Timothy C. Eisele
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Timothy C. Eisele has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
- Jeffrey Allen
Michigan Technological University
2 shared publications - Aaron S. Krieg
Michigan Technological University, Houghton, MI-49931, USA
1 shared publication - Akash Gawde1 shared publication
- Akintunde Stephen Samakinde
Department of Geological Engineering, Michigan Technological University, Houghton, USA
1 shared publication Andrew C. Abbott
1 shared publicationBrian Johnson
1 shared publication
Latest Publications
- Open Access
- 11 April 2026
- Published by Springer Nature in Mining, Metallurgy & Exploration
- Vol. 43 (3) , 2749-2764
Iron Ore Tailings Reprocessing by Electrostatic Separation Plus Two-Stage Froth Flotation
The reprocessing of tailings is crucial for recovering valuable iron and reducing the environmental impact associated with tailings disposal. The raw iron ore tailings used in this study had an initial iron oxide content of 24.05 wt% Fe 2 O 3 , as determined by ICP-OES analysis. This study investigates the practicality of tailings reprocessing to enhance iron oxide content by integrating electrostatic separation with a two-stage froth flotation process consisting of direct anionic flotation using oleic acid followed by reverse cationic flotation using amine collectors. The primary goal is to efficiently recover valuable iron from tailings, thereby reducing waste and promoting sustainable resource utilization. The process aims to upgrade the iron oxide content above 93 wt% Fe 2 O 3 , making the recovered material suitable for direct-reduced iron production. Electrostatic separation was first employed as a pre-concentration step to reject a substantial portion of silicate gangue and to partition the feed into tailings, middlings, and concentrate fractions. The middlings fraction was subsequently subjected to direct anionic flotation, enriching the iron oxide content to approximately 72.76 wt% Fe 2 O 3 and serving as an effective bulk separation stage, removing a significant portion of the non-iron-bearing components. Reverse flotation was then conducted separately on the direct flotation concentrate and on the electrostatic separation concentrate to further improve product purity. This integrated approach produced final iron oxide concentrate of approximately 96.90 wt% Fe 2 O 3 . The final concentrate exhibits high iron oxide content with low gangue and impurity levels, demonstrating potential suitability as a feedstock for direct-reduced iron (DRI) production, subject to final industrial qualification. Overall, the results demonstrate a promising beneficiation strategy for iron ore tailings valorization while reducing reliance on primary iron ore resources.
- 11 April 2026
- Published by Springer Nature in Mining, Metallurgy & Exploration
- Vol. 43 (3) , 2749-2764
Open AccessIron Ore Tailings Reprocessing by Electrostatic Separation Plus Two-Stage Froth Flotation
The reprocessing of tailings is crucial for recovering valuable iron and reducing the environmental impact associated with tailings disposal. The raw iron ore tailings used in this study had an initial iron oxide content of 24.05 wt% Fe 2 O 3 , as determined by ICP-OES analysis. This study investigates the practicality of tailings reprocessing to enhance iron oxide content by integrating electrostatic separation with a two-stage froth flotation process consisting of direct anionic flotation using oleic acid followed by reverse cationic flotation using amine collectors. The primary goal is to efficiently recover valuable iron from tailings, thereby reducing waste and promoting sustainable resource utilization. The process aims to upgrade the iron oxide content above 93 wt% Fe 2 O 3 , making the recovered material suitable for direct-reduced iron production. Electrostatic separation was first employed as a pre-concentration step to reject a substantial portion of silicate gangue and to partition the feed into tailings, middlings, and concentrate fractions. The middlings fraction was subsequently subjected to direct anionic flotation, enriching the iron oxide content to approximately 72.76 wt% Fe 2 O 3 and serving as an effective bulk separation stage, removing a significant portion of the non-iron-bearing components. Reverse flotation was then conducted separately on the direct flotation concentrate and on the electrostatic separation concentrate to further improve product purity. This integrated approach produced final iron oxide concentrate of approximately 96.90 wt% Fe 2 O 3 . The final concentrate exhibits high iron oxide content with low gangue and impurity levels, demonstrating potential suitability as a feedstock for direct-reduced iron (DRI) production, subject to final industrial qualification. Overall, the results demonstrate a promising beneficiation strategy for iron ore tailings valorization while reducing reliance on primary iron ore resources.
- 19 June 2025
- Published by Elsevier in Advances In Space Research
- Vol. 76 (5) , 3048-3059
Thermal prospecting for lunar water with a percussive hot cone penetrometer
- 19 June 2025
- Published by Elsevier in Advances In Space Research
- Vol. 76 (5) , 3048-3059
Thermal prospecting for lunar water with a percussive hot cone penetrometer
- Open Access
- 28 June 2024
- Published by Office of Scientific and Technical Information (OSTI)
In-Situ Bioleaching of Manganese by Dissimilatory Reduction
This report describes the development of a biological leaching process for recovery of manganese from low-grade ores, with a high degree of selectivity against contaminants such as iron. This results in the production of manganese that is suitable for battery manufacture and other electrical applications. The leaching process makes use of a community of metal reducing organisms that solubilize manganese at a pH of approximately 4.5. These organisms are nourished by simple organic molecules such as acetate that are generated by decomposition of biomass. A series of long-term laboratory experiments were carried out to determine the necessary operating parameters, followed by construction of a small pilot plant processing approximately 100 kg of ore. This pilot unit was operated for two years, demonstrating the ability to consistently produce high-grade manganese at a commercially viable rate.
- 28 June 2024
- Published by Office of Scientific and Technical Information (OSTI)
Open AccessIn-Situ Bioleaching of Manganese by Dissimilatory Reduction
This report describes the development of a biological leaching process for recovery of manganese from low-grade ores, with a high degree of selectivity against contaminants such as iron. This results in the production of manganese that is suitable for battery manufacture and other electrical applications. The leaching process makes use of a community of metal reducing organisms that solubilize manganese at a pH of approximately 4.5. These organisms are nourished by simple organic molecules such as acetate that are generated by decomposition of biomass. A series of long-term laboratory experiments were carried out to determine the necessary operating parameters, followed by construction of a small pilot plant processing approximately 100 kg of ore. This pilot unit was operated for two years, demonstrating the ability to consistently produce high-grade manganese at a commercially viable rate.
- 30 May 2024
- Published by Elsevier in Composites Part B: Engineering
- Vol. 282
Carbon nanotube as a conductive rheological modifier for carbon fiber-reinforced epoxy 3D printing inks
- 30 May 2024
- Published by Elsevier in Composites Part B: Engineering
- Vol. 282
Carbon nanotube as a conductive rheological modifier for carbon fiber-reinforced epoxy 3D printing inks
- Open Access
- 31 March 2006
- Published by Office of Scientific and Technical Information (OSTI)
Novel Binders and Methods for Agglomeration of Ore
Many metal extraction operations, such as leaching of copper, leaching of precious metals, and reduction of metal oxides to metal in high-temperature furnaces, require agglomeration of ore to ensure that reactive liquids or gases are evenly distributed throughout the ore being processed. Agglomeration of ore into coarse, porous masses achieves this even distribution of fluids by preventing fine particles from migrating and clogging the spaces and channels between the larger ore particles. Binders are critically necessary to produce agglomerates that will not break down during processing. However, for many important metal extraction processes there are no binders known that will work satisfactorily at a reasonable cost. A primary example of this is copper heap leaching, where there are no binders currently encountered in this acidic environment process. As a result, operators of many facilities see a large loss of process efficiency due to their inability to take advantage of agglomeration. The large quantities of ore that must be handled in metal extraction processes also means that the binder must be inexpensive and useful at low dosages to be economical. The acid-resistant binders and agglomeration procedures developed in this project will also be adapted for use in improving the energy efficiencymore » and performance of a broad range of mineral agglomeration applications, particularly heap leaching. The active involvement of our industrial partners will help to ensure rapid commercialization of any agglomeration technologies developed by this project. « less
- 31 March 2006
- Published by Office of Scientific and Technical Information (OSTI)
Open AccessNovel Binders and Methods for Agglomeration of Ore
Many metal extraction operations, such as leaching of copper, leaching of precious metals, and reduction of metal oxides to metal in high-temperature furnaces, require agglomeration of ore to ensure that reactive liquids or gases are evenly distributed throughout the ore being processed. Agglomeration of ore into coarse, porous masses achieves this even distribution of fluids by preventing fine particles from migrating and clogging the spaces and channels between the larger ore particles. Binders are critically necessary to produce agglomerates that will not break down during processing. However, for many important metal extraction processes there are no binders known that will work satisfactorily at a reasonable cost. A primary example of this is copper heap leaching, where there are no binders currently encountered in this acidic environment process. As a result, operators of many facilities see a large loss of process efficiency due to their inability to take advantage of agglomeration. The large quantities of ore that must be handled in metal extraction processes also means that the binder must be inexpensive and useful at low dosages to be economical. The acid-resistant binders and agglomeration procedures developed in this project will also be adapted for use in improving the energy efficiencymore » and performance of a broad range of mineral agglomeration applications, particularly heap leaching. The active involvement of our industrial partners will help to ensure rapid commercialization of any agglomeration technologies developed by this project. « less
- 1 July 2005
- Published by Taylor & Francis in Mineral Processing and Extractive Metallurgy Review
- Vol. 26 (3-4) , 295-305
WATER CHEMISTRY EFFECTS IN IRON ORE CONCENTRATE AGGLOMERATION FEED
In two different iron ore processing plants, it was demonstrated that when magnetite concentrate was filtered to prepare it for use as pelletization feed, the moisture that remained in the filter cake had greatly elevated levels of cations compared to the water removed by the filtration process. In particular, calcium concentrations in the filter cake were 565 times higher than in the filtrate water in Plant 1 and 19.4 times higher than the filtrate water in Plant 2. This effect is due to the adsorption of divalent cations on the magnetite surfaces resulting from electrostatic attraction when the pH of the solution is in the range where magnetite has a negative Zeta potential. Measurements of the Zeta potential as a function of pH for magnetite from Plant 2 determined that its point of zero charge (PZC) occurred at pH 3.0 to 3.5, which was much lower than is commonly reported in the literature and demonstrates that the PZC for magnetite is much more variable than is commonly thought. Plant experiments were carried out using carbon dioxide to reduce the pH of filter slurry so that the PZC could be approached. This was intended to allow adsorbed cations to be released from the magnetite surfaces during filtration. The pH adjustment was demonstrated to improve filtration rates by as much as 23%.
- 1 July 2005
- Published by Taylor & Francis in Mineral Processing and Extractive Metallurgy Review
- Vol. 26 (3-4) , 295-305
WATER CHEMISTRY EFFECTS IN IRON ORE CONCENTRATE AGGLOMERATION FEED
In two different iron ore processing plants, it was demonstrated that when magnetite concentrate was filtered to prepare it for use as pelletization feed, the moisture that remained in the filter cake had greatly elevated levels of cations compared to the water removed by the filtration process. In particular, calcium concentrations in the filter cake were 565 times higher than in the filtrate water in Plant 1 and 19.4 times higher than the filtrate water in Plant 2. This effect is due to the adsorption of divalent cations on the magnetite surfaces resulting from electrostatic attraction when the pH of the solution is in the range where magnetite has a negative Zeta potential. Measurements of the Zeta potential as a function of pH for magnetite from Plant 2 determined that its point of zero charge (PZC) occurred at pH 3.0 to 3.5, which was much lower than is commonly reported in the literature and demonstrates that the PZC for magnetite is much more variable than is commonly thought. Plant experiments were carried out using carbon dioxide to reduce the pH of filter slurry so that the PZC could be approached. This was intended to allow adsorbed cations to be released from the magnetite surfaces during filtration. The pH adjustment was demonstrated to improve filtration rates by as much as 23%.