  • Interfacial Properties of Alloying Interlayers in Anode-Free Sodium Metal Batteries

    by Alexis Luglio, Aaron Max Melemed, Anna Poirier, Daniel W. Liao, Neil P. Dasgupta

    Due to the low price and abundance of sodium, researchers have gained interest in developing sodium-ion batteries as a more sustainable energy storage option to lithium-ion batteries. Although the energy density of sodium-ion batteries is relatively lower than lithium, the “anode-free” battery (AFB) has the potential to be competitive with lithium-ion energy densities. In the anode-free configuration, sodium is entirely sourced from the cathode and is plated/stripped directly on the aluminum current collector (CC). However, plating of sodium on the current collector can be inhomogeneous in morphology, lowering the coulombic efficiency and decreasing cycle life. The incorporation of a metaling alloying interlayer on the CC has been previously shown to promote homogeneous deposition due to the enhanced sodium wetting on the substrate, resulting in reduced plating overpotentials and improved cycle life.[1,2] However, there has been a general lack of in situ/operando observations of the morphological evolution of sodium in the presence of an alloying interlayer, or quantitative analysis of sodium contact angles on these interlayers. Additionally, these interlayers are reported to delaminate from the CC throughout cycling and expose the underlying CC surface, which is detrimental to battery performance over time. In this work, we explore the sodium morphological evolution and adhesion on nanoscale gold interlayers that were deposited on an aluminum CC, to better understand how the interlayer improves sodium AFB performance. We further introduce an intermediate adhesion bi-layer structure to mitigate delamination and promote improved stability. To observe the morphological evolution of sodium on the interlayers compared to an uncoated CC, we utilized operando video microscopy,[3] together with complimentary post-mortem optical imaging and scanning electron microscopy (SEM). Sodium exhibited increased adhesion and uniformity on the gold interlayer compared to the uncoated CC; however, sodium preferentially plates onto microstructural features on the CC surface, suggesting there is current focusing in these regions. The alloying interlayer elements were also observed to migrate along the surface during plating, exposing the underlying aluminum foil. To further analyze sodium adhesion, quantitative contact angle measurements between molten sodium and these substrates were performed,[4] which revealed increased sodiophilicity and a higher work of adhesion on the interlayer. We further performed quantitative peel tests, which suggests that the interfacial toughness of gold on the CC substrate is poor. Therefore, to increase the adhesion of the gold to the CC to prevent interlayer delamination during subsequent cycling we introduce a bi-layer structure. Preliminary results suggest that the bilayer provides stronger interfacial toughness of the interlayer on the CC, which can circumvent the limitations of a pure gold layer. These fundamental studies will inform design requirements for metallic interlayers for sodium AFBs, and highlight the coupled importance of wetting, adhesion, and nucleation. [1] Tang, S.; Qiu, Z.; Wang, X.-Y.; Gu, Y.; Zhang, X.-G.; Wang, W.-W.; Yan, J.-W.; Zheng, M.-S.; Dong, Q.-F.; Mao, B.-W. A Room-Temperature Sodium Metal Anode Enabled by a Sodiophilic Layer. Nano Energy 2018 , 48 , 101–106. https://doi.org/10.1016/j.nanoen.2018.03.039. [2] Tang, S.; Zhang, Y.; Zhang, X.; Li, J.; Wang, X.; Yan, J.; Wu, D.; Zheng, M.; Dong, Q.; Mao, B. Stable Na Plating and Stripping Electrochemistry Promoted by In Situ Construction of an Alloy‐Based Sodiophilic Interphase. Adv. Mater. 2019 , 31 (16), 1807495. https://doi.org/10.1002/adma.201807495. [3] Sanchez, A. J.; Kazyak, E.; Chen, Y.; Chen, K.-H.; Pattison, E. R.; Dasgupta, N. P. Plan-View Operando Video Microscopy of Li Metal Anodes: Identifying the Coupled Relationships among Nucleation, Morphology, and Reversibility. ACS Energy Lett. 2020 , 5 (3), 994–1004. https://doi.org/10.1021/acsenergylett.0c00215. [4] Yoon, J. S.; Liao, D. W.; Greene, S. M.; Cho, T. H.; Dasgupta, N. P.; Siegel, D. J. Thermodynamics, Adhesion, and Wetting at Li/Cu(-Oxide) Interfaces: Relevance for Anode-Free Lithium–Metal Batteries. ACS Appl. Mater. Interfaces 2024 , 16 (15), 18790–18799. https://doi.org/10.1021/acsami.3c19034.

  • Impact of Electrolyte Formulation on Solid Electrolyte Interphase Formation in Anode-Free Sodium Batteries

    by Aaron Max Melemed, Alexis Luglio, Ethan Bennett Rose, Neil P. Dasgupta

    Given concerns about the low earth abundance of lithium (Li) in Li-ion batteries, there is growing interest in developing a beyond-Li materials basis for rechargeable batteries. Batteries based on sodium (Na) are a compelling alternative due to the ~1000-fold higher concentration of Na in the earth’s crust, along with high charge capacities (1166 mAh/g, 1128 mAh/cm 3 ) if Na is used as a metallic anode. A major issue with Na metal, however, is its chemical reactivity. Conventional carbonate-based battery electrolytes react with Na to form a thick, heterogeneous, and organic-rich solid electrolyte interphase (SEI) that exacerbates plating nonuniformity and capacity loss during cycling. [1,2] In comparison, ether-based electrolytes have been observed to promote the formation of a relatively compact, inorganic-rich SEI on plated Na, which can enable extended cycle life in certain formulations such as NaPF 6 in glyme. [1,2] One important yet underexplored aspect of Na electrochemistry, however, is the “pre-cycling” SEI, which forms on the current collector (CC) via electrolyte decomposition before Na plating onset. In Li metal systems, for example, chemical inhomogeneities on the CC can cause current focusing during Li nucleation, intensifying the heterogeneity of Li deposits, [3] and plated Li has even been found to chemically react with surface oxide species on the CC [4] — which is of elevated concern for Na. This study quantitatively examines the pre-cycling SEI formation in a range of relevant ether-based Na electrolytes; we systematically examine various Na salts in glymes of different lengths in order to explore the relationship between the Na + coordination environment, SEI composition, and ensuing electrochemical behavior. The electrolytes examined herein are 1 M of a Na salt (NaPF 6 , NaBF 4 , NaFSI, or NaTFSI) in either 1,2-dimethoxyethane (G1), bis(2-methoxyethyl) ether (G2), triethylene glycol dimethyl ether (G3), or tetraethylene glycol dimethyl ether (G4), if soluble. Raman spectroscopy measurements in different glymes demonstrate varying degrees of ion pairing, providing an avenue for quantitative comparison between Na + --anion coordination and SEI formation products. Na-Al cells are utilized for electrochemical analysis; both galvanostatic reduction and linear sweep voltammetry (LSV) at slow rates reveal small but significant reductive capacities (~0.005 mA/cm 2 ) before Na plating onset in each electrolyte. Cyclic voltammetry is then performed between 0 and 2 V vs. Na, revealing that roughly half of the 1 st cycle reductive capacity can in fact be attributed to irreversible electrolyte decomposition. LSV of G3- and G4-based electrolytes in three different Na salts exhibit distinct current density peaks, providing electrochemical signatures of enhanced decomposition for these particular glymes. Next, Al electrodes are systematically polarized to different positive potentials vs. Na; XPS and FTIR analyses reveal both anion and solvent decomposition products on the CC surface. Interphase composition is dependent on polarization potential, which suggests the presence of different electrolyte decomposition pathways. Finally, the impact of the pre-cycling SEI on ensuing electrochemistry is examined. This work further reveals the impact that electrolyte composition can have on the very early stages of battery operation, with lessons relevant to both Na metal and Na-ion battery research. [1] Seh, Z. W., Sun, J., Sun, Y. & Cui, Y. A Highly Reversible Room-Temperature Sodium Metal Anode. ACS Central Science 1 , 449-455 (2015). [2] Sayahpour, B. et al. Quantitative analysis of sodium metal deposition and interphase in Na metal batteries. Energy & Environmental Science 17 , 1216-1228 (2024). [3] Sanchez, A. J. & Dasgupta, N. P. Lithium Metal Anodes: Advancing our Mechanistic Understanding of Cycling Phenomena in Liquid and Solid Electrolytes. Journal of the American Chemical Society 146 , 4282-4300 (2024). [4] Yoon, J. S. et al. Thermodynamics, Adhesion, and Wetting at Li/Cu(-Oxide) Interfaces: Relevance for Anode-Free Lithium–Metal Batteries. ACS Applied Materials & Interfaces 16 , 18790-18799 (2024).

  • Area-Selective Lithium Deposition in Anode-Free Solid-State Batteries Using Patterned Atomic Layer Deposition Interlayers

    by Davy Zeng, Alexis Luglio, Daniel W. Liao, Younggyu Kim, Tae H. Cho, Neil P. Dasgupta

    Anode-free solid-state batteries (SSBs) are a promising alternative to traditional lithium-ion batteries (LIBs) with higher energy density, better manufacturability, and improved safety. The key challenge associated with the widespread use of anode-free batteries lies in the irreversible cycling of lithium metal. The nucleation of lithium on a bare copper surface occurs stochastically due to “hot spots”, resulting in uneven plating and lithium dendrite growth which causes cell failure. While significant efforts have been devoted to improving the uniformity of lithium plating in LIBs by modifying the current collector using patterned interlayers and 3D geometries [1,2], it is unclear if these techniques are directly translatable to solid-state batteries due to the uniquely complex chemo-mechanics of the solid-solid interface. Therefore, in this study we explore the use of patterned ALD deposited interlayers to control in situ lithium metal formation at the current collector and argyrodite (Li 6 PS 5 Cl) solid electrolyte interface. ALD thin films that range from lithiophilic to lithiophobic (ZnO, Al 2 O 3 , and LiF) were patterned spatially on copper current collectors using photolithography. Molten lithium contact angle measurements were obtained to quantify wetting behavior of the ALD interlayers [3]. Lithium metal nucleation and early growth selectivity on the resulting patterns were studied at various current densities, stack pressures, and areal capacities using post-mortem optical microscopy and focused ion-beam/scanning electron microscopy (FIB-SEM) techniques. Lithium selectivity was quantified by comparing deposition on active (lithiophilic) and inactive (lithiophobic) regions of the current collector through image segmentation. Lithium was observed to preferentially deposit on lithiophilic regions in single material patterns, and selectivity was significantly improved using dual patterns that employed ZnO in active areas and Al 2 O 3 in inactive regions. The highly customizable process of patterning which was developed allows for the design of interlayers with complex 2D shapes, enabling controlled area selective deposition of lithium. This platform opens the possibility of investigating challenging phenomena in SSBs, such as void formation during fast discharge. [1] Jung, W.-B. et al. ACS Appl. Mater. Interfaces 13 , 60978–60986 (2021) [2] Chen, K.-H., Sanchez, A. J., Kazyak, E., Davis, A. L. & Dasgupta, N. P. Adv. Energy Mater. 9 , 1802534 (2019) [3] J. S. Yoon, D. W. Liao, S. M. Greene, T. H. Cho, N. P. Dasgupta, D. J. Siegel, ACS Appl. Mater. Interfaces 16 , 18790 (2024)

  • Open Access

    Maximizing calendering effects through the mechanical pulverization of Co-free nickel-rich cathodes in lithium-ion cells

    by Alexis Luglio, Kae Fink, Francois Usseglio-Viretta, Andrew Colclasure, Patrick Walker, John S. Mangum, Ryan Brow

    Calendering is a technique used to maximize the volumetric energy density of battery electrodes. However, higher amounts of calendering result in increased tortuosity and particle cracking. We propose a novel packing structure of electrode particles to maximize calendering benefits while minimizing particle fracture. Cobalt-free layered oxide cathode LiNi0.92Mn0.04Al0.04O2 (NMA) particles are pulverized through ball-milling and coated with lithium phosphate. Pulverized and pristine NMA are fabricated into “bimodal” electrodes, whereas “unimodal” electrodes consist of only pristine NMA. Each electrode type was made into 30% porosity, 40% porosity, and uncalendered coin cell samples. X-ray diffraction suggests that the unimodal samples suffer from more particle fracture than the bimodal samples when calendered to the same porosity of 30%. Electrochemical impedance spectroscopy suggests that the bimodal electrodes exhibit lower surface film resistance. This is supported by enhanced capacity retention for the bimodal samples after 100 cycles. Graphical Impact statement: Calendering is an essential manufacturing process for Li-ion batteries (LIBs). Despite calendering increasing the energy density of electrodes and improving ionic and electronic connections, it also enhances particle cracking and hinders Li-ion migration. In this article, we investigate a novel “bimodal” packing configuration of a Co-free cathode material and analyze the configuration’s impact on particle cracking at different levels of calendering. There is an increasing effort to eliminate Co in LIB cathode materials due to its expensive and controversial mining conditions. Through electrochemical and structural characterization techniques, we probe particle cracking at different levels of calendering in bimodal and control electrodes. We report the ability of our bimodal configuration to decrease particle cracking and enhance capacity retention. We believe this work is highly impactful because it suggests a direct application to manufacture design of next-generation, Co-free cathodes which have accelerated intragranular cracking compared to current LIB cathodes.