Gemma E. Howard
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Gemma E. Howard has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Jason Gill
HSE Science and Research Centre, Harpur Hill, Buxton Derbyshire SK17 9JN, UK
6 shared publications - Jonathan E. H. Buston
HSE Science and Research Centre, Harpur Hill, Buxton Derbyshire SK17 9JN, UK
6 shared publications - Steven L. Goddard
HSE Science and Research Centre, Harpur Hill, Buxton Derbyshire SK17 9JN, UK
6 shared publications - Jack W. Mellor
HSE Science and Research Centre, Harpur Hill, Buxton SK17 9JN, UK
4 shared publications - Philip A. P. Reeve
HSE Science and Research Centre, Harpur Hill, Buxton Derbyshire SK17 9JN, UK
4 shared publications - Daniel Howard
HSE Science and Research Centre, Harpur Hill, Buxton SK17 9JN, UK
1 shared publication
Latest Publications
- Open Access
Failure Characteristics of Cylindrical Cells (18650 and 26700) Across Sodium-Ion, Lithium Nickel Manganese Cobalt Oxide (NMC), Lithium Iron Phosphate (LFP) and Lithium Titanate (LTO) Chemistries
This study compares the failure characteristics of four 1.5 Ah 18650 cells, including lithium nickel manganese cobalt oxide (NMC), lithium iron phosphate (LFP), lithium titanate (LTO), and sodium-ion (NFM), alongside a 3 Ah 26700 NFM cell. Cells at a 100% state of charge (SoC) were evaluated using three types of failure methods. Open-field external heat testing was used to characterise visible failure behaviour, including venting, flames, and sparking. Accelerating rate calorimetry (ARC) provided high-resolution temperature data for key failure points, including venting onset, thermal runaway (TR), and peak temperature. Pressure vessel tests under an inert atmosphere enabled quantification of total gas volume and analysis of major gas species (H2, CO2, CO, and light hydrocarbons). Three open-field results for each cell type showed no ignition in any LTO or LFP tests, while NMC and NFM cells were ignited in one and two tests, respectively. ARC measurements found that LTO exhibited the lowest TR onset temperature, while that of LFP exceeded 130 °C, with NMC and NFM cells falling between. Pressure vessel results indicated that when gas volumes were normalised to L/Ah, NFM2 cells generated the largest volume of gas, and 1.23 L/Ah and NMF1 cells generated the least (0.59 L/Ah). LFP cells showed the highest H2 concentration, with LTO producing minimal gas. These findings highlight the need for application-specific assessment of cell chemistry safety.
Open AccessFailure Characteristics of Cylindrical Cells (18650 and 26700) Across Sodium-Ion, Lithium Nickel Manganese Cobalt Oxide (NMC), Lithium Iron Phosphate (LFP) and Lithium Titanate (LTO) Chemistries
This study compares the failure characteristics of four 1.5 Ah 18650 cells, including lithium nickel manganese cobalt oxide (NMC), lithium iron phosphate (LFP), lithium titanate (LTO), and sodium-ion (NFM), alongside a 3 Ah 26700 NFM cell. Cells at a 100% state of charge (SoC) were evaluated using three types of failure methods. Open-field external heat testing was used to characterise visible failure behaviour, including venting, flames, and sparking. Accelerating rate calorimetry (ARC) provided high-resolution temperature data for key failure points, including venting onset, thermal runaway (TR), and peak temperature. Pressure vessel tests under an inert atmosphere enabled quantification of total gas volume and analysis of major gas species (H2, CO2, CO, and light hydrocarbons). Three open-field results for each cell type showed no ignition in any LTO or LFP tests, while NMC and NFM cells were ignited in one and two tests, respectively. ARC measurements found that LTO exhibited the lowest TR onset temperature, while that of LFP exceeded 130 °C, with NMC and NFM cells falling between. Pressure vessel results indicated that when gas volumes were normalised to L/Ah, NFM2 cells generated the largest volume of gas, and 1.23 L/Ah and NMF1 cells generated the least (0.59 L/Ah). LFP cells showed the highest H2 concentration, with LTO producing minimal gas. These findings highlight the need for application-specific assessment of cell chemistry safety.
- Open Access
Experimental Investigations into the Failure Modes of Different Formats of Lithium-Ion Cells and the Potential Impact on Building Materials
Lithium-ion battery (LIB) cells are available in various sizes, formats, and chemistries. Should a LIB be exposed to conditions outside its operating parameters, each variation affects the cell failure mechanisms and any resultant fire dynamic. Battery fires can be dynamic events that differ significantly from those solid-, liquid- or gas-based fire curves often used in standard building material fire resistance tests. This preliminary research aimed to investigate how standard building materials, sometimes used as a compartment fire envelope, such as gypsum plasterboard, react when exposed to a dynamic battery fire. The research explored batteries that produced jet fires, could act as projectiles, or produced overpressures when they failed. The results showed that cylindrical cells can travel at significant speeds and distances due to expulsing the cell’s contents through the cell’s vent or ejected end cap. These cells were shown to be capable of piercing plasterboard and remain hot enough to present a fire risk where they fall on the far side of the plasterboard. It was also found that the overpressures produced by failing prismatic cells affected the structural integrity of some building materials. The results show a need for further research into the effectiveness of standard building fire controls when exposed to LIB fires.
Open AccessExperimental Investigations into the Failure Modes of Different Formats of Lithium-Ion Cells and the Potential Impact on Building Materials
Lithium-ion battery (LIB) cells are available in various sizes, formats, and chemistries. Should a LIB be exposed to conditions outside its operating parameters, each variation affects the cell failure mechanisms and any resultant fire dynamic. Battery fires can be dynamic events that differ significantly from those solid-, liquid- or gas-based fire curves often used in standard building material fire resistance tests. This preliminary research aimed to investigate how standard building materials, sometimes used as a compartment fire envelope, such as gypsum plasterboard, react when exposed to a dynamic battery fire. The research explored batteries that produced jet fires, could act as projectiles, or produced overpressures when they failed. The results showed that cylindrical cells can travel at significant speeds and distances due to expulsing the cell’s contents through the cell’s vent or ejected end cap. These cells were shown to be capable of piercing plasterboard and remain hot enough to present a fire risk where they fall on the far side of the plasterboard. It was also found that the overpressures produced by failing prismatic cells affected the structural integrity of some building materials. The results show a need for further research into the effectiveness of standard building fire controls when exposed to LIB fires.
- Open Access
Experimental Investigations into the Ignitability of Real Lithium Iron Phosphate (LFP) Battery Vent Gas at Concentrations Below the Theoretical Lower Explosive Limit (LEL)
Lithium iron phosphate (LFP) batteries have become a popular choice for energy storage, electrified mobility, and plants. All lithium-based batteries produce flammable vent gas as a result of failure through thermal runaway. LFP cells produce less gas by volume than nickel-based cells, but the composition of this gas most often contains less carbon dioxide and more hydrogen. However, when LFP cells fail, they generate lower temperatures, so the vent gas is rarely ignited. Therefore, the hazard presented by a LFP cell in thermal runaway is less of a direct battery fire hazard but more of a flammable gas source hazard. This research identified the constituents and components of the vent gas for different sized LFP prismatic cells when overcharged to failure. This data was used to calculate the maximum homogenous concentration of gas that would be released into a 1.73 m3 test rig and the percentage of the lower explosive limit (LEL). Overcharge experiments were conducted using the same type of cells in the test rig in the presence of remote ignition sources. Ignition and deflagration of the vent gas were possible at concentrations below the theoretical LEL of the vent gas if it was homogeneously mixed.
Open AccessExperimental Investigations into the Ignitability of Real Lithium Iron Phosphate (LFP) Battery Vent Gas at Concentrations Below the Theoretical Lower Explosive Limit (LEL)
Lithium iron phosphate (LFP) batteries have become a popular choice for energy storage, electrified mobility, and plants. All lithium-based batteries produce flammable vent gas as a result of failure through thermal runaway. LFP cells produce less gas by volume than nickel-based cells, but the composition of this gas most often contains less carbon dioxide and more hydrogen. However, when LFP cells fail, they generate lower temperatures, so the vent gas is rarely ignited. Therefore, the hazard presented by a LFP cell in thermal runaway is less of a direct battery fire hazard but more of a flammable gas source hazard. This research identified the constituents and components of the vent gas for different sized LFP prismatic cells when overcharged to failure. This data was used to calculate the maximum homogenous concentration of gas that would be released into a 1.73 m3 test rig and the percentage of the lower explosive limit (LEL). Overcharge experiments were conducted using the same type of cells in the test rig in the presence of remote ignition sources. Ignition and deflagration of the vent gas were possible at concentrations below the theoretical LEL of the vent gas if it was homogeneously mixed.
- Open Access
The Effects of Cell Chemistry, State of Charge, and Abuse Method on Gas Generation in Li-Ion Cell Failure
We report on the effect state of charge (SoC), cell format, and chemistry have on the volume and composition (H2, CO2, CO, CH4, C2H4, C2H6, C3H6, and C3H8) of cell failure gas from Li-ion cells. Nickel manganese cobalt oxide (NMC) 21700 cells with a 5 Ah capacity were externally heated to failure at a 5–100% SoC under an inert atmosphere. This showed that the volume of gas increased with cell SoC (1.8 L at 5% SoC vs. 8.3 L at 100% SoC). The effect of the cell chemistry format and abuse method was also investigated using 18650, pouch, and prismatic cells (2.3–50 Ah) with Ni-based or lithium cobalt oxide (LCO) cathodes or lithium titanium oxide (LTO) anodes. The results showed that at higher SoCs, larger quantities of gas were generated; however, there was no correlation between the cell SoC and the composition of gases produced. Tests on the other cells found that the Ni-based cell generated 1.29–1.89 L/Ah of gas. The main constituents of this were H2, CO, and CO2; however, all other hydrocarbons were identified in varying quantities. The LTO cells generated lower volumes of gas, 0.8 L/Ah compared to Ni-based cells, and the gas was found to contain lower H2 concentrations but higher concentrations of CO2. The LCO cell was found to generate a gas volume of 1.2 L/Ah. This forms the final of four papers which cover a total of 213 tests on 29 cell types with six different chemistries, all tested using a single robust testing method.
Open AccessThe Effects of Cell Chemistry, State of Charge, and Abuse Method on Gas Generation in Li-Ion Cell Failure
We report on the effect state of charge (SoC), cell format, and chemistry have on the volume and composition (H2, CO2, CO, CH4, C2H4, C2H6, C3H6, and C3H8) of cell failure gas from Li-ion cells. Nickel manganese cobalt oxide (NMC) 21700 cells with a 5 Ah capacity were externally heated to failure at a 5–100% SoC under an inert atmosphere. This showed that the volume of gas increased with cell SoC (1.8 L at 5% SoC vs. 8.3 L at 100% SoC). The effect of the cell chemistry format and abuse method was also investigated using 18650, pouch, and prismatic cells (2.3–50 Ah) with Ni-based or lithium cobalt oxide (LCO) cathodes or lithium titanium oxide (LTO) anodes. The results showed that at higher SoCs, larger quantities of gas were generated; however, there was no correlation between the cell SoC and the composition of gases produced. Tests on the other cells found that the Ni-based cell generated 1.29–1.89 L/Ah of gas. The main constituents of this were H2, CO, and CO2; however, all other hydrocarbons were identified in varying quantities. The LTO cells generated lower volumes of gas, 0.8 L/Ah compared to Ni-based cells, and the gas was found to contain lower H2 concentrations but higher concentrations of CO2. The LCO cell was found to generate a gas volume of 1.2 L/Ah. This forms the final of four papers which cover a total of 213 tests on 29 cell types with six different chemistries, all tested using a single robust testing method.
- Open Access
Comprehensive Study of the Gas Volume and Composition Produced by Different 3–230 Ah Lithium Iron Phosphate (LFP) Cells Failed Using External Heat, Overcharge and Nail Penetration Under Air and Inert Atmospheres
This paper reports on the failure of cells with lithium iron phosphate (LFP) chemistry tested under a range of conditions to understand their effect on the volume and composition of gas generated. Cells of the following formats, 26,650, pouch, and prismatic, and capacities ranging from 3 to 230 Ah, were subjected to external heat, overcharge, and nail penetration tests. Gas volume was calculated, and the following gases analysed: H2, CO2, CO, CH4, C2H4, C2H6, C3H6, and C3H8. Cells that failed via external heating under inert conditions (N2 or Ar atmosphere) at 100% state of charge (SoC) typically generated 0.7 L/Ah of gas; overcharged cells, 0.11–0.68 L/Ah; and nail penetration between 0.3 and 0.5 L/Ah. In general, for all test configurations, regardless of atmosphere, the total gas volume contained a 40% concentration of H2, 15% of CO2, and the remaining gas consisted of varying concentrations of CO and flammable hydrocarbons. This demonstrates that despite differences in gas volume, the failure gas composition of LFP cells remains similar.
Open AccessComprehensive Study of the Gas Volume and Composition Produced by Different 3–230 Ah Lithium Iron Phosphate (LFP) Cells Failed Using External Heat, Overcharge and Nail Penetration Under Air and Inert Atmospheres
This paper reports on the failure of cells with lithium iron phosphate (LFP) chemistry tested under a range of conditions to understand their effect on the volume and composition of gas generated. Cells of the following formats, 26,650, pouch, and prismatic, and capacities ranging from 3 to 230 Ah, were subjected to external heat, overcharge, and nail penetration tests. Gas volume was calculated, and the following gases analysed: H2, CO2, CO, CH4, C2H4, C2H6, C3H6, and C3H8. Cells that failed via external heating under inert conditions (N2 or Ar atmosphere) at 100% state of charge (SoC) typically generated 0.7 L/Ah of gas; overcharged cells, 0.11–0.68 L/Ah; and nail penetration between 0.3 and 0.5 L/Ah. In general, for all test configurations, regardless of atmosphere, the total gas volume contained a 40% concentration of H2, 15% of CO2, and the remaining gas consisted of varying concentrations of CO and flammable hydrocarbons. This demonstrates that despite differences in gas volume, the failure gas composition of LFP cells remains similar.
- Open Access
Comprehensive Study of the Gas Volume and Composition Generated by 5 Ah Nickel Manganese Cobalt Oxide (NMC) Li-Ion Pouch Cells Through Different Failure Mechanisms at Varying States of Charge
Lithium-ion batteries risk failing when subjected to different abuse tests, resulting in gas and flames. In this study, 5 Ah nickel manganese cobalt oxide (NMC) pouch cells were subjected to external heating; overcharge at rates of 2.5, 5 and 10 A; and nail penetration. Tests were conducted in air and N2 atmospheres. Additional external heat tests were performed on cells at 5, 25, 50, and 75% SoC and on two, three, and four cell blocks. Gas volumes were calculated, and the gas composition was given for H2, CO, CO2, C2H4, C2H6, CH4, C3H6, and C3H8. For tests under an air atmosphere at 100% SoC, the volume of gas varied between abuse methods: 3.9 L (external heat), 6.4 L (overcharge), and 8.9 L (nail penetration). The gas composition was found to predominantly contain H2, CO2, and CO for all abuse methods; however, higher concentrations of H2 and CO were present in tests performed under N2. External heat tests at different SoCs showed that the gas volume decreased with SoC. Overall, the type of abuse method can have a large effect on the gas volume and composition produced by cell failure.
Open AccessComprehensive Study of the Gas Volume and Composition Generated by 5 Ah Nickel Manganese Cobalt Oxide (NMC) Li-Ion Pouch Cells Through Different Failure Mechanisms at Varying States of Charge
Lithium-ion batteries risk failing when subjected to different abuse tests, resulting in gas and flames. In this study, 5 Ah nickel manganese cobalt oxide (NMC) pouch cells were subjected to external heating; overcharge at rates of 2.5, 5 and 10 A; and nail penetration. Tests were conducted in air and N2 atmospheres. Additional external heat tests were performed on cells at 5, 25, 50, and 75% SoC and on two, three, and four cell blocks. Gas volumes were calculated, and the gas composition was given for H2, CO, CO2, C2H4, C2H6, CH4, C3H6, and C3H8. For tests under an air atmosphere at 100% SoC, the volume of gas varied between abuse methods: 3.9 L (external heat), 6.4 L (overcharge), and 8.9 L (nail penetration). The gas composition was found to predominantly contain H2, CO2, and CO for all abuse methods; however, higher concentrations of H2 and CO were present in tests performed under N2. External heat tests at different SoCs showed that the gas volume decreased with SoC. Overall, the type of abuse method can have a large effect on the gas volume and composition produced by cell failure.