Anthony Owen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Anthony Owen has a total of 1 co-authors. Here are the top co-authors by number of shared publications:
Antje Bergmann
Institute of Applied Physics, University of Regensburg, 93040 Regensburg, Germany
3 shared publications
Latest Publications
- 6 May 2004
- Published by Wiley in Polymer International
- Vol. 53 (7) , 863-868
Dielectric relaxation spectroscopy of poly[(R)‐3‐hydroxybutyrate] (PHB) during crystallization
The dielectric response of poly [(R)‐3‐hydroxybutyrate] (PHB) was investigated as a function of time after quenching a film from the melt to a crystallization temperature of 20 °C. In the frequency range investigated (20 to 106 Hz) a relaxation maximum was observed–attributable to the glass transition–which could be analysed by the Havriliak–Negami relation. Changes in the complex dielectric constant were monitored both during spherulite growth (primary crystallization) and subsequently during a period of progressive crystallization (secondary crystallization) at room temperature. The relaxation strength changed only slightly during primary crystallization and its peak position remained at a constant frequency. Subsequently a continuous decrease in relaxation strength occurred, indicating considerable changes in molecular mobility after spherulite growth had been completed. The results provide further evidence that molecular mobility in the amorphous regions decreases significantly with time, and that this would be the reason why PHB shows embrittlement on ageing at room temperature. Copyright © 2004 Society of Chemical Industry
- 6 May 2004
- Published by Wiley in Polymer International
- Vol. 53 (7) , 863-868
Dielectric relaxation spectroscopy of poly[(R)‐3‐hydroxybutyrate] (PHB) during crystallization
The dielectric response of poly [(R)‐3‐hydroxybutyrate] (PHB) was investigated as a function of time after quenching a film from the melt to a crystallization temperature of 20 °C. In the frequency range investigated (20 to 106 Hz) a relaxation maximum was observed–attributable to the glass transition–which could be analysed by the Havriliak–Negami relation. Changes in the complex dielectric constant were monitored both during spherulite growth (primary crystallization) and subsequently during a period of progressive crystallization (secondary crystallization) at room temperature. The relaxation strength changed only slightly during primary crystallization and its peak position remained at a constant frequency. Subsequently a continuous decrease in relaxation strength occurred, indicating considerable changes in molecular mobility after spherulite growth had been completed. The results provide further evidence that molecular mobility in the amorphous regions decreases significantly with time, and that this would be the reason why PHB shows embrittlement on ageing at room temperature. Copyright © 2004 Society of Chemical Industry
- 8 December 2003
- Published by Wiley in Polymer International
- Vol. 53 (1) , 12-14
On the fractal character of polymer spherulites: an ultra‐small‐angle X‐ray scattering study of poly[(R)‐3‐hydroxybutyrate]
Ultra‐small‐angle X‐ray scattering (USAXS) and small‐angle X‐ray scattering (SAXS) measurements are presented for poly[(R)‐3‐hydroxybutyrate] (PHB) crystallized at room temperature. The USAXS patterns indicated that the spherulites had a radially orientated fibrillar nanostructure with fractal geometry over a length scale ranging from 12 nm up to at least 300 nm, with a mass fractal dimension of approximately 2.7 in aged samples. The SAXS patterns indicated that the fibrils themselves were built up of bundles of crystalline lamellae separated by layers of disordered material, with a period length of approximately 6 nm. The SAXS measurements during primary crystallization gave an initial fractal dimension of 4 during spherulite growth, due to the sharp phase boundary between the spherulites and the melt. Copyright © 2004 Society of Chemical Industry
- 8 December 2003
- Published by Wiley in Polymer International
- Vol. 53 (1) , 12-14
On the fractal character of polymer spherulites: an ultra‐small‐angle X‐ray scattering study of poly[(R)‐3‐hydroxybutyrate]
Ultra‐small‐angle X‐ray scattering (USAXS) and small‐angle X‐ray scattering (SAXS) measurements are presented for poly[(R)‐3‐hydroxybutyrate] (PHB) crystallized at room temperature. The USAXS patterns indicated that the spherulites had a radially orientated fibrillar nanostructure with fractal geometry over a length scale ranging from 12 nm up to at least 300 nm, with a mass fractal dimension of approximately 2.7 in aged samples. The SAXS patterns indicated that the fibrils themselves were built up of bundles of crystalline lamellae separated by layers of disordered material, with a period length of approximately 6 nm. The SAXS measurements during primary crystallization gave an initial fractal dimension of 4 during spherulite growth, due to the sharp phase boundary between the spherulites and the melt. Copyright © 2004 Society of Chemical Industry
- 19 June 2003
- Published by Wiley in Polymer International
- Vol. 52 (7) , 1145-1152
Hydroxyapatite as a filler for biosynthetic PHB homopolymer and P(HB–HV) copolymers
This paper deals with some of the fundamental problems encountered when using a semicrystalline polymer as the matrix phase for a particulate‐filled composite. As our model system we adopted poly‐(R)‐3‐hydroxybutyrate, PHB, and two copolymers of (R)‐3‐hydroxybutyrate and (R)‐3‐hydroxyvalerate, P(HB–HV), for the matrix phase, and the mineral calcium hydroxyapatite as a particulate filler. The structure and properties of compression‐moulded films of various compositions were investigated by polarized light microscopy, wide‐angle X‐ray scattering and mechanical testing. It was found that the degree of crystallinity of the matrix was lower in filled samples, and that the spherulitic crystallization of the matrix appeared to cause the filler particles to form agglomerates, which would not be as effective a reinforcement as finely dispersed primary filler particles. The tensile strength, strain‐to‐break and tensile modulus of samples of different compositions were analysed using well‐known theories for composite behaviour. Copyright © 2003 Society of Chemical Industry
- 19 June 2003
- Published by Wiley in Polymer International
- Vol. 52 (7) , 1145-1152
Hydroxyapatite as a filler for biosynthetic PHB homopolymer and P(HB–HV) copolymers
This paper deals with some of the fundamental problems encountered when using a semicrystalline polymer as the matrix phase for a particulate‐filled composite. As our model system we adopted poly‐(R)‐3‐hydroxybutyrate, PHB, and two copolymers of (R)‐3‐hydroxybutyrate and (R)‐3‐hydroxyvalerate, P(HB–HV), for the matrix phase, and the mineral calcium hydroxyapatite as a particulate filler. The structure and properties of compression‐moulded films of various compositions were investigated by polarized light microscopy, wide‐angle X‐ray scattering and mechanical testing. It was found that the degree of crystallinity of the matrix was lower in filled samples, and that the spherulitic crystallization of the matrix appeared to cause the filler particles to form agglomerates, which would not be as effective a reinforcement as finely dispersed primary filler particles. The tensile strength, strain‐to‐break and tensile modulus of samples of different compositions were analysed using well‐known theories for composite behaviour. Copyright © 2003 Society of Chemical Industry