Yu. Yu. Efimova
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yu. Yu. Efimova has a total of 23 co-authors. Here are the top co-authors by number of shared publications:
- I. V. Belevskaya
Магнитогорский государственный технический университет (МГТУ) им. Г.И. Носова
4 shared publications N. V. Koptseva
4 shared publications- Natalia V. Koptseva
Nosov Magnitogorsk State Technical University
4 shared publications E. V. Gubarev
Магнитогорский государственный технический университет (МГТУ) им. Г.И. Носова
2 shared publications- Irina A. Saprykina
Institute of Archaeology, Russian Academy of Sciences, Moscow, Russia
2 shared publications L. S. Belevskii
Магнитогорский государственный технический университет (МГТУ) им. Г.И. Носова
2 shared publications
Latest Publications
- Open Access
- 22 July 2026
- Published by MDPI AG in Materials Proceedings
- Vol. 33 (1) , 7
Influence of Thermomechanical Processing Modes on the Formation of Structure and Properties of Rolled Strip for Coiled Tubing
This study presents the results of investigations into a new low-alloyed steel grade CT80 designed for coiled tubing (CT) with increased cold resistance requirements. Based on data concerning the structural-phase transformations of overcooled austenite, various thermomechanical treatment modes were defined and tested on a reversing hot rolling mill DUO-500 combined with an accelerated cooling system. Controlled rolling and accelerated cooling regimes were established, ensuring the formation of the most favorable microstructure for achieving a high level of ductile-plastic properties at the specified strength level of CT80-class steel.
- 22 July 2026
- Published by MDPI AG in Materials Proceedings
- Vol. 33 (1) , 7
Open AccessInfluence of Thermomechanical Processing Modes on the Formation of Structure and Properties of Rolled Strip for Coiled Tubing
This study presents the results of investigations into a new low-alloyed steel grade CT80 designed for coiled tubing (CT) with increased cold resistance requirements. Based on data concerning the structural-phase transformations of overcooled austenite, various thermomechanical treatment modes were defined and tested on a reversing hot rolling mill DUO-500 combined with an accelerated cooling system. Controlled rolling and accelerated cooling regimes were established, ensuring the formation of the most favorable microstructure for achieving a high level of ductile-plastic properties at the specified strength level of CT80-class steel.
- 30 March 2025
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- No. 3,p. 17-23
Thermal EMF hysteresis depending on the heating and cooling conditions of thermocouples from different manufacturers of platinum-rhodium wire
Studies have been conducted to identify patterns of changes in the thermal EMF values of platinum-rhodium type B thermocouples made of PR30 (30% Rh) and PR6 (6% Rh) alloys from different manufacturers. They were studied at the stages of heating to a temperature of 1300 oC and cooling to 300 оC, as well as during repeated cycles of thermal exposure at high heating and cooling rates of 10 оC/s, in order to determine the possible causes of the discrepancy between the thermocouple parameters and the required measurement accuracy. The effects of thermal EMF hysteresis are revealed, consisting in the discrepancy of thermocouple parameters during heating and cooling, as well as a narrowing of the thermal EMF hysteresis loop during repeated heating and cooling cycles. No impurity elements were detected in the wires of PR30 (30% Rh) and PR6 (6% Rh) compositions from different manufacturers, and there are no significant changes in the chemical composition after thermal exposure when heated to a temperature of 1300 оC. It has been established that there is no discrepancy between the thermocouple parameters and the actual temperatures of the technological conditions due to deviations in the regulated requirements for the chemical composition of the wire making up the thermocouple or incorrectly selected welding modes. It is shown that the degree of penetration of the welded joint of the elements of the studied products does not affect the value of thermal EMF. It was found that during the assembly of thermocouples, there are traces of deformation effects from the rollers feeding the wire into the welding unit. It is determined that this may be the reason for the incomplete course of the recrystallization process and the occurrence of temperature discrepancies in thermocouples.
- 30 March 2025
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- No. 3,p. 17-23
Thermal EMF hysteresis depending on the heating and cooling conditions of thermocouples from different manufacturers of platinum-rhodium wire
Studies have been conducted to identify patterns of changes in the thermal EMF values of platinum-rhodium type B thermocouples made of PR30 (30% Rh) and PR6 (6% Rh) alloys from different manufacturers. They were studied at the stages of heating to a temperature of 1300 oC and cooling to 300 оC, as well as during repeated cycles of thermal exposure at high heating and cooling rates of 10 оC/s, in order to determine the possible causes of the discrepancy between the thermocouple parameters and the required measurement accuracy. The effects of thermal EMF hysteresis are revealed, consisting in the discrepancy of thermocouple parameters during heating and cooling, as well as a narrowing of the thermal EMF hysteresis loop during repeated heating and cooling cycles. No impurity elements were detected in the wires of PR30 (30% Rh) and PR6 (6% Rh) compositions from different manufacturers, and there are no significant changes in the chemical composition after thermal exposure when heated to a temperature of 1300 оC. It has been established that there is no discrepancy between the thermocouple parameters and the actual temperatures of the technological conditions due to deviations in the regulated requirements for the chemical composition of the wire making up the thermocouple or incorrectly selected welding modes. It is shown that the degree of penetration of the welded joint of the elements of the studied products does not affect the value of thermal EMF. It was found that during the assembly of thermocouples, there are traces of deformation effects from the rollers feeding the wire into the welding unit. It is determined that this may be the reason for the incomplete course of the recrystallization process and the occurrence of temperature discrepancies in thermocouples.
- 1 October 2023
- Published by Pleiades Publishing Ltd in Nanobiotechnology Reports
- Vol. 18 (5) , 664-669
Microanalysis of the Chemical Composition of the Surface of Rhescuporis V Staters of AD 274/275
The chemical composition of the surface of staters of the Bosporan King Rhescuporis V with an erroneous date AΞΦ (561 Bosporan era (BE) = AD 264/265) instead of AOΦ (571 BE = AD 274/275) is studied. The depletion-silvering technique used for the AD 242/243–267/268 staters of Rhescuporis V with a higher amount of silver in the alloy than in that of AD 274/275 was apparently applied to enrich the surface of these staters with silver. The growing shortage of silver from AD 275/276, however, led to further deterioration of the coin and replacement of the depletion-silvering technique with the silvering of the surface of the coins by special pastes.
- 1 October 2023
- Published by Pleiades Publishing Ltd in Nanobiotechnology Reports
- Vol. 18 (5) , 664-669
Microanalysis of the Chemical Composition of the Surface of Rhescuporis V Staters of AD 274/275
The chemical composition of the surface of staters of the Bosporan King Rhescuporis V with an erroneous date AΞΦ (561 Bosporan era (BE) = AD 264/265) instead of AOΦ (571 BE = AD 274/275) is studied. The depletion-silvering technique used for the AD 242/243–267/268 staters of Rhescuporis V with a higher amount of silver in the alloy than in that of AD 274/275 was apparently applied to enrich the surface of these staters with silver. The growing shortage of silver from AD 275/276, however, led to further deterioration of the coin and replacement of the depletion-silvering technique with the silvering of the surface of the coins by special pastes.
- 31 October 2022
- Published by Ore and Metals Publishing House in Chernye Metally
- p. 39-44
Investigation of the features of the formation of the structure of steel 08Yu during asymmetric rolling on a new mill 400
A study of the 08Yu steel structure during cold rolling at a new rolling mill in the Zhilyaev Laboratory of Mechanics of Gradient Nanomaterials of the Nosov Magnitogorsk State Technical University. It has been found that asymmetric rolling in rollers with speeds that differ 5 times and all other things being equal, resulted in the formation of a gradient structure. In the upper part of the strip section on the side where the rolling speed was lower, a uniform structure is observed, which is formed at more than half the strip thickness and consists of ultra-fine practically equiaxial grains of less than 1000 nm in size. The formation of the ultrafine structure is explained by the dynamic recrystallization under the conditions of heating the strip to a temperature of 250–300 ºC during rolling. In the lower part, on the side where the rolling speed was higher, a fibrous structure with smaller fragments up to 200 nm in size within individual fibers is clearly revealed. The hardness after asymmetric rolling compared to symmetrical rolling increased slightly and turned out to be more evenly distributed over the section. The difference in its values of different sections was not more than 15 % compared to symmetrical rolling, where the hardness in the central and perephyrian sections of the strip section differed by about 35 %. It has been found that these asymmetric rolling conditions lead to a simultaneous increase in reduction from 50 to 80 % and a decrease in force of almost 3 times per pass compared to symmetrical rolling, which can be explained by grinding the structure.The study was carried out within the framework of grants from the Russian Science Foundation (No. 20-69-46042 dated May 20, 2020), RFBR (No. 20-38-90097 dated September 3, 2020) and Megagrant (No. 075-15-2021-627 dated June 8, 2021).
- 31 October 2022
- Published by Ore and Metals Publishing House in Chernye Metally
- p. 39-44
Investigation of the features of the formation of the structure of steel 08Yu during asymmetric rolling on a new mill 400
A study of the 08Yu steel structure during cold rolling at a new rolling mill in the Zhilyaev Laboratory of Mechanics of Gradient Nanomaterials of the Nosov Magnitogorsk State Technical University. It has been found that asymmetric rolling in rollers with speeds that differ 5 times and all other things being equal, resulted in the formation of a gradient structure. In the upper part of the strip section on the side where the rolling speed was lower, a uniform structure is observed, which is formed at more than half the strip thickness and consists of ultra-fine practically equiaxial grains of less than 1000 nm in size. The formation of the ultrafine structure is explained by the dynamic recrystallization under the conditions of heating the strip to a temperature of 250–300 ºC during rolling. In the lower part, on the side where the rolling speed was higher, a fibrous structure with smaller fragments up to 200 nm in size within individual fibers is clearly revealed. The hardness after asymmetric rolling compared to symmetrical rolling increased slightly and turned out to be more evenly distributed over the section. The difference in its values of different sections was not more than 15 % compared to symmetrical rolling, where the hardness in the central and perephyrian sections of the strip section differed by about 35 %. It has been found that these asymmetric rolling conditions lead to a simultaneous increase in reduction from 50 to 80 % and a decrease in force of almost 3 times per pass compared to symmetrical rolling, which can be explained by grinding the structure.The study was carried out within the framework of grants from the Russian Science Foundation (No. 20-69-46042 dated May 20, 2020), RFBR (No. 20-38-90097 dated September 3, 2020) and Megagrant (No. 075-15-2021-627 dated June 8, 2021).
- 1 October 2022
- Published by Pleiades Publishing Ltd in Nanobiotechnology Reports
- Vol. 17 (5) , 638-643
Microanalysis of the Chemical Composition of the Surface of Teiranes Staters of AD 276/7–278/9: Silvering Technique
The results of studying the chemical composition of the surface of staters of the Bosporan king Teiranes of AD 276/7–278/9 are considered. Metallographic investigation and X-ray spectral microanalysis make it possible for the first time to establish the fact of silvering the surface of staters made of an alloy based on copper with a small amount of silver, sometimes tin and lead. Also, for the first time in the silver surface layer of these coins, the presence of chlorine, calcium, sodium and magnesium is revealed. This indicates the possible use of special pastes containing chlorides of silver, sodium, ammonium and mercury, potassium hydrotartrate and chalk for the silvering of late Bosporan staters from AD 275.
- 1 October 2022
- Published by Pleiades Publishing Ltd in Nanobiotechnology Reports
- Vol. 17 (5) , 638-643
Microanalysis of the Chemical Composition of the Surface of Teiranes Staters of AD 276/7–278/9: Silvering Technique
The results of studying the chemical composition of the surface of staters of the Bosporan king Teiranes of AD 276/7–278/9 are considered. Metallographic investigation and X-ray spectral microanalysis make it possible for the first time to establish the fact of silvering the surface of staters made of an alloy based on copper with a small amount of silver, sometimes tin and lead. Also, for the first time in the silver surface layer of these coins, the presence of chlorine, calcium, sodium and magnesium is revealed. This indicates the possible use of special pastes containing chlorides of silver, sodium, ammonium and mercury, potassium hydrotartrate and chalk for the silvering of late Bosporan staters from AD 275.
- 1 September 2019
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 61 (5-6) , 267-273
Deformation Behavior of Finely-Lamellar Pearlite During Multiple Cold Plastic Deformation of Eutectoid Steel
- 1 September 2019
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 61 (5-6) , 267-273
Deformation Behavior of Finely-Lamellar Pearlite During Multiple Cold Plastic Deformation of Eutectoid Steel
- Open Access
- 19 March 2018
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
- No. 1,p. 36-43
INVESTIGATION OF SURFACE STRUCTURE, CRYSTALLOGRAPHIC TEXTURE, MICROTOPOGRAPHY OF FUNCTIONAL COATINGS DEPOSITED USING FLEXIBLE TOOL AND SOME APPLICATIONS. PART 2. INVESTIGATION OF THE EFFECT OF FUNCTIONAL COATINGS APPLIED USING FLEXIBLE TOOL ON SOME PROPERTIES OF MATERIALS AND APPLICATIONS
Для наноструктурирования поверхности использован один из простых методов модифицирования поверхности с одновременным нанесением покрытий – фрикционное плакирование (ФП). При ФП интенсивная пластическая деформация осуществляется вращающейся проволочной щеткой (ВПЩ), ворсинки которой оказывают на обрабатываемую поверхность ударно-фрикционное воздействие и одновременно наносят покрытие. Проведено исследование износостойкости стальных образцов (диаметром 45 мм, шириной 10 мм) из стали марки 45, подвергнутых нормализации. Медьсодержащие покрытия наносили на круглошлифовальном станке. Испытания образцов, обработанных по различным режимам, проводили на машине трения СМЦ-2 по схеме «диск по диску». Установлено, что образцы с медным (М1) и латунным (Л63) покрытиями имели, в зависимости от режима обработки, износостойкость выше эталонных в 2–10 раз. Наибольшую износостойкость показали образцы с латунным покрытием толщиной 10–15 мкм, нанесенным за 6 проходов с натягом (подача ВПЩ на обрабатываемое изделие) 2 мм при скорости скольжения 25 м/c. Для изучения влияния режимов процесса ФП на усталостную прочность проведены испытания гладких образцов (4 серии – 60 шт.) из стали марки 20ХН в соответствии с ГОСТ 25502-82 «Методы испытаний на усталость». Анализ результатов показал, что наиболее эффективным является поверхностное пластическое деформирование с нанесением латунного покрытия. Коэффициент повышения предела выносливости составлял Kυ = 1,41. Выявлено, что получение покрытий методом ФП не влияет на механические свойства стали (σв, σт, δ10). Нанесение медного покрытия на штоки и плунжеры гидравлики позволило увеличить срок их службы в 1,4– 3,0 раза, на зубья колес волновых передач торцевого исполнения – в 6 раз.
- 19 March 2018
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
- No. 1,p. 36-43
Open AccessINVESTIGATION OF SURFACE STRUCTURE, CRYSTALLOGRAPHIC TEXTURE, MICROTOPOGRAPHY OF FUNCTIONAL COATINGS DEPOSITED USING FLEXIBLE TOOL AND SOME APPLICATIONS. PART 2. INVESTIGATION OF THE EFFECT OF FUNCTIONAL COATINGS APPLIED USING FLEXIBLE TOOL ON SOME PROPERTIES OF MATERIALS AND APPLICATIONS
Для наноструктурирования поверхности использован один из простых методов модифицирования поверхности с одновременным нанесением покрытий – фрикционное плакирование (ФП). При ФП интенсивная пластическая деформация осуществляется вращающейся проволочной щеткой (ВПЩ), ворсинки которой оказывают на обрабатываемую поверхность ударно-фрикционное воздействие и одновременно наносят покрытие. Проведено исследование износостойкости стальных образцов (диаметром 45 мм, шириной 10 мм) из стали марки 45, подвергнутых нормализации. Медьсодержащие покрытия наносили на круглошлифовальном станке. Испытания образцов, обработанных по различным режимам, проводили на машине трения СМЦ-2 по схеме «диск по диску». Установлено, что образцы с медным (М1) и латунным (Л63) покрытиями имели, в зависимости от режима обработки, износостойкость выше эталонных в 2–10 раз. Наибольшую износостойкость показали образцы с латунным покрытием толщиной 10–15 мкм, нанесенным за 6 проходов с натягом (подача ВПЩ на обрабатываемое изделие) 2 мм при скорости скольжения 25 м/c. Для изучения влияния режимов процесса ФП на усталостную прочность проведены испытания гладких образцов (4 серии – 60 шт.) из стали марки 20ХН в соответствии с ГОСТ 25502-82 «Методы испытаний на усталость». Анализ результатов показал, что наиболее эффективным является поверхностное пластическое деформирование с нанесением латунного покрытия. Коэффициент повышения предела выносливости составлял Kυ = 1,41. Выявлено, что получение покрытий методом ФП не влияет на механические свойства стали (σв, σт, δ10). Нанесение медного покрытия на штоки и плунжеры гидравлики позволило увеличить срок их службы в 1,4– 3,0 раза, на зубья колес волновых передач торцевого исполнения – в 6 раз.
- Open Access
- 1 January 2017
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
- No. 4,p. 62-70
INVESTIGATION OF SURFACE STRUCTURE, CRYSTALLOGRAPHIC TEXTURE, MICROTOPOGRAPHY OF FUNCTIONAL COATINGS DEPOSITED USING FLEXIBLE TOOL AND SOME APPLICATIONS. Part 1. Surface structure, crystallographic texture, microtopography of copper and brass coatings deposited on steel base using flexible tool
ИССЛЕДОВАНИЕ СТРУКТУРЫ, КРИСТАЛЛОГРАФИЧЕСКОЙ ТЕКСТУРЫ, МИКРОТОПОГРАФИИ ПОВЕРХНОСТИ ФУНКЦИОНАЛЬНЫХ ПОКРЫТИЙ, НАНЕСЕННЫХ ГИБКИМ ИНСТРУМЕНТОМ, И НЕКОТОРЫЕ ОБЛАСТИ ИХ ПРИМЕНЕНИЯ. Часть 1. Структура, кристаллографическая текстура и микротопография поверхности медных и латунных покрытий, нанесенных гибким инструментом на стальную основу
- 1 January 2017
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
- No. 4,p. 62-70
Open AccessINVESTIGATION OF SURFACE STRUCTURE, CRYSTALLOGRAPHIC TEXTURE, MICROTOPOGRAPHY OF FUNCTIONAL COATINGS DEPOSITED USING FLEXIBLE TOOL AND SOME APPLICATIONS. Part 1. Surface structure, crystallographic texture, microtopography of copper and brass coatings deposited on steel base using flexible tool
ИССЛЕДОВАНИЕ СТРУКТУРЫ, КРИСТАЛЛОГРАФИЧЕСКОЙ ТЕКСТУРЫ, МИКРОТОПОГРАФИИ ПОВЕРХНОСТИ ФУНКЦИОНАЛЬНЫХ ПОКРЫТИЙ, НАНЕСЕННЫХ ГИБКИМ ИНСТРУМЕНТОМ, И НЕКОТОРЫЕ ОБЛАСТИ ИХ ПРИМЕНЕНИЯ. Часть 1. Структура, кристаллографическая текстура и микротопография поверхности медных и латунных покрытий, нанесенных гибким инструментом на стальную основу
- Open Access
- 10 March 2016
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 59 (2) , 123-127
ULTRAFINE-GRAINED STRUCTURE FORMATION IN CARBON STEEL BY HIGH-SPEED COMPRESSION DEFORMATION AT INCREASED TEMPERATURES
Увеличение скорости пластической деформации приводит к значительным изменениям в микроструктуре металлических материалов. Структуру и свойства металла определяют такие факторы, как величина давления (или импульса), скорость деформации (или продолжительность процесса) и температура. В работе исследовано влияние высокоскоростной деформации на микроструктуру материалов. С использованием исследовательского комплекса Gleeble 3500 осуществлена высокоскоростная деформация стали 20 при температурах 800, 900, 1000 и 1200 °С. Изучена микроструктура и определена микротвердость образцов. Показана принципиальная возможность обеспечить деформационное измельчение структуры низкоуглеродистой стали 20 при высокоскоростной деформации при температурах 800 – 1000 °С до размера зерна около 400 нм подобно тому, как это достигается при больших пластических деформациях без нагрева металла или с небольшим нагревом, не превышающим температуру рекристаллизации.
- 10 March 2016
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 59 (2) , 123-127
Open AccessULTRAFINE-GRAINED STRUCTURE FORMATION IN CARBON STEEL BY HIGH-SPEED COMPRESSION DEFORMATION AT INCREASED TEMPERATURES
Увеличение скорости пластической деформации приводит к значительным изменениям в микроструктуре металлических материалов. Структуру и свойства металла определяют такие факторы, как величина давления (или импульса), скорость деформации (или продолжительность процесса) и температура. В работе исследовано влияние высокоскоростной деформации на микроструктуру материалов. С использованием исследовательского комплекса Gleeble 3500 осуществлена высокоскоростная деформация стали 20 при температурах 800, 900, 1000 и 1200 °С. Изучена микроструктура и определена микротвердость образцов. Показана принципиальная возможность обеспечить деформационное измельчение структуры низкоуглеродистой стали 20 при высокоскоростной деформации при температурах 800 – 1000 °С до размера зерна около 400 нм подобно тому, как это достигается при больших пластических деформациях без нагрева металла или с небольшим нагревом, не превышающим температуру рекристаллизации.
- 1 September 2015
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2015 (9) , 753-758
Deformation of a surface layer and coating application using a flexible tool
- 1 September 2015
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2015 (9) , 753-758
Deformation of a surface layer and coating application using a flexible tool