Kerong Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Kerong Wang has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Jiapeng Chen
School of Electro-Mechanical Engineering, Zhongyuan Institute of Science and Technology, Xuchang 461000, China
2 shared publications - Anjie He
Research Center for Advanced Micro-/Nano-Fabrication Materials, School of Chemistry and Chemical Engineering, Shanghai University of Engineering Science, Shanghai 201620, China
1 shared publication - Baoxiu Wang
College of Chemistry and Chemical Engineering, Research Center for Advanced Micro-Nano-Fabrication Materials, Shanghai University of Engineering Science, Shanghai 201620, China
1 shared publication - Haixu Liu
Jiangsu Key Laboratory of Precision and Micro-manufacturing Technology, College of Mechanical and Electrical Engineering, Nanjing University of Aeronautics and Astronautics, Nanjing 210016, China
1 shared publication - Jie Lin
Research Center for Advanced Micro-/Nano-Fabrication Materials, School of Chemistry and Chemical Engineering, Shanghai University of Engineering Science, Shanghai 201620, China
1 shared publication - Ning Liu
Jiangsu Key Laboratory of Precision and Micro-manufacturing Technology, College of Mechanical and Electrical Engineering, Nanjing University of Aeronautics and Astronautics, Nanjing 210016, China
1 shared publication
Latest Publications
- Open Access
- 10 July 2024
- Published by MDPI AG in Micromachines
- Vol. 15 (7) , 900
A Novel Noise Reduction Approach of Acoustic Emission (AE) Signals in the SiC Lapping Process on Fixed Abrasive Pads
Acoustic emission (AE) technology has been widely utilized to monitor the SiC wafer lapping process. The root-mean-square (RMS) of the time–domain eigenvalues of the AE signal has a linear relationship with the material removal rate (MRR). However, the existence of background noise severely reduces signal monitoring accuracy. Noise interference often leads to increased RMS deviation and signal distortion. In the study presented in this manuscript, a frequency threshold noise reduction approach was developed by combining and improving wavelet packet noise reduction and spectral subtraction noise reduction techniques. Three groups of SiC lapping experiments were conducted on a fixed abrasive pad, and the lapping acoustic signals were processed using three different noise reduction approaches: frequency threshold, wavelet packet, and spectral subtraction. The results show that the noise reduction method using the frequency threshold is the most effective, with the best coefficient of determination (R2) for the linear fit of the RMS to the MRR.
- 10 July 2024
- Published by MDPI AG in Micromachines
- Vol. 15 (7) , 900
Open AccessA Novel Noise Reduction Approach of Acoustic Emission (AE) Signals in the SiC Lapping Process on Fixed Abrasive Pads
Acoustic emission (AE) technology has been widely utilized to monitor the SiC wafer lapping process. The root-mean-square (RMS) of the time–domain eigenvalues of the AE signal has a linear relationship with the material removal rate (MRR). However, the existence of background noise severely reduces signal monitoring accuracy. Noise interference often leads to increased RMS deviation and signal distortion. In the study presented in this manuscript, a frequency threshold noise reduction approach was developed by combining and improving wavelet packet noise reduction and spectral subtraction noise reduction techniques. Three groups of SiC lapping experiments were conducted on a fixed abrasive pad, and the lapping acoustic signals were processed using three different noise reduction approaches: frequency threshold, wavelet packet, and spectral subtraction. The results show that the noise reduction method using the frequency threshold is the most effective, with the best coefficient of determination (R2) for the linear fit of the RMS to the MRR.
- Open Access
Effect of Oxidant Concentration on the Oxide Layer Thickness of 304 Stainless Steel
Ultra-thin 304 stainless steel can be used to flexibly display substrates after they have been subjected to chemical mechanical polishing (CMP). The thickness of the chemical oxide layer directly affects the polishing efficiency and surface quality of 304 stainless steel. In the study presented in the following paper, the thickness variation of the chemical oxide layer of 304 stainless steel was analyzed following electrochemical corrosion under different oxidant concentration conditions. Furthermore, the impact of the oxidant concentration on the grooves, chips, and scratch depth–displacement–load curves was investigated during a nano-scratching experiment. Through this process, we were able to reveal the chemical reaction mechanism between 304 stainless steel materials and oxidizers. The corrosion rate was found to be faster at 8% oxidant content. The maximum values of the scratch depth and elastic–plastic critical load were determined to be 2153 nm and 58.47 mN, respectively.
Open AccessEffect of Oxidant Concentration on the Oxide Layer Thickness of 304 Stainless Steel
Ultra-thin 304 stainless steel can be used to flexibly display substrates after they have been subjected to chemical mechanical polishing (CMP). The thickness of the chemical oxide layer directly affects the polishing efficiency and surface quality of 304 stainless steel. In the study presented in the following paper, the thickness variation of the chemical oxide layer of 304 stainless steel was analyzed following electrochemical corrosion under different oxidant concentration conditions. Furthermore, the impact of the oxidant concentration on the grooves, chips, and scratch depth–displacement–load curves was investigated during a nano-scratching experiment. Through this process, we were able to reveal the chemical reaction mechanism between 304 stainless steel materials and oxidizers. The corrosion rate was found to be faster at 8% oxidant content. The maximum values of the scratch depth and elastic–plastic critical load were determined to be 2153 nm and 58.47 mN, respectively.