Kawkb M. El-Tamimi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Kawkb M. El-Tamimi has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Dalia A. Bayoumi
Department of Dental Biomaterials, Faculty of Dentistry, Suez Canal University, 41522 Ismailia, Egypt
2 shared publications - Mohamed Mohamed Zaky Ahmed
Mechanical Engineering Department, College of Engineering at Al-Kharj, Prince Sattam Bin Abdulaziz University, Al-Kharj, Saudi Arabia
2 shared publications - Mohammed E. El-Sayed
Department of Removable Prosthodontics, Faculty of Dentistry, Suez Canal University, 41522 Ismailia, Egypt
2 shared publications - Ahmed M. Hebeshi
Faculty of Dentistry, Ain Shams University Cairo Egypt
1 shared publication Dalia A. Bayoumi
Department of Dental Biomaterials, Faculty of Dentistry, Suez Canal University, Ismailia, 41522, Egypt
1 shared publicationDalia A. El‐Bayoumi
Faculty of Dentistry, Suez Canal University Ismailia Egypt
1 shared publication
Latest Publications
- Open Access
- 25 May 2026
- Published by Springer Nature in BMC Oral Health
- Vol. 26 (1)
Impact of simulated gastric acid on electrochemical behavior, surface morphology, and topography of 3D printed cobalt chromium and titanium alloys for dental applications
Background: Additive manufacturing of cobalt–chromium (Co–Cr) and titanium (Ti-6Al-4 V) alloys is increasingly used in prosthetic dentistry. Acidic oral environments associated with gastroesophageal reflux disease (GERD) may negatively influence the surface integrity and corrosion resistance of dental materials. This in vitro study assessed the effects of simulated gastric acid on the corrosion resistance, surface morphology, and topographical changes of selective laser melting (SLM) Co–Cr and Ti-6Al-4 V alloys. Methods: Thirty-two additively manufactured specimens ( n = 16 per alloy) were randomly distributed into acidic (pH 1.2) and neutral control (pH 6.7 distilled water) subgroups ( n = 8). A cyclic static immersion protocol was used to simulate GERD-related acid exposure. Specimens in the acidic group were immersed for 2 min in acidic solution, rinsed without scrubbing to preserve the delicate surface topography, and stored in distilled water at 37 °C, repeated six times daily over nine days with a 24-hour interval maintained between each daily cycle. Control specimens were stored continuously in distilled water at 37 °C. Surface morphology, elemental composition, and topography were evaluated using scanning electron microscopy (SEM) and Abbott–Firestone curve analysis. Results: In the Co–Cr alloy, immersion in an acidic solution resulted in a decrease in the percentage of all elements, except O, which increased to 6.37 ± 1.77%, with the change being statistically significant ( P ≤ 0.05). In contrast, Ti-6Al-4 V also showed a decrease in all elements after immersion, with O rising to 2.26 ± 1.22%, although no changes were statistically significant ( P ≥ 0.05). SEM images indicated more oxide deposits on Co-Cr in an acidic solution, which also showed a notable increase in surface roughness, whereas Ti-6Al-4 V exhibited greater stability. The Abbott–Firestone analysis further confirmed that Co-Cr underwent more significant changes in peak formation and exploitation zones than Ti-6Al-4 V did in acidic environments. Conclusions: Under simulated gastric acid exposure, Ti-6Al-4 V alloys exhibited superior corrosion resistance and surface stability compared with Co–Cr alloys. These findings support the clinical preference for Ti-6Al-4 V in dental restorations for patients experiencing frequent acidic challenges, such as those with severe GERD.
- 25 May 2026
- Published by Springer Nature in BMC Oral Health
- Vol. 26 (1)
Open AccessImpact of simulated gastric acid on electrochemical behavior, surface morphology, and topography of 3D printed cobalt chromium and titanium alloys for dental applications
Background: Additive manufacturing of cobalt–chromium (Co–Cr) and titanium (Ti-6Al-4 V) alloys is increasingly used in prosthetic dentistry. Acidic oral environments associated with gastroesophageal reflux disease (GERD) may negatively influence the surface integrity and corrosion resistance of dental materials. This in vitro study assessed the effects of simulated gastric acid on the corrosion resistance, surface morphology, and topographical changes of selective laser melting (SLM) Co–Cr and Ti-6Al-4 V alloys. Methods: Thirty-two additively manufactured specimens ( n = 16 per alloy) were randomly distributed into acidic (pH 1.2) and neutral control (pH 6.7 distilled water) subgroups ( n = 8). A cyclic static immersion protocol was used to simulate GERD-related acid exposure. Specimens in the acidic group were immersed for 2 min in acidic solution, rinsed without scrubbing to preserve the delicate surface topography, and stored in distilled water at 37 °C, repeated six times daily over nine days with a 24-hour interval maintained between each daily cycle. Control specimens were stored continuously in distilled water at 37 °C. Surface morphology, elemental composition, and topography were evaluated using scanning electron microscopy (SEM) and Abbott–Firestone curve analysis. Results: In the Co–Cr alloy, immersion in an acidic solution resulted in a decrease in the percentage of all elements, except O, which increased to 6.37 ± 1.77%, with the change being statistically significant ( P ≤ 0.05). In contrast, Ti-6Al-4 V also showed a decrease in all elements after immersion, with O rising to 2.26 ± 1.22%, although no changes were statistically significant ( P ≥ 0.05). SEM images indicated more oxide deposits on Co-Cr in an acidic solution, which also showed a notable increase in surface roughness, whereas Ti-6Al-4 V exhibited greater stability. The Abbott–Firestone analysis further confirmed that Co-Cr underwent more significant changes in peak formation and exploitation zones than Ti-6Al-4 V did in acidic environments. Conclusions: Under simulated gastric acid exposure, Ti-6Al-4 V alloys exhibited superior corrosion resistance and surface stability compared with Co–Cr alloys. These findings support the clinical preference for Ti-6Al-4 V in dental restorations for patients experiencing frequent acidic challenges, such as those with severe GERD.
- 22 July 2024
- Published by Wiley in Journal of Prosthodontics
- Vol. 35 (5) , 760-767
Trueness of 3D‐printed cobalt chromium versus titanium removable partial denture clasps
Purpose: The purpose of this in vitro study was to evaluate the trueness of removable partial denture clasps fabricated with titanium (Ti) through the selective laser melting (SLM) technique compared to cobalt‐chromium alloys (CoCr). Materials and Methods: A virtual Aker clasp was designed on a scanned tooth, and SLM printers were used to print 20 claps using cobalt chromium ( n = 10) and titanium alloy ( n = 10). The deviation between the printed clasps and reference design was measured using the surface matching software (Geomagic control x) at rest, retentive tip, reciprocal tip, retentive shoulder, and reciprocal shoulder. An Independent t ‐test was used to determine the influence of 3D‐printed material on the trueness ( a = 0.05). Results: The gap distance in mm between the reference design and printed in titanium showed an average of 0.0001 ±0.0544, 0.0256 ±0.1309, 0.0230 ±0.1028, 0.0701 ±0.1234, and 0.0013 ±0.0735 mm in rest, reciprocal arm tip, retentive arm tip, retentive arm shoulder, and reciprocal arm shoulder, respectively. The gap distance in mm between the reference design and printed clasps in CoCr alloy showed an average of 0.0316 ±0.0692, 0.2783 ±0.1678, 0.1446 ±0.1528, 0.0315 ±0.0906, and 0.0419 ±0.1088 mm in rest, reciprocal arm tip, retentive arm tip, retentive arm shoulder, and reciprocal arm shoulder, respectively. The difference between titanium and CoCr alloys at each observation site was significant. Conclusion: Clasps fabricated from titanium with SLM printing have the least deviation and better trueness compared to those fabricated from cobalt chromium.
- 22 July 2024
- Published by Wiley in Journal of Prosthodontics
- Vol. 35 (5) , 760-767
Trueness of 3D‐printed cobalt chromium versus titanium removable partial denture clasps
Purpose: The purpose of this in vitro study was to evaluate the trueness of removable partial denture clasps fabricated with titanium (Ti) through the selective laser melting (SLM) technique compared to cobalt‐chromium alloys (CoCr). Materials and Methods: A virtual Aker clasp was designed on a scanned tooth, and SLM printers were used to print 20 claps using cobalt chromium ( n = 10) and titanium alloy ( n = 10). The deviation between the printed clasps and reference design was measured using the surface matching software (Geomagic control x) at rest, retentive tip, reciprocal tip, retentive shoulder, and reciprocal shoulder. An Independent t ‐test was used to determine the influence of 3D‐printed material on the trueness ( a = 0.05). Results: The gap distance in mm between the reference design and printed in titanium showed an average of 0.0001 ±0.0544, 0.0256 ±0.1309, 0.0230 ±0.1028, 0.0701 ±0.1234, and 0.0013 ±0.0735 mm in rest, reciprocal arm tip, retentive arm tip, retentive arm shoulder, and reciprocal arm shoulder, respectively. The gap distance in mm between the reference design and printed clasps in CoCr alloy showed an average of 0.0316 ±0.0692, 0.2783 ±0.1678, 0.1446 ±0.1528, 0.0315 ±0.0906, and 0.0419 ±0.1088 mm in rest, reciprocal arm tip, retentive arm tip, retentive arm shoulder, and reciprocal arm shoulder, respectively. The difference between titanium and CoCr alloys at each observation site was significant. Conclusion: Clasps fabricated from titanium with SLM printing have the least deviation and better trueness compared to those fabricated from cobalt chromium.
- Open Access
- 1 June 2024
- Published by Springer Nature in The Saudi Dental Journal
- Vol. 36 (6) , 947-953
Deformation and retentive forces variations of the additively manufactured cobalt-chromium and titanium alloys dental clasps
This in vitro study aimed to evaluate the additive manufacturing (AM) of cobalt chromium Co-Cr and titanium Ti alloy clasps for clinical use. After scanning the Ni-Cr die of the first molar, Akers' clasps were designed using computer-aided design/ computer-aided manufacturing (CAD/CAM). The clasps were manufactured from Co-Cr-W dental alloy and Ti-6Al-4V alloy powder using AM machines. Then, they were divided into two groups. The initial retentive force of the clasps was measured using a universal testing machine. Cyclic loading of the clasps was carried out by a specially designed insertion-removal testing apparatus in wet condition up to 5000 cycles. Retentive force was measured at 1000, 2000, 3000, 4000, and 5000 cycles. Moreover, the intaglio surface of each clasp was scanned using the scanner; and superimposition between the pre- and post-cycling clasp files was performed to evaluate deformation after cyclic loading. The fitting surfaces of retentive clasp tips were examined with a scanning electron microscope (SEM). Finally, it has been found that the initial retentive force for the Co-Cr group was 10.81 ± 0.37 N, and for the Ti group was 5.41 ± 0.18 N. Additionally, during the testing periods, both Co-Cr and Ti clasps continued to lose retentive force within the cycles of placement and removal. This effect was more prominent in the Co-Cr than in the Ti clasps. The distances between pre- and post-cycling in the retentive arm were -0.290 ± 0.11 mm and -0.004 ± 0.01 mm in Co-Cr and Ti alloys, respectively, and in the reciprocal arm were -0.072 ± 0.04 mm and -0.032 ± 0.04 mm in Co-Cr and Ti alloys, respectively. The retentive force required to remove the Ti clasps was found to be significantly lower than those required to dislodge the Co-Cr clasps. Co-Cr and Ti clasps lost significant amounts of retentive force from the initial use to the 3.5-year periods of simulated clinical use.
- 1 June 2024
- Published by Springer Nature in The Saudi Dental Journal
- Vol. 36 (6) , 947-953
Open AccessDeformation and retentive forces variations of the additively manufactured cobalt-chromium and titanium alloys dental clasps
This in vitro study aimed to evaluate the additive manufacturing (AM) of cobalt chromium Co-Cr and titanium Ti alloy clasps for clinical use. After scanning the Ni-Cr die of the first molar, Akers' clasps were designed using computer-aided design/ computer-aided manufacturing (CAD/CAM). The clasps were manufactured from Co-Cr-W dental alloy and Ti-6Al-4V alloy powder using AM machines. Then, they were divided into two groups. The initial retentive force of the clasps was measured using a universal testing machine. Cyclic loading of the clasps was carried out by a specially designed insertion-removal testing apparatus in wet condition up to 5000 cycles. Retentive force was measured at 1000, 2000, 3000, 4000, and 5000 cycles. Moreover, the intaglio surface of each clasp was scanned using the scanner; and superimposition between the pre- and post-cycling clasp files was performed to evaluate deformation after cyclic loading. The fitting surfaces of retentive clasp tips were examined with a scanning electron microscope (SEM). Finally, it has been found that the initial retentive force for the Co-Cr group was 10.81 ± 0.37 N, and for the Ti group was 5.41 ± 0.18 N. Additionally, during the testing periods, both Co-Cr and Ti clasps continued to lose retentive force within the cycles of placement and removal. This effect was more prominent in the Co-Cr than in the Ti clasps. The distances between pre- and post-cycling in the retentive arm were -0.290 ± 0.11 mm and -0.004 ± 0.01 mm in Co-Cr and Ti alloys, respectively, and in the reciprocal arm were -0.072 ± 0.04 mm and -0.032 ± 0.04 mm in Co-Cr and Ti alloys, respectively. The retentive force required to remove the Ti clasps was found to be significantly lower than those required to dislodge the Co-Cr clasps. Co-Cr and Ti clasps lost significant amounts of retentive force from the initial use to the 3.5-year periods of simulated clinical use.
- Open Access
The Effect of Salinized Nano ZrO2 Particles on the Microstructure, Hardness, and Wear Behavior of Acrylic Denture Tooth Nanocomposite
The wear of acrylic denture teeth is a serious problem that can change the vertical dimensions of dentures. This study evaluates the effect of adding salinized nano ZrO2 particles on the microstructure, hardness, and wear resistance of acrylic denture teeth. Heat polymerizing polymethyl methacrylate resin was mixed with salinized ZrO2 at concentrations of 5 wt.% and 10 wt.%. Acrylic resin specimens without filler addition were used as a control group. SEM/EDS analyses were performed and the Vickers’ hardness was evaluated. Two-body wear testing was performed using a chewing simulator with a human enamel antagonist. After subjecting the samples to 37,500 cycles, both height loss and weight loss were used to evaluate the wear behavior. The microstructural investigation of the reinforced-denture teeth indicates sound nanocomposite preparation using the applied regime without porosity or macro defects. The addition of zirconium oxide nanofillers to PMMA at both 5% and 10% increased the microhardness, with values of up to 49.7 HV. The wear mechanism in the acrylic base material without nanoparticle addition was found to be fatigue wear; a high density of microcracks were found. The addition of 5 wt.% ZrO2 improved the wear resistance. Increasing the nanoparticles to 10 wt.% ZrO2 further improved the wear resistance, with no microcracks found.
Open AccessThe Effect of Salinized Nano ZrO2 Particles on the Microstructure, Hardness, and Wear Behavior of Acrylic Denture Tooth Nanocomposite
The wear of acrylic denture teeth is a serious problem that can change the vertical dimensions of dentures. This study evaluates the effect of adding salinized nano ZrO2 particles on the microstructure, hardness, and wear resistance of acrylic denture teeth. Heat polymerizing polymethyl methacrylate resin was mixed with salinized ZrO2 at concentrations of 5 wt.% and 10 wt.%. Acrylic resin specimens without filler addition were used as a control group. SEM/EDS analyses were performed and the Vickers’ hardness was evaluated. Two-body wear testing was performed using a chewing simulator with a human enamel antagonist. After subjecting the samples to 37,500 cycles, both height loss and weight loss were used to evaluate the wear behavior. The microstructural investigation of the reinforced-denture teeth indicates sound nanocomposite preparation using the applied regime without porosity or macro defects. The addition of zirconium oxide nanofillers to PMMA at both 5% and 10% increased the microhardness, with values of up to 49.7 HV. The wear mechanism in the acrylic base material without nanoparticle addition was found to be fatigue wear; a high density of microcracks were found. The addition of 5 wt.% ZrO2 improved the wear resistance. Increasing the nanoparticles to 10 wt.% ZrO2 further improved the wear resistance, with no microcracks found.