    Comparative study of ISO 15614-1 and VGB-S-013 requirements for welded joints of steel X10CrMoVNb9-1

    by Aleksandra Krstevska, Filip Zdraveski, Marjan Gavriloski, Martin Petreski

    The martensitic steel X10CrMoVNb9‑1 is widely used in high temperature components in power plants where strict welding and post weld heat treatment (PWHT) requirements are important to ensure long term safe operation. International standards and technical regulations define different qualification criteria for welded joints and PWHT parameters. This paper presents a comparative analysis of the requirements specified in ISO 15614-1 and VGB-S-013 guidelines for the qualification of welded joints in X10CrMoVNb9-1 steel. The analysis focuses on PWHT temperature ranges, holding times, acceptance criteria for mechanical properties and overall welding procedures specifications. The paper highlights how varying normative approaches can influence the qualification of welded joints in power plant components and provides practical insight involved in welding procedure selection and approval. The presented study provides a foundation for further investigation of the metallurgical and mechanical properties resulting from the standard that defines welding procedure specifications and technical regulations requirements.

  • Open Access

    Investigation of the possibility of direct welding of X10CrMoVNb9-1 steel tubes with austenitic filler material without post-weld heat treatment

    by Vladan Jeremić, Miloš Pavlović, Filip Zdraveski, Aleksandra Krstevska

    The idea for this paper was motivated by a practical problem encountered during the replacement of a boiler reheater coils made of X10CrMoVNb9-1 steel tubes with dimensions 32x4mm. Specifically, welding this material requires post-weld heat treatment (PWHT). Welding the site joints between the header tube ends and the coil tube ends, within a confined space, presents a particular challenge because there are to many. This is more demanding when the welding sequence is not arbitrary but must be strictly followed. Under these conditions, post-weld heat treatment of every welded joint significantly complicates the reheater assembly procedure, and substantially extends the downtime required for job completion. Therefore, the study examines whether the joint could be made via direct welding, using austenitic filler material based on Ni, to avoid post-weld heat treatment, especially considering the small diameter and wall thickness used in the coil tubes.

  • A review study on hydrogen embrittlement of steel

    by Elena Anastasovska, Elisaveta Doncheva, Filip Zdraveski

    A common and intricate phenomenon known as hydrogen embrittlement of steel is the deterioration of the mechanical properties of metal in relation to stress corrosion cracking. This phenomenon has been extensively studied, with numerous works proposed over the last two decades, but there is still a lack of unified solutions and a solid understanding of the phenomenon. The purpose of this paper is to provide a review of the literature and publications on hydrogen embrittlement in steel. It focuses on recent developments and methods that have contributed to a better understanding of the relationship between steel structure, properties, and performance, with a particular emphasis on hydrogen diffusion, characterisation, mechanisms, and prevention of hydrogen embrittlement in structural steel. Furthermore, the paper discusses recent advances in experimental and multi-scale modelling and proposes future studies to address challenges related to hydrogen embrittlement in steels.