Bahtiyor Medeshev
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Bahtiyor Medeshev has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- A. D. Mamitova
Auezov South Kazakhstan State University
2 shared publications - Alexandr Kolesnikov
Department of Life Safety and Environmental Protection, M. Auezov South Kazakhstan University, Shymkent 160012, Kazakhstan
2 shared publications - Olga Kolesnikova
Scientific Research Laboratory «Building Materials, Construction and Architecture», M. Auezov South Kazakhstan University, Shymkent 160012, Kazakhstan
2 shared publications - Aigali Donayev
Department of Life Safety and Environmental Protection, M. Auezov South Kazakhstan University, Shymkent 160012, Kazakhstan
1 shared publication - Askat Yessenaliyev
Civil Law and Civil Procedure, M.Auezov South Kazakhstan State University, Shymkent, Kazakhstan, Kazakhstan
1 shared publication - Gulbanu Baisarova
Department of Construction Engineering, NAO “Caspian University of Technology and Engineering Named After Sh. Yessenov”, Aktau 130002, Kazakhstan
1 shared publication
Latest Publications
- Open Access
- 30 October 2026
- Published by MDPI AG in Journal of Composites Science
- Vol. 10 (11) , 585
Physico-Chemical Studies of the Formation of the Main Minerals of Cement Clinker and Zinc Sublimation Using Thermodynamic Modeling
The paper presents the results of thermodynamic modeling of the processes of formation of the main minerals of Portland cement clinker (alite C3S, belite C2S, tricalcium aluminate C3A and fourcalcium alumoferrite C4AF) when tailings containing zinc oxide (ZnO) and zinc carbonate (ZnCO3) are introduced into the feedstock. The study was performed using the HSC Chemistry 6.0 software package and the SGTE database in the temperature range of 500–1500 °C. The relevance of the work is due to the need to dispose of large-tonnage zinc-containing man-made waste as a secondary raw material. The standard clinker formation reaction is compared with model reactions involving ZnO and ZnCO3, and the sequence of transformations of zinc-containing compounds in the Zn–C-O system is studied. It is shown that at 500 °C the Gibbs energy of the clinker formation reaction with ZnO is +965.9 kJ, whereas for the reaction with ZnCO3 it is +839.6 kJ. The temperatures at which the condition ΔG ≈ 0 is reached are about 1057 °C for the reaction with ZnO and 906 °C for the reaction with ZnCO3. At a temperature of 1450 °C, the reaction with ZnCO3 is characterized by a more negative value of ΔG (−900.0 kJ) compared with the variant with ZnO (−540.0 kJ). Additional analysis showed the sequence of transformations ZnCO3 → ZnO → Zn(g). The reduction of ZnO by carbon becomes thermodynamically possible at about 950 °C, while the reaction of ZnO with CO reaches the condition ΔG ≈ 0 at about 1317 °C. The direct dissociation of ZnO with the formation of Zn and O2 remains thermodynamically unfavorable in the range of 500–1500 °C. The results obtained indicate the fundamental possibility of combining clinker formation and zinc distillation during high-temperature tailings processing, followed by the capture of the zinc-containing gas phase.
- 30 October 2026
- Published by MDPI AG in Journal of Composites Science
- Vol. 10 (11) , 585
Open AccessPhysico-Chemical Studies of the Formation of the Main Minerals of Cement Clinker and Zinc Sublimation Using Thermodynamic Modeling
The paper presents the results of thermodynamic modeling of the processes of formation of the main minerals of Portland cement clinker (alite C3S, belite C2S, tricalcium aluminate C3A and fourcalcium alumoferrite C4AF) when tailings containing zinc oxide (ZnO) and zinc carbonate (ZnCO3) are introduced into the feedstock. The study was performed using the HSC Chemistry 6.0 software package and the SGTE database in the temperature range of 500–1500 °C. The relevance of the work is due to the need to dispose of large-tonnage zinc-containing man-made waste as a secondary raw material. The standard clinker formation reaction is compared with model reactions involving ZnO and ZnCO3, and the sequence of transformations of zinc-containing compounds in the Zn–C-O system is studied. It is shown that at 500 °C the Gibbs energy of the clinker formation reaction with ZnO is +965.9 kJ, whereas for the reaction with ZnCO3 it is +839.6 kJ. The temperatures at which the condition ΔG ≈ 0 is reached are about 1057 °C for the reaction with ZnO and 906 °C for the reaction with ZnCO3. At a temperature of 1450 °C, the reaction with ZnCO3 is characterized by a more negative value of ΔG (−900.0 kJ) compared with the variant with ZnO (−540.0 kJ). Additional analysis showed the sequence of transformations ZnCO3 → ZnO → Zn(g). The reduction of ZnO by carbon becomes thermodynamically possible at about 950 °C, while the reaction of ZnO with CO reaches the condition ΔG ≈ 0 at about 1317 °C. The direct dissociation of ZnO with the formation of Zn and O2 remains thermodynamically unfavorable in the range of 500–1500 °C. The results obtained indicate the fundamental possibility of combining clinker formation and zinc distillation during high-temperature tailings processing, followed by the capture of the zinc-containing gas phase.
- Open Access
- 6 August 2024
- Published by MDPI AG in Journal of Composites Science
- Vol. 8 (8) , 306
Investigation of the Physico-Chemical and Mechanical Properties of Expanded Ceramsite Granules Made on the Basis of Coal Mining Waste
In this article, one of the main scientific directions was the search for ways of recycling coal mining waste to produce expanded clay granules. There are a number of scientific studies devoted to the use of various industrial wastes in the production of thermal insulation and fireproof expanded clay granules. The authors consider the production of granular porous aggregates based on pulverized fractions of igneous rocks—basalt, granite, and synertite, as well as man-made materials of various origins, to be promising. According to the results of the conducted studies, it was found that the optimal interval of the amount of waste in expanded clay was 4.0–6.0%, and the optimal firing temperature was 1150 °C with the production of samples with a bulk density of 0.337–0.348 t/m3 and with a compressive strength of 1.37–1.51 MPa under these conditions.
- 6 August 2024
- Published by MDPI AG in Journal of Composites Science
- Vol. 8 (8) , 306
Open AccessInvestigation of the Physico-Chemical and Mechanical Properties of Expanded Ceramsite Granules Made on the Basis of Coal Mining Waste
In this article, one of the main scientific directions was the search for ways of recycling coal mining waste to produce expanded clay granules. There are a number of scientific studies devoted to the use of various industrial wastes in the production of thermal insulation and fireproof expanded clay granules. The authors consider the production of granular porous aggregates based on pulverized fractions of igneous rocks—basalt, granite, and synertite, as well as man-made materials of various origins, to be promising. According to the results of the conducted studies, it was found that the optimal interval of the amount of waste in expanded clay was 4.0–6.0%, and the optimal firing temperature was 1150 °C with the production of samples with a bulk density of 0.337–0.348 t/m3 and with a compressive strength of 1.37–1.51 MPa under these conditions.