Jixin Chen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Jixin Chen has a total of 37 co-authors. Here are the top co-authors by number of shared publications:
Meishuan Li
Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Peoples R China
6 shared publicationsHao Zhang
5 shared publicationsYongheng Zhang
5 shared publicationsGuorui Zhao
3 shared publicationsJinxing Yang
Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Peoples R China
3 shared publicationsMinmin Hu
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 110016, China
3 shared publications
Latest Publications
- 1 January 2026
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 41 (1) , 37
Preparation and Properties of Ytterbium Aluminosilicate Glass and SiC Modified h-BN-based Composites
- 1 January 2026
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 41 (1) , 37
Preparation and Properties of Ytterbium Aluminosilicate Glass and SiC Modified h-BN-based Composites
- 15 April 2025
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 20 (1) , 347-361
Research on the Influence of Raw Material Microstructures and Properties on the Quality of the Face-Coat in Ceramic Shell
- 15 April 2025
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 20 (1) , 347-361
Research on the Influence of Raw Material Microstructures and Properties on the Quality of the Face-Coat in Ceramic Shell
- 11 March 2025
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 45 (10)
Hexagonal boron nitride ceramic reinforced with a dispersed glass phase and microdomain-extruded glass fibers
- 11 March 2025
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 45 (10)
Hexagonal boron nitride ceramic reinforced with a dispersed glass phase and microdomain-extruded glass fibers
- 2 August 2024
- Published by Elsevier in Journal of Non-Crystalline Solids
- Vol. 642
Bulk ytterbium aluminosilicate glass with excellent mechanical properties and plasma etching resistance
- 2 August 2024
- Published by Elsevier in Journal of Non-Crystalline Solids
- Vol. 642
Bulk ytterbium aluminosilicate glass with excellent mechanical properties and plasma etching resistance
- 27 July 2023
- Published by Elsevier in Journal of Materials Science & Technology
- Vol. 171, 209-221
Hydrolysis mechanism of YbB2C2 and the microstructure of the carbon derived from the hydrolysis reaction
- 27 July 2023
- Published by Elsevier in Journal of Materials Science & Technology
- Vol. 171, 209-221
Hydrolysis mechanism of YbB2C2 and the microstructure of the carbon derived from the hydrolysis reaction
- Open Access
- 1 January 2022
- Published by Elsevier in SSRN Electronic Journal
Preparation and Properties of Ytterbium Aluminosilicate Glasses
In this work, bulk ytterbium aluminosilicate glasses were prepared by h-BN embedding method at 1800 oC under a flowing argon atmosphere. Yb2O3, Al2O3 and SiO2 powders were used as raw materials. The glass forming ability, mechanical properties, thermal properties and optical properties of the ytterbium aluminosilicate glasses were investigated. The results show that the composition 15Yb2O3-25Al2O3-60SiO2 (mol%) has the best glass forming ability and excellent properties. Its flexural strength, compressive strength and Vickers hardness are 166 ± 6 MPa, 1104 ± 59 MPa and 7.9 ± 0.2 GPa, respectively. The prepared glass is a kind of low thermal conductivity material (0.934 W·m-1·K-1 at 100 oC) with a high transformation temperature (847 oC). The average infrared transmittivity and refractive index are 74.24% and 2.25, respectively, in 1400-3000 nm wave-band.
- 1 January 2022
- Published by Elsevier in SSRN Electronic Journal
Open AccessPreparation and Properties of Ytterbium Aluminosilicate Glasses
In this work, bulk ytterbium aluminosilicate glasses were prepared by h-BN embedding method at 1800 oC under a flowing argon atmosphere. Yb2O3, Al2O3 and SiO2 powders were used as raw materials. The glass forming ability, mechanical properties, thermal properties and optical properties of the ytterbium aluminosilicate glasses were investigated. The results show that the composition 15Yb2O3-25Al2O3-60SiO2 (mol%) has the best glass forming ability and excellent properties. Its flexural strength, compressive strength and Vickers hardness are 166 ± 6 MPa, 1104 ± 59 MPa and 7.9 ± 0.2 GPa, respectively. The prepared glass is a kind of low thermal conductivity material (0.934 W·m-1·K-1 at 100 oC) with a high transformation temperature (847 oC). The average infrared transmittivity and refractive index are 74.24% and 2.25, respectively, in 1400-3000 nm wave-band.
- 6 February 2021
- Published by Elsevier in Acta Metallurgica Sinica (English Letters)
- Vol. 34 (7) , 1021-1027
Raman Spectroscopy of Layered Compound YbB2C2
- 6 February 2021
- Published by Elsevier in Acta Metallurgica Sinica (English Letters)
- Vol. 34 (7) , 1021-1027
Raman Spectroscopy of Layered Compound YbB2C2
- Open Access
- 19 November 2020
- Published by Springer Nature in Scientific Reports
- Vol. 10 (1) , 1-10
Unique chemical activity in porous YbB2C2 ceramics with high porosity and high compressive strength
High purity layered YbB2C2 powder is synthesized by a boro/carbothermic reduction method using YbBO3, B4C and graphite powders as raw materials. Its X-ray diffraction data are presented, and the space group P4/mbm (No. 127) is confirmed. The lattice parameters are a = b = 5.3389 Å and c = 3.5683 Å, and the atom positions are Yb (0.0000, 0.0000, 0.0000), B (0.3621, 0.8621, 0.5000), and C (0.1606, 0.6606, 0.5000). Porous YbB2C2 ceramics have a high porosity in the range of 69.89–58.11% and a high compressive strength in the range of 19.49–63.44 MPa. Furthermore, the as-produced porous YbB2C2 ceramics show unique chemical activity. Porous YbB2C2 ceramic with a porosity of 69.89% emits so much heat that it can burn a piece of paper when this ceramic is wetted by water. The rate of reaction between the porous YbB2C2 ceramic and water can be simply controlled by adjusting the porosity. The solid reaction products are YbB6, C and an unknown amorphous phase.
- 19 November 2020
- Published by Springer Nature in Scientific Reports
- Vol. 10 (1) , 1-10
Open AccessUnique chemical activity in porous YbB2C2 ceramics with high porosity and high compressive strength
High purity layered YbB2C2 powder is synthesized by a boro/carbothermic reduction method using YbBO3, B4C and graphite powders as raw materials. Its X-ray diffraction data are presented, and the space group P4/mbm (No. 127) is confirmed. The lattice parameters are a = b = 5.3389 Å and c = 3.5683 Å, and the atom positions are Yb (0.0000, 0.0000, 0.0000), B (0.3621, 0.8621, 0.5000), and C (0.1606, 0.6606, 0.5000). Porous YbB2C2 ceramics have a high porosity in the range of 69.89–58.11% and a high compressive strength in the range of 19.49–63.44 MPa. Furthermore, the as-produced porous YbB2C2 ceramics show unique chemical activity. Porous YbB2C2 ceramic with a porosity of 69.89% emits so much heat that it can burn a piece of paper when this ceramic is wetted by water. The rate of reaction between the porous YbB2C2 ceramic and water can be simply controlled by adjusting the porosity. The solid reaction products are YbB6, C and an unknown amorphous phase.
- 1 December 2018
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 38 (15) , 4867-4873
Mechanical and thermal properties of h-BN based composite containing dual glass phases at elevated temperatures
- 1 December 2018
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 38 (15) , 4867-4873
Mechanical and thermal properties of h-BN based composite containing dual glass phases at elevated temperatures
- Open Access
- 21 November 2018
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 7 (4) , 317-324
Microstructure and mechanical properties of h-BN/Yb4Si2O7N2 composites
A series of h-BN based composites with Yb4Si2O7N2 as a secondary phase were successfully synthesized by an in situ reaction hot pressing method. It was found that the relative density and room-temperature mechanical properties monotonically increased with increasing the content of Yb4Si2O7N2 from 20 to 50 vol%. When 50 vol% Yb4Si2O7N2 was introduced, the relative density of the composite reached 98.75%, and its flexural strength, compressive strength, fracture toughness, and hardness reached 338±10 MPa, 803±49 MPa, 2.06±0.06 MPa·m1/2, and 2.69±0.10 GPa, respectively. The strengthening effect of Yb4Si2O7N2 was mainly attributed to its high modulus and high hardness. Fine microstructure was also advantageous to strength and could lead to more tortuous crack propagation paths and then improve the fracture toughness of the composites simultaneously. Meanwhile, the composites maintained good machinability.
- 21 November 2018
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 7 (4) , 317-324
Open AccessMicrostructure and mechanical properties of h-BN/Yb4Si2O7N2 composites
A series of h-BN based composites with Yb4Si2O7N2 as a secondary phase were successfully synthesized by an in situ reaction hot pressing method. It was found that the relative density and room-temperature mechanical properties monotonically increased with increasing the content of Yb4Si2O7N2 from 20 to 50 vol%. When 50 vol% Yb4Si2O7N2 was introduced, the relative density of the composite reached 98.75%, and its flexural strength, compressive strength, fracture toughness, and hardness reached 338±10 MPa, 803±49 MPa, 2.06±0.06 MPa·m1/2, and 2.69±0.10 GPa, respectively. The strengthening effect of Yb4Si2O7N2 was mainly attributed to its high modulus and high hardness. Fine microstructure was also advantageous to strength and could lead to more tortuous crack propagation paths and then improve the fracture toughness of the composites simultaneously. Meanwhile, the composites maintained good machinability.