Stjepan Kožuh
Research Subjects
Stjepan Kožuh has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Ladislav Vrsalović
Faculty of Chemistry and Technology, University of Split, 21000 Split, Croatia
2 shared publications - Senka Gudić
Faculty of Chemistry and Technology, University of Split, 21000 Split, Croatia
2 shared publications B. Kosec
University of Ljubljana, Faculty of Natural Sciences and Engineering, Ljubljana, Slovenia
1 shared publicationBorut Kosec
University of Ljubljana, Faculty of Natural Science and Engineering, Aškerčeva 12, 1000, Ljubljana, Slovenia
1 shared publication- Ivan Anžel
University of Maribor
1 shared publication - Ivana Ivanić
Department of Physical Metallurgy, Faculty of Metallurgy, University of Zagreb, Aleja Narodnih Heroja 3, 44000 Sisak, Croatia
1 shared publication
Latest Publications
- Open Access
- 11 April 2025
- Published by University of Nis in Facta Universitatis, Series: Mechanical Engineering
- p. 033-047
BENEFICIAL EFFECT OF CU CONTENT AND AUSTEMPERING PARAMETERS ON THE HARDNESS AND CORROSION PROPERTIES OF AUSTEMPERED DUCTILE IRON (ADI)
The effect of copper content (0.031 wt.% Cu, 0.32 wt.% Cu, 0.51 wt.% Cu and 0.91 wt.% Cu) on the hardness and corrosion properties of ADI was investigated. Samples austenitization were carried out at 850°C for 60 min followed by its austempering at temperatures from 250°C to 420°C for different time (30 to 60 min) in 50% (KNO3 + NaNO3) salt bath. It was concluded that hardness rises with copper content but decreases with higher austempering temperatures and times. The corrosion properties of the samples with minimum and maximum Cu content were investigated by electrochemical methods in 0.5 M NaCl solution. Samples with a higher copper content have shown higher values of polarization resistance (Rp) and lower values of corrosion current (icorr). After polarization measurements, corroded surfaces were analyzed with SEM/EDS analysis.
- 11 April 2025
- Published by University of Nis in Facta Universitatis, Series: Mechanical Engineering
- p. 033-047
Open AccessBENEFICIAL EFFECT OF CU CONTENT AND AUSTEMPERING PARAMETERS ON THE HARDNESS AND CORROSION PROPERTIES OF AUSTEMPERED DUCTILE IRON (ADI)
The effect of copper content (0.031 wt.% Cu, 0.32 wt.% Cu, 0.51 wt.% Cu and 0.91 wt.% Cu) on the hardness and corrosion properties of ADI was investigated. Samples austenitization were carried out at 850°C for 60 min followed by its austempering at temperatures from 250°C to 420°C for different time (30 to 60 min) in 50% (KNO3 + NaNO3) salt bath. It was concluded that hardness rises with copper content but decreases with higher austempering temperatures and times. The corrosion properties of the samples with minimum and maximum Cu content were investigated by electrochemical methods in 0.5 M NaCl solution. Samples with a higher copper content have shown higher values of polarization resistance (Rp) and lower values of corrosion current (icorr). After polarization measurements, corroded surfaces were analyzed with SEM/EDS analysis.
- Open Access
- 22 January 2018
- Published by Croatian Society of Chemical Engineers/HDKI in Kemija u industriji
- Vol. 67 (1-2) , 11-17
The Effect of Heat Treatment on the Microstructure and Mechanical Properties of Cu-Al-Mn Shape Memory Alloy
- 22 January 2018
- Published by Croatian Society of Chemical Engineers/HDKI in Kemija u industriji
- Vol. 67 (1-2) , 11-17
Open AccessThe Effect of Heat Treatment on the Microstructure and Mechanical Properties of Cu-Al-Mn Shape Memory Alloy
- Open Access
- 1 January 2016
- Published by National Library of Serbia in Journal of Mining and Metallurgy, Section B: Metallurgy
- Vol. 52 (1) , 53-61
Comparison of the corrosion behavior and surface morphology of NiTi alloy and stainless steels in sodium chloride solution
The corrosion behavior of NiTi alloy and stainless steels (AISI 316L and X2CrNiMoN22-5-3) in 0.9% sodium chloride (0.154 moll-1) solution was investigated using open circuit potential measurements, potentiodynamic polarization and electrochemical impedance spectroscopy measurements. Microstructural analyses before and after electrochemical tests were performed with the scanning electron microscopy (SEM) equipped with energy dispersive spectrometry (EDS). The lowest corrosion current density has NiTi alloy and the extent of the passive range increased in the order AISI 316L stainless steel < NiTi alloy < X2CrNiMoN22-5-3 duplex stainless steel. The oxide film formed on all samples has a double-layer structure consisting of a barrier-type inner layer and a porous outer layer. Oxide films formed on the surface of steels mainly contains iron oxides and chromium oxide, while the surface film of the NiTi alloy mainly contains TiO2 oxide.
- 1 January 2016
- Published by National Library of Serbia in Journal of Mining and Metallurgy, Section B: Metallurgy
- Vol. 52 (1) , 53-61
Open AccessComparison of the corrosion behavior and surface morphology of NiTi alloy and stainless steels in sodium chloride solution
The corrosion behavior of NiTi alloy and stainless steels (AISI 316L and X2CrNiMoN22-5-3) in 0.9% sodium chloride (0.154 moll-1) solution was investigated using open circuit potential measurements, potentiodynamic polarization and electrochemical impedance spectroscopy measurements. Microstructural analyses before and after electrochemical tests were performed with the scanning electron microscopy (SEM) equipped with energy dispersive spectrometry (EDS). The lowest corrosion current density has NiTi alloy and the extent of the passive range increased in the order AISI 316L stainless steel < NiTi alloy < X2CrNiMoN22-5-3 duplex stainless steel. The oxide film formed on all samples has a double-layer structure consisting of a barrier-type inner layer and a porous outer layer. Oxide films formed on the surface of steels mainly contains iron oxides and chromium oxide, while the surface film of the NiTi alloy mainly contains TiO2 oxide.