Maksim A. Sysoev
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Maksim A. Sysoev has a total of 17 co-authors. Here are the top co-authors by number of shared publications:
A.YU. Mironovich
1 shared publication- Adolf Sergeevich Nogai
Energy Institute, Saken Seifullin Kazakh Agrotechnical University, Zhenis Ave., 62, Astana 010011, Kazakhstan
1 shared publication - Albert A. Alekseev
JSC “NPP “Istok” named after Shokin”, Fryazino, Russia
1 shared publication - Aleksey I. Ril’
Kurnakov Institute of General and Inorganic Chemistry, Russian Academy of Sciences, Moscow, Russia
1 shared publication - Alexander A. Bush
MIREA - Russian Technological University, Moscow, Russia
1 shared publication - Alexey Valentinovich Trukhanov
SSPA “Scientific and practical materials research center of NAS of Belarus”, 220072 Minsk, Belarus
1 shared publication
Latest Publications
- Open Access
- 30 June 2025
- Published by Pensoft Publishers in Modern Electronic Materials
- Vol. 11 (2) , 111-123
Crystal and magnetic structure of hexagonal anisotropic polycrystalline ferrites SrFe12O19 obtained by radiation-thermal sintering
Hexagonal anisotropic strontium ferrite has found wide application in the fabrication of permanent magnets, active media of UHF electronic devices, and photonics. The performance of hexagonal strontium ferrites depends largely on the synthesis technology. Anisotropic SrFe12O19 samples have been for the first time synthesized using radiation-thermal sintering (RTS) in a fast electron beam from an electron accelerator. The RTS temperature was varied between 1200 and 1400 °C, and the process time, from 10 to 90 min. The phase composition and lattice parameters of the samples have been monitored using X-ray diffraction and Mössbauer spectroscopy. The X-ray spectra have been recorded with a DRON-8 diffractometer in CoKα1 radiation, and the Mössbauer spectra, using an MS1104E spectrometer with a constant acceleration at room temperature, the radiation source being Со57 in a chromium matrix. The density of the specimens has been studied in accordance with Archimedes’ law on a UW620H electronic balance with a density measurement attachment. The X-ray diffraction and Mössbauer spectroscopy data show that the samples are single-phase and have the P63/mmc (No. 194) space group, corresponding to the hexagonal ferrite structure. The unit cell parameters a and c and the volume V of the samples have been studied as a function of RTS temperature for the sintering time t = 30 and 60 min. Also, the unit cell parameters a and c and the volume V of the samples have been studied as a function of sintering time for the RTS temperature T = 1300 °C. The lattice parameters a and c of the samples exhibit opposite dependences, suggesting anisotropic lattice distortion. The maximum magnetic texture degree achieved using RTS in anisotropic SrFe12O19 proves to be about 92%. It has been concluded on the basis of the Mössbauer spectroscopy data that the optimum magnetization degree of the SrFe12O19 samples is achieved for the following RTS modes (RTS temperature, °C / RTS time, min): 1300/60 and 1350/40. We show that the sintering temperature plays a considerably greater role in the RTS technology than the sintering time. Conclusion has been made that RTS can be used as an alternative technology of synthesizing polycrystalline anisotropic hexagonal SrFe12O19 ferrite. As compared to the conventional ceramic technology, RTS proves to be highly energy-efficient and cheap.
- 30 June 2025
- Published by Pensoft Publishers in Modern Electronic Materials
- Vol. 11 (2) , 111-123
Open AccessCrystal and magnetic structure of hexagonal anisotropic polycrystalline ferrites SrFe12O19 obtained by radiation-thermal sintering
Hexagonal anisotropic strontium ferrite has found wide application in the fabrication of permanent magnets, active media of UHF electronic devices, and photonics. The performance of hexagonal strontium ferrites depends largely on the synthesis technology. Anisotropic SrFe12O19 samples have been for the first time synthesized using radiation-thermal sintering (RTS) in a fast electron beam from an electron accelerator. The RTS temperature was varied between 1200 and 1400 °C, and the process time, from 10 to 90 min. The phase composition and lattice parameters of the samples have been monitored using X-ray diffraction and Mössbauer spectroscopy. The X-ray spectra have been recorded with a DRON-8 diffractometer in CoKα1 radiation, and the Mössbauer spectra, using an MS1104E spectrometer with a constant acceleration at room temperature, the radiation source being Со57 in a chromium matrix. The density of the specimens has been studied in accordance with Archimedes’ law on a UW620H electronic balance with a density measurement attachment. The X-ray diffraction and Mössbauer spectroscopy data show that the samples are single-phase and have the P63/mmc (No. 194) space group, corresponding to the hexagonal ferrite structure. The unit cell parameters a and c and the volume V of the samples have been studied as a function of RTS temperature for the sintering time t = 30 and 60 min. Also, the unit cell parameters a and c and the volume V of the samples have been studied as a function of sintering time for the RTS temperature T = 1300 °C. The lattice parameters a and c of the samples exhibit opposite dependences, suggesting anisotropic lattice distortion. The maximum magnetic texture degree achieved using RTS in anisotropic SrFe12O19 proves to be about 92%. It has been concluded on the basis of the Mössbauer spectroscopy data that the optimum magnetization degree of the SrFe12O19 samples is achieved for the following RTS modes (RTS temperature, °C / RTS time, min): 1300/60 and 1350/40. We show that the sintering temperature plays a considerably greater role in the RTS technology than the sintering time. Conclusion has been made that RTS can be used as an alternative technology of synthesizing polycrystalline anisotropic hexagonal SrFe12O19 ferrite. As compared to the conventional ceramic technology, RTS proves to be highly energy-efficient and cheap.
- Open Access
- 30 May 2024
- Published by World Scientific Pub Co Pte Ltd in Journal of Advanced Dielectrics
- Vol. 15 (01)
Synthesis and study of structural and electrophysical characteristics of piezoceramic section (1–x)(0.8PbMg1∕3Nb2∕3O3⋅0.2BiScO3)⋅ x(0.8PbTiO3⋅0.2BiScO3) of the ternary system BiScO3–PbTiO3–PbMg1∕3Nb2∕3O3
X-ray diffraction and dielectric studies were performed on synthesized ceramic samples of the section (1–x) (0.8PbMg[ ]Nb[ ]O[ ]BiScO3)⋅ x(0.8PbTiO[ ]BiScO3) with [ ]–1 of the ternary BiScO3–PbTiO3–PbMg[ ]Nb[ ]O3 (BS–PT–PMN) system, including the temperature dependence of thermally stimulated depolarization currents (TSDC). It was found that the samples are solid solutions with a perovskite structure, which have cubic symmetry in the range of x = 0–0.587 and tetragonal symmetry in the range of x = 0.680–1. In the intermediate composition range of x = 0.587–0.680 (morphotropic region — MR), the samples consist of a mixture of solid solutions of different symmetries. Data on the change in dielectric properties and TSDC(T) dependencies of solid solutions with a change in their composition were obtained. It was found that samples of compositions x =0–0.625 and 0.6875–1 exhibit relaxor-ferroelectric and conventional ferroelectric properties, respectively, while samples of compositions x = 0.625–0.6875 combine ferroelectric and relaxor-ferroelectric properties.
- 30 May 2024
- Published by World Scientific Pub Co Pte Ltd in Journal of Advanced Dielectrics
- Vol. 15 (01)
Open AccessSynthesis and study of structural and electrophysical characteristics of piezoceramic section (1–x)(0.8PbMg1∕3Nb2∕3O3⋅0.2BiScO3)⋅ x(0.8PbTiO3⋅0.2BiScO3) of the ternary system BiScO3–PbTiO3–PbMg1∕3Nb2∕3O3
X-ray diffraction and dielectric studies were performed on synthesized ceramic samples of the section (1–x) (0.8PbMg[ ]Nb[ ]O[ ]BiScO3)⋅ x(0.8PbTiO[ ]BiScO3) with [ ]–1 of the ternary BiScO3–PbTiO3–PbMg[ ]Nb[ ]O3 (BS–PT–PMN) system, including the temperature dependence of thermally stimulated depolarization currents (TSDC). It was found that the samples are solid solutions with a perovskite structure, which have cubic symmetry in the range of x = 0–0.587 and tetragonal symmetry in the range of x = 0.680–1. In the intermediate composition range of x = 0.587–0.680 (morphotropic region — MR), the samples consist of a mixture of solid solutions of different symmetries. Data on the change in dielectric properties and TSDC(T) dependencies of solid solutions with a change in their composition were obtained. It was found that samples of compositions x =0–0.625 and 0.6875–1 exhibit relaxor-ferroelectric and conventional ferroelectric properties, respectively, while samples of compositions x = 0.625–0.6875 combine ferroelectric and relaxor-ferroelectric properties.