Arne Schiller
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Arne Schiller has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Chiara Bisagni
Department of Aerospace Science and Technology, Politecnico di Milano, Via La Masa 34, 20156 Milano, Italy
2 shared publications Andreas Dengg
1 shared publicationChiara Bisagni
Politecnico di Milano
1 shared publication- Christoph Kralovec
Institute of Structural Lightweight Design, Johannes Kepler University Linz, Altenberger Strasse 69, 4040 Linz, Austria
1 shared publication - Jan Haubrich
Institute for Frontier Materials on Earth and in Space, German Aerospace Center (DLR e.V. Deutsches Zentrum für Luft-und Raumfahrt), Linder Höhe, D-51147 Cologne, Germany
1 shared publication Martin Schagerl
1 shared publication
Latest Publications
- Open Access
- 15 June 2026
- Published by SAGE Publications in Journal of Thermoplastic Composite Materials
Experimental investigation of thermoplastic welded single-lap shear joints with a recycled core
Thermoplastic welded single-lap shear joints made from sandwich-like adherends with a recycled core and virgin face sheets are tested to measure their load-carrying capacity and to quantify damage growth. The results are compared with single-lap shear joints entirely made from laminates consisting of virgin materials. The adherend constituents are T300/polyphenylene sulfide (T300/PPS) and T700/low-melt polyaryletherketone (T700/LM-PAEK), joined via induction and conduction welding, respectively. Test bench data, digital image correlation, a high-speed camera, and microscopy are used to evaluate the structural response of the specimens. Damage initiation and propagation are heavily influenced by the actually welded interface regions. While the virgin joints only experience damage growth along the welded interface, adherend failure can also occur in the recycled core joints. The recycled core joints show a reduced lap shear strength compared to their virgin counterparts, limited to less than 14% for the induction welded T300/PPS specimens and around 40% for the conduction welded T700/LM-PAEK specimens. Despite the reduction in load-carrying capacity, recycled core joints may be considered as a suitable alternative in scenarios where the requirements for mechanical properties are less dominant and environmental considerations are more relevant.
- 15 June 2026
- Published by SAGE Publications in Journal of Thermoplastic Composite Materials
Open AccessExperimental investigation of thermoplastic welded single-lap shear joints with a recycled core
Thermoplastic welded single-lap shear joints made from sandwich-like adherends with a recycled core and virgin face sheets are tested to measure their load-carrying capacity and to quantify damage growth. The results are compared with single-lap shear joints entirely made from laminates consisting of virgin materials. The adherend constituents are T300/polyphenylene sulfide (T300/PPS) and T700/low-melt polyaryletherketone (T700/LM-PAEK), joined via induction and conduction welding, respectively. Test bench data, digital image correlation, a high-speed camera, and microscopy are used to evaluate the structural response of the specimens. Damage initiation and propagation are heavily influenced by the actually welded interface regions. While the virgin joints only experience damage growth along the welded interface, adherend failure can also occur in the recycled core joints. The recycled core joints show a reduced lap shear strength compared to their virgin counterparts, limited to less than 14% for the induction welded T300/PPS specimens and around 40% for the conduction welded T700/LM-PAEK specimens. Despite the reduction in load-carrying capacity, recycled core joints may be considered as a suitable alternative in scenarios where the requirements for mechanical properties are less dominant and environmental considerations are more relevant.
- Open Access
- 29 April 2026
- Published by MDPI AG in Journal of Composites Science
- Vol. 10 (5) , 241
Experimental Evaluation of Induction- and Conduction-Welded Thermoplastic Composite Single-Lap Shear Joints
Single-lap shear joints made from fabric T300/polyphenylene sulfide (T300/PPS) and unidirectional T700/low-melt polyaryletherketone (T700/LM-PAEK) laminates are joined via induction and conduction welding at different processing temperatures. The joints are tested experimentally to investigate the influence of the processing temperature on the damage evolution in the specimens which is tracked using digital image correlation. Cracks grow rapidly in the unwelded parts of the joint interface but assume a stable steady-state propagation rate when reaching the fully welded overlap region. It is found that higher welding temperatures lead to longer weld lengths, which improve the strength and stiffness of the specimens and delay damage initiation. An accelerated crack growth rate indicates that the structure is close to its ultimate load after which the joint fails abruptly as the crack growth becomes unstable. Induction welding temperatures at the upper end of the recommended processing window (330 °C for T300/PPS and 385 °C for T700/LM-PAEK) result in the joints with the highest load-carrying capacity and slowest crack propagation, but also the least damage tolerance.
- 29 April 2026
- Published by MDPI AG in Journal of Composites Science
- Vol. 10 (5) , 241
Open AccessExperimental Evaluation of Induction- and Conduction-Welded Thermoplastic Composite Single-Lap Shear Joints
Single-lap shear joints made from fabric T300/polyphenylene sulfide (T300/PPS) and unidirectional T700/low-melt polyaryletherketone (T700/LM-PAEK) laminates are joined via induction and conduction welding at different processing temperatures. The joints are tested experimentally to investigate the influence of the processing temperature on the damage evolution in the specimens which is tracked using digital image correlation. Cracks grow rapidly in the unwelded parts of the joint interface but assume a stable steady-state propagation rate when reaching the fully welded overlap region. It is found that higher welding temperatures lead to longer weld lengths, which improve the strength and stiffness of the specimens and delay damage initiation. An accelerated crack growth rate indicates that the structure is close to its ultimate load after which the joint fails abruptly as the crack growth becomes unstable. Induction welding temperatures at the upper end of the recommended processing window (330 °C for T300/PPS and 385 °C for T700/LM-PAEK) result in the joints with the highest load-carrying capacity and slowest crack propagation, but also the least damage tolerance.
- Open Access
- 6 December 2024
- Published by Elsevier in Composite Structures
- Vol. 354
Static strength and fatigue life of pinned hybrid titanium-composite single-lap-shear joints
- 6 December 2024
- Published by Elsevier in Composite Structures
- Vol. 354
Open AccessStatic strength and fatigue life of pinned hybrid titanium-composite single-lap-shear joints