Xiaoying Guo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Xiaoying Guo has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Gang Li
College of Mines, Liaoning Technical University, Fuxin 123000, China
2 shared publications - Haifang Ren
School of Materials Science and Engineering, Yingkou Institute of Technology, Yingkou 115000, China
2 shared publications - Sinan Li
School of Metallurgy and Materials Engineering, Liaoning Institute of Science and Technology, Benxi 117004, China
2 shared publications - Xiangran Meng
College of Mines, Liaoning Technical University, Fuxin 123000, China
2 shared publications - Ying Tao
School of Metallurgy and Materials Engineering, Liaoning Institute of Science and Technology, Benxi, Liaoning, China
2 shared publications - Chongshuo Wang
Yingkou Institute of Technology, Yingkou 115000, China, China
1 shared publication
Latest Publications
- Open Access
Microstructure and Properties of AlxCr1−xCoFeNi High-Entropy Alloys Prepared by Spark Plasma Sintering
CoCrFeNi high-entropy alloys represent a novel structural material with considerable application potential in a variety of fields, including aerospace, automobiles, ships, machining, energy, soft magnetic materials, and hydrogen storage materials. The present study investigates the impact of the Al element on the structure and properties of the alloy. The preparation of the AlxCr1−xCoFeNi (x = 0.1, 0.2, 0.3, 0.4, 0.5) powders involved the use of a variety of elemental metal powders as raw materials and a mechanical alloying process at 350 rpm for 40 h. The sintering of the alloy powders was subsequently conducted using spark plasma sintering at 1000 °C. The microstructure of the alloys was analyzed using XRD, SEM, and EDS, and the properties were analyzed using a universal testing machine, a hardness measurement, friction and wear measurement, and an electrochemical workstation. The study shows that when x = 0.1, the crystal structure of Al0.1Cr0.9CoFeNi consists of a double FCC phase and a trace amount of σ phase. As the aluminum content increases, part of the FCC phase begins to transform to BCC. When x = 0.2~0.5, the alloy consists of a double FCC phase and a BCC phase and a trace amount of a sigma phase. As the BCC phase in the alloy increases, the tensile strength of the alloy increases, the ability to deform plastically decreases, and the hardness increases. The highest ultimate tensile strength of 1163.14 MPa is exhibited by Al0.5Cr0.5CoFeNi, while the minimum elongation is 26.98% and the maximum hardness value is 412.6 HV. In the initial stage of friction measurement, the wear mechanism of AlxCr1−xCoFeNi is adhesive wear. However, as the test time progresses, an oxide layer begins to form on the alloy’s surface, leading to a gradual increase in the friction coefficient. At this stage, the wear mechanism becomes a combination of both adhesive and abrasive wear. Once the oxidation process and the wear process have reached a dynamic equilibrium, the friction coefficient stabilizes, and the wear mechanism transitions to a state of abrasive wear. The Al0.1Cr0.9CoFeNi alloy demonstrates the lowest friction coefficient and wear rate, exhibiting values of 0.513 and 0.020 × 10−3 mm3/Nm, respectively, while the Al0.5Cr0.5CoFeNi alloy demonstrates the highest performance, with a self-corrosion voltage of 0.202 V in a 3.5 wt.% NaCl solution. The experimental findings demonstrate that, in the presence of a decline in the Cr element within a high-entropy alloy, an augmentation in the Al element can facilitate the transition of the FCC phase to the BCC phase within the alloy, thereby enhancing its mechanical properties. However, in the AlxCr1−xCoFeNi HEAs, the presence of the Cr-rich and Cr-poor phases invariably results in selective corrosion in a neutral NaCl solution. The corrosion resistance of this alloy is weaker than that of a single-phase solid solution alloy with a similar chemical composition that only undergoes pitting corrosion.
Open AccessMicrostructure and Properties of AlxCr1−xCoFeNi High-Entropy Alloys Prepared by Spark Plasma Sintering
CoCrFeNi high-entropy alloys represent a novel structural material with considerable application potential in a variety of fields, including aerospace, automobiles, ships, machining, energy, soft magnetic materials, and hydrogen storage materials. The present study investigates the impact of the Al element on the structure and properties of the alloy. The preparation of the AlxCr1−xCoFeNi (x = 0.1, 0.2, 0.3, 0.4, 0.5) powders involved the use of a variety of elemental metal powders as raw materials and a mechanical alloying process at 350 rpm for 40 h. The sintering of the alloy powders was subsequently conducted using spark plasma sintering at 1000 °C. The microstructure of the alloys was analyzed using XRD, SEM, and EDS, and the properties were analyzed using a universal testing machine, a hardness measurement, friction and wear measurement, and an electrochemical workstation. The study shows that when x = 0.1, the crystal structure of Al0.1Cr0.9CoFeNi consists of a double FCC phase and a trace amount of σ phase. As the aluminum content increases, part of the FCC phase begins to transform to BCC. When x = 0.2~0.5, the alloy consists of a double FCC phase and a BCC phase and a trace amount of a sigma phase. As the BCC phase in the alloy increases, the tensile strength of the alloy increases, the ability to deform plastically decreases, and the hardness increases. The highest ultimate tensile strength of 1163.14 MPa is exhibited by Al0.5Cr0.5CoFeNi, while the minimum elongation is 26.98% and the maximum hardness value is 412.6 HV. In the initial stage of friction measurement, the wear mechanism of AlxCr1−xCoFeNi is adhesive wear. However, as the test time progresses, an oxide layer begins to form on the alloy’s surface, leading to a gradual increase in the friction coefficient. At this stage, the wear mechanism becomes a combination of both adhesive and abrasive wear. Once the oxidation process and the wear process have reached a dynamic equilibrium, the friction coefficient stabilizes, and the wear mechanism transitions to a state of abrasive wear. The Al0.1Cr0.9CoFeNi alloy demonstrates the lowest friction coefficient and wear rate, exhibiting values of 0.513 and 0.020 × 10−3 mm3/Nm, respectively, while the Al0.5Cr0.5CoFeNi alloy demonstrates the highest performance, with a self-corrosion voltage of 0.202 V in a 3.5 wt.% NaCl solution. The experimental findings demonstrate that, in the presence of a decline in the Cr element within a high-entropy alloy, an augmentation in the Al element can facilitate the transition of the FCC phase to the BCC phase within the alloy, thereby enhancing its mechanical properties. However, in the AlxCr1−xCoFeNi HEAs, the presence of the Cr-rich and Cr-poor phases invariably results in selective corrosion in a neutral NaCl solution. The corrosion resistance of this alloy is weaker than that of a single-phase solid solution alloy with a similar chemical composition that only undergoes pitting corrosion.
- Open Access
- 18 November 2024
- Published by MDPI AG in Preprints.org
Influence of Al and Cr on the Microstructure and Properties of AlxCr1-xCoFeNi High-Entropy Alloys
The AlCoCrFeNi high entropy alloys are a novel structural material with wide application prospects. In order to investigate the influence of Al and Cr elements on the structure and properties of the alloys, AlxCr1-xCoFeNi (x=0.1, 0.2; 0.3, 0.4, 0.5) HEAs were prepared by mechanical alloying and spark plasma sintering. The microstructure and properties of the AlxCr1-xCoFeNi were analysed using XRD, SEM, EDS, electrochemical workstations, hardness measurement, friction and wear measurement, and room temperature compression measurement. The hardness and friction measurement results demonstrate that when x = 0.1, the crystal structure of Al0.1Cr0.9CoFeNi is composed of dual FCC phases and a trace of σ phase. With the increment of Al content, part of the FCC phase is transformed into BCC phase. When x=0.2~0.5, the alloy is composed of dual FCC phases, BCC phase and a trace σ phase. The Al0.5Cr0.5CoFeNi alloy exhibits the most favourable corrosion resistance, with a self-corrosion voltage of 0.202 V in a 3.5 wt.% NaCl solution. The hardness of alloy increases with the increasing of Al content. The Al0.5Cr0.5CoFeNi alloy exhibits the highest hardness value of 412.6 HV. At the initial stage of friction measurement, the wear mechanism of AlxCr1-xCoFeNi was adhesive wear. As the test time increased, oxide layers began to form on the surface of the alloy, resulting in a gradual increase in the coefficient of friction. At this stage, the wear mechanism was characterised by both adhesive and abrasive wear. Once the oxide layers and the wear processes reached dynamic equilibrium, the friction coefficient stabilised, and the wear mechanism transitioned to abrasive wear. Once the oxide layer and the wear process have reached dynamic equilibrium, the friction coefficient tends to stabilise gradually, and the wear mechanism is changed to abrasive wear. Al0.1Cr0.9CoFeNi has the smallest coefficient of friction of 0.513. Al0.5Cr0.5CoFeNi had the longest compression plateau and the greatest compression strain (59.7%) in the compression tests at room temperature.
- 18 November 2024
- Published by MDPI AG in Preprints.org
Open AccessInfluence of Al and Cr on the Microstructure and Properties of AlxCr1-xCoFeNi High-Entropy Alloys
The AlCoCrFeNi high entropy alloys are a novel structural material with wide application prospects. In order to investigate the influence of Al and Cr elements on the structure and properties of the alloys, AlxCr1-xCoFeNi (x=0.1, 0.2; 0.3, 0.4, 0.5) HEAs were prepared by mechanical alloying and spark plasma sintering. The microstructure and properties of the AlxCr1-xCoFeNi were analysed using XRD, SEM, EDS, electrochemical workstations, hardness measurement, friction and wear measurement, and room temperature compression measurement. The hardness and friction measurement results demonstrate that when x = 0.1, the crystal structure of Al0.1Cr0.9CoFeNi is composed of dual FCC phases and a trace of σ phase. With the increment of Al content, part of the FCC phase is transformed into BCC phase. When x=0.2~0.5, the alloy is composed of dual FCC phases, BCC phase and a trace σ phase. The Al0.5Cr0.5CoFeNi alloy exhibits the most favourable corrosion resistance, with a self-corrosion voltage of 0.202 V in a 3.5 wt.% NaCl solution. The hardness of alloy increases with the increasing of Al content. The Al0.5Cr0.5CoFeNi alloy exhibits the highest hardness value of 412.6 HV. At the initial stage of friction measurement, the wear mechanism of AlxCr1-xCoFeNi was adhesive wear. As the test time increased, oxide layers began to form on the surface of the alloy, resulting in a gradual increase in the coefficient of friction. At this stage, the wear mechanism was characterised by both adhesive and abrasive wear. Once the oxide layers and the wear processes reached dynamic equilibrium, the friction coefficient stabilised, and the wear mechanism transitioned to abrasive wear. Once the oxide layer and the wear process have reached dynamic equilibrium, the friction coefficient tends to stabilise gradually, and the wear mechanism is changed to abrasive wear. Al0.1Cr0.9CoFeNi has the smallest coefficient of friction of 0.513. Al0.5Cr0.5CoFeNi had the longest compression plateau and the greatest compression strain (59.7%) in the compression tests at room temperature.