Steven Lam
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Steven Lam has a total of 45 co-authors. Here are the top co-authors by number of shared publications:
- Robert L. Sacci
Oak Ridge National Laboratory
6 shared publications - Gabriel M. Veith
Chemical Sciences Division, Oak Ridge National Laboratory, Oak Ridge, Tennessee 37831, USA
5 shared publications - Amanda L. Musgrove
Oak Ridge National Laboratory
4 shared publications - Marco-Tulio Fonseca Rodrigues
Argonne National Laboratory
3 shared publications - Andrew M. Colclasure
National Renewable Energy Laboratory
2 shared publications - Ankit Verma
National Laboratory of the Rockies
2 shared publications
Latest Publications
- 10 October 2026
- Published by American Chemical Society (ACS) in ACS Energy Letters
- Vol. 11 (11) , 7694-7703
Improving the Calendar Life of Silicon Anodes with Inorganic Solid–Electrolyte Interphases
Silicon anodes unlock higher energy density in Li-ion batteries but suffer from poor calendar life due to inadequately passivating solid–electrolyte interphases (SEIs). Here, we contrast the calendar aging behaviors of single- and mixed-salt locally superconcentrated electrolytes (LSCEs) against carbonate electrolytes. Mixed-salt LSCE cells retained 96% and 44% of precalendar capacity after one month and then after five months, while carbonate electrolyte cells retained 77% and 1%, respectively. The mixed-salt LSCE advantage is tied to the formation of a predominantly inorganic SEI, evidenced by nanoscale Fourier transform infrared spectromicroscopy, X-ray photoelectron spectroscopy, and 3D time-of-flight secondary ion mass spectrometry. After 5 months, however, perturbations to SEIs were evident in all cells, accelerating voltage decay and capacity loss by lithium inventory loss associated with SEI growth. These findings suggest that future electrolytes may benefit from strategies that continuously reinforce the SEI through controlled anion and solvent redox in LSCEs.
- 10 October 2026
- Published by American Chemical Society (ACS) in ACS Energy Letters
- Vol. 11 (11) , 7694-7703
Improving the Calendar Life of Silicon Anodes with Inorganic Solid–Electrolyte Interphases
Silicon anodes unlock higher energy density in Li-ion batteries but suffer from poor calendar life due to inadequately passivating solid–electrolyte interphases (SEIs). Here, we contrast the calendar aging behaviors of single- and mixed-salt locally superconcentrated electrolytes (LSCEs) against carbonate electrolytes. Mixed-salt LSCE cells retained 96% and 44% of precalendar capacity after one month and then after five months, while carbonate electrolyte cells retained 77% and 1%, respectively. The mixed-salt LSCE advantage is tied to the formation of a predominantly inorganic SEI, evidenced by nanoscale Fourier transform infrared spectromicroscopy, X-ray photoelectron spectroscopy, and 3D time-of-flight secondary ion mass spectrometry. After 5 months, however, perturbations to SEIs were evident in all cells, accelerating voltage decay and capacity loss by lithium inventory loss associated with SEI growth. These findings suggest that future electrolytes may benefit from strategies that continuously reinforce the SEI through controlled anion and solvent redox in LSCEs.
- Open Access
- 21 September 2026
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 18 (38) , 52238-52252
The Three-Component Problem: Deconvoluting Electrolyte Component Roles in Solvation Structure and Silicon Calendar Aging
In this work, we deconvolute the roles of LiPF6, ethyl methyl carbonate (EMC), and vinylene carbonate (VC) in the electrolyte solvation structure and silicon anode calendar aging. By varying the mole fractions of the electrolyte constituents and utilizing a voltage hold protocol, we extract the roles of each component in the silicon anode calendar lifetime. Interestingly, the LiPF6 concentration does not affect calendar aging, whereas increasing and decreasing the EMC and VC mole fractions, respectively, lowers the electrode surface passivity. The calendar lifetime results align with EMC coordination numbers derived from MD simulations, which indicate the inner solvation sheath’s role in calendar aging mechanisms. X-ray photoelectron spectroscopy data show that the solid electrolyte interphase (SEI) species can be tuned through the electrolyte formulation and solvation structure. Li+-EMC coordination structures decompose to form insoluble alkanes, C−O species, and lithium carbonate (Li2CO3), while the anion coordination complex decomposes into LiF and LixPOyFz. Postaging, the surface lithium content of the SEI is partially replaced by C−O species from preferential decomposition of noncoordinated VC. However, the inorganic lithium species (LiF, LixPOyFz, and Li2CO3) remain constant, suggesting the dissolution of nonpolar organolithium species due to EMC’s low dielectric constant and high coordination number. This triggers continuous electrolyte decomposition to reform the SEI, which lowers the silicon anode’s calendar lifetime.
- 21 September 2026
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 18 (38) , 52238-52252
Open AccessThe Three-Component Problem: Deconvoluting Electrolyte Component Roles in Solvation Structure and Silicon Calendar Aging
In this work, we deconvolute the roles of LiPF6, ethyl methyl carbonate (EMC), and vinylene carbonate (VC) in the electrolyte solvation structure and silicon anode calendar aging. By varying the mole fractions of the electrolyte constituents and utilizing a voltage hold protocol, we extract the roles of each component in the silicon anode calendar lifetime. Interestingly, the LiPF6 concentration does not affect calendar aging, whereas increasing and decreasing the EMC and VC mole fractions, respectively, lowers the electrode surface passivity. The calendar lifetime results align with EMC coordination numbers derived from MD simulations, which indicate the inner solvation sheath’s role in calendar aging mechanisms. X-ray photoelectron spectroscopy data show that the solid electrolyte interphase (SEI) species can be tuned through the electrolyte formulation and solvation structure. Li+-EMC coordination structures decompose to form insoluble alkanes, C−O species, and lithium carbonate (Li2CO3), while the anion coordination complex decomposes into LiF and LixPOyFz. Postaging, the surface lithium content of the SEI is partially replaced by C−O species from preferential decomposition of noncoordinated VC. However, the inorganic lithium species (LiF, LixPOyFz, and Li2CO3) remain constant, suggesting the dissolution of nonpolar organolithium species due to EMC’s low dielectric constant and high coordination number. This triggers continuous electrolyte decomposition to reform the SEI, which lowers the silicon anode’s calendar lifetime.
- Open Access
- 28 July 2026
- Published by IOP Publishing in Journal of Physics: Energy
- Vol. 8 (3) , 035006
Experimental considerations and applications for time-resolved impedance on silicon-anode battery systems
Dynamic electrochemical impedance spectroscopy (dEIS) utilizes a superimposed multi-sinusoidal waveform and enables temporally resolved investigations on various electrochemical processes; however, the signal-to-noise ratio must be maximized while retaining linearity and stationarity within the system. In the present work, we probe the impact of the waveform’s total amplitude as well as the waveform and phase profiles. The equal amplitude multi-sinusoidal waveform with 35 mV total amplitude (R CT ) associated with alloying kinetics dominates the overall impedance. R CT increases with state of charge indicating a kinetic bottleneck at higher lithiation states. To explore this further, we utilize a three-electrode Si-LiNi 0.8 Mn 0.1 Co 0.1 O 2 pouch cell to deconvolute the Si impedance contributions. The evolution of the solid electrolyte interphase (SEI) and charge transfer resistances correlate to specific Li–Si alloy phases. We attribute this to the influence of Si particle volume expansion on SEI instabilities and a kinetic bottleneck at higher lithiation states.
- 28 July 2026
- Published by IOP Publishing in Journal of Physics: Energy
- Vol. 8 (3) , 035006
Open AccessExperimental considerations and applications for time-resolved impedance on silicon-anode battery systems
Dynamic electrochemical impedance spectroscopy (dEIS) utilizes a superimposed multi-sinusoidal waveform and enables temporally resolved investigations on various electrochemical processes; however, the signal-to-noise ratio must be maximized while retaining linearity and stationarity within the system. In the present work, we probe the impact of the waveform’s total amplitude as well as the waveform and phase profiles. The equal amplitude multi-sinusoidal waveform with 35 mV total amplitude (R CT ) associated with alloying kinetics dominates the overall impedance. R CT increases with state of charge indicating a kinetic bottleneck at higher lithiation states. To explore this further, we utilize a three-electrode Si-LiNi 0.8 Mn 0.1 Co 0.1 O 2 pouch cell to deconvolute the Si impedance contributions. The evolution of the solid electrolyte interphase (SEI) and charge transfer resistances correlate to specific Li–Si alloy phases. We attribute this to the influence of Si particle volume expansion on SEI instabilities and a kinetic bottleneck at higher lithiation states.
- Open Access
- 25 July 2026
- Published by American Chemical Society (ACS) in ACS Applied Energy Materials
- Vol. 9 (15) , 10036-10046
Electrode Modification by Laser Ablation to Overcome Mechanical and Scalability Limitations of Solid-State Prealkylation of Electrode Architectures
In this work, laser ablation of Si electrode surfaces is utilized to provide localized strain relief during the Solid State Prealkylation of Electrode Architectures (SPEAR) process, in addition to volumetric expansion relief in the form of free volume channels across the electrode. A hexagonal mesh patterning was employed via laser ablation, where the hexagonal diameter (pitch) was varied from 250 to 1000 µm. It was demonstrated that these channels serve as expansion voids, accommodating the increase in electrode thickness observed during SPEAR and preventing cracking at the electrode surface. Optical microscopy and Raman mapping confirm that Li diffusion is the rate-limiting solid-state process, requiring a 24 h rest period to achieve homogeneous LixSi alloying through the electrode bulk. Electrochemical evaluations in full cells show that a 1000 μm pitch pattern yields a high initial discharge capacity of 2485 mA h g–1 and 86.4% capacity retention after 80 cycles, whereas smaller pitches (<500 μm) result in lithium plating at 4.1 V in full cells paired with NMC 811 due to excessive current collector exposure from the ablation process. XPS analysis reveals that the laser treatment modifies the electrode surface by increasing the Si–O and C–O species, changing the SEI composition observed via an increase in fluorophosphates upon cycling.
- 25 July 2026
- Published by American Chemical Society (ACS) in ACS Applied Energy Materials
- Vol. 9 (15) , 10036-10046
Open AccessElectrode Modification by Laser Ablation to Overcome Mechanical and Scalability Limitations of Solid-State Prealkylation of Electrode Architectures
In this work, laser ablation of Si electrode surfaces is utilized to provide localized strain relief during the Solid State Prealkylation of Electrode Architectures (SPEAR) process, in addition to volumetric expansion relief in the form of free volume channels across the electrode. A hexagonal mesh patterning was employed via laser ablation, where the hexagonal diameter (pitch) was varied from 250 to 1000 µm. It was demonstrated that these channels serve as expansion voids, accommodating the increase in electrode thickness observed during SPEAR and preventing cracking at the electrode surface. Optical microscopy and Raman mapping confirm that Li diffusion is the rate-limiting solid-state process, requiring a 24 h rest period to achieve homogeneous LixSi alloying through the electrode bulk. Electrochemical evaluations in full cells show that a 1000 μm pitch pattern yields a high initial discharge capacity of 2485 mA h g–1 and 86.4% capacity retention after 80 cycles, whereas smaller pitches (<500 μm) result in lithium plating at 4.1 V in full cells paired with NMC 811 due to excessive current collector exposure from the ablation process. XPS analysis reveals that the laser treatment modifies the electrode surface by increasing the Si–O and C–O species, changing the SEI composition observed via an increase in fluorophosphates upon cycling.
- 7 November 2025
- Published by American Chemical Society (ACS) in Journal of the American Chemical Society
Revealing Solvent-Assisted Li + Transport in the Solid Electrolyte Interphase operando
The performance of energy-dense lithium metal batteries is critically influenced by the properties of the solid electrolyte interphase (SEI). Yet, progress in understanding this layer has been limited by the lack of accurate operando characterization because the SEI evolves dynamically during cycling. Here, we apply dynamic electrochemical impedance spectroscopy (dEIS) to resolve the real-time evolution of the SEI on lithium metal in ether-based electrolytes with varying degrees of fluorination. We find that faster stabilization of the compact SEI resistance correlates with improved passivation and higher Coulombic efficiency. Unexpectedly, compact SEI resistance correlates directly with Li+ solvation energy, revealing that weaker Li+ solvation increases not only bulk but also interphase resistance. These findings challenge the conventional view of the SEI as a purely solid-phase conductor and instead support a solvent-assisted Li+ transport mechanism within the compact SEI. This framework emphasizes the need to balance SEI ionic conductivity with the Li+ solvation environment to maximize lithium metal battery performance.
- 7 November 2025
- Published by American Chemical Society (ACS) in Journal of the American Chemical Society
Revealing Solvent-Assisted Li + Transport in the Solid Electrolyte Interphase operando
The performance of energy-dense lithium metal batteries is critically influenced by the properties of the solid electrolyte interphase (SEI). Yet, progress in understanding this layer has been limited by the lack of accurate operando characterization because the SEI evolves dynamically during cycling. Here, we apply dynamic electrochemical impedance spectroscopy (dEIS) to resolve the real-time evolution of the SEI on lithium metal in ether-based electrolytes with varying degrees of fluorination. We find that faster stabilization of the compact SEI resistance correlates with improved passivation and higher Coulombic efficiency. Unexpectedly, compact SEI resistance correlates directly with Li+ solvation energy, revealing that weaker Li+ solvation increases not only bulk but also interphase resistance. These findings challenge the conventional view of the SEI as a purely solid-phase conductor and instead support a solvent-assisted Li+ transport mechanism within the compact SEI. This framework emphasizes the need to balance SEI ionic conductivity with the Li+ solvation environment to maximize lithium metal battery performance.
- 22 October 2025
- Published by American Chemical Society (ACS) in ACS Applied Energy Materials
- Vol. 8 (21) , 16364-16375
Role of Salt Concentration on Interphase Dynamics and Chemistry of Silicon Anodes during Electrochemical Cycling
- 22 October 2025
- Published by American Chemical Society (ACS) in ACS Applied Energy Materials
- Vol. 8 (21) , 16364-16375
Role of Salt Concentration on Interphase Dynamics and Chemistry of Silicon Anodes during Electrochemical Cycling
- 17 July 2025
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 17 (30) , 43020-43033
Surprising Relationship between Silicon Anode Calendar Aging and Electrolyte Components in a Localized High-Concentration Electrolyte System
Although localized high-concentration electrolytes (LHCEs) have been shown to improve the calendar lifetime of silicon anodes, the roles of the electrolyte constituents in calendar aging are not well understood. Here, we utilize a voltage hold protocol and an LHCE with varying molar ratios of lithium bis(fluorosulfonyl)imide (LiFSI), tetramethylene sulfone (TMS), and 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) to probe the component roles during aging. Interestingly, the estimated calendar lifetime and irreversible lithium losses from the V-hold experiments are independent of the electrolyte formulations. Contrarily, the solid electrolyte interphase (SEI) composition depends on the electrolyte formulation. X-ray photoelectron spectroscopy shows that TMS-coordinated species decompose to form insoluble alkanes and lithium hydroxide (LiOH), while lithium fluoride (LiF) originates from the anion-coordination complex. The SEI composition does not appear to play a significant role in the silicon anode passivity, as measured by parasitic current, suggesting that the SEI-electrolyte interactions dictate the calendar aging mechanisms.
- 17 July 2025
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 17 (30) , 43020-43033
Surprising Relationship between Silicon Anode Calendar Aging and Electrolyte Components in a Localized High-Concentration Electrolyte System
Although localized high-concentration electrolytes (LHCEs) have been shown to improve the calendar lifetime of silicon anodes, the roles of the electrolyte constituents in calendar aging are not well understood. Here, we utilize a voltage hold protocol and an LHCE with varying molar ratios of lithium bis(fluorosulfonyl)imide (LiFSI), tetramethylene sulfone (TMS), and 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) to probe the component roles during aging. Interestingly, the estimated calendar lifetime and irreversible lithium losses from the V-hold experiments are independent of the electrolyte formulations. Contrarily, the solid electrolyte interphase (SEI) composition depends on the electrolyte formulation. X-ray photoelectron spectroscopy shows that TMS-coordinated species decompose to form insoluble alkanes and lithium hydroxide (LiOH), while lithium fluoride (LiF) originates from the anion-coordination complex. The SEI composition does not appear to play a significant role in the silicon anode passivity, as measured by parasitic current, suggesting that the SEI-electrolyte interactions dictate the calendar aging mechanisms.