Wen Cao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Wen Cao has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Congcong Yang
School of Minerals Processing and Bioengineering, Central South University, Changsha, P.R. China
3 shared publications - Deqing Zhu
School of Minerals Processing and Bioengineering, Central South University, Changsha, P.R. China
3 shared publications - Jian Pan
School of Minerals Processing and Bioengineering, Central South University, Changsha, P.R. China
3 shared publications - Mengjie Hu
School of Minerals Processing and Bioengineering, Central South University, Changsha 410083, China
3 shared publications - Siwei Li
School of Minerals Processing and Bioengineering, Central South University, Changsha 410083, China
3 shared publications - Zhengqi Guo
School of Minerals Processing and Bioengineering, Central South University, Changsha, P.R. China
3 shared publications
Latest Publications
- Open Access
Fe–P Alloy Production from High-Phosphorus Oolitic Iron Ore via Efficient Pre-Reduction and Smelting Separation
Diverging from conventional dephosphorization approaches, this study employs a novel pre-reduction and smelting separation (PR-SS) to efficiently co-recover iron and phosphorus from high-phosphorus oolitic iron ore, directly yielding Fe–P alloy, and the Fe–P alloy shows potential as feedstock for high-phosphorus weathering steel or wear-resistant cast iron, indicating promising application prospects. Using oolitic magnetite concentrate (52.06% Fe, 0.37% P) as feedstock, optimized conditions including pre-reduction at 1050 °C for 2 h with C/Fe mass ratio of 2, followed by smelting separation at 1550 °C for 20 min with 5% coke, produced a metallic phase containing 99.24% Fe and 0.73% P. Iron and phosphorus recoveries reached 99.73% and 99.15%, respectively. EPMA microanalysis confirmed spatial correlation between iron and phosphorus in the metallic phase, with undetectable phosphorus signals in vitreous slag. This evidence suggests preferential phosphorus enrichment through interfacial mass transfer along the pathway of the slag phase to the metal interface and finally the iron matrix, forming homogeneous Fe–P solid solutions. The phosphorus migration mechanism involves sequential stages: apatite lattice decomposition liberates reactive P2O5 under SiO2/Al2O3 influence; slag–iron interfacial co-reduction generates Fe3P intermediates; Fe3P incorporation into the iron matrix establishes stable solid solutions.
Open AccessFe–P Alloy Production from High-Phosphorus Oolitic Iron Ore via Efficient Pre-Reduction and Smelting Separation
Diverging from conventional dephosphorization approaches, this study employs a novel pre-reduction and smelting separation (PR-SS) to efficiently co-recover iron and phosphorus from high-phosphorus oolitic iron ore, directly yielding Fe–P alloy, and the Fe–P alloy shows potential as feedstock for high-phosphorus weathering steel or wear-resistant cast iron, indicating promising application prospects. Using oolitic magnetite concentrate (52.06% Fe, 0.37% P) as feedstock, optimized conditions including pre-reduction at 1050 °C for 2 h with C/Fe mass ratio of 2, followed by smelting separation at 1550 °C for 20 min with 5% coke, produced a metallic phase containing 99.24% Fe and 0.73% P. Iron and phosphorus recoveries reached 99.73% and 99.15%, respectively. EPMA microanalysis confirmed spatial correlation between iron and phosphorus in the metallic phase, with undetectable phosphorus signals in vitreous slag. This evidence suggests preferential phosphorus enrichment through interfacial mass transfer along the pathway of the slag phase to the metal interface and finally the iron matrix, forming homogeneous Fe–P solid solutions. The phosphorus migration mechanism involves sequential stages: apatite lattice decomposition liberates reactive P2O5 under SiO2/Al2O3 influence; slag–iron interfacial co-reduction generates Fe3P intermediates; Fe3P incorporation into the iron matrix establishes stable solid solutions.
- Open Access
Efficient Removal of Impurities from Refractory Oolitic Magnetite Concentrate via High-Pressure Alkaline Leaching and Ultrasonic Acid Leaching Process
Acid leaching is an effective method for dephosphorization; however, it is time-consuming and requires a high amount of acid consumption, resulting in increased production costs and environmental risks. This work aims to remove silicon, aluminum, and phosphorus from high-phosphorus oolitic magnetite concentrate through high-pressure alkaline leaching and ultrasonic acid leaching. Compared with traditional acid leaching processes, the sulfuric acid dosage can be significantly reduced from 200 kg/t to 100 kg/t, and the pickling time is shortened from 60 min to 10 min. Thermodynamic and kinetic studies have demonstrated that acid leaching facilitates apatite dissolution at low temperatures, whereas the dephosphorization reaction is controlled mainly by diffusion. The application of ultrasonic waves leads to finer particle sizes and greatly increased specific surface areas, thereby accelerating the diffusion rate of the leaching agent. Furthermore, microscopic analysis revealed that under the influence of ultrasonic waves, numerous micro-fragments and pores form on particle surfaces due to cavitation effects and mechanical forces generated by ultrasonic waves. These factors promote both the reaction rates and diffusion processes of the leaching agent while enhancing the overall leaching efficiency.
Open AccessEfficient Removal of Impurities from Refractory Oolitic Magnetite Concentrate via High-Pressure Alkaline Leaching and Ultrasonic Acid Leaching Process
Acid leaching is an effective method for dephosphorization; however, it is time-consuming and requires a high amount of acid consumption, resulting in increased production costs and environmental risks. This work aims to remove silicon, aluminum, and phosphorus from high-phosphorus oolitic magnetite concentrate through high-pressure alkaline leaching and ultrasonic acid leaching. Compared with traditional acid leaching processes, the sulfuric acid dosage can be significantly reduced from 200 kg/t to 100 kg/t, and the pickling time is shortened from 60 min to 10 min. Thermodynamic and kinetic studies have demonstrated that acid leaching facilitates apatite dissolution at low temperatures, whereas the dephosphorization reaction is controlled mainly by diffusion. The application of ultrasonic waves leads to finer particle sizes and greatly increased specific surface areas, thereby accelerating the diffusion rate of the leaching agent. Furthermore, microscopic analysis revealed that under the influence of ultrasonic waves, numerous micro-fragments and pores form on particle surfaces due to cavitation effects and mechanical forces generated by ultrasonic waves. These factors promote both the reaction rates and diffusion processes of the leaching agent while enhancing the overall leaching efficiency.