Shaghayegh Jahangir
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Shaghayegh Jahangir has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Aliuska Morales Helguera
Center of Chemical Bioactives, University of Las Villas, Santa Clara 54838, Cuba
1 shared publication - Anayancy Osorio-Madrazo
University of Bayreuth, Laboratory of Organ Printing. Bayreuth, Germany
1 shared publication - Arnaud Kamdem Tamo
Laboratory of Organ Printing, University of Bayreuth, 95447 Bayreuth, Germany
1 shared publication - Christian Gorzelanny
Department of Dermatology and Venereology, University Medical Center Hamburg-Eppendorf, Hamburg, Germany
1 shared publication - Ingo Doench
Laboratory of Organ Printing, University of Bayreuth, 95447 Bayreuth, Germany
1 shared publication - Martin Helmstädter
Department of Medicine IV, University Freiburg Medical Center, Faculty of Medicine, University of Freiburg, Hugstetter Strasse 55, 79106 Freiburg, Germany
1 shared publication
Latest Publications
- Open Access
- 29 October 2025
- Published by MDPI AG in Journal of Functional Biomaterials
- Vol. 16 (11) , 405
Biopolymer Fibers of High Strength and Enhanced Orientation by the Synergy of High/Low Molecular Weight Chitosans in Hybrid Biomaterials Processed by Gel Spinning
High-performance spun bionanocomposite fibers, composed of high-molecular-weight chitosan (HMW), low-molecular-weight chitosan “oligomers” (LMW), and cellulose nanofibers (CNFs), were successfully fabricated via gel spinning of viscous aqueous chitosan (CHI) based formulations into a NaOH coagulation bath. The X-ray diffraction (XRD) analysis revealed that the incorporation of cellulose nanofibers contributed to enhance crystallinity of chitosan in spun fibers. The spinning process, which comprised sequential acidic solubilization, basic neutralization, stretching, and drying steps, produced chitosan/CNF composite fibers with high crystallinity, further enhanced by the incorporation of low molecular weight chitosan. The cellulose nanofibers seem to promote CHI crystallization, by acting as nucleation sites for the nucleation and growth of chitosan crystals, with those latter of LMW further enhancing crystallization and orientation due to higher mobility of shorter polymer chains. Two-dimensional XRD patterns demonstrated the preferential alignment of both CNFs and chitosan crystals along the fiber axis. Increasing the proportion of short-chain chitosan led to a reduction of the viscosity of collodion, facilitating the spinning of solutions with higher polymer concentrations. The X-ray diffraction (XRD) analysis revealed that the addition of low-molecular-weight chitosan (LMW), with an intermediate molecular weight Mw of ~4.4 × 104 g/mol, produced the most significant improvements in the crystallinity index (CrI) and orientation. This structural enhancement corresponded to superior mechanical properties like Young’s modulus, yield stress σy, and stress-at-break σb of the processed composite fibers. By incorporating that intermediate molecular weight chitosan, a Young’s modulus as high as 20 GPa was achieved for the spun composite fibers, which was twice higher than the modulus of around 10 GPa obtained by adding the lowest molecular weight chitosan of Mw ~ 2.9 × 104 g/mol in the composite, and largely above the modulus of around 5 GPa obtained for fiber just spun with chitosan without incorporation of cellulose nanofibers.
- 29 October 2025
- Published by MDPI AG in Journal of Functional Biomaterials
- Vol. 16 (11) , 405
Open AccessBiopolymer Fibers of High Strength and Enhanced Orientation by the Synergy of High/Low Molecular Weight Chitosans in Hybrid Biomaterials Processed by Gel Spinning
High-performance spun bionanocomposite fibers, composed of high-molecular-weight chitosan (HMW), low-molecular-weight chitosan “oligomers” (LMW), and cellulose nanofibers (CNFs), were successfully fabricated via gel spinning of viscous aqueous chitosan (CHI) based formulations into a NaOH coagulation bath. The X-ray diffraction (XRD) analysis revealed that the incorporation of cellulose nanofibers contributed to enhance crystallinity of chitosan in spun fibers. The spinning process, which comprised sequential acidic solubilization, basic neutralization, stretching, and drying steps, produced chitosan/CNF composite fibers with high crystallinity, further enhanced by the incorporation of low molecular weight chitosan. The cellulose nanofibers seem to promote CHI crystallization, by acting as nucleation sites for the nucleation and growth of chitosan crystals, with those latter of LMW further enhancing crystallization and orientation due to higher mobility of shorter polymer chains. Two-dimensional XRD patterns demonstrated the preferential alignment of both CNFs and chitosan crystals along the fiber axis. Increasing the proportion of short-chain chitosan led to a reduction of the viscosity of collodion, facilitating the spinning of solutions with higher polymer concentrations. The X-ray diffraction (XRD) analysis revealed that the addition of low-molecular-weight chitosan (LMW), with an intermediate molecular weight Mw of ~4.4 × 104 g/mol, produced the most significant improvements in the crystallinity index (CrI) and orientation. This structural enhancement corresponded to superior mechanical properties like Young’s modulus, yield stress σy, and stress-at-break σb of the processed composite fibers. By incorporating that intermediate molecular weight chitosan, a Young’s modulus as high as 20 GPa was achieved for the spun composite fibers, which was twice higher than the modulus of around 10 GPa obtained by adding the lowest molecular weight chitosan of Mw ~ 2.9 × 104 g/mol in the composite, and largely above the modulus of around 5 GPa obtained for fiber just spun with chitosan without incorporation of cellulose nanofibers.