Muti Feng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Muti Feng has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Hai Wang
School of Mathematics and Physics, China University of Geosciences, Wuhan 430079, PR China
2 shared publications - Hongxia Zhong
China University of Geosciences
2 shared publications Qingbo Wang
School of Mathematics and Physics, China University of Geosciences 1 , Wuhan 430074
2 shared publications- Yuzheng Guo
School of Power and Mechanical Engineering, Wuhan University, Wuhan, China
2 shared publications - Zi-Qiang Zhang
China University of Geosciences
2 shared publications Bo Xiang
School of Mathematics and Physics, China University of Geosciences 1 , Wuhan 430074
1 shared publication
Latest Publications
- Open Access
- 5 May 2026
- Published by AIP Publishing in APL Electronic Devices
- Vol. 2 (2)
Oxygen vacancies and carrier mobility at the a-ZrO2/Si(001) interface
Based on density-functional theory combined with molecular dynamics simulations, we systematically investigate the effects of oxygen vacancy defects on the electronic structure, interfacial charge transfer, and carrier transport properties of the amorphous ZrO2/Si (a-ZrO2/Si) interface. The band edges are dominated by the Si side, yielding band offsets exceeding 1 eV. Among six representative oxygen vacancies (three single and three double vacancies), double vacancies induce substantially stronger bandgap perturbations, with VO2 and VO12 introducing quasi-flat defect bands. While oxygen vacancies do not alter the overall direction of interfacial charge transfer, VO12 markedly enhances electron accumulation on the a-ZrO2 side. Notably, under both n-type and p-type conditions, the carrier mobility of the perfect interface is primarily limited by polar optical phonon scattering. Oxygen vacancies significantly degrade the mobility, whereas hydrogen passivation suppresses defect states and partially restores the mobility. In particular, at 300 K under n-type doping, the total mobility of VO2 and VO12 is below 8.5 cm2 V−1 s−1 and increases to 20.3–23.4 cm2 V−1 s−1 after passivation. These findings elucidate the microscopic mechanisms of oxygen vacancy and hydrogen passivation in regulating a-ZrO2/Si interface and provide atomic scale insights for high-k interface defect modulation.
- 5 May 2026
- Published by AIP Publishing in APL Electronic Devices
- Vol. 2 (2)
Open AccessOxygen vacancies and carrier mobility at the a-ZrO2/Si(001) interface
Based on density-functional theory combined with molecular dynamics simulations, we systematically investigate the effects of oxygen vacancy defects on the electronic structure, interfacial charge transfer, and carrier transport properties of the amorphous ZrO2/Si (a-ZrO2/Si) interface. The band edges are dominated by the Si side, yielding band offsets exceeding 1 eV. Among six representative oxygen vacancies (three single and three double vacancies), double vacancies induce substantially stronger bandgap perturbations, with VO2 and VO12 introducing quasi-flat defect bands. While oxygen vacancies do not alter the overall direction of interfacial charge transfer, VO12 markedly enhances electron accumulation on the a-ZrO2 side. Notably, under both n-type and p-type conditions, the carrier mobility of the perfect interface is primarily limited by polar optical phonon scattering. Oxygen vacancies significantly degrade the mobility, whereas hydrogen passivation suppresses defect states and partially restores the mobility. In particular, at 300 K under n-type doping, the total mobility of VO2 and VO12 is below 8.5 cm2 V−1 s−1 and increases to 20.3–23.4 cm2 V−1 s−1 after passivation. These findings elucidate the microscopic mechanisms of oxygen vacancy and hydrogen passivation in regulating a-ZrO2/Si interface and provide atomic scale insights for high-k interface defect modulation.
- 27 August 2025
- Published by IOP Publishing in Journal of Physics: Condensed Matter
- Vol. 37 (36)
Band offsets, charge transfers, and formation energies of oxygen vacancies inc-ZrO2/Si interface
Due to the high dielectric constant and wide band gap, ZrO2 has become a widely used gate dielectric material in complementary metal-oxide-semiconductor (CMOS) devices, and the ZrO2/Si interface plays a critical role in determining overall device performance. In this work, we systematically study the effects of oxygen vacancy defects on the band structure, band offset, and charge transfer in cubic ZrO2/Si (c-ZrO2/Si) interface structure. Our results reveal that the constructed (c-ZrO2)9/(Si)9 interface is an indirect band gap semiconductor, with the band edges contributed by Si and a band offset greater than 2 eV. The three oxygen vacancy defects reduce the band gap and induces quasi-flat band. The band offset is partially influenced by the location of oxygen vacancies, but the valence band offset (VBO) and conduction band offset (CBO) always exceed 1 eV. Notably, the VO1 and VO2 alter the bonding environment and charge transfer of adjacent Si atoms, whereas VO3 , located farther from the interface, preserves the native charge transfer characteristics of the (c-ZrO2)9/(Si)9 interface. The VO1 0 defect exhibits the lowest formation energy across all conditions, with the value in O-poor conditions being 6.992 eV lower than that in the O-rich environment. These findings suggest that the presence of oxygen vacancies may significantly affect the electrical and carrier properties of c-ZrO2/Si interface, providing theoretical insights into optimizing the design and fabrication of Si-based semiconductor devices.
- 27 August 2025
- Published by IOP Publishing in Journal of Physics: Condensed Matter
- Vol. 37 (36)
Band offsets, charge transfers, and formation energies of oxygen vacancies inc-ZrO2/Si interface
Due to the high dielectric constant and wide band gap, ZrO2 has become a widely used gate dielectric material in complementary metal-oxide-semiconductor (CMOS) devices, and the ZrO2/Si interface plays a critical role in determining overall device performance. In this work, we systematically study the effects of oxygen vacancy defects on the band structure, band offset, and charge transfer in cubic ZrO2/Si (c-ZrO2/Si) interface structure. Our results reveal that the constructed (c-ZrO2)9/(Si)9 interface is an indirect band gap semiconductor, with the band edges contributed by Si and a band offset greater than 2 eV. The three oxygen vacancy defects reduce the band gap and induces quasi-flat band. The band offset is partially influenced by the location of oxygen vacancies, but the valence band offset (VBO) and conduction band offset (CBO) always exceed 1 eV. Notably, the VO1 and VO2 alter the bonding environment and charge transfer of adjacent Si atoms, whereas VO3 , located farther from the interface, preserves the native charge transfer characteristics of the (c-ZrO2)9/(Si)9 interface. The VO1 0 defect exhibits the lowest formation energy across all conditions, with the value in O-poor conditions being 6.992 eV lower than that in the O-rich environment. These findings suggest that the presence of oxygen vacancies may significantly affect the electrical and carrier properties of c-ZrO2/Si interface, providing theoretical insights into optimizing the design and fabrication of Si-based semiconductor devices.