Vagner Kretiska Medeiros
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Interests
Vagner Kretiska Medeiros has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Aloisio Nelmo Klein
LabMat (Materials Laboratory) Department of Mechanical Engineering Federal University of Santa Catarina Florianópolis 88040‐370 Brazil
1 shared publication Antonio Itamar Ramos Filho
1 shared publication- Bruno Borges Ramos
Materials Laboratory (LABMat), Mechanical Engineering Department, Federal University of Santa Catarina (UFSC), Rua Delfino Conti, S/N, Campus Trindade, Florianópolis 88040-900, Brazil
1 shared publication - Bruno Henriques
Post-Graduation Program of Dentistry, Center for Education and Research on Dental Implants, Federal University of Santa Catarina, Florianópolis, Brazil
1 shared publication - Claudio Aguilar
Universidad Tecnica Federico Santa Maria
1 shared publication - Cristiano Binder
Materials Laboratory (LabMat), Mechanical Engineering Department, Federal University of Santa Catarina (UFSC), Rua Delfino Conti, S/N, Florianópolis 88040-900, Brazil
1 shared publication
Latest Publications
- Open Access
- 15 October 2026
- Published by Elsevier in SSRN Electronic Journal
In-Situ Formation of Double-Layer Insulating Coatings in Soft Magnetic Composites using Graphene Oxide and Boric Acid
This work addresses the development of a soft magnetic composite (SMC) by applying a double-layer hybrid electrical insulating coating of graphene oxide (GO) and boric acid on iron powder. During heat treatment, boric acid decomposes into a continuous glassy boron oxide barrier that effectively suppresses eddy currents. The coating architecture relies on a minimal, strictly controlled GO concentration (0.1 g/L) to provide interfacial anchoring, alongside boric acid, which thermally decomposes into a continuous glassy boron oxide barrier to suppress eddy currents. The study found that higher concentrations of GO are detrimental, as the agglomeration and partial thermal reduction of GO to a conductive state (rGO) form electrical percolation paths that drastically increase dynamic losses. Ultimately, combining this optimal minimal carbon fraction with boric acid and a 450 °C heat treatment yielded a double-layer SMC with total core losses of 49.36 W/kg (at 1.0 T and 400 Hz). This represents a 15% reduction in total core losses compared to previous studies, yielding a competitive soft magnetic composite for electrical applications.
- 15 October 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessIn-Situ Formation of Double-Layer Insulating Coatings in Soft Magnetic Composites using Graphene Oxide and Boric Acid
This work addresses the development of a soft magnetic composite (SMC) by applying a double-layer hybrid electrical insulating coating of graphene oxide (GO) and boric acid on iron powder. During heat treatment, boric acid decomposes into a continuous glassy boron oxide barrier that effectively suppresses eddy currents. The coating architecture relies on a minimal, strictly controlled GO concentration (0.1 g/L) to provide interfacial anchoring, alongside boric acid, which thermally decomposes into a continuous glassy boron oxide barrier to suppress eddy currents. The study found that higher concentrations of GO are detrimental, as the agglomeration and partial thermal reduction of GO to a conductive state (rGO) form electrical percolation paths that drastically increase dynamic losses. Ultimately, combining this optimal minimal carbon fraction with boric acid and a 450 °C heat treatment yielded a double-layer SMC with total core losses of 49.36 W/kg (at 1.0 T and 400 Hz). This represents a 15% reduction in total core losses compared to previous studies, yielding a competitive soft magnetic composite for electrical applications.
- Open Access
Synthesis and Characterization of Ti-13Ta-6Sn Foams Produced Using Mechanical Alloying, the Space Holder Method and Plasma-Assisted Sintering
Highly porous titanium foams are great candidates for replacing bone structures with a low elastic modulus owing to their ability to avoid the stress shielding effect. However, the production of highly porous foams (>70 vol.%) with well-distributed, stable, and predictable porous architectures using powder compaction and space holders is challenging. In this study, pure titanium powder and mechanically alloyed Ti-13Ta-6Sn were mixed with 50, 70, and 80 vol.% KCl powders as a space holder, cold-compacted, and sintered in a plasma-assisted sintering reactor to produce highly porous foams. The space holder was completely removed using heat and plasma species collisions prior to sintering. A Ti-13Ta-6Sn alloy powder with α, β, and metastable FCC-γ phases was synthesized. The characteristics of the alloyed powder, mixing step, and the resulting sintered samples were compared to those of CP-Ti. After sintering, the alloy exhibited α and β phases and a reduced elastic modulus. Foams with an elastic modulus in the range of the cortical and trabecular bones were obtained. The results showed the effects of the space holder volume fractions on the volume fraction, size, distribution, interconnectivity, and shape of the pores. The Ti-13Ta-6Sn foams exhibited a uniform open-celled porous architecture, lower elastic modulus, higher yield strength, and higher passivation resistance than CP-Ti. Ti-13Ta-6Sn exhibited a nontoxic effect for the mouse fibroblast cell line.
Open AccessSynthesis and Characterization of Ti-13Ta-6Sn Foams Produced Using Mechanical Alloying, the Space Holder Method and Plasma-Assisted Sintering
Highly porous titanium foams are great candidates for replacing bone structures with a low elastic modulus owing to their ability to avoid the stress shielding effect. However, the production of highly porous foams (>70 vol.%) with well-distributed, stable, and predictable porous architectures using powder compaction and space holders is challenging. In this study, pure titanium powder and mechanically alloyed Ti-13Ta-6Sn were mixed with 50, 70, and 80 vol.% KCl powders as a space holder, cold-compacted, and sintered in a plasma-assisted sintering reactor to produce highly porous foams. The space holder was completely removed using heat and plasma species collisions prior to sintering. A Ti-13Ta-6Sn alloy powder with α, β, and metastable FCC-γ phases was synthesized. The characteristics of the alloyed powder, mixing step, and the resulting sintered samples were compared to those of CP-Ti. After sintering, the alloy exhibited α and β phases and a reduced elastic modulus. Foams with an elastic modulus in the range of the cortical and trabecular bones were obtained. The results showed the effects of the space holder volume fractions on the volume fraction, size, distribution, interconnectivity, and shape of the pores. The Ti-13Ta-6Sn foams exhibited a uniform open-celled porous architecture, lower elastic modulus, higher yield strength, and higher passivation resistance than CP-Ti. Ti-13Ta-6Sn exhibited a nontoxic effect for the mouse fibroblast cell line.