Junfeng Cheng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Junfeng Cheng has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Wei Sun
School of Minerals Processing and Bioengineering, Central South University, Changsha 410083, China
3 shared publications - Weiping Liu
School of Minerals Processing and Bioengineering, Central South University, Changsha, China
3 shared publications - Yujie Zhao
School of Minerals Processing and Bioengineering, Central South University, Changsha 410083, China
3 shared publications - Saiya Li
School of Minerals Processing and Bioengineering, Central South University, Changsha 410083, China
2 shared publications - Shafiq Alam
University of Saskatchewan
2 shared publications - Fang Wu
Key Laboratory of Tungsten and Rare Earth Resource Recycling and New Material Application of Jiangxi Education Institutes, Jiangxi College of Applied Technology, Ganzhou 341000, China
1 shared publication
Latest Publications
- Open Access
Water–HCl Sequential Leaching of Waste Barrier Material from Aluminum Electrolysis Cell
The Hall–Héroult aluminum production process generates lithium-rich waste barrier materials, which are challenging to process using conventional acid leaching due to the environmental risks posed by hydrofluoric acid (HF) emissions. This research introduces a two-stage water–HCl sequential leaching (WHSL) approach to recover lithium while reducing these environmental impacts. The method evaluates key factors, such as the liquid–solid ratio, temperature, duration, rotation speed, and HCl concentration, and compares its efficacy with traditional HCl leaching using XRD, FTIR, DBP, and SEM techniques. The findings indicate that initial water leaching dissolves NaF salts, creating surface grooves and cracks. Subsequent HCl leaching selectively extracts lithium from aluminum and silicon, forming silica gel while preserving the nepheline phase due to its structural integrity. The process produces a porous residue with smaller particles, reduced surface potential, and promotes colloidal aggregation. This two-step process achieves efficient lithium recovery while reducing acid consumption and minimizing hydrogen fluoride (HF) emissions.
Open AccessWater–HCl Sequential Leaching of Waste Barrier Material from Aluminum Electrolysis Cell
The Hall–Héroult aluminum production process generates lithium-rich waste barrier materials, which are challenging to process using conventional acid leaching due to the environmental risks posed by hydrofluoric acid (HF) emissions. This research introduces a two-stage water–HCl sequential leaching (WHSL) approach to recover lithium while reducing these environmental impacts. The method evaluates key factors, such as the liquid–solid ratio, temperature, duration, rotation speed, and HCl concentration, and compares its efficacy with traditional HCl leaching using XRD, FTIR, DBP, and SEM techniques. The findings indicate that initial water leaching dissolves NaF salts, creating surface grooves and cracks. Subsequent HCl leaching selectively extracts lithium from aluminum and silicon, forming silica gel while preserving the nepheline phase due to its structural integrity. The process produces a porous residue with smaller particles, reduced surface potential, and promotes colloidal aggregation. This two-step process achieves efficient lithium recovery while reducing acid consumption and minimizing hydrogen fluoride (HF) emissions.
- Open Access
Removal of Chloride Ions from Mg(OH)2 Using NaOH with Ethanol
China’s salt lake-based magnesium industry faces chloride removal challenges, which limit applications and cause pollution. Addressing this enables higher-quality Mg(OH)2 production. In this regard, chloride ion removal from magnesium hydroxide in a sodium hydroxide solution with ethanol was investigated for the first time. Ethanol and NaOH enhance chloride removal efficiency. Under optimized conditions, the chloride removal efficiency was 68.9%, and the Cl− content in Mg(OH)2 was reduced to 0.14%. Kinetic analysis suggests that the removal of chloride ions is primarily controlled by internal diffusion. These results underscore the potential of NaOH and ethanol in enhancing chloride removal efficiency during magnesium hydroxide production, supporting the advancement of cleaner and more versatile magnesium-based materials.
Open AccessRemoval of Chloride Ions from Mg(OH)2 Using NaOH with Ethanol
China’s salt lake-based magnesium industry faces chloride removal challenges, which limit applications and cause pollution. Addressing this enables higher-quality Mg(OH)2 production. In this regard, chloride ion removal from magnesium hydroxide in a sodium hydroxide solution with ethanol was investigated for the first time. Ethanol and NaOH enhance chloride removal efficiency. Under optimized conditions, the chloride removal efficiency was 68.9%, and the Cl− content in Mg(OH)2 was reduced to 0.14%. Kinetic analysis suggests that the removal of chloride ions is primarily controlled by internal diffusion. These results underscore the potential of NaOH and ethanol in enhancing chloride removal efficiency during magnesium hydroxide production, supporting the advancement of cleaner and more versatile magnesium-based materials.
- Open Access
Leaching Behavior of Waste Barrier Material with Sulfuric Acid
The comprehensive recycling of aluminum electrolysis cell waste barrier material is urgent. This study focuses on the sulfuric acid leaching of waste barrier material, systematically examining the effects of factors such as reaction temperature, liquid-to-solid ratio, sulfuric acid concentration, and reaction time on the leaching of elements like lithium, aluminum, sodium, and silicon. The experimental results show that under the conditions of 0.9 mol/L sulfuric acid concentration, a liquid-to-solid ratio of 20:1, a reaction temperature of 90 °C, and a reaction time of 1.5 h, the leaching rates were 84.5% for lithium, 85.6% for aluminum, 98.5% for sodium, and 4.8% for silicon. The sulfuric acid leaching process of the waste barrier material follows a shrinking core model and is controlled by internal diffusion. The apparent activation energies for the leaching reactions of lithium, aluminum, and sodium were 4.29 kJ/mol, 8.99 kJ/mol, and 9.11 kJ/mol, respectively. The selective leaching of lithium, sodium, and aluminum from silicon was successfully achieved in the sulfuric acid leaching of the waste barrier material.
Open AccessLeaching Behavior of Waste Barrier Material with Sulfuric Acid
The comprehensive recycling of aluminum electrolysis cell waste barrier material is urgent. This study focuses on the sulfuric acid leaching of waste barrier material, systematically examining the effects of factors such as reaction temperature, liquid-to-solid ratio, sulfuric acid concentration, and reaction time on the leaching of elements like lithium, aluminum, sodium, and silicon. The experimental results show that under the conditions of 0.9 mol/L sulfuric acid concentration, a liquid-to-solid ratio of 20:1, a reaction temperature of 90 °C, and a reaction time of 1.5 h, the leaching rates were 84.5% for lithium, 85.6% for aluminum, 98.5% for sodium, and 4.8% for silicon. The sulfuric acid leaching process of the waste barrier material follows a shrinking core model and is controlled by internal diffusion. The apparent activation energies for the leaching reactions of lithium, aluminum, and sodium were 4.29 kJ/mol, 8.99 kJ/mol, and 9.11 kJ/mol, respectively. The selective leaching of lithium, sodium, and aluminum from silicon was successfully achieved in the sulfuric acid leaching of the waste barrier material.