Volker Ventzke
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Volker Ventzke has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
- Nikolai Kashaev
Helmholtz-Zentrum Hereon
4 shared publications - Benjamin Klusemann
Leuphana University Lüneburg
2 shared publications Falk Dorn
2 shared publications- Mustafa Koçak
İSTANBUL GEDİK ÜNİVERSİTESİ, MÜHENDİSLİK FAKÜLTESİ, MAKİNE MÜHENDİSLİĞİ BÖLÜMÜ
2 shared publications - Stefan Riekehr
Helmholtz-Zentrum Geesthacht
2 shared publications A. I. Koruk
1 shared publication
Latest Publications
- Open Access
- 1 April 2026
- Published by Elsevier in Materials & Design
- Vol. 265
Mechanical properties and hot forming potential of micro-perforated titanium sheets for laminar flow control structures
- 1 April 2026
- Published by Elsevier in Materials & Design
- Vol. 265
Open AccessMechanical properties and hot forming potential of micro-perforated titanium sheets for laminar flow control structures
- Open Access
- 7 March 2026
- Published by Elsevier in Materials & Design
- Vol. 264
Fatigue characteristics improvement of the TIG-welded 316L specimens with T-joint geometry using laser shock peening
- 7 March 2026
- Published by Elsevier in Materials & Design
- Vol. 264
Open AccessFatigue characteristics improvement of the TIG-welded 316L specimens with T-joint geometry using laser shock peening
- Open Access
- 1 December 2024
- Published by Walter de Gruyter GmbH in Fatigue of Aircraft Structures
- Vol. 2024 (16) , 29-44
On the Application of Laser Shock Peening as a Manufacturing and Repair Process to Improve the Fatigue Performance of Refill Friction Stir Spot-Welded AA2024-T3 Joints
The refill friction stir spot welding (refill FSSW) process is an innovative solid-state spot-welding method, which has evolved from the concept of friction stir welding. Compared to riveting, the process has the advantage of avoiding stress concentration by eliminating holes. In addition, weight can be saved compared to riveting as no additional material is needed. However, the fatigue strength of refill FSSW joints under cyclic loading is still not satisfactory. To address this challenge, laser shock peening (LSP) is investigated as an innovative residual stress engineering technique to improve the fatigue performance of refill FSSW AA2024-T3 joints. Two application scenarios are investigated, one investigating the LSP technique as a complementary manufacturing process to the refill FSSW technology, and the other investigating the LSP technique as a repair process for damaged joints. The fatigue test results showed that the application of the LSP treatment can significantly improve the fatigue behaviour of the refill FSSW overlap joints. In terms of Basquin fatigue strength, the LSP treatment resulted in an improvement by a factor of 1.51 and 2.82 for the one- and two-sided LSP-treated specimens, respectively. The life of specimens with refill FSSW joints that had been specifically pre-damaged by stopping the fatigue test at approximately 51%, 75% and 83% of the number of cycles to the Basquin fatigue strength, applying LSP treatment and continuing the fatigue test was also significantly extended. The results of this study show that LSP is a very effective technique for significantly extending the fatigue life of refill FSSW joints. Therefore, the combination of these two manufacturing processes, refill FSSW and LSP, represents a promising technology for industrial companies that require high fatigue performance for their structural components.
- 1 December 2024
- Published by Walter de Gruyter GmbH in Fatigue of Aircraft Structures
- Vol. 2024 (16) , 29-44
Open AccessOn the Application of Laser Shock Peening as a Manufacturing and Repair Process to Improve the Fatigue Performance of Refill Friction Stir Spot-Welded AA2024-T3 Joints
The refill friction stir spot welding (refill FSSW) process is an innovative solid-state spot-welding method, which has evolved from the concept of friction stir welding. Compared to riveting, the process has the advantage of avoiding stress concentration by eliminating holes. In addition, weight can be saved compared to riveting as no additional material is needed. However, the fatigue strength of refill FSSW joints under cyclic loading is still not satisfactory. To address this challenge, laser shock peening (LSP) is investigated as an innovative residual stress engineering technique to improve the fatigue performance of refill FSSW AA2024-T3 joints. Two application scenarios are investigated, one investigating the LSP technique as a complementary manufacturing process to the refill FSSW technology, and the other investigating the LSP technique as a repair process for damaged joints. The fatigue test results showed that the application of the LSP treatment can significantly improve the fatigue behaviour of the refill FSSW overlap joints. In terms of Basquin fatigue strength, the LSP treatment resulted in an improvement by a factor of 1.51 and 2.82 for the one- and two-sided LSP-treated specimens, respectively. The life of specimens with refill FSSW joints that had been specifically pre-damaged by stopping the fatigue test at approximately 51%, 75% and 83% of the number of cycles to the Basquin fatigue strength, applying LSP treatment and continuing the fatigue test was also significantly extended. The results of this study show that LSP is a very effective technique for significantly extending the fatigue life of refill FSSW joints. Therefore, the combination of these two manufacturing processes, refill FSSW and LSP, represents a promising technology for industrial companies that require high fatigue performance for their structural components.
- Open Access
- 7 April 2020
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 43 (7) , 1500-1513
On the application of laser shock peening for retardation of surface fatigue cracks in laser beam‐welded AA6056
The present study aims to investigate the extent to which the fatigue behaviour of laser beam‐welded AA6056‐T6 butt joints with an already existing crack can be improved through the application of laser shock peening. Ultrasonic testing was utilized for in situ (nondestructive) measurement of fatigue crack growth during the fatigue test. This procedure allowed the preparation of welded specimens with surface fatigue cracks with a depth of approximately 1.2 mm. The precracked specimens showed a 20% reduction in the fatigue limit compared with specimens without cracks in the as‐welded condition. Through the application of laser shock peening on the surfaces of the precracked specimens, it was possible to recover the fatigue life to the level of the specimens tested in the as‐welded condition. The results of this study show that laser shock peening is a very promising technique to recover the fatigue life of welded joints with surface cracks, which can be detected by nondestructive testing.
- 7 April 2020
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 43 (7) , 1500-1513
Open AccessOn the application of laser shock peening for retardation of surface fatigue cracks in laser beam‐welded AA6056
The present study aims to investigate the extent to which the fatigue behaviour of laser beam‐welded AA6056‐T6 butt joints with an already existing crack can be improved through the application of laser shock peening. Ultrasonic testing was utilized for in situ (nondestructive) measurement of fatigue crack growth during the fatigue test. This procedure allowed the preparation of welded specimens with surface fatigue cracks with a depth of approximately 1.2 mm. The precracked specimens showed a 20% reduction in the fatigue limit compared with specimens without cracks in the as‐welded condition. Through the application of laser shock peening on the surfaces of the precracked specimens, it was possible to recover the fatigue life to the level of the specimens tested in the as‐welded condition. The results of this study show that laser shock peening is a very promising technique to recover the fatigue life of welded joints with surface cracks, which can be detected by nondestructive testing.
- 1 July 2016
- Published by Elsevier in Materials & Design
- Vol. 101, 137-145
Influence of crystallographic texture on the microstructure, tensile properties and residual stress state of laser-welded titanium joints
- 1 July 2016
- Published by Elsevier in Materials & Design
- Vol. 101, 137-145
Influence of crystallographic texture on the microstructure, tensile properties and residual stress state of laser-welded titanium joints
- 1 August 2007
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 12 (6) , 508-515
Failure behaviour of laser spot welds of TRIP800 steel sheets under coach–peel loading
This study is carried out to investigate the laser spot welds (LSWs) of advanced high strength steel sheets of 1·0 mm thickness for application to the automotive industry. Mechanical properties and failure behaviour of LSWs for transformation induced plasticity steel sheets (TRIP800) subjected to monotonic coach–peel loading are investigated by experimental and finite element (FE) simulation methods. Microstucture of LSW and fracture surfaces of the welded specimens were examined by scanning electron microscopy (SEM) to describe the microstructural features and to clarify the crack initiation mechanism respectively. Based on simulation solutions equivalent plastic strain was obtained to describe local deformation of LSW joints. Experimental results revealed a ‘plug type’ of failure mode of the circular LSW joints under ‘peel–coach’ loading condition. This type of ductile failure is the most common failure mode for spot welds used in the automotive industry. Numerical simulation of damage process was compared with experimental results and this revealed that fracture path was successfully predicted.
- 1 August 2007
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 12 (6) , 508-515
Failure behaviour of laser spot welds of TRIP800 steel sheets under coach–peel loading
This study is carried out to investigate the laser spot welds (LSWs) of advanced high strength steel sheets of 1·0 mm thickness for application to the automotive industry. Mechanical properties and failure behaviour of LSWs for transformation induced plasticity steel sheets (TRIP800) subjected to monotonic coach–peel loading are investigated by experimental and finite element (FE) simulation methods. Microstucture of LSW and fracture surfaces of the welded specimens were examined by scanning electron microscopy (SEM) to describe the microstructural features and to clarify the crack initiation mechanism respectively. Based on simulation solutions equivalent plastic strain was obtained to describe local deformation of LSW joints. Experimental results revealed a ‘plug type’ of failure mode of the circular LSW joints under ‘peel–coach’ loading condition. This type of ductile failure is the most common failure mode for spot welds used in the automotive industry. Numerical simulation of damage process was compared with experimental results and this revealed that fracture path was successfully predicted.
- 1 December 2004
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 9 (6) , 513-518
Transient liquid phase (TLP) bonding of TiAl using various insert foils
TiAl intermetallic alloys have been joined using the diffusion brazing technique with Ti insert foil metal combined with Cu, Ni or Fe foils. Defect-free joints can be fabricated successfully, no matter which kind of foil combination is used as insert metal. The interface structures of the joints were also investigated and results showed various interface structures in the joined zones. A mechanism for the development of the interface structure is proposed. It is suggested that the formation process of the liquid phase was responsible for the resulting interface structures. Post-bond heat treatment (PBHT) had no obvious effect on the interface structure of the joints because of the low diffusion coefficient of Cu, Ni and Fe in the parent material. Microhardness results showed a slight decrease in the joint area as a result of PBHT.
- 1 December 2004
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 9 (6) , 513-518
Transient liquid phase (TLP) bonding of TiAl using various insert foils
TiAl intermetallic alloys have been joined using the diffusion brazing technique with Ti insert foil metal combined with Cu, Ni or Fe foils. Defect-free joints can be fabricated successfully, no matter which kind of foil combination is used as insert metal. The interface structures of the joints were also investigated and results showed various interface structures in the joined zones. A mechanism for the development of the interface structure is proposed. It is suggested that the formation process of the liquid phase was responsible for the resulting interface structures. Post-bond heat treatment (PBHT) had no obvious effect on the interface structure of the joints because of the low diffusion coefficient of Cu, Ni and Fe in the parent material. Microhardness results showed a slight decrease in the joint area as a result of PBHT.