Xiaotong Zhang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Xiaotong Zhang has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Shifeng Liu
School of Metallurgical Engineering, Xi’an University of Architecture and Technology, Xi’an 710055, China
1 shared publication - Shihao Zhang
School of Metallurgical Engineering, Xi’an University of Architecture and Technology, Xi’an 710055, China
1 shared publication - Xin Chu
National Engineering Laboratory for Modern Materials Surface Engineering Technology, Institute of New Materials, Guangdong Academy of Sciences, Guangzhou, China
1 shared publication - Yaojia Ren
School of Metallurgical Engineering, Xi’an University of Architecture and Technology, Xi’an 710055, China
1 shared publication - Yingkang Wei
School of Metallurgical Engineering, Xi’an University of Architecture and Technology, Xi’an 710055, China
1 shared publication - Yufeng Zhang
School of Metallurgical Engineering, Xi’an University of Architecture and Technology, Xi’an 710055, China
1 shared publication
Latest Publications
- Open Access
Heterogeneous Distribution of Microstructure and Mechanical Properties in M2 High-Speed Steel Fabricated by Laser Powder Bed Fusion
In this study, crack-free M2 high-speed steel (HSS) was successfully fabricated by laser powder bed fusion (L-PBF) using a relatively high substrate preheating temperature of 260 °C. The influence of the resulting microstructure on the hardness and tensile properties along the build direction was thoroughly investigated. The results demonstrate that M2 HSS achieves a relative density of 99.6% when processed with a laser power of 280 W and a scanning speed of 0.8 m s−1. The microstructure predominantly consists of fine martensite, along with retained austenite, lower bainite, and a small quantity of eutectic carbide. With increasing build height (from 0 to 9 mm), the fraction of lower bainite decreases from 32.1 to 13.1%, while the austenite content increases from 0.9 to 29.1%. These microstructural changes lead to a gradual reduction in the material’s strength along the build direction. Specifically, the hardness and tensile strength decrease from 845 HV0.3 and 1520 MPa to 745 HV0.3 and 1251 MPa, respectively. Additionally, the elongation varies between 2.6% and 3.3% across the different build heights.
Open AccessHeterogeneous Distribution of Microstructure and Mechanical Properties in M2 High-Speed Steel Fabricated by Laser Powder Bed Fusion
In this study, crack-free M2 high-speed steel (HSS) was successfully fabricated by laser powder bed fusion (L-PBF) using a relatively high substrate preheating temperature of 260 °C. The influence of the resulting microstructure on the hardness and tensile properties along the build direction was thoroughly investigated. The results demonstrate that M2 HSS achieves a relative density of 99.6% when processed with a laser power of 280 W and a scanning speed of 0.8 m s−1. The microstructure predominantly consists of fine martensite, along with retained austenite, lower bainite, and a small quantity of eutectic carbide. With increasing build height (from 0 to 9 mm), the fraction of lower bainite decreases from 32.1 to 13.1%, while the austenite content increases from 0.9 to 29.1%. These microstructural changes lead to a gradual reduction in the material’s strength along the build direction. Specifically, the hardness and tensile strength decrease from 845 HV0.3 and 1520 MPa to 745 HV0.3 and 1251 MPa, respectively. Additionally, the elongation varies between 2.6% and 3.3% across the different build heights.