Jack Bollard
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Jack Bollard has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Emily Heppell
Clarendon Laboratory, Department of Physics, University of Oxford, Oxford OX1 3PU, UK
3 shared publications - Gerrit van der Laan
Diamond Light Source, Harwell Science and Innovation Campus, Didcot, UK
3 shared publications - Joshua Bibby
Clarendon Laboratory, Department of Physics, University of Oxford, Oxford OX1 3PU, UK
3 shared publications - Thorsten Hesjedal
University of Oxford
3 shared publications - Angadjit Singh
Clarendon Laboratory, Department of Physics, University of Oxford, Oxford OX1 3PU, UK
2 shared publications - Balati Kuerbanjiang
Clarendon Laboratory, Department of Physics, University of Oxford, Oxford OX1 3PU, UK
2 shared publications
Latest Publications
- Open Access
Structural and Magnetic Properties of Sputtered Chromium-Doped Sb2Te3 Thin Films
Magnetron sputtering offers a scalable route to magnetic topological insulators (MTIs) based on Cr-doped Sb2Te3. We combine a range of X-ray diffraction (XRD), reciprocal-space mapping (RSM), scanning transmission electron microscopy (STEM), scanning TEM-energy-dispersive X-ray spectroscopy (STEM-EDS), and X-ray absorption spectroscopy, and X-ray magnetic circular dichroism (XAS/XMCD) techniques to study the structure and magnetism of Cr-doped Sb2Te3 films. Symmetric -2 XRD and RSM establish a solubility window. Layered tetradymite order persists up to ∼10 at.-% Cr, while higher doping yields CrTe/Cr2Te3 secondary phases. STEM reveals nanocrystalline layered stacking at low Cr and loss of long-range layering at higher Cr concentrations, consistent with XRD/RSM. Magnetometry on a 6% film shows soft ferromagnetism at 5 K. XAS and XMCD at the Cr edges exhibits a depth dependence: total electron yield (TE; surface sensitive) shows both nominal Cr2+ and Cr3+, whereas fluorescence yield (FY; bulk sensitive) shows a much higher Cr2+ weight. Sum rules applied to TEY give /Cr, and /Cr, whereby we note that the applied maximum field (3 T) likely underestimates . These results define a practical growth window and outline key parameters for MTI films.Open AccessStructural and Magnetic Properties of Sputtered Chromium-Doped Sb2Te3 Thin Films
Magnetron sputtering offers a scalable route to magnetic topological insulators (MTIs) based on Cr-doped Sb2Te3. We combine a range of X-ray diffraction (XRD), reciprocal-space mapping (RSM), scanning transmission electron microscopy (STEM), scanning TEM-energy-dispersive X-ray spectroscopy (STEM-EDS), and X-ray absorption spectroscopy, and X-ray magnetic circular dichroism (XAS/XMCD) techniques to study the structure and magnetism of Cr-doped Sb2Te3 films. Symmetric -2 XRD and RSM establish a solubility window. Layered tetradymite order persists up to ∼10 at.-% Cr, while higher doping yields CrTe/Cr2Te3 secondary phases. STEM reveals nanocrystalline layered stacking at low Cr and loss of long-range layering at higher Cr concentrations, consistent with XRD/RSM. Magnetometry on a 6% film shows soft ferromagnetism at 5 K. XAS and XMCD at the Cr edges exhibits a depth dependence: total electron yield (TE; surface sensitive) shows both nominal Cr2+ and Cr3+, whereas fluorescence yield (FY; bulk sensitive) shows a much higher Cr2+ weight. Sum rules applied to TEY give /Cr, and /Cr, whereby we note that the applied maximum field (3 T) likely underestimates . These results define a practical growth window and outline key parameters for MTI films. - Open Access
- 28 August 2025
- Published by Wiley in Physica Status Solidi (RRL) – Rapid Research Letters
- Vol. 19 (10)
Sputter‐Grown MnBi 2 Te 4 Thin Films: Magnetic Ground States and Phase Control
The synthesis and magnetic properties of the intrinsic magnetic topological insulator MnBi 2 Te 4 , grown by magnetron sputtering, are investigated. While this growth method enables smoother morphologies than molecular beam epitaxy and is compatible with scalable processing, the metastable nature of MnBi 2 Te 4 presents considerable challenges in phase control and magnetic uniformity. By systematically varying the relative sputter powers of Mn, Bi 2 Te 3 , and Te targets, conditions that favor the formation of near‐stoichiometric MnBi 2 Te 4 , as supported by X‐ray diffraction, atomic force microscopy, and energy‐dispersive X‐ray spectroscopy, are identified. These films exhibit reduce surface roughness and lower twin‐domain density compared to Mn‐rich counterparts, which show evidence of phase separation and structural disorder. Magnetometry and X‐ray magnetic circular dichroism reveal that both film types exhibit sizable Mn moments, although signatures of antiferromagnetic order are only weakly expressed and appear sensitive to composition and morphology. Despite producing structurally well‐ordered films, clear linear dichroism attributable to A‐type antiferromagnetic ordering is not observed, suggesting magnetic inhomogeneity or suppression of interlayer coupling. These results highlight the compositional sensitivity of sputtered MnBi 2 Te 4 and underline the difficulties in stabilizing the intrinsic magnetic topological phase in thin‐film form.
- 28 August 2025
- Published by Wiley in Physica Status Solidi (RRL) – Rapid Research Letters
- Vol. 19 (10)
Open AccessSputter‐Grown MnBi 2 Te 4 Thin Films: Magnetic Ground States and Phase Control
The synthesis and magnetic properties of the intrinsic magnetic topological insulator MnBi 2 Te 4 , grown by magnetron sputtering, are investigated. While this growth method enables smoother morphologies than molecular beam epitaxy and is compatible with scalable processing, the metastable nature of MnBi 2 Te 4 presents considerable challenges in phase control and magnetic uniformity. By systematically varying the relative sputter powers of Mn, Bi 2 Te 3 , and Te targets, conditions that favor the formation of near‐stoichiometric MnBi 2 Te 4 , as supported by X‐ray diffraction, atomic force microscopy, and energy‐dispersive X‐ray spectroscopy, are identified. These films exhibit reduce surface roughness and lower twin‐domain density compared to Mn‐rich counterparts, which show evidence of phase separation and structural disorder. Magnetometry and X‐ray magnetic circular dichroism reveal that both film types exhibit sizable Mn moments, although signatures of antiferromagnetic order are only weakly expressed and appear sensitive to composition and morphology. Despite producing structurally well‐ordered films, clear linear dichroism attributable to A‐type antiferromagnetic ordering is not observed, suggesting magnetic inhomogeneity or suppression of interlayer coupling. These results highlight the compositional sensitivity of sputtered MnBi 2 Te 4 and underline the difficulties in stabilizing the intrinsic magnetic topological phase in thin‐film form.
- Open Access
Synthesis of Nanocrystalline Mn-Doped Bi2Te3 Thin Films via Magnetron Sputtering
This study reports the structural and magnetic properties of Mn-doped thin films grown by magnetron sputtering. The films exhibit a ferromagnetic response that depends on the Mn doping concentration, as revealed by X-ray magnetic circular dichroism measurements. At an Mn concentration of ∼6.0%, a magnetic moment of (3.48 ± 0.25) /Mn was determined. Structural analysis indicated the presence of a secondary phase, which complicates the interpretation of the magnetic properties. Additionally, the incorporation of Mn ions within the van der Waals gap and substitutional doping on Bi sites contributes to the observed complex magnetic properties. Intriguingly, a decrease in magnetic moment per Mn was observed with increasing Mn concentration, which is consistent with the formation of the intrinsic magnetic topological insulator .Open AccessSynthesis of Nanocrystalline Mn-Doped Bi2Te3 Thin Films via Magnetron Sputtering
This study reports the structural and magnetic properties of Mn-doped thin films grown by magnetron sputtering. The films exhibit a ferromagnetic response that depends on the Mn doping concentration, as revealed by X-ray magnetic circular dichroism measurements. At an Mn concentration of ∼6.0%, a magnetic moment of (3.48 ± 0.25) /Mn was determined. Structural analysis indicated the presence of a secondary phase, which complicates the interpretation of the magnetic properties. Additionally, the incorporation of Mn ions within the van der Waals gap and substitutional doping on Bi sites contributes to the observed complex magnetic properties. Intriguingly, a decrease in magnetic moment per Mn was observed with increasing Mn concentration, which is consistent with the formation of the intrinsic magnetic topological insulator .