Cong Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Cong Wang has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
Bingliang Gao
2 shared publications- Bingliang Gao
School of Metallurgy, Northeastern University, Shenyang, China
2 shared publications - Sen Zhou
School of Metallurgy, Northeastern University, Shenyang, People’s Republic of China
2 shared publications Tianshuo Yang
School of Metallurgy, Northeastern University, Shenyang, China
2 shared publicationsZhiwei Liu
School of Metallurgy, Northeastern University, Shenyang, China
2 shared publicationsFengguo Liu
School of Metallurgy, Northeastern University, Shenyang, China
1 shared publication
Latest Publications
- 28 October 2026
- Published by Springer Nature in Journal of Sustainable Metallurgy
- p. 1-26
A Unified Dimensionless Instability Index for Anodic Bubble Dynamics in Low-Temperature AlCl3 Electrolysis
- 28 October 2026
- Published by Springer Nature in Journal of Sustainable Metallurgy
- p. 1-26
A Unified Dimensionless Instability Index for Anodic Bubble Dynamics in Low-Temperature AlCl3 Electrolysis
- 15 January 2026
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 173 (2) , 023501
The Influence of Electrolyte Chemistry and Anode Temperature on the Anode Effect in Aluminum Electrolysis
This study examines how electrolyte composition and anode temperature govern the occurrence and characteristics of anode effects, particularly high-voltage anode effects (HVAE) and low-voltage anode effects (LVAE), in aluminum electrolysis. Combining electrolysis experiments with sessile drop measurements of contact angles between the electrolyte and carbon anode, X-ray photoelectron spectroscopy and gas chromatograph analyses, the synergistic mechanisms of LiF and KF on interfacial wettability, bubble dynamics, electrode polarization, and the formation of CF x passivation layers are elucidated. The results indicate that the high-Li electrolyte (6Li3K) compromises wettability, promoting LVAE and continuous low-concentration CF 4 emissions. In contrast, the high-K electrolyte (2Li6K) facilitates the formation of highly fluorinated CF x films, leading to HVAE. These findings highlight the importance of optimizing electrolyte formulation and anode thermal management to mitigate anode effects and reduce PFC emissions, thereby supporting the development of more sustainable and environmentally friendly aluminum smelting processes.
- 15 January 2026
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 173 (2) , 023501
The Influence of Electrolyte Chemistry and Anode Temperature on the Anode Effect in Aluminum Electrolysis
This study examines how electrolyte composition and anode temperature govern the occurrence and characteristics of anode effects, particularly high-voltage anode effects (HVAE) and low-voltage anode effects (LVAE), in aluminum electrolysis. Combining electrolysis experiments with sessile drop measurements of contact angles between the electrolyte and carbon anode, X-ray photoelectron spectroscopy and gas chromatograph analyses, the synergistic mechanisms of LiF and KF on interfacial wettability, bubble dynamics, electrode polarization, and the formation of CF x passivation layers are elucidated. The results indicate that the high-Li electrolyte (6Li3K) compromises wettability, promoting LVAE and continuous low-concentration CF 4 emissions. In contrast, the high-K electrolyte (2Li6K) facilitates the formation of highly fluorinated CF x films, leading to HVAE. These findings highlight the importance of optimizing electrolyte formulation and anode thermal management to mitigate anode effects and reduce PFC emissions, thereby supporting the development of more sustainable and environmentally friendly aluminum smelting processes.
- 1 May 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (5) , 053503
Numerical and On-Site Validation of Current Fluctuations and Cathode Wear on Melt Flow Stability in Flexible Aluminum Electrolysis Cells
The integration of clean energy sources, such as wind and solar, into flexible aluminum electrolysis cells introduces current fluctuations that challenge melt flow stability and interface dynamics. This study employs a 3D coupled electro-magneto-flow numerical model to examine the effects of current fluctuations, cathode W-type wear, and erosion hole repair across different operational stages. In early operation, without W-wear, fluctuating currents increasing from 0.925I₀ to 1.150I₀ raise melt flow velocities from 0.175 m s−1 to 0.201 m s−1 and interface deformation from 2.15 cm to 3.38 cm, within safe anode-cathode distance (ACD). In the middle stage, W-wear reduces flow velocity by 0.016 m s−1 and interface fluctuation by 0.49 cm, allowing limited fluctuations but promoting erosion. Late-stage erosion holes lead to localized current density peaks (13,492 A m−2), destabilizing flow. Mitigation strategies like alumina sludge repair and steel bar disconnection reduce interface fluctuation by 0.06 cm but cannot sustain safe current fluctuations. These findings provide critical guidance for optimizing clean energy integration in aluminum production.
- 1 May 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (5) , 053503
Numerical and On-Site Validation of Current Fluctuations and Cathode Wear on Melt Flow Stability in Flexible Aluminum Electrolysis Cells
The integration of clean energy sources, such as wind and solar, into flexible aluminum electrolysis cells introduces current fluctuations that challenge melt flow stability and interface dynamics. This study employs a 3D coupled electro-magneto-flow numerical model to examine the effects of current fluctuations, cathode W-type wear, and erosion hole repair across different operational stages. In early operation, without W-wear, fluctuating currents increasing from 0.925I₀ to 1.150I₀ raise melt flow velocities from 0.175 m s−1 to 0.201 m s−1 and interface deformation from 2.15 cm to 3.38 cm, within safe anode-cathode distance (ACD). In the middle stage, W-wear reduces flow velocity by 0.016 m s−1 and interface fluctuation by 0.49 cm, allowing limited fluctuations but promoting erosion. Late-stage erosion holes lead to localized current density peaks (13,492 A m−2), destabilizing flow. Mitigation strategies like alumina sludge repair and steel bar disconnection reduce interface fluctuation by 0.06 cm but cannot sustain safe current fluctuations. These findings provide critical guidance for optimizing clean energy integration in aluminum production.