Jochen Markert
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Jochen Markert has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Andreas J. Beinert
Fraunhofer Institute for Solar Energy Systems image/svg+xml
2 shared publications Daniel Philipp
Fraunhofer Institute for Solar Energy Systems ISE, Freiburg, Germany
2 shared publicationsDennys Koch
RWE Renewables GmbH
1 shared publication- Enzo Job
Fraunhofer Institute for Solar Energy Systems
1 shared publication - Frank Ensslen
Fraunhofer Institute for Solar Energy Systems
1 shared publication Ingrid Haedrich
Fraunhofer Institute for Solar Energy Systems ISE, Freiburg, Germany
1 shared publication
Latest Publications
- Open Access
- 10 November 2026
- Published by TIB Open Publishing in PV-Symposium Proceedings
- Vol. 3
Influence of the Mounting Clamps and Adhesive Joint on Glass Breakage of PV Modules
This study investigates how mounting clamp geometry and adhesive joint quality influence glass fracture in glass-glass PV modules. Combining field fracture analysis with finite element method modeling (FEM), the work identifies the mounting clamp region as a frequent initiation point for glass fractures in glass-glass modules (~2 mm glass, >2.5 m²). Fracture pattern analysis reveals origins at the front glass near the clamp edge, confirmed by FEM stress concentrations around the clamp. Experimental observations show frequent off-center PV-laminate positioning and inhomogeneous adhesive distribution, creating zones of direct glass–frame contact that enhance fracture risk. Two clamp designs are compared: a grounding-groove clamp and a flat-contact clamp. FEM results demonstrate that, under identical torque, clamps with grounding grooves produce significantly higher first principal stresses (tensile stress equivalent) in the glass (e.g., 75 MPa at 18 Nm vs. 26 MPa for flat clamps), due to lever-arm effects and frame deformation transferring load to the front glass. The adhesive joint quality influence these stresses: an ideal adhesive joint reduces localized stresses by distributing forces, whereas a missing front adhesive joint increases tensile stress and promotes fracture. Conclusions emphasize that grounding grooves in clamps can elevate fracture risk, especially with incomplete front adhesive joints, and that FEM is a robust predictive tool to screen clamp designs before manufacturing.
- 10 November 2026
- Published by TIB Open Publishing in PV-Symposium Proceedings
- Vol. 3
Open AccessInfluence of the Mounting Clamps and Adhesive Joint on Glass Breakage of PV Modules
This study investigates how mounting clamp geometry and adhesive joint quality influence glass fracture in glass-glass PV modules. Combining field fracture analysis with finite element method modeling (FEM), the work identifies the mounting clamp region as a frequent initiation point for glass fractures in glass-glass modules (~2 mm glass, >2.5 m²). Fracture pattern analysis reveals origins at the front glass near the clamp edge, confirmed by FEM stress concentrations around the clamp. Experimental observations show frequent off-center PV-laminate positioning and inhomogeneous adhesive distribution, creating zones of direct glass–frame contact that enhance fracture risk. Two clamp designs are compared: a grounding-groove clamp and a flat-contact clamp. FEM results demonstrate that, under identical torque, clamps with grounding grooves produce significantly higher first principal stresses (tensile stress equivalent) in the glass (e.g., 75 MPa at 18 Nm vs. 26 MPa for flat clamps), due to lever-arm effects and frame deformation transferring load to the front glass. The adhesive joint quality influence these stresses: an ideal adhesive joint reduces localized stresses by distributing forces, whereas a missing front adhesive joint increases tensile stress and promotes fracture. Conclusions emphasize that grounding grooves in clamps can elevate fracture risk, especially with incomplete front adhesive joints, and that FEM is a robust predictive tool to screen clamp designs before manufacturing.
- Open Access
- 7 November 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 15 (1) , 24-29
Comparison of Commercial TOPCon PV Modules in Accelerated Aging Tests
Tunnel oxide passivated contact (TOPCon) is set to become the new mainstream cell technology despite pending reliability concerns. This work compares commercially available TOPCon photovoltaic (PV) module types from five different manufacturers in a variety of electrical characterization and accelerated aging tests. This case study represents a selection process of PV modules for larger PV installations. Therefore, the work features an in-depth comparison of the electrical performance (energy rating) that can serve as a reference for state-of-the-art TOPCon modules. The aging results confirm previously reported degradation mechanisms of the TOPCon technology due to humidity ingress. In the case of UV aging, a new pattern of strong degradation (up to –12% after 60 kWh/m 2 ;) and subsequent recovery after humidity freeze test is presented, which could have implications on the results of certification tests (IEC61730-2, Sequence B). Though not directly connected to the TOPCon cell technology, the mechanical load tests revealed weaknesses of several module types, related to module dimensions, frame height, and glass properties. Based on the results, the necessity for more focused testing and technological development is highlighted.
- 7 November 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 15 (1) , 24-29
Open AccessComparison of Commercial TOPCon PV Modules in Accelerated Aging Tests
Tunnel oxide passivated contact (TOPCon) is set to become the new mainstream cell technology despite pending reliability concerns. This work compares commercially available TOPCon photovoltaic (PV) module types from five different manufacturers in a variety of electrical characterization and accelerated aging tests. This case study represents a selection process of PV modules for larger PV installations. Therefore, the work features an in-depth comparison of the electrical performance (energy rating) that can serve as a reference for state-of-the-art TOPCon modules. The aging results confirm previously reported degradation mechanisms of the TOPCon technology due to humidity ingress. In the case of UV aging, a new pattern of strong degradation (up to –12% after 60 kWh/m 2 ;) and subsequent recovery after humidity freeze test is presented, which could have implications on the results of certification tests (IEC61730-2, Sequence B). Though not directly connected to the TOPCon cell technology, the mechanical load tests revealed weaknesses of several module types, related to module dimensions, frame height, and glass properties. Based on the results, the necessity for more focused testing and technological development is highlighted.
- Open Access
- 5 August 2024
- Published by TIB Open Publishing in PV-Symposium Proceedings
- Vol. 1
Mechanical Stability of PV Modules
A significant increase in reported glass breakages from the field was recognized during the past three years, where a disproportionately high number of modules were affected by glass breakage. Different substructures and module designs are affected, framed and unframed modules, tracked and fixed systems. What all inquiries have in common, however, is that modules with a double-glazed design with ≤ 2.5 mm glass thicknesses are affected and the problems were observed after just a few months in field operation. Various factors such as heavy weather events, faulty installation or errors in the structural design could be excluded as root causes and our experience points on additional, more fundamental problems that are associated in particular with the continuing trend towards larger modules > 3 m2 and thinner module glass ≤ 2mm. Furthermore, it seems that the residual compressive surface stress of the glass as one major parameter that determines the stability of glass panes has not been considered in this context in the PV module industry yet. In this work, we focus on the glass thickness in combination with the compressive surface stress. Besides qualitative methods, one possibility to investigate the surface stress quantitatively is a scattered light polariscope (SCALP), previously used in the glass industry. In particular, the aim is to validate the SCALP measurement method for the use on PV modules. Furthermore, a potential correlation between the surface compressive stress and the mechanical stability of various common module designs with 2 mm and 1.6 mm glass is investigated.
- 5 August 2024
- Published by TIB Open Publishing in PV-Symposium Proceedings
- Vol. 1
Open AccessMechanical Stability of PV Modules
A significant increase in reported glass breakages from the field was recognized during the past three years, where a disproportionately high number of modules were affected by glass breakage. Different substructures and module designs are affected, framed and unframed modules, tracked and fixed systems. What all inquiries have in common, however, is that modules with a double-glazed design with ≤ 2.5 mm glass thicknesses are affected and the problems were observed after just a few months in field operation. Various factors such as heavy weather events, faulty installation or errors in the structural design could be excluded as root causes and our experience points on additional, more fundamental problems that are associated in particular with the continuing trend towards larger modules > 3 m2 and thinner module glass ≤ 2mm. Furthermore, it seems that the residual compressive surface stress of the glass as one major parameter that determines the stability of glass panes has not been considered in this context in the PV module industry yet. In this work, we focus on the glass thickness in combination with the compressive surface stress. Besides qualitative methods, one possibility to investigate the surface stress quantitatively is a scattered light polariscope (SCALP), previously used in the glass industry. In particular, the aim is to validate the SCALP measurement method for the use on PV modules. Furthermore, a potential correlation between the surface compressive stress and the mechanical stability of various common module designs with 2 mm and 1.6 mm glass is investigated.