Roxana Ciobanu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Roxana Ciobanu has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Catalin Borcia
Iasi Plasma Advanced Research Center (IPARC), Faculty of Physics, Alexandru Ioan Cuza University, Blvd. Carol I No. 11, 700506 Iasi, Romania
2 shared publications - Gabriela Borcia
Iasi Plasma Advanced Research Center (IPARC), Faculty of Physics, Alexandru Ioan Cuza University, Blvd. Carol I No. 11, 700506 Iasi, Romania
2 shared publications - Ilarion Mihaila
Alexandru Ioan Cuza University Blvd. Carol I 11
1 shared publication - Iustina Hatescu
Iasi Plasma Advanced Research Center (IPARC), Faculty of Physics, Alexandru Ioan Cuza University, Blvd. Carol I No. 11, 700506 Iasi, Romania
1 shared publication
Latest Publications
- Open Access
Discharge Energy Versus Exposure Time in Atmospheric-Pressure Air Plasma Surface Treatment of Polyimide and Polyamide 6 Films
Polyimide (PI) and polyamide 6 (PA6) films are treated under exposure times of 0.5 s and 1.0 s, and energy levels of 1.5, 2.0, and 2.3 mJ/pulse. PI exhibits the most substantial improvement in wettability and adhesion-related properties compared to PA6 and other studied polar polymers. The threshold level for stable surface modification is reduced, achieving a minimum water contact angle of 45°. The stability is markedly enhanced, with aged PI surfaces showing a 40% relative increase in adhesion work compared to untreated samples. The oxygen content on the PI surface reaches 22 at. %, surpassing the maximum of 18 at. % O observed for PA6. The surface roughness of PI increases by approximately a factor of 2, while PA6 shows an average increase of only 25%, attributed to higher ablation rates in the amorphous phase compared to the crystalline phase. The degree of surface modification achieved with [1.0 s; 1.5 mJ] treatment parameters is comparable to that with [0.5 s; 2.0 mJ], demonstrating that higher discharge energy can effectively shorten the required exposure time. This plasma treatment, even at very short exposure times, enables significant enhancement of the surface properties of PI, typically characterized by high chemical stability.
Open AccessDischarge Energy Versus Exposure Time in Atmospheric-Pressure Air Plasma Surface Treatment of Polyimide and Polyamide 6 Films
Polyimide (PI) and polyamide 6 (PA6) films are treated under exposure times of 0.5 s and 1.0 s, and energy levels of 1.5, 2.0, and 2.3 mJ/pulse. PI exhibits the most substantial improvement in wettability and adhesion-related properties compared to PA6 and other studied polar polymers. The threshold level for stable surface modification is reduced, achieving a minimum water contact angle of 45°. The stability is markedly enhanced, with aged PI surfaces showing a 40% relative increase in adhesion work compared to untreated samples. The oxygen content on the PI surface reaches 22 at. %, surpassing the maximum of 18 at. % O observed for PA6. The surface roughness of PI increases by approximately a factor of 2, while PA6 shows an average increase of only 25%, attributed to higher ablation rates in the amorphous phase compared to the crystalline phase. The degree of surface modification achieved with [1.0 s; 1.5 mJ] treatment parameters is comparable to that with [0.5 s; 2.0 mJ], demonstrating that higher discharge energy can effectively shorten the required exposure time. This plasma treatment, even at very short exposure times, enables significant enhancement of the surface properties of PI, typically characterized by high chemical stability.
- Open Access
Adhesion Properties and Stability of Polar Polymers Treated by Air Atmospheric Pressure Plasma
This study continues the discussion on the surface modification of polymers using an atmospheric pressure plasma (APP) reactor in air. These results complement prior research focusing on nonpolar polymers. Polymers, such as polyethylene terephthalate, polyetheretherketone, and polymethyl methacrylate, containing structurally bonded oxygen are studied, representing a range of properties such as oxygen content, crystalline/amorphous structure, polarity, functionality, and aliphatic/aromatic structure. APP induces superior wetting properties on the hydrophilic polymer surfaces with rapid and uniform modification within 0.5 s of exposure. The amorphous structures undergo additional modification for longer exposure. Moreover, the aliphatic chain structures require longer plasma exposure to reach surface modification equilibrium. The polar polymers reach a limit level of modification corresponding to a minimum water contact angle of about 50°. The surface polarity increases on average by a factor of approximately two. The equilibrium values of the adhesion work attained after post-processing recovery fall within a limited range of about 100–120 mJ/m2. The enhancement of surface functionality through the creation of oxidized groups primarily depends on the initial oxygen content and reaches a limit of about 40 at.% oxygen. The surface properties of the treated polar surfaces exhibit good stability, comparable to that of the previously tested nonpolar polymers.
Open AccessAdhesion Properties and Stability of Polar Polymers Treated by Air Atmospheric Pressure Plasma
This study continues the discussion on the surface modification of polymers using an atmospheric pressure plasma (APP) reactor in air. These results complement prior research focusing on nonpolar polymers. Polymers, such as polyethylene terephthalate, polyetheretherketone, and polymethyl methacrylate, containing structurally bonded oxygen are studied, representing a range of properties such as oxygen content, crystalline/amorphous structure, polarity, functionality, and aliphatic/aromatic structure. APP induces superior wetting properties on the hydrophilic polymer surfaces with rapid and uniform modification within 0.5 s of exposure. The amorphous structures undergo additional modification for longer exposure. Moreover, the aliphatic chain structures require longer plasma exposure to reach surface modification equilibrium. The polar polymers reach a limit level of modification corresponding to a minimum water contact angle of about 50°. The surface polarity increases on average by a factor of approximately two. The equilibrium values of the adhesion work attained after post-processing recovery fall within a limited range of about 100–120 mJ/m2. The enhancement of surface functionality through the creation of oxidized groups primarily depends on the initial oxygen content and reaches a limit of about 40 at.% oxygen. The surface properties of the treated polar surfaces exhibit good stability, comparable to that of the previously tested nonpolar polymers.