Petri I. Räisänen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Petri I. Räisänen has a total of 2 co-authors. Here are the top co-authors by number of shared publications:
- Markku Leskelä
Department of Chemistry, University of Helsinki, P. O. Box 55, FI-00014, Finland
1 shared publication - Mikko Ritala
Department of Chemistry University of Helsinki Helsinki Finland
1 shared publication
Latest Publications
- 25 March 2002
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry
- Vol. 12 (5) , 1415-1418
Atomic layer deposition of Al2O3 films using AlCl3 and Al(OiPr)3 as precursors
Al2O3 films have been grown by atomic layer deposition (ALD) using reactions between AlCl3 and Al(OiPr)3. In this process the aluminium alkoxide serves as both a metal and an oxygen source. No separate oxygen source is required. With this approach an Al2O3 film has been deposited on silicon without an interfacial silicon oxide layer. The film growth rate was 0.8 Å cycle−1. The residual contents of chlorine, hydrogen and carbon in the film deposited at 300 °C were 1.8, 0.7 and 2O3 ALD processes for thick films, but the permittivity decreased for very thin films. Post deposition annealing is required to improve electrical properties of thin films.
- 25 March 2002
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry
- Vol. 12 (5) , 1415-1418
Atomic layer deposition of Al2O3 films using AlCl3 and Al(OiPr)3 as precursors
Al2O3 films have been grown by atomic layer deposition (ALD) using reactions between AlCl3 and Al(OiPr)3. In this process the aluminium alkoxide serves as both a metal and an oxygen source. No separate oxygen source is required. With this approach an Al2O3 film has been deposited on silicon without an interfacial silicon oxide layer. The film growth rate was 0.8 Å cycle−1. The residual contents of chlorine, hydrogen and carbon in the film deposited at 300 °C were 1.8, 0.7 and 2O3 ALD processes for thick films, but the permittivity decreased for very thin films. Post deposition annealing is required to improve electrical properties of thin films.