Shitian Wei
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Shitian Wei has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Yu Zhang
College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124, China
2 shared publications - Jiarui Xie
College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124, China
1 shared publication - Rui Zhang
China Nuclear Power Engineering Co., Ltd., Beijing 100840, China
1 shared publication - Xiaoyu Ma
Capital Aerospace Machinery Corporation Limited, Beijing 100071, China
1 shared publication - Xiuli Liu
China Nuclear Power Engineering Co., Ltd., Beijing 100840, China
1 shared publication - Yali Xie
College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124, China
1 shared publication
Latest Publications
- Open Access
Effects of In Situ Electrical Pulse Treatment on the Microstructure and Mechanical Properties of Al-Zn-Mg-Cu Alloy Resistance Spot Welds
This study introduces a novel in situ pulsed current-assisted resistance spot welding method, which differs fundamentally from conventional post-weld heat treatments and is designed to enhance the mechanical performance of 7075-T651 aluminum alloy joints. Immediately after welding, a short-duration pulsed current is applied while the weld remains in a high excess-vacancy state, effectively accelerating precipitation reactions within the weld region. Transmission electron microscopy (TEM) observations reveal that pulsed current treatment promotes the formation of band-like solute clusters, indicating a significant acceleration of the early-stage precipitation process. Interestingly, the formation of quasicrystalline phases—rare in Al-Zn-Mg-Cu alloy systems—is incidentally observed at grain boundaries, exhibiting characteristic fivefold symmetry. Selected area electron diffraction (SAED) patterns further show that these quasicrystals undergo partial dissolution under the influence of the pulsed current, transforming into short-range ordered cluster-like structures. Lap shear tests demonstrate that joints treated with pulsed current exhibit significantly higher peak load and energy absorption compared to untreated specimens. Statistical analysis of weld size confirms that both groups possess comparable weld diameters under identical welding currents, suggesting that the observed mechanical improvements are primarily attributed to microstructural evolution rather than geometric factors.
Open AccessEffects of In Situ Electrical Pulse Treatment on the Microstructure and Mechanical Properties of Al-Zn-Mg-Cu Alloy Resistance Spot Welds
This study introduces a novel in situ pulsed current-assisted resistance spot welding method, which differs fundamentally from conventional post-weld heat treatments and is designed to enhance the mechanical performance of 7075-T651 aluminum alloy joints. Immediately after welding, a short-duration pulsed current is applied while the weld remains in a high excess-vacancy state, effectively accelerating precipitation reactions within the weld region. Transmission electron microscopy (TEM) observations reveal that pulsed current treatment promotes the formation of band-like solute clusters, indicating a significant acceleration of the early-stage precipitation process. Interestingly, the formation of quasicrystalline phases—rare in Al-Zn-Mg-Cu alloy systems—is incidentally observed at grain boundaries, exhibiting characteristic fivefold symmetry. Selected area electron diffraction (SAED) patterns further show that these quasicrystals undergo partial dissolution under the influence of the pulsed current, transforming into short-range ordered cluster-like structures. Lap shear tests demonstrate that joints treated with pulsed current exhibit significantly higher peak load and energy absorption compared to untreated specimens. Statistical analysis of weld size confirms that both groups possess comparable weld diameters under identical welding currents, suggesting that the observed mechanical improvements are primarily attributed to microstructural evolution rather than geometric factors.
- Open Access
Comparative Study on the Effect of External Magnetic Field on Aluminum Alloy 6061 and 7075 Resistance Spot-Welding Joints
This study investigates the effects of the external magnetic field on the microstructure and mechanical property aluminum alloy 6061-T6 and 7075-T651 resistance spot welding joints. The melting behavior of 6061 and 7075 was analyzed via the calculation of the phase diagram (CALPHAD) technique. The CALPHAD results indicate that, for the 6061 aluminum alloy, the liquid fraction shows a minimal increase at the beginning stage during the solid–liquid phase transition process but with a sharp rise at the ending stage (near the liquidus). In contrast, for the 7075 aluminum alloy, the liquid fraction gradually increases throughout the entire solid–liquid phase transition process. The differences in melting behavior between the 6061 and 7075 alloys lead to different liquation crack morphologies in their spot-welded joints. In the 6061 alloy, the cracks tend to be “eyebrow-shaped”, allowing the liquid metal in the nugget to feed the gaps, and this does not significantly compromise the mechanical properties of the joint. In contrast, the 7075 alloy develops slender cracks that extend through the partially melted zone (PMZ), making it difficult for the liquid metal to feed these gaps, thereby significantly deteriorating the joint’s mechanical strength. Compared to conventional resistance spot-welding joints, the heat exchange between the nugget and the workpiece is enhanced under the external magnetic field, leading to a wider PMZ. This exacerbates the detrimental effects of liquation cracks on the mechanical properties of the 7075 joints. Lap-shear tests indicate that the mechanical properties of the 6061 aluminum alloy joints are improved under electromagnetic stirring. For 7075 aluminum alloy joints, the mechanical properties improve when the welding current is below 34 kA. However, when the welding current exceeds 34 kA, because the widening of the PMZ increases the tendency for liquation cracks, the joint’s mechanical property is deteriorated.
Open AccessComparative Study on the Effect of External Magnetic Field on Aluminum Alloy 6061 and 7075 Resistance Spot-Welding Joints
This study investigates the effects of the external magnetic field on the microstructure and mechanical property aluminum alloy 6061-T6 and 7075-T651 resistance spot welding joints. The melting behavior of 6061 and 7075 was analyzed via the calculation of the phase diagram (CALPHAD) technique. The CALPHAD results indicate that, for the 6061 aluminum alloy, the liquid fraction shows a minimal increase at the beginning stage during the solid–liquid phase transition process but with a sharp rise at the ending stage (near the liquidus). In contrast, for the 7075 aluminum alloy, the liquid fraction gradually increases throughout the entire solid–liquid phase transition process. The differences in melting behavior between the 6061 and 7075 alloys lead to different liquation crack morphologies in their spot-welded joints. In the 6061 alloy, the cracks tend to be “eyebrow-shaped”, allowing the liquid metal in the nugget to feed the gaps, and this does not significantly compromise the mechanical properties of the joint. In contrast, the 7075 alloy develops slender cracks that extend through the partially melted zone (PMZ), making it difficult for the liquid metal to feed these gaps, thereby significantly deteriorating the joint’s mechanical strength. Compared to conventional resistance spot-welding joints, the heat exchange between the nugget and the workpiece is enhanced under the external magnetic field, leading to a wider PMZ. This exacerbates the detrimental effects of liquation cracks on the mechanical properties of the 7075 joints. Lap-shear tests indicate that the mechanical properties of the 6061 aluminum alloy joints are improved under electromagnetic stirring. For 7075 aluminum alloy joints, the mechanical properties improve when the welding current is below 34 kA. However, when the welding current exceeds 34 kA, because the widening of the PMZ increases the tendency for liquation cracks, the joint’s mechanical property is deteriorated.