Chan Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Chan Li has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Fei Gao
Key Laboratory of Materials Modification by Laser, Ion, and Electron Beams (Ministry of Education), School of Physics, Dalian University of Technology 1 , Dalian 116024
2 shared publications - Li-Yue Gong
Key Laboratory of Materials Modification by Laser, Ion, and Electron Beams, School of Physics, Dalian University of Technology , Dalian 116024
2 shared publications - Xianxiu Mei
Key Laboratory of Materials Modification By Laser, Ion and Electron Beams, Ministry of Education, Dalian University of Technology, Dalian 116024, People’s Republic of China
2 shared publications - Yong-Xin Liu
Dalian University of Technology
2 shared publications - Ziyan Tan
Key Laboratory of Materials Modification By Laser, Ion and Electron Beams, Ministry of Education, Dalian University of Technology, Dalian 116024, People’s Republic of China
2 shared publications - Ming-Jian Zhang
Key Laboratory of Materials Modification By Laser, Ion and Electron Beams, Ministry of Education, Dalian University of Technology, Dalian 116024, People’s Republic of China
1 shared publication
Latest Publications
- 4 September 2025
- Published by IOP Publishing in Journal of Physics D: Applied Physics
- Vol. 58 (36) , 365203
A study on etching properties of quartz and silicon by a dual-frequency (60 MHz/400 kHz) capacitively coupled NF3/Ar/O2 plasma: effect of pressure
Influence of pressure variation on the etching characteristics of various materials (including rough quartz, smooth quartz, monocrystalline silicon, polished monocrystalline silicon, and polycrystalline silicon) was investigated in a dual-frequency (60 MHz/400 kHz) capacitively coupled NF3/Ar/O2 plasma. The experimental results indicate that with increasing the pressure, the concentration of the fluorine radical in the plasma increases, which promotes the etching of quartz and silicon. Etching behavior varies for different surface types: for quartz, the rough surface exhibits a higher etch rate than the smooth surface due to the presence of more surface defects that provide additional reactive sites. It is found that after being etched, the rough quartz surface features etch pits and spherical structures. For silicon, polycrystalline silicon demonstrates the highest etch rate, attributed to its abundant grain boundaries, and developed pronounced irregular surface features. Monocrystalline silicon exhibited similar morphology after etching, while polished monocrystalline silicon shows minimal changes in surface structure due to its smoothness, resulting in weaker etching reactions. A comparison between quartz and silicon etching revealed that quartz, with its higher Si–O bond energy, had a relatively lower etch rate. In contrast, silicon, characterized by lower Si–Si bond energy, can react more readily with fluorine atom to form volatile SiF4, resulting in a higher etch rate. This study elucidates the impact of pressure and surface structure on etching behavior and discusses respective etching mechanisms of quartz and silicon. The findings provide a theoretical foundation for optimizing plasma etching processes and improving material resistance to etching.
- 4 September 2025
- Published by IOP Publishing in Journal of Physics D: Applied Physics
- Vol. 58 (36) , 365203
A study on etching properties of quartz and silicon by a dual-frequency (60 MHz/400 kHz) capacitively coupled NF3/Ar/O2 plasma: effect of pressure
Influence of pressure variation on the etching characteristics of various materials (including rough quartz, smooth quartz, monocrystalline silicon, polished monocrystalline silicon, and polycrystalline silicon) was investigated in a dual-frequency (60 MHz/400 kHz) capacitively coupled NF3/Ar/O2 plasma. The experimental results indicate that with increasing the pressure, the concentration of the fluorine radical in the plasma increases, which promotes the etching of quartz and silicon. Etching behavior varies for different surface types: for quartz, the rough surface exhibits a higher etch rate than the smooth surface due to the presence of more surface defects that provide additional reactive sites. It is found that after being etched, the rough quartz surface features etch pits and spherical structures. For silicon, polycrystalline silicon demonstrates the highest etch rate, attributed to its abundant grain boundaries, and developed pronounced irregular surface features. Monocrystalline silicon exhibited similar morphology after etching, while polished monocrystalline silicon shows minimal changes in surface structure due to its smoothness, resulting in weaker etching reactions. A comparison between quartz and silicon etching revealed that quartz, with its higher Si–O bond energy, had a relatively lower etch rate. In contrast, silicon, characterized by lower Si–Si bond energy, can react more readily with fluorine atom to form volatile SiF4, resulting in a higher etch rate. This study elucidates the impact of pressure and surface structure on etching behavior and discusses respective etching mechanisms of quartz and silicon. The findings provide a theoretical foundation for optimizing plasma etching processes and improving material resistance to etching.
- 18 February 2025
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B
- Vol. 43 (2)
Study on the etching mechanism of quartz using dual-frequency (60 MHz/400 KHz) capacitively coupled C4F8/Ar/O2 plasma
The etching characteristics of quartz (SiO2) materials were investigated in a dual-frequency (60 MHz/400 KHz) capacitively coupled C4F8/Ar/O2 plasma environment by adjusting the oxygen flow rate, and the etching behaviors of quartz with smooth and rough surfaces were comparatively studied. The experimental results indicate that as the oxygen flow rate increased from 0 to 30 SCCM, the relative concentration of F radicals gradually increased, resulting in a higher etching rate and surface roughness. When the oxygen flow rate reached 40 SCCM, the relative concentration of F radicals decreased, causing the etching rate and surface roughness to decrease accordingly. The fluorocarbon polymer layer on the smooth quartz surface was thicker, causing a slower etching rate and resulting in the formation of etching pits and spikelike protrusions. In contrast, the thinner fluorocarbon polymer layer on rough quartz, likely due to its higher surface roughness, facilitated enhanced ion bombardment, leading to uneven deposition of the fluorocarbon layer. The higher roughness of rough quartz also allowed F atoms to penetrate surface grooves more easily, resulting in a higher etching rate than that of smooth quartz and the formation of numerous small spherical particles and etching pits. These findings demonstrate that surface roughness has a significant impact on the etching behavior of quartz materials.
- 18 February 2025
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B
- Vol. 43 (2)
Study on the etching mechanism of quartz using dual-frequency (60 MHz/400 KHz) capacitively coupled C4F8/Ar/O2 plasma
The etching characteristics of quartz (SiO2) materials were investigated in a dual-frequency (60 MHz/400 KHz) capacitively coupled C4F8/Ar/O2 plasma environment by adjusting the oxygen flow rate, and the etching behaviors of quartz with smooth and rough surfaces were comparatively studied. The experimental results indicate that as the oxygen flow rate increased from 0 to 30 SCCM, the relative concentration of F radicals gradually increased, resulting in a higher etching rate and surface roughness. When the oxygen flow rate reached 40 SCCM, the relative concentration of F radicals decreased, causing the etching rate and surface roughness to decrease accordingly. The fluorocarbon polymer layer on the smooth quartz surface was thicker, causing a slower etching rate and resulting in the formation of etching pits and spikelike protrusions. In contrast, the thinner fluorocarbon polymer layer on rough quartz, likely due to its higher surface roughness, facilitated enhanced ion bombardment, leading to uneven deposition of the fluorocarbon layer. The higher roughness of rough quartz also allowed F atoms to penetrate surface grooves more easily, resulting in a higher etching rate than that of smooth quartz and the formation of numerous small spherical particles and etching pits. These findings demonstrate that surface roughness has a significant impact on the etching behavior of quartz materials.