Khawlah A. Alothman
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Khawlah A. Alothman has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Hanan Filemban
Department of Restorative Dentistry, Faculty of Dentistry, King Abdulaziz University, Jeddah 21589, Saudi Arabia
2 shared publications - Maher Saeed Hajjaj
Department of Restorative Dentistry, Faculty of Dentistry, King Abdulaziz University, Jeddah 21589, Saudi Arabia
2 shared publications - Marwa Bawazir
Department of Restorative Dentistry, Faculty of Dentistry, King Abdulaziz University, Jeddah 21589, Saudi Arabia
2 shared publications - Najla Al Turkestani
Department of Restorative Dentistry, Faculty of Dentistry, King Abdulaziz University, Jeddah 21589, Saudi Arabia
2 shared publications - Saeed Jamaan Alzahrani
Department of Restorative Dentistry, Faculty of Dentistry, King Abdulaziz University, Jeddah 21589, Saudi Arabia
2 shared publications - Yasser Merdad
Department of Restorative Dentistry, Faculty of Dentistry, King Abdulaziz University, P.O. Box 80209, Jeddah 21589, Saudi Arabia
2 shared publications
Latest Publications
- Open Access
- 1 June 2026
- Published by MDPI AG in Applied Sciences
- Vol. 16 (11) , 5493
Comparison of Shear Bond Strength and Interfacial Failure Patterns of Glass Hybrid Ionomer, Resin-Modified Glass Ionomer, and Nanofilled Composite to Dentin: An In Vitro Study
This in vitro study evaluated and compared the shear bond strength (SBS) of three restorative materials bonded to dentin: a glass hybrid ionomer (EQUIA Forte HT), a resin-modified glass ionomer (RIVA Light Cure), and a nanofilled composite resin (Filtek Z350 XT). Additionally, their modes of failure were assessed. Thirty extracted human teeth were prepared and randomly assigned to three groups (n = 10) by restorative material: Group 1: Filtek Z350 XT; Group 2: EQUIA Forte HT; Group 3: RIVA Light Cure. All materials were applied following manufacturer instructions. SBS testing used a universal testing machine, applying a load at the tooth–restoration interface at 1 mm/min until failure. SBS values were recorded in megapascals (MPa). Failure modes were examined under a stereomicroscope at 40× magnification. A one-way ANOVA compared mean SBS among groups, with post hoc tests for pairwise group comparisons. Results: Filtek Z350 XT had the highest mean SBS (21 MPa), followed by RIVA Light Cure (7.5 MPa) and EQUIA Forte HT (7.2 MPa). One-way ANOVA indicated a statistically significant difference in SBS (p < 0.05). Post hoc analysis showed Filtek Z350 XT had significantly higher SBS than the glass ionomer-based materials, while EQUIA Forte HT and RIVA Light Cure did not differ significantly. Conclusions: Filtek Z350 XT demonstrated significantly higher shear bond strength to dentin than the glass ionomer-based materials. No significant SBS difference was found between the resin-modified and hybrid glass ionomers.
- 1 June 2026
- Published by MDPI AG in Applied Sciences
- Vol. 16 (11) , 5493
Open AccessComparison of Shear Bond Strength and Interfacial Failure Patterns of Glass Hybrid Ionomer, Resin-Modified Glass Ionomer, and Nanofilled Composite to Dentin: An In Vitro Study
This in vitro study evaluated and compared the shear bond strength (SBS) of three restorative materials bonded to dentin: a glass hybrid ionomer (EQUIA Forte HT), a resin-modified glass ionomer (RIVA Light Cure), and a nanofilled composite resin (Filtek Z350 XT). Additionally, their modes of failure were assessed. Thirty extracted human teeth were prepared and randomly assigned to three groups (n = 10) by restorative material: Group 1: Filtek Z350 XT; Group 2: EQUIA Forte HT; Group 3: RIVA Light Cure. All materials were applied following manufacturer instructions. SBS testing used a universal testing machine, applying a load at the tooth–restoration interface at 1 mm/min until failure. SBS values were recorded in megapascals (MPa). Failure modes were examined under a stereomicroscope at 40× magnification. A one-way ANOVA compared mean SBS among groups, with post hoc tests for pairwise group comparisons. Results: Filtek Z350 XT had the highest mean SBS (21 MPa), followed by RIVA Light Cure (7.5 MPa) and EQUIA Forte HT (7.2 MPa). One-way ANOVA indicated a statistically significant difference in SBS (p < 0.05). Post hoc analysis showed Filtek Z350 XT had significantly higher SBS than the glass ionomer-based materials, while EQUIA Forte HT and RIVA Light Cure did not differ significantly. Conclusions: Filtek Z350 XT demonstrated significantly higher shear bond strength to dentin than the glass ionomer-based materials. No significant SBS difference was found between the resin-modified and hybrid glass ionomers.
- Open Access
Effects of Preheating on the Mechanical Properties of Dental Composites
The aim of this study was to evaluate the mechanical properties (flexural strength (FS), flexural modulus (FM), Vickers microhardness (VMN), and shear bond strength (SBS)) of preheated composites. Two preheated composites (Z350XT and Proclinic) and one self-adhesive resin cement (RelyX™ U200) were used to fabricate specimens. All the specimens were subjected to thermocycling before their mechanical properties were evaluated. One-way ANOVA was used for statistical analysis, followed by Tukey’s post hoc test. The chi-square test was used to evaluate the failure modes after SBS test. Results: RelyX™ U200 had a significantly higher FS (106.22 ± 14.23 MPa) than Proclinic (85.76 ± 12.75 MPa) and Z350 (71.47 ± 22.98 MPa). Z350 (118.10 ± 11.3 GPa) and RelyX™ U200 (110.88 ± 13.44 GPa) had significantly higher FMs than Proclinic (83.72 ± 9.3 GPa). A significantly higher VHN was seen with Z350 (136.84 ± 11.52 VHN) compared to Proclinic (115.25 ± 17.15 VHN) and RelyX™ U200 (100.83 ± 12.69 VHN). Z350 had a higher SBS (20.75 ± 5.6 MPa) than RelyX™ U200 (15.4 ± 3.46 MPa), while Proclinic was the weakest among all the groups (6.76 ± 1.44 MPa). In the failure mode analysis, the mixed failure mode was predominantly seen in all groups. In conclusion, not all preheated composites behave the same and it is the clinician’s responsibility to select the appropriate material for every clinical situation.
Open AccessEffects of Preheating on the Mechanical Properties of Dental Composites
The aim of this study was to evaluate the mechanical properties (flexural strength (FS), flexural modulus (FM), Vickers microhardness (VMN), and shear bond strength (SBS)) of preheated composites. Two preheated composites (Z350XT and Proclinic) and one self-adhesive resin cement (RelyX™ U200) were used to fabricate specimens. All the specimens were subjected to thermocycling before their mechanical properties were evaluated. One-way ANOVA was used for statistical analysis, followed by Tukey’s post hoc test. The chi-square test was used to evaluate the failure modes after SBS test. Results: RelyX™ U200 had a significantly higher FS (106.22 ± 14.23 MPa) than Proclinic (85.76 ± 12.75 MPa) and Z350 (71.47 ± 22.98 MPa). Z350 (118.10 ± 11.3 GPa) and RelyX™ U200 (110.88 ± 13.44 GPa) had significantly higher FMs than Proclinic (83.72 ± 9.3 GPa). A significantly higher VHN was seen with Z350 (136.84 ± 11.52 VHN) compared to Proclinic (115.25 ± 17.15 VHN) and RelyX™ U200 (100.83 ± 12.69 VHN). Z350 had a higher SBS (20.75 ± 5.6 MPa) than RelyX™ U200 (15.4 ± 3.46 MPa), while Proclinic was the weakest among all the groups (6.76 ± 1.44 MPa). In the failure mode analysis, the mixed failure mode was predominantly seen in all groups. In conclusion, not all preheated composites behave the same and it is the clinician’s responsibility to select the appropriate material for every clinical situation.