Yanqi Ran
Yanqi Ran has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Xinze Li
School of Engineering, China University of Petroleum (Beijing) at Karamay, Karamay 834000, China
2 shared publications - Dezhong Wang
School of Engineering, China University of Petroleum (Beijing) at Karamay, Karamay 834000, China
1 shared publication - Fengming Li
School of Engineering, China University of Petroleum (Beijing) at Karamay, Karamay 834000, China
1 shared publication - Jiajia Chen
School of Arts and Sciences, China University of Petroleum (Beijing) at Karamay, Karamay 834000, China
1 shared publication - Ting Mao
Research Institute of Natural Gas Technology, PetroChina Southwest Oil and Gasfield Company, Chengdu 610213, China
1 shared publication - Zhiming Yu
Research Institute of Natural Gas Technology, PetroChina Southwest Oil and Gas Field Company, Chengdu 610213, China
1 shared publication
Latest Publications
- Open Access
Study on Sulfide Stress Corrosion Cracking Susceptibility of 20# Steel Weld Joints in H2S-Rich Environments
This study aims to clarify the influence of H2S concentration and temperature on the sulfide stress corrosion cracking (SSCC) susceptibility of 20# steel weld joints. 20# steel is a commonly selected pipe material for ground gas pipelines, and there is a risk of welds cracking after years of service. The selection of a corrosive environment is based on the working conditions of high-sulfur oil fields on site. Slow strain rate tensile (SSRT) tests were conducted under simulated high-sulfur gathering and transportation conditions across varying temperatures and H2S concentrations. The mechanical properties, SSCC susceptibility, fracture morphology, and elemental composition of fracture surfaces were systematically analyzed. As H2S concentration increased (5%, 7.5%, 10%) and temperature decreased (30–60 °C), the elongation after fracture and the reduction in area of 20# steel decreased, while the yield strength and SSCC susceptibility increased. The H2S concentration range of 0–5% represented a critical sensitivity interval for the material, where elongation after fracture decreased by up to 74%. Within the 5–10% H2S range, elongation decreased by only 2.11%, indicating a slowing trend of fracture toughness deterioration, though SSCC susceptibility still increased by 12%. Increasing the temperature from 30 °C to 60 °C reduced SSCC susceptibility by approximately 30%, confirming higher susceptibility at lower temperatures. Temperature exerts a lesser influence on material performance than H2S concentration. Also, 20# steel remains within the SSCC brittle fracture sensitivity zone in sulfur-containing environments, necessitating strict quality control to avoid defects and stress concentrations. In high-sulfur environments (H2S > 5%), further increases in H2S concentration have a diminished effect on cracking susceptibility.
Open AccessStudy on Sulfide Stress Corrosion Cracking Susceptibility of 20# Steel Weld Joints in H2S-Rich Environments
This study aims to clarify the influence of H2S concentration and temperature on the sulfide stress corrosion cracking (SSCC) susceptibility of 20# steel weld joints. 20# steel is a commonly selected pipe material for ground gas pipelines, and there is a risk of welds cracking after years of service. The selection of a corrosive environment is based on the working conditions of high-sulfur oil fields on site. Slow strain rate tensile (SSRT) tests were conducted under simulated high-sulfur gathering and transportation conditions across varying temperatures and H2S concentrations. The mechanical properties, SSCC susceptibility, fracture morphology, and elemental composition of fracture surfaces were systematically analyzed. As H2S concentration increased (5%, 7.5%, 10%) and temperature decreased (30–60 °C), the elongation after fracture and the reduction in area of 20# steel decreased, while the yield strength and SSCC susceptibility increased. The H2S concentration range of 0–5% represented a critical sensitivity interval for the material, where elongation after fracture decreased by up to 74%. Within the 5–10% H2S range, elongation decreased by only 2.11%, indicating a slowing trend of fracture toughness deterioration, though SSCC susceptibility still increased by 12%. Increasing the temperature from 30 °C to 60 °C reduced SSCC susceptibility by approximately 30%, confirming higher susceptibility at lower temperatures. Temperature exerts a lesser influence on material performance than H2S concentration. Also, 20# steel remains within the SSCC brittle fracture sensitivity zone in sulfur-containing environments, necessitating strict quality control to avoid defects and stress concentrations. In high-sulfur environments (H2S > 5%), further increases in H2S concentration have a diminished effect on cracking susceptibility.
- Open Access
Research on Carbon Dioxide Pipeline Leakage Localization Based on Gaussian Plume Model
Carbon dioxide (CO2) is a non-toxic asphyxiant gas that, once released, can pose severe risks, including suffocation, poisoning, frostbite, and even death. As a critical component of carbon capture, utilization, and storage (CCUS) technology, CO2 pipeline transportation requires reliable leakage detection and precise localization to safeguard the environment, ensure pipeline operational safety, and support emergency response strategies. This study proposes an inversion model that integrates wireless sensor networks (WSNs) with the Gaussian plume model for CO2 pipeline leakage monitoring. The WSN is employed to collect real-time CO2 concentration data and environmental parameters around the pipeline, while the Gaussian plume model is used to simulate and invert the dispersion process, enabling both leak source localization and emission rate estimation. Simulation results demonstrate that the proposed model achieves a source localization error of 12.5% and an emission rate error of 3.5%. Field experiments further confirm the model’s applicability, with predicted concentrations closely matching the measurements, yielding an error range of 3.5–14.7%. These findings indicate that the model satisfies engineering accuracy requirements and provides a technical foundation for emergency response following CO2 pipeline leakage.
Open AccessResearch on Carbon Dioxide Pipeline Leakage Localization Based on Gaussian Plume Model
Carbon dioxide (CO2) is a non-toxic asphyxiant gas that, once released, can pose severe risks, including suffocation, poisoning, frostbite, and even death. As a critical component of carbon capture, utilization, and storage (CCUS) technology, CO2 pipeline transportation requires reliable leakage detection and precise localization to safeguard the environment, ensure pipeline operational safety, and support emergency response strategies. This study proposes an inversion model that integrates wireless sensor networks (WSNs) with the Gaussian plume model for CO2 pipeline leakage monitoring. The WSN is employed to collect real-time CO2 concentration data and environmental parameters around the pipeline, while the Gaussian plume model is used to simulate and invert the dispersion process, enabling both leak source localization and emission rate estimation. Simulation results demonstrate that the proposed model achieves a source localization error of 12.5% and an emission rate error of 3.5%. Field experiments further confirm the model’s applicability, with predicted concentrations closely matching the measurements, yielding an error range of 3.5–14.7%. These findings indicate that the model satisfies engineering accuracy requirements and provides a technical foundation for emergency response following CO2 pipeline leakage.