YFYizheng Feng

Yizheng Feng

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Yizheng Feng has a total of 9 co-authors. Here are the top co-authors by number of shared publications:

  • Xiling Wang

    Jiangsu Jiaotong Coll, Zhenjiang 212100, Peoples R China

    2 shared publications
  • Chunzhi Xia

    School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang, China

    1 shared publication
  • Hong Teng

    1 shared publication
  • Jiasheng Zou

    College of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212100, People’s Republic of China

    1 shared publication
  • Lingyu Wang

    College of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212100, People’s Republic of China

    1 shared publication
  • Shangbo Ma

    School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang, 212100, People’s Republic of China

    1 shared publication

Latest Publications

  • Study on the friction and wear properties of nickel-based-WC-10Ni composite coatings prepared on the surface of TC4 titanium alloy

    by Shangbo Ma, Xiangping Xu, Xiling Wang, Yizheng Feng, Chunzhi Xia, Hong Teng

    A nickel-based WC-10Ni composite coating was fabricated via vacuum brazing at 1160 °C, using TC4 titanium alloy as the matrix, WC-10Ni powder as the hard phase, and BNi-5 as the brazing material. The study examined the coating’s microstructure and analyzed the impact of the WC-10Ni ratio and friction test temperature on its wear resistance, alongside a discussion of the wear mechanism. The results revealed that the hard layer of the composite coating comprised TiC, W, and minor amounts of Ti5Si3 and α-Ti, while the interface layer displayed a network structure of Ti2Ni and Ti5Si3. Using a Si3N4 ceramic ball as the counter-wear material, under conditions of a 10N load, 318 r min−1 rotational speed, 3 mm wear radius, and 30 min wear duration, the average friction coefficients of the three composite coatings were 0.289, 0.241, and 0.271, and their wear rates were 65.8%, 39.7%, and 52.7% of the substrate, respectively. The 50% WC-10Ni coating exhibited the best wear resistance, with adhesive wear being the dominant mechanism, accompanied by minor abrasive wear. Friction tests on the 50% WC-10Ni coating at 200 °C, 400 °C, 600 °C, and 800 °C revealed that the lowest wear rate, 0.35 × 10−5 mm3 N−1 m−1, occurred at 600 °C, where the average friction coefficient was 0.432 and oxidative wear was predominant. At 800 °C, the coating suffered significant damage, resulting in deteriorated wear resistance.

  • Effect of heat treatment on microstructure and mechanical properties of AG728 steel joints welded with ER90S-G wires

    by Yizheng Feng, Xiangping Xu, Xiling Wang, Lingyu Wang, Jiasheng Zou, Ziqing Wang

    This study utilised self-developed ER90S-G wires for butt welding tests on AG728 plates to investigate the influence of heat treatment on the microstructure and mechanical properties of welded joints. Furthermore, it aimed to analyse the microstructure and metallurgical mechanisms of these joints. The findings reveal that the microstructure of the welded joints primarily consists of acicular ferrite with a minor presence of granular bainite. Following heat treatment, there is a noticeable growth in acicular ferrite and the emergence of tempered sorbite and massive ferrite; concurrently, austenite grain boundaries vanish, carbide aggregation increases, the quantity of large angular grain boundaries diminishes, and the martensite–austenite constituent elements gradually disappear. The physical phase of the base material, the heat-affected zone (HAZ), and the welded joints uniformly transition to α-Fe. Additionally, inclusions measuring 0.5 μm, predominantly MnSiO3, evidently promote the formation of ferrite. The tensile strength and impact toughness experience a minor reduction while the hardness of the HAZ and weld seam significantly decreases. The micro-morphology of the welded joint’s tensile fracture is predominantly characterised by dimples, within which inclusions or precipitated phase particles are distinctly visible, indicating a microporous coalescence-type fracture. At −45 °C, the impact test of welded joints reveals that the HAZ impact fracture micro-morphology exhibits brittle deconstructive fracture patterns, which, through heat treatment, transition to quasi-cleavage characteristics with reduced and shorter river patterns. The base material and weld fracture micro-morphology are primarily defined by the presence of dimples.