Huawei Sun
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Huawei Sun has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Juan Pu
School of Intelligent Manufacturing and Control Engineering, Shanghai Polytechnic University, Shanghai 201209, China
3 shared publications - Tingmu Chen
Fujian Special Equipment Inspection and Research Institute, National Quality Supervision and Inspection Center of Special Robot Product (Fujian), Quanzhou 362000, China
2 shared publications - Yubo Sun
School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China
2 shared publications - Yunxia Chen
School of Intelligent Manufacturing and Control Engineering, Shanghai Polytechnic University, Shanghai 201209, China
2 shared publications - Changhua Jiang
School of Intelligent Manufacturing and Control Engineering, Shanghai Polytechnic University, Shanghai 201209, China
1 shared publication - Di Wu
School of Intelligent Manufacturing and Control Engineering, Shanghai Polytechnic University, Shanghai 201209, China
1 shared publication
Latest Publications
- Open Access
The Effects of CeO2 Content on the Microstructure and Property of Duplex Stainless Steel Layer Obtained by Plasma Arc Cladding Technology
The mixture powders were designed by adding 0 wt.%~1.0 wt.% CeO2 into the 2205 duplex stainless steel (DSS) powders. The 2205 DSS cladding layer was prepared on the surface of Q345 steel by plasma arc cladding technology. The effects of different CeO2 contents on the macro-morphology, microstructure composition, and corrosion resistance of the cladding layer were studied. The action mechanism of CeO2 in the cladding layer was also discussed. The results showed that the addition of CeO2 modified the appearance and decreased the defect of the cladding layer. Also, the austenite grains were refined, and the austenite proportion was increased under the action of CeO2. When the CeO2 content was 0.5 wt.%, the appearance of the cladding layer was optimum; the austenite proportion in the upper cladding layer and the lower cladding layer reached up to 52.6% and 55.5%, respectively, and the crystal changed from columnar to equiaxed. CeO2 decomposes into Ce element and O element under the action of the plasma arc, after which Ce element is easily absorbed at the grain boundary to reduce the surface tension and improve the fluidity of the liquid metal so as to modify the appearance of the cladding layer. Meanwhile, Ce element primarily reacts with O, S, Al, and Si elements to form low-melting-point oxygen sulfides and are then removed, which eliminates the defect of the cladding layer. Moreover, the high melting point of CeO2 acts as heterogeneous nucleation sites during solidification, thus improving the value of nucleation rate/growth rate of the grain and promoting the transformation from ferrite to austenite. According to the electrochemical corrosion testing result, Ce element inhibited the enrichment of Cr element at grain boundaries and promoted the formation of Cr2O3, which improved the corrosion resistance of the 2205 DSS cladding layer. It was optimum with the CeO2 content of 0.5 wt.%.
Open AccessThe Effects of CeO2 Content on the Microstructure and Property of Duplex Stainless Steel Layer Obtained by Plasma Arc Cladding Technology
The mixture powders were designed by adding 0 wt.%~1.0 wt.% CeO2 into the 2205 duplex stainless steel (DSS) powders. The 2205 DSS cladding layer was prepared on the surface of Q345 steel by plasma arc cladding technology. The effects of different CeO2 contents on the macro-morphology, microstructure composition, and corrosion resistance of the cladding layer were studied. The action mechanism of CeO2 in the cladding layer was also discussed. The results showed that the addition of CeO2 modified the appearance and decreased the defect of the cladding layer. Also, the austenite grains were refined, and the austenite proportion was increased under the action of CeO2. When the CeO2 content was 0.5 wt.%, the appearance of the cladding layer was optimum; the austenite proportion in the upper cladding layer and the lower cladding layer reached up to 52.6% and 55.5%, respectively, and the crystal changed from columnar to equiaxed. CeO2 decomposes into Ce element and O element under the action of the plasma arc, after which Ce element is easily absorbed at the grain boundary to reduce the surface tension and improve the fluidity of the liquid metal so as to modify the appearance of the cladding layer. Meanwhile, Ce element primarily reacts with O, S, Al, and Si elements to form low-melting-point oxygen sulfides and are then removed, which eliminates the defect of the cladding layer. Moreover, the high melting point of CeO2 acts as heterogeneous nucleation sites during solidification, thus improving the value of nucleation rate/growth rate of the grain and promoting the transformation from ferrite to austenite. According to the electrochemical corrosion testing result, Ce element inhibited the enrichment of Cr element at grain boundaries and promoted the formation of Cr2O3, which improved the corrosion resistance of the 2205 DSS cladding layer. It was optimum with the CeO2 content of 0.5 wt.%.
- Open Access
Study on the Microstructure and Properties of Al Alloy/Steel CMT Welding–Brazing Joints Under Different Pulse Magnetic Field Intensities
Butt welding experiments on 6061 Al alloy and Q235B steel of 2 mm thickness were conducted using an ER4047F flux-cored wire as the filler metal, after adding a pulsed magnetic field into the process of cold metal transfer (CMT) welding. The effect of the pulsed magnetic field intensity on the macro morphology, microstructure, tensile strength and corrosion resistance of the welding–brazing joint was analyzed. The results showed that when the pulsed magnetic field intensity increased from 0 to 60 mT, the wettability and spreadability of the liquid metal were improved. As a result, the appearance of the Al alloy/steel joint was nice. However, when the pulsed magnetic field intensity was 80 mT, the stability of the arc and the forming quality of the joint decreased, which resulted in a deterioration in the appearance of the joint. A pulsed magnetic field with different intensities did not alter the microstructure of the joint. All of the joint was composed of θ-Fe2(Al,Si)5 and τ5-Al7.2Fe1.8Si at the interface and Al-Si eutectic phase and α-Al solid solution at the weld seam zone. Actually, with the pulsed magnetic field intensity increasing from 0 mT to 60 mT, the IMC thickness in the interfacial layer gradually reduced under the action of electromagnetic stirring. Also, the grain in the weld seam was refined, and elements were distributed uniformly. But when the pulsed magnetic field intensity was 80 mT, the grain in the weld seam began to coarsen, and the intermetallic compound (IMC) thickness was too small, which was unfavorable for the metallurgical bonding of Al alloy and steel. Therefore, with the increase in pulsed magnetic field intensity, the tensile strength of the joints first increased and then decreased, and it reached its maximum of 187.7 MPa with a pulsed magnetic field intensity of 60 mT. Similarly, the corrosion resistance of the joint first increased and then decreased, and it was best when the pulse magnetic field intensity was 60 mT. The Nyquist plot and Bode plot confirmed this result. The addition of a pulsed magnetic field caused less fluctuation in the anode current density, resulting in less localized corrosion of the joint using the scanning vibrating electrode technique (SVET). The XPS analysis showed the Al-Fe-Si compounds replacing the Fe-Al compounds in the joint was the main reason for improving its corrosion resistance under the action of a pulsed magnetic field.
Open AccessStudy on the Microstructure and Properties of Al Alloy/Steel CMT Welding–Brazing Joints Under Different Pulse Magnetic Field Intensities
Butt welding experiments on 6061 Al alloy and Q235B steel of 2 mm thickness were conducted using an ER4047F flux-cored wire as the filler metal, after adding a pulsed magnetic field into the process of cold metal transfer (CMT) welding. The effect of the pulsed magnetic field intensity on the macro morphology, microstructure, tensile strength and corrosion resistance of the welding–brazing joint was analyzed. The results showed that when the pulsed magnetic field intensity increased from 0 to 60 mT, the wettability and spreadability of the liquid metal were improved. As a result, the appearance of the Al alloy/steel joint was nice. However, when the pulsed magnetic field intensity was 80 mT, the stability of the arc and the forming quality of the joint decreased, which resulted in a deterioration in the appearance of the joint. A pulsed magnetic field with different intensities did not alter the microstructure of the joint. All of the joint was composed of θ-Fe2(Al,Si)5 and τ5-Al7.2Fe1.8Si at the interface and Al-Si eutectic phase and α-Al solid solution at the weld seam zone. Actually, with the pulsed magnetic field intensity increasing from 0 mT to 60 mT, the IMC thickness in the interfacial layer gradually reduced under the action of electromagnetic stirring. Also, the grain in the weld seam was refined, and elements were distributed uniformly. But when the pulsed magnetic field intensity was 80 mT, the grain in the weld seam began to coarsen, and the intermetallic compound (IMC) thickness was too small, which was unfavorable for the metallurgical bonding of Al alloy and steel. Therefore, with the increase in pulsed magnetic field intensity, the tensile strength of the joints first increased and then decreased, and it reached its maximum of 187.7 MPa with a pulsed magnetic field intensity of 60 mT. Similarly, the corrosion resistance of the joint first increased and then decreased, and it was best when the pulse magnetic field intensity was 60 mT. The Nyquist plot and Bode plot confirmed this result. The addition of a pulsed magnetic field caused less fluctuation in the anode current density, resulting in less localized corrosion of the joint using the scanning vibrating electrode technique (SVET). The XPS analysis showed the Al-Fe-Si compounds replacing the Fe-Al compounds in the joint was the main reason for improving its corrosion resistance under the action of a pulsed magnetic field.
- Open Access
Effect of Heat Treatment Temperature on the Microstructure and Properties of Titanium-Clad Steel Plate Prepared by Vacuum Hot Rolling
Titanium-clad steel plates are widely used in chemical equipment and nuclear power equipment due to their excellent corrosion resistance and high strength. However, the Ti-C and Fe-Ti compounds generated easily at the titanium/steel interface deteriorate the bonding strength of titanium and steel, especially in high-temperature service environments. In this study, pure Fe DT4 was chosen as an intermediate layer to control the formation of interfacial compounds. The plates of titanium/DT4/steel were manufactured by hot rolling technology with a small hole vacuuming. Then, titanium-clad steel plates were annealed at temperatures of 450 °C, 550 °C, and 650 °C to modify microstructure and properties. The interfacial microstructure composition, mechanical properties of titanium-clad steel plates, and the corrosion resistance property of titanium plates were studied in the as-rolled state and under different annealing temperatures. The results showed that compounds of TiC, FeTi, and Fe2Ti were generated at the interface of titanium-clad steel plates in the as-rolled state. After the annealing treatment, the types and quantities of the interfacial compounds were reduced, and these compounds were mainly TiC and FeTi at an annealing temperature of 450 °C. The interfacial compound was only TiC at an annealing temperature of 550 °C. However, the compounds of TiC and FeTi appeared at the interface at an annealing temperature of 650 °C. The variation of interfacial compounds determined the hardness and the shear strength of the titanium-clad steel plates. The more the interfacial compounds, the higher the hardness and the lower the shear strength. Therefore, when the annealing temperature was 550 °C, the interfacial hardness was lowest and the shear strength was highest. Meanwhile, the corrosion resistance of the titanium-clad plates showed significant improvement, indicating that this temperature provides favorable conditions for enhancing the corrosion performance of the plate.
Open AccessEffect of Heat Treatment Temperature on the Microstructure and Properties of Titanium-Clad Steel Plate Prepared by Vacuum Hot Rolling
Titanium-clad steel plates are widely used in chemical equipment and nuclear power equipment due to their excellent corrosion resistance and high strength. However, the Ti-C and Fe-Ti compounds generated easily at the titanium/steel interface deteriorate the bonding strength of titanium and steel, especially in high-temperature service environments. In this study, pure Fe DT4 was chosen as an intermediate layer to control the formation of interfacial compounds. The plates of titanium/DT4/steel were manufactured by hot rolling technology with a small hole vacuuming. Then, titanium-clad steel plates were annealed at temperatures of 450 °C, 550 °C, and 650 °C to modify microstructure and properties. The interfacial microstructure composition, mechanical properties of titanium-clad steel plates, and the corrosion resistance property of titanium plates were studied in the as-rolled state and under different annealing temperatures. The results showed that compounds of TiC, FeTi, and Fe2Ti were generated at the interface of titanium-clad steel plates in the as-rolled state. After the annealing treatment, the types and quantities of the interfacial compounds were reduced, and these compounds were mainly TiC and FeTi at an annealing temperature of 450 °C. The interfacial compound was only TiC at an annealing temperature of 550 °C. However, the compounds of TiC and FeTi appeared at the interface at an annealing temperature of 650 °C. The variation of interfacial compounds determined the hardness and the shear strength of the titanium-clad steel plates. The more the interfacial compounds, the higher the hardness and the lower the shear strength. Therefore, when the annealing temperature was 550 °C, the interfacial hardness was lowest and the shear strength was highest. Meanwhile, the corrosion resistance of the titanium-clad plates showed significant improvement, indicating that this temperature provides favorable conditions for enhancing the corrosion performance of the plate.