Pavel Potapov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Pavel Potapov has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Alexey Vereschaka
Institute of Design and Technological Informatics of the Russian Academy of Sciences (IDTI RAS), Vadkovsky per. 18-1a, Moscow 127994, Russia
3 shared publications - Catherine Sotova
Department of High-Efficiency Machining Technologies, Moscow State Technological University «STANKIN», Vadkovsky per. 1, Moscow 127994, Russia
3 shared publications - Filipp O. Milovich
Materials Science and Metallurgy Shared Use Research and Development Center, National University of Science and Technology “MISiS”, Leninsky Prospect 4, Moscow 119049, Russia
3 shared publications - Sergey Nikolaevich Grigoriev
Moscow State University of Technology "STANKIN
3 shared publications - Anton Seleznev
Department of High-Efficiency Machining Technologies, Moscow State University of Technology “STANKIN”, Vadkovsky Lane 3a, 127055 Moscow, Russia
2 shared publications - Kirill Makarevich
Federal State Budget Educational Institution of Higher Education, MIREA—Russian Technological University, 119454 Moscow, Russia
2 shared publications
Latest Publications
- Open Access
- 20 September 2026
- Published by MDPI AG in Technologies
- Vol. 14 (9) , 594
Improving the Performance Properties of Stainless Steel Products by Depositing Modifying Coatings Containing Layers of Copper, Chromium and Zirconium
This article presents the potential for enhancing the corrosion resistance of stainless steel components by depositing modifying coatings containing copper, chromium, and zirconium layers on their surfaces while optimising the deposition process parameters. Coatings with an outer zirconium nitride (ZrN) or chromium nitride (CrN) layer and adhesive-corrosion-resistant Zr–Cu–Zr, Cr–Cu–Cr, and Cu–Zr sublayers were studied. The highest deposition rate of the copper layer was achieved with a copper cathode arc current of Icat = 85 A and a substrate bias voltage of Usub = 100 V. The proposed coatings reduced corrosion intensity by up to 30 times compared to an uncoated sample and up to three times compared to coatings with an adhesive sublayer without copper (zirconium or chromium only). The use of the proposed coatings reduced corrosion intensity by up to 15 times compared to an uncoated sample and up to 1.6 times compared to coatings with an adhesive layer without copper (chromium only). The Cr–Cu–Cr–CrN coating provided the best corrosion resistance in a 3.0% NaCl solution with a calculated corrosion current icor of 0.36 μA/cm2. These results indicate that the inclusion of a copper layer in the adhesive sublayer provides additional corrosion protection. The sample with a Cr–Cu–Cr–CrN coating exhibited better corrosion resistance, but its adhesive bond to the substrate was not very strong. The sample with a Zr–Cu–Zr–ZrN coating demonstrated high adhesive strength with relatively high corrosion resistance.
- 20 September 2026
- Published by MDPI AG in Technologies
- Vol. 14 (9) , 594
Open AccessImproving the Performance Properties of Stainless Steel Products by Depositing Modifying Coatings Containing Layers of Copper, Chromium and Zirconium
This article presents the potential for enhancing the corrosion resistance of stainless steel components by depositing modifying coatings containing copper, chromium, and zirconium layers on their surfaces while optimising the deposition process parameters. Coatings with an outer zirconium nitride (ZrN) or chromium nitride (CrN) layer and adhesive-corrosion-resistant Zr–Cu–Zr, Cr–Cu–Cr, and Cu–Zr sublayers were studied. The highest deposition rate of the copper layer was achieved with a copper cathode arc current of Icat = 85 A and a substrate bias voltage of Usub = 100 V. The proposed coatings reduced corrosion intensity by up to 30 times compared to an uncoated sample and up to three times compared to coatings with an adhesive sublayer without copper (zirconium or chromium only). The use of the proposed coatings reduced corrosion intensity by up to 15 times compared to an uncoated sample and up to 1.6 times compared to coatings with an adhesive layer without copper (chromium only). The Cr–Cu–Cr–CrN coating provided the best corrosion resistance in a 3.0% NaCl solution with a calculated corrosion current icor of 0.36 μA/cm2. These results indicate that the inclusion of a copper layer in the adhesive sublayer provides additional corrosion protection. The sample with a Cr–Cu–Cr–CrN coating exhibited better corrosion resistance, but its adhesive bond to the substrate was not very strong. The sample with a Zr–Cu–Zr–ZrN coating demonstrated high adhesive strength with relatively high corrosion resistance.
- Open Access
- 15 September 2025
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 9 (9) , 316
Increasing the Wear Resistance of Stainless Steel Products by Depositing Modifying Coatings Based on Zirconium Nitride with the Addition of Niobium, Hafnium, and Titanium
To increase wear resistance, (Zr,Nb)N, ZrN and (Zr,Hf)N coatings with columnar structures and (Zr,Ti)N and (Zr,Nb,Hf)N coatings with nanolayer structures were deposited on an AISI 321 stainless steel substrate. The samples with (Zr,Nb)N and ZrN coatings exhibited the best resistance to failure in the scratch test. The sample with the (Zr,Nb)N coating had the best wear resistance for the first 16,000 s. However, eventually the wear of this sample became notable, and after 20,000 s of testing, the lowest degree of wear was observed in the sample with the (Zr,Nb,Hf)N coating. The wear rate of the uncoated sample was 1.5 times greater than that of the sample with the (Zr,Nb,Hf)N coating. The (Zr,Nb,Hf)N coating also exhibited a low degree of indenter mass loss. The (Zr,Nb,Hf)N and ZrN coatings reduced the coefficient of friction (COF) most (COF of approximately 0.20–0.21, compared to COF = 0.28 for the uncoated sample). Defects (nanocavities) were detected in the interface area between the coatings and the substrate, which in some cases can have a negative effect on the wear resistance of the coating. The (Zr,Nb,Hf)N coating (72.07 at.% Zr, 24.87 at.% Nb and 3.05 at.% Hf) had the best wear resistance and a low friction coefficient.
- 15 September 2025
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 9 (9) , 316
Open AccessIncreasing the Wear Resistance of Stainless Steel Products by Depositing Modifying Coatings Based on Zirconium Nitride with the Addition of Niobium, Hafnium, and Titanium
To increase wear resistance, (Zr,Nb)N, ZrN and (Zr,Hf)N coatings with columnar structures and (Zr,Ti)N and (Zr,Nb,Hf)N coatings with nanolayer structures were deposited on an AISI 321 stainless steel substrate. The samples with (Zr,Nb)N and ZrN coatings exhibited the best resistance to failure in the scratch test. The sample with the (Zr,Nb)N coating had the best wear resistance for the first 16,000 s. However, eventually the wear of this sample became notable, and after 20,000 s of testing, the lowest degree of wear was observed in the sample with the (Zr,Nb,Hf)N coating. The wear rate of the uncoated sample was 1.5 times greater than that of the sample with the (Zr,Nb,Hf)N coating. The (Zr,Nb,Hf)N coating also exhibited a low degree of indenter mass loss. The (Zr,Nb,Hf)N and ZrN coatings reduced the coefficient of friction (COF) most (COF of approximately 0.20–0.21, compared to COF = 0.28 for the uncoated sample). Defects (nanocavities) were detected in the interface area between the coatings and the substrate, which in some cases can have a negative effect on the wear resistance of the coating. The (Zr,Nb,Hf)N coating (72.07 at.% Zr, 24.87 at.% Nb and 3.05 at.% Hf) had the best wear resistance and a low friction coefficient.
- Open Access
- 13 September 2025
- Published by MDPI AG in Journal of Composites Science
- Vol. 9 (9) , 498
Increasing the Corrosion Resistance of Austenitic Stainless Steel Products by Depositing Vanadium Nitride-Based Coatings on Their Surface
This study investigated the anticorrosive properties of nitride coatings (V,Zr,Nb)N, VN and (Zr,V)N with a thickness of approximately 3 μm, deposited on a substrate of AISI 321 steel. Experiments were conducted in 3.0 and 0.9% aqueous NaCl solutions. The results indicate that the use of (V,Zr,Nb)N, VN and (Zr,V)N coatings to protect AISI 321 steel in corrosive environments (e.g., chloride-containing solutions) allowed corrosion currents to be reduced by 10–20 times (from 7.0 to 0.29 μA/cm2) for a sample with a (Zr,V)N coating in a 3.0% aqueous NaCl solution, and by 2 times (from 0.36 to 0.18 μA/cm2) for a sample with a (V,Zr,Nb)N coating in a 0.9% aqueous NaCl solution. Based on the distribution of elements on the surface of the samples after holding for 168 h in a 3.0% aqueous NaCl solution at 25 °C, it can be qualitatively concluded that the oxidation intensity of the (Zr,V)N coating was the lowest under this condition, and that the VN coating exhibited the highest oxidation intensity among the considered coatings. Analysis of the structure of the (Zr,V)N coating after holding in a 3.0% aqueous NaCl solution for 168 h at 25 °C shows the presence of nanometre-sized chips, while the analysis of the distribution of elements does not record the presence of anything other than the elements comprising the coating. Based on the distribution of elements on the surface of the VN coating, it can be assumed that the destruction of this coating mainly occurs due to peeling off from the substrate; however, corrosion processes also occur in the VN coating itself. Analysis of the distribution of elements in the surface layers of the (V,Zr,Nb)N coating did not show noticeable signs of oxidation. The destruction of this coating occurs due to fragments peeling off from the substrate, while oxidation processes and substrate corrosion do not have a significant effect on the process of (V,Zr,Nb)N coating destruction.
- 13 September 2025
- Published by MDPI AG in Journal of Composites Science
- Vol. 9 (9) , 498
Open AccessIncreasing the Corrosion Resistance of Austenitic Stainless Steel Products by Depositing Vanadium Nitride-Based Coatings on Their Surface
This study investigated the anticorrosive properties of nitride coatings (V,Zr,Nb)N, VN and (Zr,V)N with a thickness of approximately 3 μm, deposited on a substrate of AISI 321 steel. Experiments were conducted in 3.0 and 0.9% aqueous NaCl solutions. The results indicate that the use of (V,Zr,Nb)N, VN and (Zr,V)N coatings to protect AISI 321 steel in corrosive environments (e.g., chloride-containing solutions) allowed corrosion currents to be reduced by 10–20 times (from 7.0 to 0.29 μA/cm2) for a sample with a (Zr,V)N coating in a 3.0% aqueous NaCl solution, and by 2 times (from 0.36 to 0.18 μA/cm2) for a sample with a (V,Zr,Nb)N coating in a 0.9% aqueous NaCl solution. Based on the distribution of elements on the surface of the samples after holding for 168 h in a 3.0% aqueous NaCl solution at 25 °C, it can be qualitatively concluded that the oxidation intensity of the (Zr,V)N coating was the lowest under this condition, and that the VN coating exhibited the highest oxidation intensity among the considered coatings. Analysis of the structure of the (Zr,V)N coating after holding in a 3.0% aqueous NaCl solution for 168 h at 25 °C shows the presence of nanometre-sized chips, while the analysis of the distribution of elements does not record the presence of anything other than the elements comprising the coating. Based on the distribution of elements on the surface of the VN coating, it can be assumed that the destruction of this coating mainly occurs due to peeling off from the substrate; however, corrosion processes also occur in the VN coating itself. Analysis of the distribution of elements in the surface layers of the (V,Zr,Nb)N coating did not show noticeable signs of oxidation. The destruction of this coating occurs due to fragments peeling off from the substrate, while oxidation processes and substrate corrosion do not have a significant effect on the process of (V,Zr,Nb)N coating destruction.