Latest Publications

  • Differentiation of electrode contributions to the total impedance of lithium-sulfur cells using the distribution function of relaxation times

    by Dmitry V. Kolosnitsyn, Nadezhda V. Egorova, Regina V. Khasanova, Elena V. Karaseva, Vladimir S. Kolosnitsyn

    The analysis of electrochemical impedance of lithium-sulfur cells is complicated by the complexity of the processes occurring inside them. Both electrochemical processes and mass transport processes simultaneously occur on the lithium and sulfur electrodes of the cells, as well as in the bulk electrolyte. A comparative analysis of the distribution functions of relaxation times of symmetric Li||Li, S||Sand and the full lithium-sulfur cell has been conducted. Being a model-independent approach, the distribution functions of relaxation times method lets us objectively identify the number of relaxation processes and their relaxation times. The subsequent comparison of the data from the full and the symmetrical cells enables us to make a physically reasonable correlation of peaks on the distribution functions of relaxation times to specific electrodes.

  • Effect of Graphite Properties on Reversible Capacitance and Coulomb Efficiency

    by E. Kuzmina, A. Yusupova, N. Egorova, E. Gaifullina, V. Kolosnitsyn, A. Samodurov, V. Arkhipov, A. Kudashov

    The effect of structural characteristics of graphites (specific surface area, porosity, interplanar distance d002, crystallite size, amorphous fraction) on their electrochemical parameters (reversible capacity, Coulomb efficiency (CE) in the first cycle) was studied. It was found that changing the specific surface area of graphites in the range of 0.5–5 m2/g does not have a noticeable effect on the reversible capacity. High reversible capacity (350–370 mA h/g) is typical for graphites with d002 < 3.37 Å, LC, and LA > 400 Å. It was found that high specific surface area (>5 m2/g) and the presence of micropores reduce the Coulomb efficiency of graphite electrodes in the first cycle. Increasing the amorphous fraction by more than >0.7% reduces the Coulomb efficiency.

  • Open Access

    Electrochemical characteristics of lithium-sulfur pouch cells. Effect of compression force of electrode modules

    by Dmitrii V. Kolosnitsyn, Nadezhda V. Egorova, Alena M. Ionina, Elena V. Karaseva, Vladimir S. Kolosnitsyn

    The effect of the electrode sizes, the cell design and the compression force of the electrode modules on the impedance and discharge characteristics of lithium-sulfur cells was studied. It was shown that Swagelok and pouch cells with identical electrodes have different electrochemical characteristics – charge transfer resistance, discharge capacity and cycling duration. It was found that the discharge capacity at the first cycle of Swagelok and pouch cells differs by 20% approximately. The capacity of pouch cells decreases faster during cycling. The cycling of pouch cells in a compressed state (similar to Swagelok cells) does not improve the electrochemical characteristics of pouch cells.