Jue Han
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Jue Han has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Hao Lian
School of Civil Engineering, Nanyang Institute of Technology, Nanyang 473004, China
1 shared publication Qianqian Ma
School of Civil Engineering, Nanyang Institute of Technology 1 , Nanyang 473004
1 shared publication- Qianqian Ma
School of Civil Engineering, Nanyang Institute of Technology, Nanyang 473004, China
1 shared publication - Xinke Xiao
School of Civil Engineering, Nanyang Institute of Technology, Nanyang 473004, China
1 shared publication - Yifan Kong
School of Civil Engineering, Nanyang Institute of Technology, Nanyang 473004, China
1 shared publication - Yubo Gao
Key Laboratory of Impact and Safety Engineering (MOE) Ningbo University Ningbo Zhejiang China
1 shared publication
Latest Publications
- Open Access
- 1 October 2026
- Published by AIP Publishing in AIP Advances
- Vol. 16 (10)
Stress-state redistribution and thickness-ratio dependence of ballistic resistance in ductile-front 2024-T351/7075-T651 bilayer targets under ogive-nosed projectile impact
Thin high-strength 7075-T651 aluminum plates are susceptible to radial cracking, petaling, and rear-face fragmentation under ogive-nosed projectile impact. This study investigates the influence of a ductile 2024-T351 front layer on the ballistic response and failure evolution of a thin 7075-T651 substrate. Ballistic experiments were conducted on 1.59-mm monolithic 7075-T651 targets and 2.4/1.59-mm 2024-T351/7075-T651 bilayer targets, and the results were combined with three-dimensional finite-element simulations employing material-specific constitutive and fracture models. The bilayer configuration exhibited an experimental ballistic-limit velocity of 184.8 m/s, compared with 102.4 m/s for the monolithic 7075-T651 target, corresponding to a configuration-level increase of 80.5%. At comparable normalized impact velocities, the selected failed elements in the 7075-T651 rear plate of the bilayer target exhibited a distribution shifted toward higher positive damage-averaged stress triaxiality compared with those in the monolithic target. This shift was accompanied by a more localized damaged region and petaling in the bilayer rear plate, linking the presence of the 2024-T351 front layer to changes in both stress-state histories and failure morphology. Buckingham π analysis and seven parametric simulations further established a dimensionally consistent semi-empirical relation between ballistic-limit velocity and front-to-rear thickness ratio, Vbl=153.7trR2=0.997, while the incremental ballistic benefit decreased with increasing tr. These results link ductile-front-induced stress-state redistribution with failure-mode evolution and provide a quantitative framework for thickness allocation in layered aluminum targets.
- 1 October 2026
- Published by AIP Publishing in AIP Advances
- Vol. 16 (10)
Open AccessStress-state redistribution and thickness-ratio dependence of ballistic resistance in ductile-front 2024-T351/7075-T651 bilayer targets under ogive-nosed projectile impact
Thin high-strength 7075-T651 aluminum plates are susceptible to radial cracking, petaling, and rear-face fragmentation under ogive-nosed projectile impact. This study investigates the influence of a ductile 2024-T351 front layer on the ballistic response and failure evolution of a thin 7075-T651 substrate. Ballistic experiments were conducted on 1.59-mm monolithic 7075-T651 targets and 2.4/1.59-mm 2024-T351/7075-T651 bilayer targets, and the results were combined with three-dimensional finite-element simulations employing material-specific constitutive and fracture models. The bilayer configuration exhibited an experimental ballistic-limit velocity of 184.8 m/s, compared with 102.4 m/s for the monolithic 7075-T651 target, corresponding to a configuration-level increase of 80.5%. At comparable normalized impact velocities, the selected failed elements in the 7075-T651 rear plate of the bilayer target exhibited a distribution shifted toward higher positive damage-averaged stress triaxiality compared with those in the monolithic target. This shift was accompanied by a more localized damaged region and petaling in the bilayer rear plate, linking the presence of the 2024-T351 front layer to changes in both stress-state histories and failure morphology. Buckingham π analysis and seven parametric simulations further established a dimensionally consistent semi-empirical relation between ballistic-limit velocity and front-to-rear thickness ratio, Vbl=153.7trR2=0.997, while the incremental ballistic benefit decreased with increasing tr. These results link ductile-front-induced stress-state redistribution with failure-mode evolution and provide a quantitative framework for thickness allocation in layered aluminum targets.
- Open Access
An Experimental and Numerical Investigation on Enhancing the Ballistic Resistance of 316L Stainless Steel Plates Against Blunt Projectiles by Covering with 2024-T351 Aluminum Alloy Thin Plates
To improve the ballistic resistance of hydrogen storage tank-grade 316L austenitic stainless steel (ASS) plates that are prone to shear plugging failure under blunt projectile impact, this study proposes a non-bonded bilayer protective configuration: covering the 316L ASS substrate with a thin front layer of 2024-T351 aluminum alloy (AA) plate. Ballistic impact tests were performed on monolithic 5 mm thick 316L ASS plates and bilayer targets composed of a 2.05 mm thick 2024-T351 AA plate and a 5 mm thick 316L ASS substrate (total thickness: 7.05 mm), using a single-stage light gas gun combined with high-speed photography. Parallel explicit dynamics models were established using ABAQUS/Explicit, incorporating a modified Johnson–Cook constitutive model and a Lode-dependent Modified Mohr–Coulomb (MMC) fracture criterion, thereby enabling rigorous mutual validation between experimental results and numerical simulations. Results demonstrate that the addition of a mere 2.05 mm thick aluminum alloy front layer significantly enhances the ballistic limit velocity (BLV) of the 5 mm thick 316L stainless steel target plate, increasing it from 167.5 m/s to 250.7 m/s. The enhancement mechanism is closely related to the transition in the failure mode from localized shear plugging to a combination of bulging, dishing, and plugging. This shift substantially improves the structure’s overall plastic deformation capacity and energy dissipation efficiency. This research provides an effective solution and establishes a reliable experimental–numerical benchmark for the lightweight, impact-resistant design of hydrogen storage tanks.
Open AccessAn Experimental and Numerical Investigation on Enhancing the Ballistic Resistance of 316L Stainless Steel Plates Against Blunt Projectiles by Covering with 2024-T351 Aluminum Alloy Thin Plates
To improve the ballistic resistance of hydrogen storage tank-grade 316L austenitic stainless steel (ASS) plates that are prone to shear plugging failure under blunt projectile impact, this study proposes a non-bonded bilayer protective configuration: covering the 316L ASS substrate with a thin front layer of 2024-T351 aluminum alloy (AA) plate. Ballistic impact tests were performed on monolithic 5 mm thick 316L ASS plates and bilayer targets composed of a 2.05 mm thick 2024-T351 AA plate and a 5 mm thick 316L ASS substrate (total thickness: 7.05 mm), using a single-stage light gas gun combined with high-speed photography. Parallel explicit dynamics models were established using ABAQUS/Explicit, incorporating a modified Johnson–Cook constitutive model and a Lode-dependent Modified Mohr–Coulomb (MMC) fracture criterion, thereby enabling rigorous mutual validation between experimental results and numerical simulations. Results demonstrate that the addition of a mere 2.05 mm thick aluminum alloy front layer significantly enhances the ballistic limit velocity (BLV) of the 5 mm thick 316L stainless steel target plate, increasing it from 167.5 m/s to 250.7 m/s. The enhancement mechanism is closely related to the transition in the failure mode from localized shear plugging to a combination of bulging, dishing, and plugging. This shift substantially improves the structure’s overall plastic deformation capacity and energy dissipation efficiency. This research provides an effective solution and establishes a reliable experimental–numerical benchmark for the lightweight, impact-resistant design of hydrogen storage tanks.