Latest Publications

  • Open Access

    Modelling the Wear Effects During the Forming of Steel and Aluminium for Tailored Forming

    by Simon Peddinghaus, Armin Piwek, Hendrik Wester, Julius Peddinghaus, Johanna Uhe, Bernd-Arno Behrens

    In industrial bulk metal forming processes the die wear has a major influence on the process stability and the overall economical profitability. In Tailored Forming processes, the semi-finished products consist of different materials, such as aluminium and steel. These hybrid semi-finished products are formed together. The predominant wear mechanism in steel forming processes is abrasive wear, whereas in aluminium forming processes mainly adhesive wear occurs. Due to the alternating material contact, the dies are exposed to alternating wear mechanisms. Although both wear mechanisms can separately be predicted numerically using models such as the approach of Archard, interactions between the mechanisms are not taken into account. The present work is therefore dedicated to investigating the wear effects during a hybrid bulk forming process. Therefore, first upsetting experiments with mono-materials were carried out. The experiments were then repeated whilst alternating the workpiece materials each stroke and then compared to the first trial. Finite element (FE) simulations were used to recreate the upsetting processes numerically. The wear depth was determined numerically through an adapted simulation model to take the alternating wear mechanisms into account. The numerical results were compared to the experiments to analyse the interactions of the wear mechanisms and derive suitable wear coefficients. The findings allow the development of an improved numerical approach for the prediction of the alternating die wear effects in Tailored Forming processes in the future.

  • Open Access

    Parameter Variation in Planetary Ball Milling of Titanium Aluminide Powder in XHV‐Adequate Atmosphere

    by Jytte Möckelmann, Armin Piwek, Julius Peddinghaus, Kai Brunotte, Bernd-Arno Behrens

    Given the high oxygen affinity of titanium aluminides, their powder particle surfaces develop an oxide layer. Due to the oxides, processing via the conventional powder metallurgy route is not possible, as they reduce particle cohesion and thus compromise the green strength of TiAl‐billets. To prevent oxidation, this study utilizes an extremely high vacuum‐equivalent process atmosphere with an oxygen content of −16 ppm v . By performing ball milling in a silane‐doped, low‐oxygen environment, oxide‐free metal surfaces on the prealloyed TiAl powder particles are created. The milling parameters, including milling speed, milling duration, and ball‐to‐powder ratio, are varied to enhance the processability of the powder. The goal is to achieve a mechanically stable green body with the highest possible density. The milled powder is analyzed in terms of particle size distribution and morphology. The resulting green compacts are evaluated for their density, vibration resistance, and tensile splitting strength. Green bodies with tensile splitting strengths up to 11.9 ± 1.0 MPa could be achieved from TiAl powder with an effective milling time of 2 h. This highlights the influence of milling conditions on the mechanical properties of the green bodies, as the milling conditions determine the formation of the reactive surfaces.

  • Open Access

    Potentials of Heat Superimposed Rotary Friction Welding for Steel-Aluminium Joints

    by Armin Piwek, Julius Peddinghaus, Johanna Uhe, Kai Brunotte, Bernd Arno Behrens

    Hybrid joints made of steel and aluminium alloy produced by rotary friction welding enable load-adapted lightweight components. However, a major challenge is the inhomogeneous radial temperature distribution caused by different relative velocities between the specimen centre and edge during rotation. This effect leads to local insufficient bonding and reduces the overall joint strength, especially in the centre, where low relative rotation speeds occur. Previous studies mainly addressed preheating before the friction phase, whereas superimposed heating during the upsetting phase has not been investigated so far. To achieve temperature equalisation along the cross-section during rotary friction welding, a modified KUKA Genius plus machine equipped with joule heating was used to introduce an electric current during the upsetting phase. Experiments were conducted on EN AW-6082 (AA-6082) joined to 20MnCr5 (AISI 5120H). A three-step variation of current intensity (10, 24 and 36 A/mm 2 ), alongside a reference without current, was investigated. Temperatures were monitored using type K thermocouples, confirming temperature equalisation. Mechanical performance was assessed by uniaxial tensile tests, while hardness measurements and metallographic analyses characterised the influence of superimposed heating on the interfacial microstructure. Joint strength improves up to 17% with increasing current, even under otherwise unsuitable welding parameters that would normally result in insufficient bond strength. This improvement is linked to a uniform temperature distribution and enhanced material flow, resulting in a defect-free specimen centre.

  • Open Access

    Experimental and Numerical Study of Steel-Aluminium Rotary Friction Welding with Heat Flux via Subroutine

    by Amith Tom Mathew, Armin Piwek, Jakub Mayer, Norman Mohnfeld, Bernd Arno Behrens, Johanna Uhe

    Rotary friction welding (RFW) is a solid-state process used to join similar and dissimilar materials, such as steel and aluminium. In RFW, interface temperature development and its distribution are essential factors influencing material bonding. It governs bond strength, the formation of intermetallic phases (IMPs) and the evolution of the heat-affected zone (HAZ). Thus, precise prediction of temperature distribution is vital for the reliable design and optimization of the RFW process, as well as for the prediction and control of IMP formation. This work presents an experimental investigation of the thermo-mechanical behaviour of EN AW-6082 and 20MnCr5 during RFW in addition to a corresponding novel numerical modelling framework. A systematic parameter study was conducted to evaluate the influence of the friction pressure, friction time, forging pressure, forging time and rotational speed on the peak temperature, sledge path and flash formation. In-situ temperature measurements were performed using thermocouples (TC) embedded in the steel component, while axial force, displacement and rotational speed were recorded. The results demonstrate that, within the investigated parameter ranges, the rotational speed is the dominant factor governing frictional heat generation and the peak temperature, while the friction pressure primarily influences the sledge path. In parallel, a 2D axisymmetric finite-element model with a user-defined subroutine was developed to compute the heat flux based on process parameters and contact conditions, providing a transparent and extensible numerical framework for RFW. The experimental findings establish a robust basis for the calibration and future validation of the numerical model.

  • Open Access

    Microstructure Modification of Hot Formed Shafts through Customised Spray Cooling from the Forming Heat

    by Matthias Hammes, Armin Piwek, Norman Mohnfeld, Julius Peddinghaus, Johanna Uhe, Bernd Arno Behrens

    In order to achieve a long service life for highly stressed parts such as shafts for drivetrains, a combination of a bainitic microstructure with compressive surface residual stresses is beneficial. While a bainitic microstructure offers a good balance between strength and toughness, compressive residual stresses especially near the surface have a positive impact on service life. Research has shown that this is due to a shift of the crack initiation towards the core and a reduced crack growth . These properties can be achieved by hot forming as an established method for manufacturing highly stressed parts followed by an adapted cooling strategy. As this general approach was demonstrated for a simplified process in a prior study , the present article is dedicated to the functionalisation for hot forming processes. In detail, a customised spray cooling is presented for a hot impact extrusion process whereby shafts made of AISI 4140 are cooled down from the forming heat in a single step with adjusted cooling rates. In a finite element-based process design, different cooling strategies were investigated and adequate heat treatments to achieve the combined properties were identified. Following this process design, shafts are formed via hot impact extrusion and spray cooled according to the cooling strategy for experimental validation of the numerical model. Additionally, shafts with air cooling are produced as a reference. During forming, force-displacement curves are measured, which are used for the validation of the numerical hot impact extrusion simulation. The resulting plastic strain and temperature distribution significantly influence the following cooling simulation. The final microstructure as well as hardness values of the produced shafts are determined and compared for the varying cooling strategies.

  • Open Access

    Analysis of Temperature and Stress Distribution on the Bond Properties of Hybrid Tailored Formed Components

    by Armin Piwek, Eduard Ortlieb, Caner‐Veli Ince, Julius Peddinghaus, Hendrik Wester, Johanna Uhe, Annika Raatz, Kai Brunotte

    Processing of hybrid materials is particularly challenging due to the different physical properties and requires extensive knowledge to produce defect‐free components. When serially combining steel and aluminum through rotary friction welding and subsequent cup backward extrusion in Tailored Forming, the strongly different yield stresses are a decisive factor. The following study analyzes the temperature and stress distribution after the compensatory heating step with additional cooling and during cup backward extrusion within a preform of a hybrid hollow shaft using experimental heating tests and finite element simulations. The influence on the bond strength is quantified by uniaxial tensile tests along the interface. Compared to uncooled samples, local cooled samples exhibit higher compressive stresses in the joining zone and hence higher forming resistance due to higher temperature gradients. Therefore, delamination and cracks can be prevented. While areas at the edge or in the center indicate reduced strengths overall, areas with high surface enlargement do not fail in the joining zone, but in the base material of the aluminum. To further enhance process stability and process control measures, a preliminary concept for the implicit determination of component temperatures using integrated sensor systems on the handling system is presented.


  • Open Access

    Rotationsreibschweißen unter wechselnden Bedingungen/Rotary friction welding under changing conditions

    by Armin Piwek, Alexej Verschinin, Julian Bosse, Julius Peddinghaus, Sebastian Barton, Johanna Uhe, Kai Brunotte

    Aufgrund der unterschiedlichen Materialeigenschaften können beim Rotationsreibschweißen von Verbindungen aus Stahl und Aluminiumlegierungen geringe Abweichungen bezüglich Oberflächenzustand, Bauteiltemperatur und Reibfläche den Verbund deutlich beeinträchtigen. Die Auswirkungen dieser Eingangsbedingungen auf den Materialfluss, die Wulstbildung und die resultierende Verbundfestigkeit wurden systematisch in experimentellen Versuchen untersucht und per Ultraschallprüfung sowie Zugversuch bewertet.

  • Open Access

    Wear effects on coated tools during the alternating forming of case-hardening steel and aluminium wrought alloy

    by A. Piwek, J. Peddinghaus, J. Uhe, K. Brunotte

    A major factor for a high economic profitability in industrial bulk metal forming is the material-specific wear of the forming tools, which has a significant influence on process reproducibility. Particularly in Tailored Forming, in which hybrid material combinations are processed, narrow and sensitive process windows are characteristic. During impact extrusion of joined hybrid semi-finished workpieces made of steel and aluminium, the extrusion shoulder is subjected to combined wear phenomena. Adhesion and abrasion are superimposed, whose interactions lead to process fluctuations and premature failures in the absence of sufficient wear resistance. To investigate the yet unknown combination of the interactions, upsetting tests are carried out in cycles of 100, in which steel (AISI 5120H) and aluminium (AA-6082) are hot-formed alternately. In addition to tempered and nitrided tools, duplex coatings such as chromium nitride and titanium aluminium nitride are used to evaluate the potential of reducing the occurring wear phenomena through surface engineering methods. After the first cycles, the tools exhibit needle-shaped adhesion marks consisting of aluminium, which were subsequently transferred primarily to the steel workpieces during upsetting. Since adhesion is more present at the tool edge, an increased adhesive tendency with longer flow paths is observed. Due to the improved tribological conditions, duplex coatings minimise the wear volume on the tool and potentially on the formed workpiece with short contact times.


  • Open Access

    Intermetallic Compound Layer Morphology and Distribution in Friction‐Welded Steel–Aluminum Components

    by Christoph Kahra, Armin Piwek, Julius Peddinghaus, Kai Brunotte, Hans Jürgen Maier, Florian Nürnberger, Sebastian Herbst

    In this study, the morphology, distribution, and local thickness of the intermetallic compound layer (IMC‐layer) in friction‐welded steel‐aluminum hybrid components used for Tailored Forming applications are investigated. By friction‐welding of steel and aluminum, which is the first step in the Tailored Forming process chain, an IMC‐layer in the joining zone is formed. In this study, the influence of friction‐welding parameters, such as rotational speed, friction pressure, friction length, upsetting pressure, and upsetting time, on local IMC‐layer thickness and distribution is examined. For characterization, a detailed analysis over the whole joining surface by means of scanning electron microscopy and a thorough statistical evaluation are employed. In the results, it is indicated that lower rotational speeds (700 rpm) in the friction phase result in more uniform and thinner IMC‐layer (<0.5 μm), while higher speeds (1600 rpm) produce a thicker and more heterogeneous IMC‐ layer (up to 0.9 μm). Tensile tests show that specimens with thinner mean IMC‐layer (0.17 μm) feature a higher tensile strength (244 MPa). The morphology and distribution of the IMC‐layer over the cross section of the friction‐welded specimen have a significant effect on the mechanical properties of the joint, with a uniform thin layer improving the tensile strength.


  • Open Access

    Influence of enlarged joining zone interfaces on the bond properties of tailored formed hybrid components made of 20MnCr5 steel and EN AW-6082 aluminium

    by A. Piwek, J. Peddinghaus, J. Uhe, K. Brunotte

    Hybrid material compounds offer an extension of the technological application range of monolithic components by combining positive material-specific properties. In the case of steel and aluminium, a load-adapted component with high strength areas and a reduced weight can be created. Tailored Forming enables the joining zone created by a pre-joining process to be modified and enhanced by a subsequent forming step. Derived from previous studies, an enlarged joining zone interface through spherical joining zone curvature and an equalisation of yield stresses through an inhomogeneous induction heating with partial cooling are necessary to achieve a defect free bond with high strength and ductility. In order to further enlarge the joining zone interface and hence to increase the surface ratio of juvenile welding spots without brittle intermetallic compounds, different local plastic strains are induced. Additionally, an alternative spray cooling concept is used to evaluate the effect of steeper temperature gradients on the bond quality. Rotary friction welded specimens made of 20MnCr5 steel and EN AW-6082 aluminium are cup backward extruded with different extrusion ratios using punch diameters of 22 mm and 30 mm. Metallographic images, SEM analysis and hardness tests of cross-sections are used to evaluate the bond quality with regard to the joining zone formation, occurring defects and the resulting intermetallic compound. With cooling, higher yield stresses could be set in the aluminium, which counteract material failure even with larger punch diameters due to a higher deformability. However, the surface enlargement of the joining zone is reduced. Despite the higher surface enlargement in uncooled specimens, insufficient bonds were achieved due to existing cracks in the aluminium in or near the joining zone interface, as well as significant thicker intermetallic compounds.