Nilesh Rajendran
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Nilesh Rajendran has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Emiel DenHartog
Wilson College of Textiles, North Carolina State University, Raleigh, NC 27606, USA
6 shared publications - Brady Clapsaddle
TDA Research Inc., Wheat Ridge, USA
4 shared publications David Eisenberg
2 shared publications- David P. Eisenberg
TDA Research, Inc., 4680 Table Mountain Drive, Suite 100B, Golden, CO 80403, USA
2 shared publications Emiel DenHartog
2 shared publicationsGirish Srinivas
2 shared publications
Latest Publications
- Open Access
- 28 September 2026
- Published by Elsevier in Polymer Degradation and Stability
- Vol. 254
Characterization of early-stage mechanical degradation of high-tensile nylon 6,6 webbings under abrasive wear
- 28 September 2026
- Published by Elsevier in Polymer Degradation and Stability
- Vol. 254
Open AccessCharacterization of early-stage mechanical degradation of high-tensile nylon 6,6 webbings under abrasive wear
- Open Access
- 16 September 2026
- Published by Elsevier in Polymer Degradation and Stability
- Vol. 253
Correlating spectroscopic and crystalline changes with strength loss due to accelerated UV degradation of high-tensile nylon 6, 6 webbing
- 16 September 2026
- Published by Elsevier in Polymer Degradation and Stability
- Vol. 253
Open AccessCorrelating spectroscopic and crystalline changes with strength loss due to accelerated UV degradation of high-tensile nylon 6, 6 webbing
- Open Access
- 9 June 2026
- Published by Elsevier in SSRN Electronic Journal
Correlating Spectroscopic and Crystalline Changes with Strength Loss Due to Accelerated UV Degradation of High-Tensile Nylon 6, 6 Webbing
The study investigated the degradation of Nylon 6, 6 webbings under accelerated UV weathering and developed a predictive model for tensile strength loss. Changes in the webbings' chemical and physical properties were characterized using Fourier-transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), and differential scanning calorimetry (DSC).,Key findings show that degradation is a surface-dominated phenomenon. XRD analysis revealed that surface crystallinity was significantly affected by an interaction between color and exposure duration, with an initial increase attributed to chemi-crystallization. In contrast, bulk properties measured by DSC and chemical changes measured by FTIR (via the Carbonyl Index) showed no significant interaction effect, suggesting a more uniform degradation mechanism within the polymer's bulk.,A multiple linear regression (MLR) model was developed to predict tensile strength using the results from the analytical data. The model demonstrated a moderately strong correlation (R² ≈ 0.66). Notably, the significant predictors were Color, Carbonyl Index, and surface crystallinity (XRD) with p-values <0.001, while bulk crystallinity (DSC) was found to be insignificant. This confirms that the loss of mechanical integrity is primarily driven by changes occurring on the material's surface. These results also validate the use of non-destructive, surface-sensitive techniques as a potential method for estimating the residual strength of weathered webbings materials used as safety harness during their service life
- 9 June 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessCorrelating Spectroscopic and Crystalline Changes with Strength Loss Due to Accelerated UV Degradation of High-Tensile Nylon 6, 6 Webbing
The study investigated the degradation of Nylon 6, 6 webbings under accelerated UV weathering and developed a predictive model for tensile strength loss. Changes in the webbings' chemical and physical properties were characterized using Fourier-transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), and differential scanning calorimetry (DSC).,Key findings show that degradation is a surface-dominated phenomenon. XRD analysis revealed that surface crystallinity was significantly affected by an interaction between color and exposure duration, with an initial increase attributed to chemi-crystallization. In contrast, bulk properties measured by DSC and chemical changes measured by FTIR (via the Carbonyl Index) showed no significant interaction effect, suggesting a more uniform degradation mechanism within the polymer's bulk.,A multiple linear regression (MLR) model was developed to predict tensile strength using the results from the analytical data. The model demonstrated a moderately strong correlation (R² ≈ 0.66). Notably, the significant predictors were Color, Carbonyl Index, and surface crystallinity (XRD) with p-values <0.001, while bulk crystallinity (DSC) was found to be insignificant. This confirms that the loss of mechanical integrity is primarily driven by changes occurring on the material's surface. These results also validate the use of non-destructive, surface-sensitive techniques as a potential method for estimating the residual strength of weathered webbings materials used as safety harness during their service life
- Open Access
- 9 June 2026
- Published by Elsevier in SSRN Electronic Journal
Mapping the Initial Mechanism of Degradation Caused by Abrasive Wear of High-Tensile Nylon 6,6 Webbings
This study investigates the initial degradation mechanisms of high-tensile nylon 6,6 webbings used in safety harnesses when subjected to mechanical abrasion. Understanding these mechanisms is essential for predicting the service life and ensuring the reliability of textiles in safety-critical applications. Webbing samples were subjected to controlled abrasive wear from 5 to 1000 cycles using a Wyzenbeek tester (ASTM D4157) with P60 sandpaper. The degradation was assessed through changes in tensile strength, mass, temperature, and surface chemistry.,The primary finding was that the webbing’s tensile strength decreases logarithmically with increasing abrasion cycles (R² = 0.753, p < 0.05), with a rapid loss of strength initially that subsequently plateaus. This behavior is attributed to a transition in the dominant wear mechanism from a severe two-body cohesive wear process at yarn interlacement points to a less aggressive three-body abrasion as eroded fiber debris fills the hard asperities. This conclusion is strongly supported by the inconsistent mass loss data, which reflects the competing processes of fretting (mass loss) and debris redeposition (mass transfer).,While the minor temperature increase (1–2°C) was found to be insufficient to cause significant thermal degradation, the results suggest mechanochemical mechanism involving tribochemistry and oxidation is active at the fiber surface. This work provides a crucial mechanistic understanding of textile wear, identifying the transition between wear regimes as a key factor in performance loss, which is vital for developing more durable materials and predictive life-cycle models.
- 9 June 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessMapping the Initial Mechanism of Degradation Caused by Abrasive Wear of High-Tensile Nylon 6,6 Webbings
This study investigates the initial degradation mechanisms of high-tensile nylon 6,6 webbings used in safety harnesses when subjected to mechanical abrasion. Understanding these mechanisms is essential for predicting the service life and ensuring the reliability of textiles in safety-critical applications. Webbing samples were subjected to controlled abrasive wear from 5 to 1000 cycles using a Wyzenbeek tester (ASTM D4157) with P60 sandpaper. The degradation was assessed through changes in tensile strength, mass, temperature, and surface chemistry.,The primary finding was that the webbing’s tensile strength decreases logarithmically with increasing abrasion cycles (R² = 0.753, p < 0.05), with a rapid loss of strength initially that subsequently plateaus. This behavior is attributed to a transition in the dominant wear mechanism from a severe two-body cohesive wear process at yarn interlacement points to a less aggressive three-body abrasion as eroded fiber debris fills the hard asperities. This conclusion is strongly supported by the inconsistent mass loss data, which reflects the competing processes of fretting (mass loss) and debris redeposition (mass transfer).,While the minor temperature increase (1–2°C) was found to be insufficient to cause significant thermal degradation, the results suggest mechanochemical mechanism involving tribochemistry and oxidation is active at the fiber surface. This work provides a crucial mechanistic understanding of textile wear, identifying the transition between wear regimes as a key factor in performance loss, which is vital for developing more durable materials and predictive life-cycle models.
- Open Access
Investigating Color as a Non-Destructive Indicator of Strength Loss in High Tensile Nylon 6,6 Webbings
High-performance nylon 6,6 webbings used in critical applications degrade under solar exposure, necessitating reliable methods to assess their residual strength non-destructively. This study investigates the feasibility of using instrumental color change as a predictive indicator for the loss of breaking strength. Four colors of nylon 6,6 webbings were subjected to accelerated xenon-arc solar weathering for up to 15 days. The resulting color change was quantified using both the CIELab and CIEDE2000 formulas, and residual breaking strength was measured following ASTM D6775. A regression analysis was performed to correlate these properties. The results demonstrate that a strong predictive relationship exists, but its efficacy is highly color-dependent. Webbing with high initial chroma, namely tan (R2 = 0.889) and navy (R2 = 0.817), showed a strong correlation between color change and strength loss. In contrast, the models for low-chroma black and white webbings were weak and unreliable. Furthermore, the simpler CIELab (ΔE*ab) formula provided slightly more accurate predictions than the more complex CIEDE2000 (ΔE*00) metric. It is concluded that colorimetry can be a viable non-destructive tool for predicting mechanical degradation, but its application is limited to specific high-chroma materials, precluding a universal model based entirely on colorimetry.
Open AccessInvestigating Color as a Non-Destructive Indicator of Strength Loss in High Tensile Nylon 6,6 Webbings
High-performance nylon 6,6 webbings used in critical applications degrade under solar exposure, necessitating reliable methods to assess their residual strength non-destructively. This study investigates the feasibility of using instrumental color change as a predictive indicator for the loss of breaking strength. Four colors of nylon 6,6 webbings were subjected to accelerated xenon-arc solar weathering for up to 15 days. The resulting color change was quantified using both the CIELab and CIEDE2000 formulas, and residual breaking strength was measured following ASTM D6775. A regression analysis was performed to correlate these properties. The results demonstrate that a strong predictive relationship exists, but its efficacy is highly color-dependent. Webbing with high initial chroma, namely tan (R2 = 0.889) and navy (R2 = 0.817), showed a strong correlation between color change and strength loss. In contrast, the models for low-chroma black and white webbings were weak and unreliable. Furthermore, the simpler CIELab (ΔE*ab) formula provided slightly more accurate predictions than the more complex CIEDE2000 (ΔE*00) metric. It is concluded that colorimetry can be a viable non-destructive tool for predicting mechanical degradation, but its application is limited to specific high-chroma materials, precluding a universal model based entirely on colorimetry.
- Open Access
- 10 October 2025
- Published by Springer Nature in Journal of Polymer Research
- Vol. 32 (10) , 1-11
Accelerated UV degradation behavior of high tensile nylon 6, 6 webbings
The paper investigates the UV degradation behavior of high tensile nylon 6, 6 webbings used in military applications. Webbings of four colors (navy, black, tan, and white) were selected according to military specification MIL-DTL-4088. The webbings were then subjected to up to 15 days of continuous exposure using a modified ASTM D2565 test standard in xenon-arc Weather-Ometer with 1.5x narrowband irradiance or 0.83 W/m 2 ∙ nm at 340 nm under Arizona conditions (43 °C, 30% RH), a duration equivalent to 107 days of outdoor Arizona conditions. SEM analysis showed no morphological changes even after 15 days of continuous exposure, contrary to literature available on the degradation of nylon polymer. However, FTIR spectroscopy showed evidence of change in molecular structure of nylon webbings with increasing UV exposure duration. This finding showed that the peak at 1740 cm −1 associated with -COOH bond energy increased as exposure increased, confirming that the hydrolysis phenomenon was initiated by UV radiation. This was also confirmed by tensile test results, which showed that the strength of the webbings decreased by 20% for all color except the white webbings (6% reduction) after 15 days in the weatherometer. A full factorial analysis confirmed that exposure duration had the largest effect on breaking strength (Partial η² = 0.67), followed by color (Partial η² = 0.54). A significant interaction effect (Partial η² = 0.37, p < .0001) confirmed that the rate of degradation was color-dependent, which could be the result of the dye chemistry associated with different colors. This study highlights the use of chemical characterization is essential for monitoring material integrity when surface changes are not visible due to UV degradation in nylon 6, 6 webbings. Future work should aim to quantify these chemical changes to develop a non-destructive method for predicting the residual strength of in-service webbings. Graphical abstract
- 10 October 2025
- Published by Springer Nature in Journal of Polymer Research
- Vol. 32 (10) , 1-11
Open AccessAccelerated UV degradation behavior of high tensile nylon 6, 6 webbings
The paper investigates the UV degradation behavior of high tensile nylon 6, 6 webbings used in military applications. Webbings of four colors (navy, black, tan, and white) were selected according to military specification MIL-DTL-4088. The webbings were then subjected to up to 15 days of continuous exposure using a modified ASTM D2565 test standard in xenon-arc Weather-Ometer with 1.5x narrowband irradiance or 0.83 W/m 2 ∙ nm at 340 nm under Arizona conditions (43 °C, 30% RH), a duration equivalent to 107 days of outdoor Arizona conditions. SEM analysis showed no morphological changes even after 15 days of continuous exposure, contrary to literature available on the degradation of nylon polymer. However, FTIR spectroscopy showed evidence of change in molecular structure of nylon webbings with increasing UV exposure duration. This finding showed that the peak at 1740 cm −1 associated with -COOH bond energy increased as exposure increased, confirming that the hydrolysis phenomenon was initiated by UV radiation. This was also confirmed by tensile test results, which showed that the strength of the webbings decreased by 20% for all color except the white webbings (6% reduction) after 15 days in the weatherometer. A full factorial analysis confirmed that exposure duration had the largest effect on breaking strength (Partial η² = 0.67), followed by color (Partial η² = 0.54). A significant interaction effect (Partial η² = 0.37, p < .0001) confirmed that the rate of degradation was color-dependent, which could be the result of the dye chemistry associated with different colors. This study highlights the use of chemical characterization is essential for monitoring material integrity when surface changes are not visible due to UV degradation in nylon 6, 6 webbings. Future work should aim to quantify these chemical changes to develop a non-destructive method for predicting the residual strength of in-service webbings. Graphical abstract
- Open Access
- 10 September 2025
- Published by MDPI AG in Preprints.org
Investigating Color as a Non-Destructive Indicator of Strength Loss in High Tensile Nylon 66 Webbings
High-performance nylon 6,6 webbings used in critical applications degrade under UV exposure, necessitating reliable methods to assess their residual strength non-destructively. This study investigates the feasibility of using instrumental color change as a predictive indicator for the loss of tensile strength. Four colors of nylon 6,6 webbings were subjected to accelerated xenon-arc UV weathering for up to 15 days. The resulting color change was quantified using both the CIELab and CIEDE2000 formulas, and residual tensile strength was measured following ASTM D6775. A regression analysis was performed to correlate these properties. The results demonstrate that a strong predictive relationship exists, but its efficacy is highly color dependent. Webbing with high initial chroma, namely tan (R2 = 0.889) and navy (R2 = 0.817), showed a strong correlation between color change and strength loss. In contrast, the models for low-chroma black and white webbings were weak and un-reliable. Furthermore, the simpler CIELab (ΔEab) formula provided slightly more accurate predictions than the more complex CIEDE2000 metric. It is concluded that colorimetry can be a viable non-destructive tool for predicting mechanical degradation, but its application is limited to specific high-chroma materials, precluding a universal model based entirely on colorimetry.
- 10 September 2025
- Published by MDPI AG in Preprints.org
Open AccessInvestigating Color as a Non-Destructive Indicator of Strength Loss in High Tensile Nylon 66 Webbings
High-performance nylon 6,6 webbings used in critical applications degrade under UV exposure, necessitating reliable methods to assess their residual strength non-destructively. This study investigates the feasibility of using instrumental color change as a predictive indicator for the loss of tensile strength. Four colors of nylon 6,6 webbings were subjected to accelerated xenon-arc UV weathering for up to 15 days. The resulting color change was quantified using both the CIELab and CIEDE2000 formulas, and residual tensile strength was measured following ASTM D6775. A regression analysis was performed to correlate these properties. The results demonstrate that a strong predictive relationship exists, but its efficacy is highly color dependent. Webbing with high initial chroma, namely tan (R2 = 0.889) and navy (R2 = 0.817), showed a strong correlation between color change and strength loss. In contrast, the models for low-chroma black and white webbings were weak and un-reliable. Furthermore, the simpler CIELab (ΔEab) formula provided slightly more accurate predictions than the more complex CIEDE2000 metric. It is concluded that colorimetry can be a viable non-destructive tool for predicting mechanical degradation, but its application is limited to specific high-chroma materials, precluding a universal model based entirely on colorimetry.
- Open Access
- 19 May 2025
- Published by Springer Nature in Research Square
Accelerated UV Degradation Behavior of High Tensile Nylon 6, 6 Webbings
The paper sought to investigate the UV degradation behaviour of high tensile nylon 6, 6 webbings used in military applications. Following the military specification MIL-DTL-4088, webbings of 4 colors – navy, black, tan and white, were selected. The webbings were then subjected to a modified ASTM D2565 test standard in xenon-arc Weather-Ometer with 1.5x narrowband irradiance or 0.83 W/m2 ∙ nm at 340nm under Arizona conditions (43°C, 30% RH). SEM analysis showed no morphological changes even after 15 days of continuous exposure, contrary to literature available on degradation of nylon polymer. However, FTIR spectroscopy showed evidence of change in molecular structure of nylon webbings with increasing UV exposure duration. The finding showed that the peak at 1740cm− 1 associated with -COOH bond energy increased as exposure increased confirming hydrolysis phenomena being initiated by UV radiation. This was also confirmed by tensile test results, that showed that the strength of the webbings decreased by 20% for all color expect white webbings. The full factorial analysis showed that while exposure duration increased degradation, color of webbing also played an important role which could be the result of the dye chemistry associated with different colors. This study highlights the use of chemical characterization techniques to understand UV degradation in nylon 6, 6. Further analytical chemistry tools are necessary to quantify and correlate the chemical changes in the nylon 6, 6 webbings to breaking strength loss due to UV degradation.
- 19 May 2025
- Published by Springer Nature in Research Square
Open AccessAccelerated UV Degradation Behavior of High Tensile Nylon 6, 6 Webbings
The paper sought to investigate the UV degradation behaviour of high tensile nylon 6, 6 webbings used in military applications. Following the military specification MIL-DTL-4088, webbings of 4 colors – navy, black, tan and white, were selected. The webbings were then subjected to a modified ASTM D2565 test standard in xenon-arc Weather-Ometer with 1.5x narrowband irradiance or 0.83 W/m2 ∙ nm at 340nm under Arizona conditions (43°C, 30% RH). SEM analysis showed no morphological changes even after 15 days of continuous exposure, contrary to literature available on degradation of nylon polymer. However, FTIR spectroscopy showed evidence of change in molecular structure of nylon webbings with increasing UV exposure duration. The finding showed that the peak at 1740cm− 1 associated with -COOH bond energy increased as exposure increased confirming hydrolysis phenomena being initiated by UV radiation. This was also confirmed by tensile test results, that showed that the strength of the webbings decreased by 20% for all color expect white webbings. The full factorial analysis showed that while exposure duration increased degradation, color of webbing also played an important role which could be the result of the dye chemistry associated with different colors. This study highlights the use of chemical characterization techniques to understand UV degradation in nylon 6, 6. Further analytical chemistry tools are necessary to quantify and correlate the chemical changes in the nylon 6, 6 webbings to breaking strength loss due to UV degradation.