Roland Ten Klooster
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Interests
Roland Ten Klooster has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
Cristina Ortiz Avila
Department of Design, Production and Management, Faculty of Engineering Technology University of Twente Enschede The Netherlands
1 shared publication- Daniel Sean Bezzina
Department of Design, Production and Management, Faculty of Engineering Technology University of Twente Enschede The Netherlands
1 shared publication - Ilknur Ilhan
Faculty of Engineering Technology, Department of Design Production and Management, Packaging Design and Management Chair University of Twente Enschede The Netherlands
1 shared publication - Max Vanhouttem
Brightlands Materials Center Geleen The Netherlands
1 shared publication - Mieke van Den Berg
The LCA Centre Beuningen the Netherlands
1 shared publication - Niek Knoben
Brightlands Materials Center Geleen The Netherlands
1 shared publication
Latest Publications
- Open Access
- 25 July 2026
- Published by Wiley in Packaging Technology and Science
- Vol. 39 (12) , 1501-1516
Effect of Antioxidants and Compatibilizers on Gel Formation and Film Quality of Polyethylene Films With Recycled Content
Adding recycled content is paramount for achieving circular packaging. However, packaging films produced from postindustry or postconsumer recycled polyethylene (PCR PE) have been reported to have various visual and mechanical issues related to impurities and degradation, which affect their performance. This paper studies the gel presence and seal characteristics of packaging films produced from 100% monolayer PCR PE with the addition of antioxidants and compatibilizers. It additionally evaluates the performance of commercially produced multilayer PE films that contain 30% and 50% PCR PE in the core layers and virgin sealant and top layers, checking the quality variations that arise from the difference in PCR PE batches. In the research, the presence and surface area ratio of gels related to recycled content are analyzed using FTIR, microscopy and a newly introduced image analysis method; seal performance is measured via hot‐tack and cold‐tack tests, and material performance is evaluated via tensile testing. According FTIR findings, some spherical and fibre like impurities coming from PCR PE were found to be polyamide or cellulose based, respectively. In nonfood contact commercial films with PCR PE content, the quality varied largely from batch to batch as well as the hot and cold seal strength. In 100% PCR PE films produced in laboratory settings, adding antioxidants during film production did not significantly influence the gel presence while one of the maleic anhydride‐based (MAH) compatibilizers used in the research reduced both the gel number (from 432 to 375 pcs/9 cm 2 ) and gel area ratio (from 0.81% to 0.67%). On the other hand, both types of additives delayed the breakage failure providing a larger operation window in hot‐tack tests. During the cold‐tack test, stronger attachment at the seal interphase is observed at 100°C sealing temperature in samples with added compatibilizer. Finally, according to tensile test results, the Young's modulus and the elongation at break only showed slight changes with the addition of antioxidants and compatibilizers. The results can be used for guidelines for design from recycling working with PE films.
- 25 July 2026
- Published by Wiley in Packaging Technology and Science
- Vol. 39 (12) , 1501-1516
Open AccessEffect of Antioxidants and Compatibilizers on Gel Formation and Film Quality of Polyethylene Films With Recycled Content
Adding recycled content is paramount for achieving circular packaging. However, packaging films produced from postindustry or postconsumer recycled polyethylene (PCR PE) have been reported to have various visual and mechanical issues related to impurities and degradation, which affect their performance. This paper studies the gel presence and seal characteristics of packaging films produced from 100% monolayer PCR PE with the addition of antioxidants and compatibilizers. It additionally evaluates the performance of commercially produced multilayer PE films that contain 30% and 50% PCR PE in the core layers and virgin sealant and top layers, checking the quality variations that arise from the difference in PCR PE batches. In the research, the presence and surface area ratio of gels related to recycled content are analyzed using FTIR, microscopy and a newly introduced image analysis method; seal performance is measured via hot‐tack and cold‐tack tests, and material performance is evaluated via tensile testing. According FTIR findings, some spherical and fibre like impurities coming from PCR PE were found to be polyamide or cellulose based, respectively. In nonfood contact commercial films with PCR PE content, the quality varied largely from batch to batch as well as the hot and cold seal strength. In 100% PCR PE films produced in laboratory settings, adding antioxidants during film production did not significantly influence the gel presence while one of the maleic anhydride‐based (MAH) compatibilizers used in the research reduced both the gel number (from 432 to 375 pcs/9 cm 2 ) and gel area ratio (from 0.81% to 0.67%). On the other hand, both types of additives delayed the breakage failure providing a larger operation window in hot‐tack tests. During the cold‐tack test, stronger attachment at the seal interphase is observed at 100°C sealing temperature in samples with added compatibilizer. Finally, according to tensile test results, the Young's modulus and the elongation at break only showed slight changes with the addition of antioxidants and compatibilizers. The results can be used for guidelines for design from recycling working with PE films.
- Open Access
- 20 October 2025
- Published by Wiley in Packaging Technology and Science
- Vol. 39 (2) , 137-159
Steps Towards a Template for Fair Comparisons Between Single‐Use and Reusable Items
In this paper, the factors taken up in LCA studies comparing single‐use to reuse are evaluated. Based on literature research, the insight was obtained that there are many single‐use vs. reuse comparisons that do not take into account the full picture of a reuse system. These factors are defined and further explored using single‐use/reuse system comparison case studies. A method to calculate the impact of reuse systems and to compare it to single‐use systems is presented in terms of equations based on the case studies. The equations are used to show the relevance of taking up specific parameters using different input values. Significance is shown for the following factors: Single‐use components in a reuse system Constant factors in a reuse system Pool size compared to system size in a reuse system Loss percentage With this method, several factors are taken up outside of LCA software in order to determine a break‐even point or to understand the trajectory of the system impact over rotations. Together with inventory reporting according to ISO 14040/14044 this can be the basis for transparent reuse system impact calculations and its fair comparison to single‐use system impact.
- 20 October 2025
- Published by Wiley in Packaging Technology and Science
- Vol. 39 (2) , 137-159
Open AccessSteps Towards a Template for Fair Comparisons Between Single‐Use and Reusable Items
In this paper, the factors taken up in LCA studies comparing single‐use to reuse are evaluated. Based on literature research, the insight was obtained that there are many single‐use vs. reuse comparisons that do not take into account the full picture of a reuse system. These factors are defined and further explored using single‐use/reuse system comparison case studies. A method to calculate the impact of reuse systems and to compare it to single‐use systems is presented in terms of equations based on the case studies. The equations are used to show the relevance of taking up specific parameters using different input values. Significance is shown for the following factors: Single‐use components in a reuse system Constant factors in a reuse system Pool size compared to system size in a reuse system Loss percentage With this method, several factors are taken up outside of LCA software in order to determine a break‐even point or to understand the trajectory of the system impact over rotations. Together with inventory reporting according to ISO 14040/14044 this can be the basis for transparent reuse system impact calculations and its fair comparison to single‐use system impact.