Roza Latifi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Roza Latifi has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
Abderraouf Boucherif
2 shared publicationsDenis Machon
1 shared publication- Denis Machon
Institut Interdisciplinaire d'Innovation Technologique (3IT), Université de Sherbrooke, 3000 Boulevard de l'Université, Sherbrooke, J1K 0AE Québec, Canada
1 shared publication Lionel Roué
Institut National de la Recherche Scientifique – Centre Énergie Matériaux Télécommunications (INRS‐EMT) 1650 boulevard Lionel Boulet Varennes QC J3X 1P7 Canada
1 shared publicationSamuel Quéméré
Institut National de la Recherche Scientifique – Centre Énergie Matériaux Télécommunications (INRS‐EMT) 1650 boulevard Lionel Boulet Varennes QC J3X 1P7 Canada
1 shared publication
Latest Publications
- Open Access
- 11 April 2026
- Published by Elsevier in SSRN Electronic Journal
Thermally Driven Surface Densification Optimizes Porous Silicon for High-Performance On-Chip Microbatteries
Engineering high-performance microbattery anodes requires architectures that combine high areal capacity, fast ion transport, long-term interfacial stability, and full compatibility with microelectronics fabrication processes. Here, we uncover how rapid thermal annealing (RTA) governs the hierarchical reconstruction of electrochemically etched mesoporous silicon and, in turn, its electrochemical behavior. By tracking the coupled densification–coarsening mechanisms activated between 800–1000 °C, we reveal a nonmonotonic structural evolution in which an optimal- annealing temperature (900 °C) produces a ∼700 nm dense surface layer atop a porous network. This morphology minimizes electrolyte-accessible surface area while preserving efficient Li+ transport, suppressing early solid electrolyte interphase formation and enabling a balanced capacitive–diffusive storage regime. The resulting monolithic anode delivers ≈9 mAh cm−2 at 6 mA cm−2 for 100 cycles, withstands ~500 cycles at high rate, and reaches 20 mAh cm−2 with thicker layers. These performances rank among the highest reported for on-chip silicon microbatteries. By establishing surface densification as a mechanistic design principle linking microstructure, interfacial stability, and transport kinetics, this work positions porous silicon as a scalable platform for high-energy, high-power microscale storage with potential relevance to advanced microelectronics fabrication.
- 11 April 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessThermally Driven Surface Densification Optimizes Porous Silicon for High-Performance On-Chip Microbatteries
Engineering high-performance microbattery anodes requires architectures that combine high areal capacity, fast ion transport, long-term interfacial stability, and full compatibility with microelectronics fabrication processes. Here, we uncover how rapid thermal annealing (RTA) governs the hierarchical reconstruction of electrochemically etched mesoporous silicon and, in turn, its electrochemical behavior. By tracking the coupled densification–coarsening mechanisms activated between 800–1000 °C, we reveal a nonmonotonic structural evolution in which an optimal- annealing temperature (900 °C) produces a ∼700 nm dense surface layer atop a porous network. This morphology minimizes electrolyte-accessible surface area while preserving efficient Li+ transport, suppressing early solid electrolyte interphase formation and enabling a balanced capacitive–diffusive storage regime. The resulting monolithic anode delivers ≈9 mAh cm−2 at 6 mA cm−2 for 100 cycles, withstands ~500 cycles at high rate, and reaches 20 mAh cm−2 with thicker layers. These performances rank among the highest reported for on-chip silicon microbatteries. By establishing surface densification as a mechanistic design principle linking microstructure, interfacial stability, and transport kinetics, this work positions porous silicon as a scalable platform for high-energy, high-power microscale storage with potential relevance to advanced microelectronics fabrication.
- Open Access
- 2 October 2025
- Published by Wiley in Energy Technology
- Vol. 14 (1)
Mesoporous Silicon with Capacity‐Limited Lithiation: A Strategy for Stable High‐Capacity Lithium‐Ion Anodes
While silicon anodes offer a high theoretical capacity for lithium‐ion batteries, they face challenges related to severe volume expansion and mechanical degradation. Herein, mesoporous structuring is systematically coupled with capacity‐limited (partial) lithiation to improve the durability of high‐Si composite anodes (70% Si). Using galvanostatic cycling and ex situ scanning electron microscopy/thickness measurements on bulk‐Si and mesoporous‐Si (PSi) electrodes at four lithiation depths (100%, 66%, 50%, 33%), it is shown that PSi consistently delivers higher capacity retention over 100 cycles and exhibits markedly lower swelling. At 33% lithiation, PSi retains ≈94% of its initial capacity, outperforming bulk Si, and expands ≈141% compared to 315% for bulk Si under the same cycling conditions. These benefits result from the porous framework's ability to accommodate the volume changes and stabilize the solid electrolyte interface (SEI), reducing the risk of fracture and electrical connectivity loss. These findings contribute to the ongoing research on mesoporous silicon materials and support a higher Si fraction in graphite‐containing anodes, delivering greater energy density with maintained SEI stability and low swelling.
- 2 October 2025
- Published by Wiley in Energy Technology
- Vol. 14 (1)
Open AccessMesoporous Silicon with Capacity‐Limited Lithiation: A Strategy for Stable High‐Capacity Lithium‐Ion Anodes
While silicon anodes offer a high theoretical capacity for lithium‐ion batteries, they face challenges related to severe volume expansion and mechanical degradation. Herein, mesoporous structuring is systematically coupled with capacity‐limited (partial) lithiation to improve the durability of high‐Si composite anodes (70% Si). Using galvanostatic cycling and ex situ scanning electron microscopy/thickness measurements on bulk‐Si and mesoporous‐Si (PSi) electrodes at four lithiation depths (100%, 66%, 50%, 33%), it is shown that PSi consistently delivers higher capacity retention over 100 cycles and exhibits markedly lower swelling. At 33% lithiation, PSi retains ≈94% of its initial capacity, outperforming bulk Si, and expands ≈141% compared to 315% for bulk Si under the same cycling conditions. These benefits result from the porous framework's ability to accommodate the volume changes and stabilize the solid electrolyte interface (SEI), reducing the risk of fracture and electrical connectivity loss. These findings contribute to the ongoing research on mesoporous silicon materials and support a higher Si fraction in graphite‐containing anodes, delivering greater energy density with maintained SEI stability and low swelling.