Xiezheng Yu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Xiezheng Yu has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Chenguang Zhu
Nanjing University of Science and Technology
2 shared publications Biyu Chen
1 shared publicationLizhi Wu
School of Chemistry and Chemical Engineering, Nanjing University of Science and Technology, Nanjing, Jiangsu 210094, China
1 shared publicationPeng Zhu
School of Chemistry and Chemical Engineering, Nanjing University of Science and Technology, Nanjing, Jiangsu 210094, China
1 shared publication- Ruiqi Shen
School of Chemistry and Chemical Engineering, Nanjing University of Science and Technology, Nanjing 210094, China
1 shared publication Wenchao Zhang
1 shared publication
Latest Publications
- Open Access
- 1 September 2026
- Published by KEAI Publishing in Defence Technology
Microstructural evolution of PTFE powder under electron beam irradiation and its influence on the processing and performance of MTV energetic materials
- 1 September 2026
- Published by KEAI Publishing in Defence Technology
Open AccessMicrostructural evolution of PTFE powder under electron beam irradiation and its influence on the processing and performance of MTV energetic materials
- Open Access
- 15 January 2025
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 10 (3) , 2940-2948
Wet Anisotropic Etching Characteristics of Si{111} in KOH-Based Solution
Wet chemical etching of silicon has been a topic of significant interest due to its importance in microelectromechanical systems (MEMS), nanotechnology, and semiconductor device fabrication. Many kinds of MEMS components (e.g., cavity, diaphragm, cantilever, etc.) are fabricated through wet anisotropic etching-based silicon bulk micromachining of {100} and {110} oriented silicon wafers. Wet anisotropic etching of silicon is primarily carried out using alkaline solutions such as potassium hydroxide (KOH), tetramethylammonium hydroxide (TMAH), etc. The etching rate of Si{111} crystal planes is significantly slower compared to other planes like Si{100} and Si{110} as a result of its atomic structure and surface properties. Therefore, the Si{111} crystal plane is of particular interest owing to its unique properties and potential applications. In this work, we report the wet anisotropic etching characteristics of Si{111} in KOH with addition of isopropyl alcohol (IPA). Surface morphology of the etched Si{111} surfaces was examined using confocal laser scanning microscopy (CLSM). In all experimental scenarios, the Si{111} crystal surface gives rise to triangular etch pits, the size and depth of these etch pits are contingent upon the etching time. Following your advice, we revised the abstract phrase "become more sharper" in the summary and quantified the angle data of the triangle. The entire statement has been specifically modified to Furthermore, when the additive IPA is incorporated into the etchant, the corners of these triangular etch pits on the surface transitions from rounded to sharp (with each angles of approximately 60°), indicating that the overall shape of these triangular etch recesses approaches that of an equilateral triangle. In addition, the theory of crystal cleavage is introduced to explain the formation mechanism of surface triangular flat-bottom etch pits during the etching process of Si{111} crystal planes. At the same time, the relevant experiments on Si{111} samples with a SiO2 mask layer on the surface have been completed, and the results verify the correctness of the analysis of the relevant mechanism. The relevant results and mechanism presented in this article are of large significance for engineering applications in both academic and industrial laboratories.
- 15 January 2025
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 10 (3) , 2940-2948
Open AccessWet Anisotropic Etching Characteristics of Si{111} in KOH-Based Solution
Wet chemical etching of silicon has been a topic of significant interest due to its importance in microelectromechanical systems (MEMS), nanotechnology, and semiconductor device fabrication. Many kinds of MEMS components (e.g., cavity, diaphragm, cantilever, etc.) are fabricated through wet anisotropic etching-based silicon bulk micromachining of {100} and {110} oriented silicon wafers. Wet anisotropic etching of silicon is primarily carried out using alkaline solutions such as potassium hydroxide (KOH), tetramethylammonium hydroxide (TMAH), etc. The etching rate of Si{111} crystal planes is significantly slower compared to other planes like Si{100} and Si{110} as a result of its atomic structure and surface properties. Therefore, the Si{111} crystal plane is of particular interest owing to its unique properties and potential applications. In this work, we report the wet anisotropic etching characteristics of Si{111} in KOH with addition of isopropyl alcohol (IPA). Surface morphology of the etched Si{111} surfaces was examined using confocal laser scanning microscopy (CLSM). In all experimental scenarios, the Si{111} crystal surface gives rise to triangular etch pits, the size and depth of these etch pits are contingent upon the etching time. Following your advice, we revised the abstract phrase "become more sharper" in the summary and quantified the angle data of the triangle. The entire statement has been specifically modified to Furthermore, when the additive IPA is incorporated into the etchant, the corners of these triangular etch pits on the surface transitions from rounded to sharp (with each angles of approximately 60°), indicating that the overall shape of these triangular etch recesses approaches that of an equilateral triangle. In addition, the theory of crystal cleavage is introduced to explain the formation mechanism of surface triangular flat-bottom etch pits during the etching process of Si{111} crystal planes. At the same time, the relevant experiments on Si{111} samples with a SiO2 mask layer on the surface have been completed, and the results verify the correctness of the analysis of the relevant mechanism. The relevant results and mechanism presented in this article are of large significance for engineering applications in both academic and industrial laboratories.