HYH. Yin

H. Yin

*This is an algorithmically generated author record based on publicly available information.

H. Yin has a total of 8 co-authors. Here are the top co-authors by number of shared publications:

  • D. K. Sadana

    IBM Semiconductor Research and Development Center Research Division T. J. Watson Research Center, Yorktown Heights, New York 10598

    2 shared publications
  • J. A. Ott

    IBM Semiconductor Research and Development Center Research Division T. J. Watson Research Center, Yorktown Heights, New York 10598

    2 shared publications
  • K. E. Fogel

    IBM Semiconductor Research and Development Center Research Division T. J. Watson Research Center, Yorktown Heights, New York 10598

    2 shared publications
  • Katherine L. Saenger

    115 Underhill Road, Ossining, New York 10562, USA

    2 shared publications
  • C. Y. Sung

    IBM, Research Division, T. J. Watson Research Center , Yorktown Heights, New York 10598

    1 shared publication
  • F.L. Wang

    Chongqing Industry Polytechnic College, School of Mechanical Engineering, Chongqing, China

    1 shared publication

Latest Publications

  • Open Access

    Eradicating Brittleness of Ti-6Al-4V/Cu Dissimilar Brazed Joint using a Nb Diffusion Barrier

    by F.L. Wang, L. Bai, H. Yin

    Directly brazing titanium (Ti) alloy and copper (Cu) using silver (Ag) based filler alloy has been recognized to be of limited success owing to the embrittlement of intermetallic compounds (IMCs) presented at joint interface. In the current investigation, strong and reliable brazing of Ti-6Al-4V and Cu was achieved by using a niobium (Nb) diffusion barrier deposited on Ti-6Al-4V base material and Ag-Cu-Ti active braze. The Nb diffusion barrier effectively suppressed the interaction between Ag-Cu-Ti filler and Ti-6Al-4V base material, avoiding formation of brittle Ti-Cu IMCs. Joint consisting of Ti-Nb solid solution, unconsumed Nb interlayer, remnant Ag-based braze and small quantity of tiny Ti-Cu IMC particles was obtained via diffusion bonding at Ti- 6Al-4V/Nb interface and active brazing between Nb interlayer and Cu based material. Bonding strength exceeding the Cu base material property was achieved in the resultant joint, ascribed to elimination of continuous bulk brittle interfacial reaction products.


  • An examination of facet formation during solid phase epitaxy of line-shaped amorphized regions in (001) and (011) Si

    by K. L. Saenger, K. E. Fogel, J. A. Ott, D. K. Sadana, H. Yin

    The shapes of the recrystallization fronts observed during solid phase epitaxy (SPE) in line-shaped amorphized Si (a-Si) regions in single-crystal (001) and (011) Si are shown to exhibit a complex time evolution inconsistent with simple models in which regrowth behavior is determined exclusively by the competition between fixed-growth-rate lateral and vertical SPE. We find that the main features of our data for ⟨110⟩-aligned a-Si lines may be explained by the propensity of the lateral and vertical growth fronts to form stable a-Si∕{111} interfaces at their edges. These same a-Si∕{111} interfaces have been previously implicated as the root cause of the trench-edge defects produced during the recrystallization of patterned a-Si regions bounded laterally by oxide-filled trenches. An extension of a nanofacet model recently developed to explain the trench-edge defects is shown to explain many of the observed recrystallization behaviors.


  • A study of trench-edge defect formation in (001) and (011) silicon recrystallized by solid phase epitaxy

    by K. L. Saenger, J. P. de Souza, K. E. Fogel, J. A. Ott, C. Y. Sung, D. K. Sadana, H. Yin

    Trench-edge defects formed during epitaxial recrystallization of trench-bounded amorphized silicon (a-Si) regions are examined as a function of Si substrate crystal orientation. In Si (001), rectilinear a-Si features having edges aligned with the crystal’s in-plane ⟨110⟩ directions recrystallize leaving trench-edge defects along all trench edges, whereas the identical features in Si (011) recrystallize without trench-edge defects along trench edges parallel to the crystal’s in-plane ⟨100⟩ direction and with trench-edge defects along trench edges parallel to the crystal’s in-plane ⟨110⟩ direction. The positions and lateral extent of these trench-edge defects suggest that their source is defective epitaxy on slow-growing {111} planes formed during recrystallization. A heuristic model proposed to explain the formation of these {111} planes correctly predicts the essentially defect-free recrystallization seen for rectilinear a-Si features in Si (001) having edges aligned with the crystal’s in-plane ⟨100⟩ directions, but cannot completely account for the distinctively curved growth fronts sometimes seen at intermediate stages of recrystallization.