Pauline Kümmerl
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Pauline Kümmerl has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
Daniel Primetzhofer
Department of Physics and Astronomy Uppsala University Regementsvägen 10 S-75120 Uppsala Sweden
3 shared publicationsGanesh Kumar Nayak
Materials Chemistry RWTH Aachen University Kopernikusstr. 10 D-52074 Aachen Germany
3 shared publicationsJochen M. Schneider
Materials Chemistry RWTH Aachen University Kopernikusstr. 10 D-52074 Aachen Germany
3 shared publicationsMarcus Hans
Materials Chemistry RWTH Aachen University Kopernikusstr. 10 D-52074 Aachen Germany
3 shared publicationsPeter Polcik
Plansee Composite Materials GmbH Siebenbürgerstraße 23 D-86983 Lechbruck am See Germany
3 shared publicationsSzilárd Kolozsvári
Plansee Composite Materials GmbH Siebenbürgerstraße 23 D-86983 Lechbruck am See Germany
3 shared publications
Latest Publications
- Open Access
Impact of O concentration on the thermal stability and decomposition mechanism of (Cr,Al)N compared to (Ti,Al)N thin films
The composition-dependent thermal stability of (Cr$_{0.47 \mp 0.03}$Al$_{0.53 \mp 0.03}$)$_{z}$(O$_{y}$N$_{1-y}$)$_{1-z}$ thin films with O concentrations of y = 0, 0.15, and 0.40 is investigated up to 1200 °C and then compared to (Ti$_{0.56}$Al$_{0.44}$)$_{z}$(O$_{y}$N$_{1-y}$)$_{1-z}$. X-ray diffraction reveals a thermal stability limit of 1150 °C independent of the O concentration, as witnessed by the formation of decomposition products, namely h-Cr$_{2}$N for (Cr$_{0.50}$Al$_{0.50}$)$_{0.49}$N$_{0.51}$ and c-Cr for both (Cr$_{0.48}$Al$_{0.52}$)$_{0.48}$(O$_{0.15}$N$_{0.85}$)$_{0.52}$ and (Cr$_{0.44}$Al$_{0.56}$)$_{0.46}$(O$_{0.40}$N$_{0.60}$)$_{0.54}$. Based on TEM and ERDA data, the thermal stability limit is extended to 1100 - 1150 °C. DFT calculations indicate that bond breaking limits the thermal stability. In (Cr,Al)N, N has the lowest activation energy for migration. Furthermore, the O vacancy formation energy is highest in (Cr,Al)(O,N). It has to be overcome to enable diffusion on the non-metal sublattice, which is necessary for forming decomposition products like w-AlN or c-Cr. However, once Cr-N bonds break, decomposition into h-Cr$_{2}$N and subsequent c-Cr together with N$_{2}$ is triggered. This results in N evaporation, generating sufficient non-metal vacancies that greatly enhance diffusion and render the extensive vacancy formation energies for non-metals irrelevant. This reduction of the activation energy for mass transport on the non-metal sublattice to the migration barrier causes the similar thermal stability in (Cr$_{0.47 \mp 0.03}$Al$_{0.53 \mp 0.03}$)$_{z}$(O$_{y}$N$_{1-y}$)$_{1-z}$. In contrast, Al bonds break first without creating non-metal vacancies in (Ti,Al)(O,N). Thus, the high O vacancy formation energy in (Ti,Al)(O,N) significantly increases the thermal stability compared to (Ti,Al)N as well as the here investigated films.
Open AccessImpact of O concentration on the thermal stability and decomposition mechanism of (Cr,Al)N compared to (Ti,Al)N thin films
The composition-dependent thermal stability of (Cr$_{0.47 \mp 0.03}$Al$_{0.53 \mp 0.03}$)$_{z}$(O$_{y}$N$_{1-y}$)$_{1-z}$ thin films with O concentrations of y = 0, 0.15, and 0.40 is investigated up to 1200 °C and then compared to (Ti$_{0.56}$Al$_{0.44}$)$_{z}$(O$_{y}$N$_{1-y}$)$_{1-z}$. X-ray diffraction reveals a thermal stability limit of 1150 °C independent of the O concentration, as witnessed by the formation of decomposition products, namely h-Cr$_{2}$N for (Cr$_{0.50}$Al$_{0.50}$)$_{0.49}$N$_{0.51}$ and c-Cr for both (Cr$_{0.48}$Al$_{0.52}$)$_{0.48}$(O$_{0.15}$N$_{0.85}$)$_{0.52}$ and (Cr$_{0.44}$Al$_{0.56}$)$_{0.46}$(O$_{0.40}$N$_{0.60}$)$_{0.54}$. Based on TEM and ERDA data, the thermal stability limit is extended to 1100 - 1150 °C. DFT calculations indicate that bond breaking limits the thermal stability. In (Cr,Al)N, N has the lowest activation energy for migration. Furthermore, the O vacancy formation energy is highest in (Cr,Al)(O,N). It has to be overcome to enable diffusion on the non-metal sublattice, which is necessary for forming decomposition products like w-AlN or c-Cr. However, once Cr-N bonds break, decomposition into h-Cr$_{2}$N and subsequent c-Cr together with N$_{2}$ is triggered. This results in N evaporation, generating sufficient non-metal vacancies that greatly enhance diffusion and render the extensive vacancy formation energies for non-metals irrelevant. This reduction of the activation energy for mass transport on the non-metal sublattice to the migration barrier causes the similar thermal stability in (Cr$_{0.47 \mp 0.03}$Al$_{0.53 \mp 0.03}$)$_{z}$(O$_{y}$N$_{1-y}$)$_{1-z}$. In contrast, Al bonds break first without creating non-metal vacancies in (Ti,Al)(O,N). Thus, the high O vacancy formation energy in (Ti,Al)(O,N) significantly increases the thermal stability compared to (Ti,Al)N as well as the here investigated films.
- Open Access
- 24 October 2024
- Published by Springer Nature in Scientific Reports
- Vol. 14 (1) , 1
Author Correction: Improved oxidation behavior of Hf0.11Al0.20B0.69 in comparison to Hf0.28B0.72 magnetron sputtered thin films
- 24 October 2024
- Published by Springer Nature in Scientific Reports
- Vol. 14 (1) , 1
Open AccessAuthor Correction: Improved oxidation behavior of Hf0.11Al0.20B0.69 in comparison to Hf0.28B0.72 magnetron sputtered thin films
- Open Access
- 17 September 2024
- Published by Springer Nature in Scientific Reports
- Vol. 14 (1) , 1-13
Improved oxidation behavior of Hf0.11Al0.20B0.69 in comparison to Hf0.28B0.72 magnetron sputtered thin films
The oxidation resistance of Hf0.28B0.72 and Hf0.11Al0.20B0.69 thin films was investigated comparatively at 700 °C for up to 8 h. Single-phase solid solution thin films were co-sputtered from HfB2 and AlB2 compound targets. After oxidation at 700 °C for 8 h an oxide scale thickness of 31 $$\pm$$ 2 nm was formed on Hf0.11Al0.20B0.69 which corresponds to 14% of the scale thickness measured on Hf0.28B0.72. The improved oxidation resistance can be rationalized based on the chemical composition and the morphology of the formed oxide scales. On Hf0.28B0.72 the formation of a porous, O, Hf, and B-containing scale and the formation of crystalline HfO2 is observed. Whereas on Hf0.11Al0.20B0.69 a dense, primarily amorphous scale containing O, Al, B as well as approximately 3 at% of Hf forms, which reduces the oxidation kinetics significantly by passivation. Benchmarking Hf0.11Al0.20B0.69 with Ti–Al-based boride and nitride thin films with similar Al concentrations reveals superior oxidation behavior of the Hf-Al-based thin film. The incorporation of few at% of Hf in the oxide scale decelerates oxidation kinetics at 700 °C and leads to a reduction in oxide scale thickness of 21% and 47% compared to Ti0.12Al0.21B0.67 and Ti0.27Al0.21N0.52, respectively. Contrary to Ti–Al-based diborides, Hf0.11Al0.20B0.69 shows excellent oxidation behavior despite B-richness.- 17 September 2024
- Published by Springer Nature in Scientific Reports
- Vol. 14 (1) , 1-13
Open AccessImproved oxidation behavior of Hf0.11Al0.20B0.69 in comparison to Hf0.28B0.72 magnetron sputtered thin films
The oxidation resistance of Hf0.28B0.72 and Hf0.11Al0.20B0.69 thin films was investigated comparatively at 700 °C for up to 8 h. Single-phase solid solution thin films were co-sputtered from HfB2 and AlB2 compound targets. After oxidation at 700 °C for 8 h an oxide scale thickness of 31 $$\pm$$ 2 nm was formed on Hf0.11Al0.20B0.69 which corresponds to 14% of the scale thickness measured on Hf0.28B0.72. The improved oxidation resistance can be rationalized based on the chemical composition and the morphology of the formed oxide scales. On Hf0.28B0.72 the formation of a porous, O, Hf, and B-containing scale and the formation of crystalline HfO2 is observed. Whereas on Hf0.11Al0.20B0.69 a dense, primarily amorphous scale containing O, Al, B as well as approximately 3 at% of Hf forms, which reduces the oxidation kinetics significantly by passivation. Benchmarking Hf0.11Al0.20B0.69 with Ti–Al-based boride and nitride thin films with similar Al concentrations reveals superior oxidation behavior of the Hf-Al-based thin film. The incorporation of few at% of Hf in the oxide scale decelerates oxidation kinetics at 700 °C and leads to a reduction in oxide scale thickness of 21% and 47% compared to Ti0.12Al0.21B0.67 and Ti0.27Al0.21N0.52, respectively. Contrary to Ti–Al-based diborides, Hf0.11Al0.20B0.69 shows excellent oxidation behavior despite B-richness.