95Sn0.05 enabled by ion implantation and flash lamp annealing with preserved alloy integrity
- Open Access
- 4 July 2026
- Published by Elsevier in SSRN Electronic Journal
High-efficiency phosphorus activation in Ge0.95Sn0.05 enabled by ion implantation and flash lamp annealing with preserved alloy integrity
Heavy n-type doping is essential for GeSn-based optoelectronic and plasmonic devices, yet remains challenging due to the low thermal stability of GeSn alloys and the resulting dopant deactivation, strain relaxation, and Sn redistribution during post-growth processing. Here, we investigate phosphorus ion implantation combined with millisecond flash lamp annealing (FLA) as a non-equilibrium doping approach for Ge0.95Sn0.05 layers grown on Ge virtual substrates. Compared with previous ex-situ doping studies, the implantation process was redesigned using reduced implantation fluences, room-temperature implantation, an amorphous Si capping layer, and FLA without substrate preheating to improve dopant activation and minimize implantation-induced damage. Raman spectroscopy identifies a narrow recrystallization window between 71 and 84 J/cm2, while Rutherford backscattering spectrometry demonstrates nearly complete recovery of the crystalline quality after annealing, with a Sn lattice-site occupancy exceeding 95%. No measurable Sn redistribution is observed after implantation and annealing within the sensitivity limits of Rutherford backscattering spectrometry and X-ray diffraction. Hall-effect measurements reveal active electron concentrations of up to 5.0 × 10^19 cm-3 and electron mobilities of around 200 cm2 V-1 s-1. These results represent a 10% improvement in maximum carrier concentration and a ninefold increase in dopant activation efficiency compared to previously reported ex-situ doping approaches, reaching approximately 54%. These results establish an optimized processing route for highly activated n-type GeSn that suppresses Sn redistribution.
- 4 July 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessHigh-efficiency phosphorus activation in Ge0.95Sn0.05 enabled by ion implantation and flash lamp annealing with preserved alloy integrity
Heavy n-type doping is essential for GeSn-based optoelectronic and plasmonic devices, yet remains challenging due to the low thermal stability of GeSn alloys and the resulting dopant deactivation, strain relaxation, and Sn redistribution during post-growth processing. Here, we investigate phosphorus ion implantation combined with millisecond flash lamp annealing (FLA) as a non-equilibrium doping approach for Ge0.95Sn0.05 layers grown on Ge virtual substrates. Compared with previous ex-situ doping studies, the implantation process was redesigned using reduced implantation fluences, room-temperature implantation, an amorphous Si capping layer, and FLA without substrate preheating to improve dopant activation and minimize implantation-induced damage. Raman spectroscopy identifies a narrow recrystallization window between 71 and 84 J/cm2, while Rutherford backscattering spectrometry demonstrates nearly complete recovery of the crystalline quality after annealing, with a Sn lattice-site occupancy exceeding 95%. No measurable Sn redistribution is observed after implantation and annealing within the sensitivity limits of Rutherford backscattering spectrometry and X-ray diffraction. Hall-effect measurements reveal active electron concentrations of up to 5.0 × 10^19 cm-3 and electron mobilities of around 200 cm2 V-1 s-1. These results represent a 10% improvement in maximum carrier concentration and a ninefold increase in dopant activation efficiency compared to previously reported ex-situ doping approaches, reaching approximately 54%. These results establish an optimized processing route for highly activated n-type GeSn that suppresses Sn redistribution.
- Open Access
- 17 March 2026
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 139 (11)
Effect of soft annealing on optoelectronic performances of Ti-hyperdoped Si photodiodes
We investigate the impact of soft furnace annealing (250–450 °C) on the optoelectronic performance of Ti-hyperdoped Si photodiodes. The annealing step, introduced between Ti ion implantation and nanosecond pulsed laser melting (ns-PLM), was designed to improve the crystalline quality of the seed layer from which ns-PLM recrystallizes the implanted region. For Ti doses of 1 × 1015 and 2 × 1015 cm−2, soft annealing enhanced the minority carrier lifetime and reduced the diffusion saturation current, leading to improved external quantum efficiency (EQE) above the Si absorption edge (photon energies higher than 1.12 eV). At higher implantation doses, however, these improvements were less pronounced, suggesting a dose-dependent interplay between defect passivation and recrystallization dynamics. However, EQE in the sub-bandgap range slightly decreased after annealing for both dose levels, while high-dose samples consistently exhibited stronger photoresponse, indicating that process-induced defects may contribute beneficially to sub-bandgap absorption in Ti-hyperdoped Si. These findings highlight soft annealing as a practical means of tailoring carrier dynamics and optical response in Ti-hyperdoped Si. By balancing defect passivation and controlled defect retention, this approach opens new opportunities for optimizing Ti-hyperdoped Si photodiodes toward applications in broadband light detection, short-wave infrared sensing, and CMOS-compatible optoelectronics.
- 17 March 2026
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 139 (11)
Open AccessEffect of soft annealing on optoelectronic performances of Ti-hyperdoped Si photodiodes
We investigate the impact of soft furnace annealing (250–450 °C) on the optoelectronic performance of Ti-hyperdoped Si photodiodes. The annealing step, introduced between Ti ion implantation and nanosecond pulsed laser melting (ns-PLM), was designed to improve the crystalline quality of the seed layer from which ns-PLM recrystallizes the implanted region. For Ti doses of 1 × 1015 and 2 × 1015 cm−2, soft annealing enhanced the minority carrier lifetime and reduced the diffusion saturation current, leading to improved external quantum efficiency (EQE) above the Si absorption edge (photon energies higher than 1.12 eV). At higher implantation doses, however, these improvements were less pronounced, suggesting a dose-dependent interplay between defect passivation and recrystallization dynamics. However, EQE in the sub-bandgap range slightly decreased after annealing for both dose levels, while high-dose samples consistently exhibited stronger photoresponse, indicating that process-induced defects may contribute beneficially to sub-bandgap absorption in Ti-hyperdoped Si. These findings highlight soft annealing as a practical means of tailoring carrier dynamics and optical response in Ti-hyperdoped Si. By balancing defect passivation and controlled defect retention, this approach opens new opportunities for optimizing Ti-hyperdoped Si photodiodes toward applications in broadband light detection, short-wave infrared sensing, and CMOS-compatible optoelectronics.
- Open Access
- 14 January 2025
- Published by Springer Nature in Research Square
A high-performance all-silicon photodetector enabling telecom-wavelength detection at room temperature
Photonic integrated circuits (PICs) are crucial for advancing optical communications, promising substantial gains in data transmission speed, bandwidth, and energy efficiency compared to conventional electronics 1 . Telecom-wavelength photodetectors, operating near 1550 nm, are indispensable in PICs, where they enable the sensitive and low-noise conversion of optical signals to electrical signals for efficient data processing. While silicon is ideal for passive optical components, its limited absorption in the optical telecommunication range (1260–1625 nm) typically necessitates integrating an alternative material, such as germanium 2 , for photodetection — a process that introduces significant fabrication challenges 3 . Here, we present a high-performance, all-silicon photodetector, grating- and waveguide-coupled, which operates at room temperature within the optical telecom C band. By introducing deep-level impurities into silicon at concentrations close to the solid-solubility limit, we enable efficient sub-bandgap absorption without compromising recombination carrier lifetimes and mobilities. This detector achieves a responsivity of 0.56 A/W, a quantum efficiency of 44.8%, a bandwidth of 5.9 GHz, and a noise-equivalent power of 4.2×10 − 10 W/Hz¹ / ² at 1550 nm, fulfilling requirements for telecom applications. Our approach provides a scalable and cost-effective solution for the monolithic integration of telecom-wavelength photodetectors into silicon-based PICs, advancing the development of compact photonic systems for modern communication infrastructures.
- 14 January 2025
- Published by Springer Nature in Research Square
Open AccessA high-performance all-silicon photodetector enabling telecom-wavelength detection at room temperature
Photonic integrated circuits (PICs) are crucial for advancing optical communications, promising substantial gains in data transmission speed, bandwidth, and energy efficiency compared to conventional electronics 1 . Telecom-wavelength photodetectors, operating near 1550 nm, are indispensable in PICs, where they enable the sensitive and low-noise conversion of optical signals to electrical signals for efficient data processing. While silicon is ideal for passive optical components, its limited absorption in the optical telecommunication range (1260–1625 nm) typically necessitates integrating an alternative material, such as germanium 2 , for photodetection — a process that introduces significant fabrication challenges 3 . Here, we present a high-performance, all-silicon photodetector, grating- and waveguide-coupled, which operates at room temperature within the optical telecom C band. By introducing deep-level impurities into silicon at concentrations close to the solid-solubility limit, we enable efficient sub-bandgap absorption without compromising recombination carrier lifetimes and mobilities. This detector achieves a responsivity of 0.56 A/W, a quantum efficiency of 44.8%, a bandwidth of 5.9 GHz, and a noise-equivalent power of 4.2×10 − 10 W/Hz¹ / ² at 1550 nm, fulfilling requirements for telecom applications. Our approach provides a scalable and cost-effective solution for the monolithic integration of telecom-wavelength photodetectors into silicon-based PICs, advancing the development of compact photonic systems for modern communication infrastructures.
- Open Access
- 8 July 2024
- Published by Wiley in Physica Status Solidi (a)
- Vol. 221 (24)
Native Oxide Layer Role during Cryogenic‐Temperature Ion Implantations in Germanium
Herein, the structural properties and chemical composition of Ge samples implanted with tellurium at cryogenic temperatures are analyzed, focusing on the role of the native oxide. For germanium, cryogenic‐temperature implantation is a requirement to achieve hyperdoped impurity concentrations while simultaneously preventing surface porosity. In this work, the critical role of the thin native germanium oxide is demonstrated when performing ion implantations at temperatures close to the liquid nitrogen temperature. The structural and chemical composition of tellurium‐implanted samples as a function of the implanted dose from 5 × 1014 to 5 × 1015 cm−2 is analyzed. After a laser melting process, the incorporated oxygen is diffused to the surface forming again a GeOx layer which retains a large fraction of the total implanted dose. These detrimental effects can be eliminated by a selective etching of the native oxide layer prior to the ion implantation process. These effects have been also observed when implanting on Si substrates. This work identifies key aspects for conducting implantations at cryogenic temperatures, that are otherwise negligible for ion implanting at room temperature.
- 8 July 2024
- Published by Wiley in Physica Status Solidi (a)
- Vol. 221 (24)
Open AccessNative Oxide Layer Role during Cryogenic‐Temperature Ion Implantations in Germanium
Herein, the structural properties and chemical composition of Ge samples implanted with tellurium at cryogenic temperatures are analyzed, focusing on the role of the native oxide. For germanium, cryogenic‐temperature implantation is a requirement to achieve hyperdoped impurity concentrations while simultaneously preventing surface porosity. In this work, the critical role of the thin native germanium oxide is demonstrated when performing ion implantations at temperatures close to the liquid nitrogen temperature. The structural and chemical composition of tellurium‐implanted samples as a function of the implanted dose from 5 × 1014 to 5 × 1015 cm−2 is analyzed. After a laser melting process, the incorporated oxygen is diffused to the surface forming again a GeOx layer which retains a large fraction of the total implanted dose. These detrimental effects can be eliminated by a selective etching of the native oxide layer prior to the ion implantation process. These effects have been also observed when implanting on Si substrates. This work identifies key aspects for conducting implantations at cryogenic temperatures, that are otherwise negligible for ion implanting at room temperature.
- Open Access
- 26 April 2024
- Published by Wiley in Physica Status Solidi (a)
- Vol. 221 (24)
Optical, Electrical, and Optoelectronic Characterization of Ti‐Supersaturated Gallium Arsenide
Herein, a detailed investigation on the properties of supersaturated gallium arsenide (GaAs) using Ti+ implantation followed by nanosecond pulsed laser melting (PLM) is presented. The supersaturated samples are analyzed by means of electrical, optical, and optoelectronic characterization. The sheet resistance results obtained using van der Pauw configuration measurements do not show activation of the implanted Ti+ in semi‐insulating GaAs after PLM. Absorptance measurements show a sub‐bandgap absorption (up to 6.5% for λ = 1000 nm) of the supersaturated GaAs:Ti and the just PLM‐processed GaAs, with the same laser melting fluence used (0.50 J/cm−2). The origin of this sub‐bandgap absorption is analyzed. Optoelectronic measurements show a similar sub‐bandgap photo‐response related to the absorption analyzed. The photo‐response measured below the bandgap originates from point defects introduced by the PLM process.
- 26 April 2024
- Published by Wiley in Physica Status Solidi (a)
- Vol. 221 (24)
Open AccessOptical, Electrical, and Optoelectronic Characterization of Ti‐Supersaturated Gallium Arsenide
Herein, a detailed investigation on the properties of supersaturated gallium arsenide (GaAs) using Ti+ implantation followed by nanosecond pulsed laser melting (PLM) is presented. The supersaturated samples are analyzed by means of electrical, optical, and optoelectronic characterization. The sheet resistance results obtained using van der Pauw configuration measurements do not show activation of the implanted Ti+ in semi‐insulating GaAs after PLM. Absorptance measurements show a sub‐bandgap absorption (up to 6.5% for λ = 1000 nm) of the supersaturated GaAs:Ti and the just PLM‐processed GaAs, with the same laser melting fluence used (0.50 J/cm−2). The origin of this sub‐bandgap absorption is analyzed. Optoelectronic measurements show a similar sub‐bandgap photo‐response related to the absorption analyzed. The photo‐response measured below the bandgap originates from point defects introduced by the PLM process.