Olha Sereda
Olha Sereda has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
- Gaëtan Bernard
Additive Manufacturing and Component Reliability Group, CSEM SA, Rue Jaquet-Droz 1, CH-2002 Neuchâtel, Switzerland
3 shared publications - Roland E. Loge
Thermomechanical Metallurgy Laboratory, PX Group Chair École Polytechnique Fédérale de Lausanne (EPFL) Neuchâtel CH‐2002 Switzerland
3 shared publications - Vaclav Pejchal
Centre Suisse d’Electronique et de Microtechnique (CSEM), Jaquet Droz 1, CH-2002 Neuchȃtel, Switzerland
3 shared publications
Latest Publications
- Open Access
Tensile Properties of Ex-Situ Ti-TiC Metal Matrix Composites Manufactured by Laser Powder Bed Fusion
Titanium-based Metal Matrix Composites (MMCs) manufactured by additive manufacturing offer tremendous lightweighting opportunities. However, processing the high reinforcement contents needed to substantially improve elastic modulus while conserving significant ductility remains a challenge. Ti-TiC MMCs fabricated in this study reported fracture strains in tension up to 1.7% for a Young’s modulus of 149 GPa. This fracture strain is 30% higher than the previously reported values for Ti-based MMCs produced by Laser Powder Bed Fusion (LPBF) displaying similar Young’s moduli. The heat treatment used after the LPBF process leads to the doubling of the fracture strain thanks to the conversion of TiCx dendrites into equiaxed TiCx grains. The as-built microstructure shows both un-dissolved TiC particles and sub-stoichiometric TiC dendrites resulting from the partial dissolution of TiC particles. The reduction of the C/Ti ratio in TiC during the process results in an increase in the reinforcement content, from a nominal 12 vol% to an effective 21.5 vol%. The variation of the TiC lattice constant with its stoichiometry is measured, and an empirical expression is proposed for its effect on TiC’s Young’s modulus. The lower TiC powder size distribution displayed higher mechanical properties thanks to a reduced number of intrinsic flaws.
Open AccessTensile Properties of Ex-Situ Ti-TiC Metal Matrix Composites Manufactured by Laser Powder Bed Fusion
Titanium-based Metal Matrix Composites (MMCs) manufactured by additive manufacturing offer tremendous lightweighting opportunities. However, processing the high reinforcement contents needed to substantially improve elastic modulus while conserving significant ductility remains a challenge. Ti-TiC MMCs fabricated in this study reported fracture strains in tension up to 1.7% for a Young’s modulus of 149 GPa. This fracture strain is 30% higher than the previously reported values for Ti-based MMCs produced by Laser Powder Bed Fusion (LPBF) displaying similar Young’s moduli. The heat treatment used after the LPBF process leads to the doubling of the fracture strain thanks to the conversion of TiCx dendrites into equiaxed TiCx grains. The as-built microstructure shows both un-dissolved TiC particles and sub-stoichiometric TiC dendrites resulting from the partial dissolution of TiC particles. The reduction of the C/Ti ratio in TiC during the process results in an increase in the reinforcement content, from a nominal 12 vol% to an effective 21.5 vol%. The variation of the TiC lattice constant with its stoichiometry is measured, and an empirical expression is proposed for its effect on TiC’s Young’s modulus. The lower TiC powder size distribution displayed higher mechanical properties thanks to a reduced number of intrinsic flaws.
- Open Access
- 14 October 2024
- Published by MDPI AG in Preprints.org
Tensile Properties of Ex-Situ Ti-TiC Metal Matrix Composites Manufactured by Laser Powder Bed Fusion
Titanium-based Metal Matrix Composites (MMCs) manufactured by additive manufacturing offer tremendous lightweighting opportunities. However, processing the high reinforcement contents needed to substantially improve elastic modulus while conserving significant ductility remains a challenge. Ti-TiC MMCs fabricated in this study report fracture strains in tension up to 1.7% for a Young’s modulus of 149 GPa. This fracture strain is 30% higher than previously reported values for Ti-based MMCs produced by Laser Powder Bed Fusion (LPBF) displaying similar Young’s moduli. The heat treatment used after the LPBF process leads to the doubling of the fracture strain due to the conversion of TiCx dendrites into equiaxed TiCx grains. As-built microstructure shows both un-dissolved TiC particles and sub-stoichiometric TiC dendrites resulting from a partial dissolution of TiC particles. Reduction of the C/Ti ratio in TiC during the process results in an increase in the reinforcement content, from a nominal 12 vol% to an effective 21.5 vol%. The variation of the TiC lattice constant with its stoichiometry is measured, and an empirical expression is proposed for its effect on TiC’s Young’s modulus. The lower TiC initial powder size distribution displayed the best mechanical performance.
- 14 October 2024
- Published by MDPI AG in Preprints.org
Open AccessTensile Properties of Ex-Situ Ti-TiC Metal Matrix Composites Manufactured by Laser Powder Bed Fusion
Titanium-based Metal Matrix Composites (MMCs) manufactured by additive manufacturing offer tremendous lightweighting opportunities. However, processing the high reinforcement contents needed to substantially improve elastic modulus while conserving significant ductility remains a challenge. Ti-TiC MMCs fabricated in this study report fracture strains in tension up to 1.7% for a Young’s modulus of 149 GPa. This fracture strain is 30% higher than previously reported values for Ti-based MMCs produced by Laser Powder Bed Fusion (LPBF) displaying similar Young’s moduli. The heat treatment used after the LPBF process leads to the doubling of the fracture strain due to the conversion of TiCx dendrites into equiaxed TiCx grains. As-built microstructure shows both un-dissolved TiC particles and sub-stoichiometric TiC dendrites resulting from a partial dissolution of TiC particles. Reduction of the C/Ti ratio in TiC during the process results in an increase in the reinforcement content, from a nominal 12 vol% to an effective 21.5 vol%. The variation of the TiC lattice constant with its stoichiometry is measured, and an empirical expression is proposed for its effect on TiC’s Young’s modulus. The lower TiC initial powder size distribution displayed the best mechanical performance.
- Open Access
- 7 October 2024
- Published by MDPI AG in Preprints.org
In-Situ Fabrication of Ductile Ti-TiCx Metal Matrix Composite by Laser Powder Bed Fusion with Enhanced Elastic Modulus
The production of high stiffness Ti-based Metal Matrix Composites (Ti-MMCs) displaying significant ductility by additive manufacturing technologies is not yet at the level of conventionally produced Ti-MMCs. This study outlines the production process of stiffness-driven Ti-TiC MMCs displaying a remarkable ductility. The process consists in powder Mechanical Blending, Laser Powder Bed Fusion (LPBF), and a heat treatment. A TiC fraction of more than 20 vol% was formed in-situ through the reaction of titanium with carbon during the LPBF process. The as-built sub-stoichiometric TiC dendrites are converted in equiaxed TiC grains during the heat treatment. The TiC C/Ti ratio was found to be close to 0.5 in as-built conditions, and 0.7 in heat treated conditions, resulting in an effective reinforcement content nearly twice the one expected for stoichiometric TiC, leading to stronger reinforcement. The mechanical analysis revealed a Young’s modulus of up to 149 GPa and total elongations of up to 2.8%. The former represents a 27% improvement compared to commercially pure Titanium and the latter exceeds by 115% reported values for LPBF Ti-MMCs with similar Young’s modulus. It is enabled by the in-situ formation of defect-free TiC reinforcements combined with their globularisation through heat treatment.
- 7 October 2024
- Published by MDPI AG in Preprints.org
Open AccessIn-Situ Fabrication of Ductile Ti-TiCx Metal Matrix Composite by Laser Powder Bed Fusion with Enhanced Elastic Modulus
The production of high stiffness Ti-based Metal Matrix Composites (Ti-MMCs) displaying significant ductility by additive manufacturing technologies is not yet at the level of conventionally produced Ti-MMCs. This study outlines the production process of stiffness-driven Ti-TiC MMCs displaying a remarkable ductility. The process consists in powder Mechanical Blending, Laser Powder Bed Fusion (LPBF), and a heat treatment. A TiC fraction of more than 20 vol% was formed in-situ through the reaction of titanium with carbon during the LPBF process. The as-built sub-stoichiometric TiC dendrites are converted in equiaxed TiC grains during the heat treatment. The TiC C/Ti ratio was found to be close to 0.5 in as-built conditions, and 0.7 in heat treated conditions, resulting in an effective reinforcement content nearly twice the one expected for stoichiometric TiC, leading to stronger reinforcement. The mechanical analysis revealed a Young’s modulus of up to 149 GPa and total elongations of up to 2.8%. The former represents a 27% improvement compared to commercially pure Titanium and the latter exceeds by 115% reported values for LPBF Ti-MMCs with similar Young’s modulus. It is enabled by the in-situ formation of defect-free TiC reinforcements combined with their globularisation through heat treatment.